Effect of Post-deposition Annealing on the Physical Properties of DC Magnetron Sputtered Molybdenum Oxide Films
Molybdenum oxide films were deposited on glass and single crystal silicon substrates held at room temperature by sputtering of molybdenum target in an oxygen partial pressure of 2xl0{sup -4} mbar. The MoO{sub 3} films were annealed in oxygen atmosphere at various temperatures in the range 473-673 K. The effect of annealing temperature on the structure, chemical binding configuration, and optical properties of the MoO{sub 3} films was studied. The X-ray diffraction studies revealed that the as-deposited MoO{sub 3} films were amorphous. It crystallizes into a layered orthorhombic phase by the post-deposition annealing at a temperature of 673 K. The Fourier transform infrared spectrum of the MoO{sub 3} films annealed at 473 K exhibits the absorption bands at 560, 840 and 995 cm{sup -1} related to the active stretching modes of MoO{sub 6} octahedra. When the films annealed at 673 K the intensity of the absorption band observed at 560 cm{sup -1} diminished and the band of 995 cm{sup -1} split into two bands of 995 and 1010 cm{sup -1} which are related to the zig--zag rows of layered structure of MoO{sub 3}. The optical band gap of the as-deposited and annealed films was 3.07 and 3.20 eV respectively. The refractive index increased with increase of annealing temperature.