Bandgap widening in thermochromic Mg-doped VO{sub 2} thin films: Quantitative data based on optical absorption
Thermochromic Mg-doped VO{sub 2} films were deposited by reactive direct current magnetron sputtering onto heated glass and carbon substrates. Elemental compositions were inferred from Rutherford backscattering. Optical bandgaps were obtained from spectral transmittance and reflectance measurements—from both the film side and the back side of the samples—and ensuing determination of absorption coefficients. The bandgap of Mg-doped films was found to increase by 3.9 ± 0.5 eV per unit of atom ratio Mg/(Mg + V) for 0 < Mg/(Mg + V) < 0.21. The presence of ∼0.45 at. % Si enhanced the bandgap even more.