Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “INTERMETALLIC COMPOUNDS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 793 records · Page 44

Magnetic properties of Fe{sub 2}P-type Tb{sub 6}FeTe{sub 2}, Tb{sub 6}CoTe{sub 2}, Tb{sub 6}NiTe{sub 2} and Er{sub 6}FeTe{sub 2} compounds

The magnetic ordering of the Fe{sub 2}P-type Tb{sub 6}FeTe{sub 2}, Tb{sub 6}CoTe{sub 2} Tb{sub 6}NiTe{sub 2} and Er{sub 6}FeTe{sub 2} phases (space group P6-bar 2m) has been investigated through magnetization measurement and neutron powder diffraction. Tb{sub 6}FeTe{sub 2}, Tb{sub 6}CoTe{sub 2} and Tb{sub 6}NiTe{sub 2} demonstrate high-temperature ferromagnetic and low-temperature spin reorientation transitions, whereas Er{sub 6}FeTe{sub 2} shows antiferromagnetic transition, only. The Tb{sub 6}FeTe{sub 2} and Tb{sub 6}NiTe{sub 2} phases show same high-temperature collinear ferromagnetic structure, whereas Tb{sub 6}FeTe{sub 2} is the commensurate non-collinear ferromagnet and Tb{sub 6}NiTe{sub 2} is the canted ferromagnetic cone with K{sub 1}=[0, 0, {+-}3/10] and K{sub 2}=[{+-}2/9, {+-}2/9, 0] wave vectors at 2 K. The magnetic structure of Er{sub 6}FeTe{sub 2} is a flat spiral with K{sub 1}=[0, 0, {+-}1/10] at 2 K. The magnetic entropy change for Tb{sub 6}NiTe{sub 2} is {Delta}S{sub m}=-4.86 J/kg K at 229 K for the field change {Delta}{mu}{sub 0}H=0-5 T. In addition, novel Fe{sub 2}P-type Gd{sub 6}FeTe{sub 2}, Zr{sub 6}FeTe{sub 2}, Hf{sub 6}FeTe{sub 2}, Dy{sub 6}NiTe{sub 2}, Zr{sub 6}NiTe{sub 2} and Hf{sub 6}NiTe{sub 2} phases have been obtained. -- Graphical abstract: The novel Fe{sub 2}P-type Tb{sub 6{l_brace}}Fe, Co, Te{r_brace}Te{sub 2} and Er{sub 6}FeTe{sub 2} phases (space group P6-bar 2m) show the complex magnetic ordering below 18-228 K. The magnetocaloric effect for Tb{sub 6}NiTe{sub 2} in terms of the isothermal entropy change, -{Delta}S{sub m}, has the maximum value of 4.86 J/kg K at 229 K for the 0-5 T field change.

36 MATERIALS SCIENCE↗

On phase equilibria and crystal structures in the systems Ce-Pd-B and Yb-Pd-B. Physical properties of R{sub 2}Pd{sub 13.6}B{sub 5} (R=Yb, Lu)

Phase equilibria and crystal structures of ternary compounds were determined in the systems Ce-Pd-B and Yb-Pd-B at 850 deg. C in the concentration ranges up to 45 and 33 at% of Ce and Yb, respectively, employing X-ray single crystal and powder diffraction. Phase relations in the Ce-Pd-B system at 850 deg. C are governed by formation of extended homogeneity fields, tau{sub 2}-CePd{sub 8}B{sub 2-x} (0.10<x<0.48); tau{sub 3}-Ce{sub 3}Pd{sub 25-x}B{sub 8-y} (1.06<x<1.87; 2.20<y<0.05), and CePd{sub 3}B{sub x} (0<x<0.65) the latter arising from binary CePd{sub 3}. Crystallographic parameters for the new structure type tau{sub 2}-CePd{sub 8}B{sub 2-x} (space group C2/c, a=1.78104(4) nm, b=1.03723(3) nm, c=1.16314(3), beta=118.515(1){sup o} for x=0.46) were established from X-ray single crystal diffraction. The crystal structures of tau{sub 2}-CePd{sub 8}B{sub 2-x} and tau{sub 3}-Ce{sub 3}Pd{sub 25-x}B{sub 3-y} are connected in a crystallographic group-subgroup relationship. Due to the lack of suitable single crystals, the novel structure of tau{sub 1}-Ce{sub 6}Pd{sub 47-x}B{sub 6} (x=0.2, C2/m space group, a=1.03594(2) nm, b=1.80782(3) nm, c=1.01997(2) nm, beta=108.321(1){sup o}) was determined from Rietveld refinement of X-ray powder diffraction data applying the structural model obtained from single crystals of homologous La{sub 6}Pd{sub 47-x}B{sub 6} (x=0.19) (X-ray single crystal diffraction, new structure type, space group C2/m, a=1.03988(2) nm, b=1.81941(5) nm, c=1.02418(2) nm, beta=108.168(1){sup o}). The Yb-Pd-B system is characterized by one ternary compound, tau{sub 1}-Yb{sub 2}Pd{sub 14}B{sub 5}, forming equilibria with extended solution YbPd{sub 3}B{sub x}, YbB{sub 6}, Pd{sub 5}B{sub 2} and Pd{sub 3}B. The crystal structures of both Yb{sub 2}Pd{sub 14}B{sub 5} and isotypic Lu{sub 2}Pd{sub 14}B{sub 5} were determined from X-ray Rietveld refinements and found to be closely related to the Y{sub 2}Pd{sub 14}B{sub 5}-type (I4{sub 1}/amd). The crystal structure of binary Yb{sub 5}Pd{sub 2-x} (Mn{sub 5}C{sub 2}-type) was confirmed from X-ray single crystal data and a slight defect on the Pd site (x=0.06) was established. The three structures tau{sub 1}-Ce{sub 6}Pd{sub 47-x}B{sub 6}, tau{sub 2}-CePd{sub 8}B{sub 2-x} and tau{sub 3}-Ce{sub 3}Pd{sub 25-x}B{sub 8-y} are related and can be considered as the packings of fragments observed in Nd{sub 2}Fe{sub 14}B structure with different stacking of common structural blocks. Physical properties for Yb{sub 2}Pd{sub 13.6}B{sub 5} (temperature dependent specific heat, electrical resistivity and magnetization) yielded a predominantly Yb-4f{sup 13} electronic configuration, presumably related with a magnetic instability below 2 K. Kondo interaction and crystalline electric field effects control the paramagnetic temperature domain. - Graphical Abstract: Crystal structure of CePd{sub 8}B{sub 2-x}.

36 MATERIALS SCIENCE↗

Evolution of Physical Properties of RE 3 Ni 5 Al 19 Family (RE = Y, Nd, Sm, Gd, Tb, Dy, Ho, and Er)

In this study, single crystals of RE 3 Ni 5 Al 19 series (RE = Y, Nd, Sm, Gd, Tb, Dy, Ho, and Er) are grown using the Al self-flux method. The crystal structure is examined by both single crystal and powder X-ray diffraction. Physical properties are studied for the first time for RE 3 Ni 5 Al 19 (RE = Y, Nd, Gd, Tb, Dy, Ho, and Er) by means of magnetic susceptibility, electrical resistivity, and heat capacity measurements. Complex magnetic behaviors, with up to three transitions present for RE = Sm, Gd, Tb, and Dy, are revealed. Y 3 Ni 5 Al 19 is found to be a nonmagnetic nonsuperconducting metal (above T = 1.8 K) with weak electron–phonon coupling strength.

36 MATERIALS SCIENCE↗

Sm 2 Ru 3 Sn 5 : A Noncentrosymmetric Cubic Member of the Ln 2 M 3 X 5 Family

An optimized synthetic method is presented for Sm 2 Ru 3 Sn 5 and investigate its physical properties and electronic structure. Sm 2 Ru 3 Sn 5 is prepared by arc-melting stoichiometric ratios of the elements and is confirmed by single crystal and powder X-ray diffraction. An antiferromagnetic transition is observed at T N = 3.8 K. A modified Curie-Weiss fit to the data in the range 50–150 K yields a Curie-Weiss temperature: θ CW = −36.6 K and an effective magnetic moment: μ eff = 0.83 μ B , in agreement with a Sm 3+ oxidation state. Field-dependent magnetization up to H = 7 T at 2 K shows a maximum response of 0.06 μ B , which is significantly lower than the expected Sm 3+ saturation moment (0.71 μ B ). Resistivity measurements indicate metallic behavior, and analysis of the magnetic entropy from the heat capacity reveals a doublet ground state due to crystal electric field splitting. The electronic structure and density of states are calculated with density function theory and further supported by the local density approximation with dynamical mean-field theory. Finally, the experimental and computational results highlight localized Sm 3+ moments and suggest a possible interplay between Ruddelman–Kitel–Kasuya–Yosida and Kondo interactions, positioning Sm 2 Ru 3 Sn 5 as a promising material for studying topology and complex physical phenomena.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Study Ab Initio of the Effect of A-Site Substitution on the Fe1.12Te System

In the present work, our aim is to verify the structural, electronic and magnetic properties of both systems Fe1.12Te and (R = Fe, X = Te and T = Ni, Co) in the P4/nmm structure. For this task, we use the density functional theory (DFT) as a theoretical tool integrated into wien2k code (Blaha 2001). The solid Fe1 − x Mx Te (M = Ni, Co) have been synthesised by Kazakov et al. (Chem. Met. Alloys 3, 155–160 2010). They have observed a systematic shift of the lattice parameters for both systems for M = Ni and Co till x = 0.1, then a secondary phase with the NiAs-type structure appeared when x passes 0.15. Fe1 − x Nix Te retains its structure in a concentration between x = 0.1 and 0.15, and Fe1 − x CoxTe retains its structure when x is between 0.05 and 0.1 (Blaha 2001).

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Switching of Coercivity Process in MnBi Alloys

MnBi-based alloys represent an interesting choice for developing rare earth-free permanent magnets due to the high magnetocrystalline anisotropy of their characteristic low-temperature intermetallic phase (LTIP) with hexagonal structure. In this work, we discuss the switching of coercivity mechanism in MnBi alloys by modulation of their phase distribution and microstructure. As-cast MnBi alloys obtained by suction-casting technique exhibited LTIP interspersed within Bi- and Mn-rich areas. A noticeable coercivity field of 282 kA/m was observed. The coercivity mechanism for this alloy was explained in terms of the nucleation of reverse domains after saturation, by means of the Kronmüller equation, which incorporates the detrimental effect of microstructure defects through fitting parameters associated to reduced intrinsic magnetic properties at grain size boundaries, interfaces, and local demagnetizing fields. Subsequent annealing at 583 K for 24 h produced a marked reduction of coercivity (down to 16 kA/m), reflecting a switching of coercivity process from nucleation to pinning of domain walls. The key microstructural feature determining this variation is the formation/suppression of Bi-rich areas, which promotes the nucleation and growth of the initial MnBi intermetallic phase.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Improvement in the Crystallographic Phase Content and Superconducting Properties of Mechanically Alloyed MgB{sub 2}

In this paper, the results of the superconductivity evaluation of MgB{sub 2} intermetallic-based superconducting materials prepared through mechanical alloying are reported. The formation of the MgB{sub 2} intermetallic phase took place through an intermediate phase reaction at the solid-state reaction temperature, which tends to favor single-phase materials. The annealing of mechanically milled Mg and B powders resulted in the highest mass fraction of MgB{sub 2} observed in this study, reaching more than 90% after annealing at 900 °C for 1 h. At that point, there were still second phases present consisting of Mg, MgO, and Fe{sub 2}B. Improved superconducting properties were obtained in samples sintered at temperatures of 850 °C and 900 °C that had a low resistivity, low critical temperature gap values, and a high residual resistivity ratio (RRR).

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structural and Phase Transformations in Superlocalization Band in Ni{sub 3}Ge Single Crystal

The paper studies the high-temperature plastic deformation in Ni{sub 3}Ge alloy single crystals localizing in a band a few tens of microns wide that reaches the shear strain of thousands of percent. The electron backscatter diffraction and synchrotron radiation techniques allow investigating the structure of the single crystal in the band of super-localized plastic deformation. It is shown that super-localization of plastic deformation occurs due to the formation of polycrystalline multi-level substructure in the initial single crystal. The grain size and grain misorientation bimodal distributions are determined in the polycrystalline substructure. Also, regions of amorphous state are observed in the super-localization band at high homologous temperature Т > 0.5T{sub m}. A partial destruction of the far atomic order is detected.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of Partial Substitution of Mn for Ni on Mechanical Properties of Friction Stir Processed Hypoeutectic Al-Ni Alloys

In this study, the mechanical properties of as-cast and FSPed Al-2Ni-xMn alloys (x = 1, 2, and 4 wt pct) were investigated and compared with those of the as-cast and FSPed Al-4Ni alloy. According to the results, the substitution of 2 wt pct Mn for 2 wt pct Ni leads to the formation of fine Mn-rich intermetallics in the microstructure increasing the tensile strength, microhardness, fracture toughness, and specific strength of alloy by 22, 56, 45, and 35 pct, respectively. At higher Mn concentrations, the formation of large Mn-rich platelets in the microstructure reduces the tensile properties. Friction stir processing at 12 mm/min and 1600 rpm significantly enhances both the strength and ductility of the alloy. The tensile strength, yield strength, fracture strain, fracture toughness, microhardness, and specific strength of FSPed Al-2Ni-4Mn alloy improved by 97, 83, 30, 380, 152, and 110 pct, respectively, as compared to those of the as-cast Al-4Ni alloy. This can be attributed to dispersion strengthening of Ni- and Mn-rich dispersoids, formation of ultrafine grains, and elimination of casting defects. The fractography results also show that the brittle fracture mode of the as-cast Mn-rich alloys turns to a more ductile mode, comprising fine and equiaxed dimples in FSPed samples.

36 MATERIALS SCIENCE↗

Thermo-chemical Fluid Flow Simulation in Hot-Dip Galvanizing: The Evaluation of Dross Build-Up Formation

This paper presents a new computational framework to investigate the driving force for the formation of intermetallic dross particles in the zinc bath and dross build-up on the bath hardware. This is a major problem in continuous hot-dip galvanizing lines. The Computational Fluid Dynamics (CFD) model calculates the turbulent thermo-chemical flow conditions within the liquid melt. A detailed modeling of the steel strip–liquid interface enhances this approach, by means of a conjugated heat transfer calculation and a spatially resolved, temperature- and concentration-dependent iron dissolution and aluminum uptake. The heart of the computational framework is a thermodynamic model, which assesses the driving force for the formation or dissolution of dross particles in the bath and dross build-up on stationary and rotating equipment. The simulation results are validated with temperature and species depth profile measurements. The applicability of the CFD model is shown by investigating the locally resolved aluminum uptake and iron dissolution at the steel-strip surface, and the multi-physics conditions in the region near the roll. The novel approach of evaluating the thermodynamic driving force enables the assessment of the formation of dross build-up at the roll surface.

36 MATERIALS SCIENCE↗

Evolution of Fe-Rich Intermetallics in Al-Si-Cu 319 Cast Alloy with Various Fe, Mo, and Mn Contents

In the present work, the precipitation and preferential selection of Fe-rich intermetallics in Al-Si-Cu 319 cast alloys with two Fe contents (0.3 and 0.7 wt pct) and various Mo contents (0 to 0.4 wt pct) were investigated. The results showed that two types of platelet β-Fe (defined as eutectic β-Fe and pre-eutectic β-Fe) and α-Fe can precipitate depending on the alloy compositions, such as the Fe and Mo contents. Generally, the addition of Mo promotes the formation of α-Fe instead of β-Fe. However, its effect on the phase competition between β-Fe and α-Fe is greatly related to the Fe content. In alloys with low Fe content (0.3 pct), an addition of 0.37 pct Mo can promote the complete precipitation of α-Fe and suppress the formation of eutectic β-Fe. However, in alloys with high Fe content (0.7 pct), only the pre-eutectic β-Fe amount decreases with increasing Mo addition, leaving the eutectic β-Fe almost unchanged, while both pre-eutectic β-Fe and eutectic β-Fe can be fully suppressed with a combined addition of Mn (0.24 pct) and Mo (0.4 pct). Compared with Mn, Mo exhibits a stronger effect on the promotion of α-Fe. The combined addition of Mn and Mo can achieve better modifications of both pre-eutectic and eutectic β-Fe in 319 alloys with high Fe content.

36 MATERIALS SCIENCE↗

Investigation of the Effect of Foaming Agent on the Fabrication of NiTi Foams Using the Self-Propagating, High-Temperature Synthesis Process

Fabrication of NiTi intermetallic foams using the self-propagating, high-temperature synthesis (SHS) process was investigated. Weighed amounts of powders taken from an equimolar mixture of Ni and Ti powders along with 0.5, 1, and 1.5 wt pct of different foaming agents were cold pressed to form cylindrical compacts 10 mm in diameter, 20 mm in height, and 7 to 8 g in weight. A novel, induction-assisted ignition method was used for indirect heating and igniting the compressed mixtures at one end. As a result of intensive exothermic reaction between Ni and Ti and decomposition of foaming agents and liberation of gases, highly porous products were obtained. Characterization of the products was carried out using X-ray diffraction (XRD) and a scanning electron microscope equipped with an energy-dispersive spectroscope (SEM-EDS). The main phase in the products was detected to be B2(NiTi) with minor amounts of NiTi{sub 2} as the secondary phase. Other undesirable phases, such as Ni{sub 4}Ti{sub 3} and Ni{sub 3}Ti, were not detected. The effect of type and percentage of foaming agent on the formation and distribution of pores within the products was studied. Final products with porosities up to ~ 80 vol pct were obtained by adding foaming agent. Under the conditions of this study, CaH{sub 2} proved to be the most effective foaming agent considering its ability to generate a uniform distribution of pores, while TiH{sub 2} was not considered favorable due to its decomposition at relatively low temperatures. In general, the addition of foaming agents in amounts higher than 1wt pct is not recommended; due to the endothermic nature of thermal decomposition reactions of foaming agents, excessive use of these agents can result in suppression of the exothermic reaction.

36 MATERIALS SCIENCE↗

High Damping of Lightweight TiNi-Ti{sub 2}Ni Shape Memory Composites for Wide Temperature Range Usage

A bimodal porous TiNi-Ti{sub 2}Ni shape memory alloy composite (SMAC) with 59% porosity was fabricated by sintering Ti-46at.%Ni elemental powders with pore-forming agent. The porous TiNi-Ti{sub 2}Ni SMAC contains two irregular pores of about 400 and 120 μm. We investigated the microstructure and pore morphology correlated with the mechanical properties and damping capacities of the SMAC. Ti{sub 2}Ni intermetallic phases with size of 1-3 μm were homogeneously distributed in the TiNi matrix. The porous TiNi-Ti{sub 2}Ni SMAC exhibits exceptionally high inverse mechanical quality factor (Q{sup −1}) of ~0.25 at < 40 °C, which is among the highest value reported for porous/dense shape memory alloys or composites to best of our knowledge, and it shows very high compressive fracture strain of about 25%. Moreover, the fabricated porous SMAC at relatively low strain amplitude can exhibit considerable high Q{sup −1} of 0.06 ~ 0.11 for a wide range of temperature between − 90 and 200 °C, which is attributed to the stress concentration distribution provided by the bimodal structure of pores and the massive interfaces between pore/matrix and TiNi/Ti{sub 2}Ni. These porous SMACs can be an ideal candidate for using as a lightweight damping material in the energy-saving applications.

36 MATERIALS SCIENCE↗

Ca Addition Effects on the Microstructure, Tensile and Corrosion Properties of Mg Matrix Alloy Containing 8 wt.% Mg{sub 2}Si

The microstructure, tensile properties and corrosion behavior of the Mg-8 wt.% Mg{sub 2}Si-x%Ca alloy have been studied by the use of optical microscopy, scanning electron microscopy equipped with energy-dispersive spectroscopy, x-ray diffraction, standard tensile testing, polarization test and electrochemical impedance spectroscopy (EIS) measurements. Microstructural studies indicated that Ca modifies both primary and eutectic Mg{sub 2}Si phase. It was found that the average size of primary Mg{sub 2}Si particles is about 60 μm, which is dropped by about 82% in the alloy containing 0.05 wt.% Ca. By the addition of different Ca contents, Ca-rich intermetallics (i.e., CaSi{sub 2} and CaMgSi) were formed. The modification mechanism of adding Ca during solidification was found to be due to the strong effect of CaMgSi phase as a heterogonous nucleation site, apart from CaSi{sub 2} which was reported before, for Mg{sub 2}Si intermetallics. Tensile testing results ascertained that Ca addition enhances both ultimate tensile strength (UTS) and elongation values. The optimum amount of Ca was found to be 0.1 wt.%, which improved UTS and elongation values from about 130 MPa and 2% to 165 MPa and 5.5%, whereas more Ca addition (i.e., 3 wt.%) reduced the tensile properties of the alloy to about 105 MPa and 1.8%, which can be due to the formation of CaMgSi intermetallics with deteriorating needle-like morphology. Polarization and EIS tests also showed that the Mg-3%Si-0.5%Ca alloy pronounces as the best anti-corrosion alloy. Nevertheless, further added Ca (up to 3 wt.%) deteriorated the corrosion resistance due to predominance of worse galvanic coupling effect stemmed from the presence of stronger CaMgSi cathode in comparison with Mg{sub 2}Si. With higher Ca additions, an adverse effect was seen on corrosion resistance of the Mg-3%Si alloy, as a result of forming a weak film on the alloy specimen surface.

36 MATERIALS SCIENCE↗

Atomic Layer-Deposited TiO{sub 2} Coatings on NiTi Surface

NiTi shape-memory alloys may release poisonous Ni ions at the alloys’ surface. In an attempt to prepare a well-performing surface layer on an NiTi sample, the thermally grown TiO{sub 2} layer, which formed during the heat treatment of NiTi, was removed and replaced with a new TiO{sub 2} layer prepared using the atomic layer deposition (ALD) method. Using x-ray photoelectron spectroscopy, it was found that the ALD layer prepared at as low a temperature as 100 °C contained Ti in oxidation states + 4 and + 3. As for static corrosion properties of the ALD-coated NiTi samples, they further improved compared to those covered by thermally grown oxide. The corrosion rate of samples with thermally grown oxide was 1.05 × 10{sup −5} mm/year, whereas the corrosion rate of the ALD-coated samples turned out to be about five times lower. However, cracking of the ALD coating occurred at about 1.5% strain during the superelastic mechanical loading in tension taking place via the propagation of a localized martensite band.

36 MATERIALS SCIENCE↗

Formation of Al/(Al{sub 13}Fe{sub 4} + Al{sub 2}O{sub 3}) Nano-composites via Mechanical Alloying and Friction Stir Processing

Combination of mechanical alloying and friction stir processing was used for the fabrication of Al/(Al{sub 13}Fe{sub 4} + Al{sub 2}O{sub 3}) nano-composites. Pre-milled hematite + Al powder mixture was introduced into the stir zone generated on 1050 aluminum alloy sheet by friction stir processing. Uniform and active milled powder mixture reacted with plasticized aluminum to produced Al{sub 13}Fe{sub 4} + Al{sub 2}O{sub 3} particles. Al{sub 13}Fe{sub 4} intermetallic showed elliptical shape with a typical size of ~ 100 nm, while nano-sized Al{sub 2}O{sub 3} exhibited irregular floc-shaped particles that formed clusters with the remnant of iron oxide particles in the fine recrystallized aluminum matrix. As the milling time (1-3 h) of the introduced powder mixture increased, the volume fraction of Al{sub 13}Fe{sub 4} + Al{sub 2}O{sub 3} particles increased in the fabricated composite. The hardness and ultimate tensile strength of the fabricated nano-composites varied from 54.5 to 75 HV and 139 to 159 MPa, respectively; these are much higher than those of the friction stir processed base alloy (33 HV and 97 UTS). The highest hardness and strength were achieved for the nano-composite fabricated using the 3-h milled powder mixture; hard nano-sized reaction products and fine recrystallized grains of Al matrix had major and minor roles on enhancing these properties, respectively.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Friction Stir Process Derived Al-TiO{sub 2} Nanocomposite

Aluminum-based composites have many advantages over their conventional counterparts. A major problem in such composites is the clustering of particles in the matrix. Friction stir processing (FSP) can homogenize particle distribution in aluminum-based composites. In this study, unannealed TiO{sub 2} particles were used to prepare Al-TiO{sub 2} nanocomposite using FSP. The TiO{sub 2} particles, about 1 µm, were dispersed into an aluminum matrix by 6 passes of FSP. The TiO{sub 2} particles were fractured by multiple FSP passes, leading to a nano-size particle distribution in the matrix. Nanoscale dispersion was confirmed by scanning electron microscopy and transmission electron microscopy. The fractured TiO{sub 2} particles reacted with the aluminum matrix to form Al{sub 3}Ti intermetallic and Al{sub 2}O{sub 3} ceramic. The progression of the Al-TiO{sub 2} reaction from the fourth to the sixth pass of FSP was revealed by x-ray diffraction. Due to the nanoscale dispersion, the yield and ultimate tensile strength of the composite increased to 97 and 145 MPa, respectively. Ductility of the composite decreased marginally compared to the as-received aluminum. As the dispersed particles pin dislocations, the strain-hardening rate of the composite was considerably increased and the same was seen in the Kocks-Mecking plot. The TiO{sub 2} particles are mechanically activated due to their fracture during FSP, hence leading to reaction with the matrix. The particle refinement and dispersion lead to a homogeneous matrix with higher strength.

36 MATERIALS SCIENCE↗