Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Densification”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 793 records · Page 44

Development of improved coating for advanced carbon-carbon components

Reaction sintered silicon nitride (RSSN) was studied as a substitute coating material on the carbon-carbon material (RCC) presently used as a heat shield on the space shuttle, and on advanced carbon-carbon (ACC), a later development. On RCC, RSSN showed potential in a 538 C (1000 F) screening test in which silicon carbide coated material exhibits its highest oxidation rate; RSSN afforded less protection to ACC because of a larger thermal expansion mismatch. Organosilicon densification and metallic silicon sealing methods were studied as means of further increasing the oxidation resistance of the coating, and some improvement was noted when these methods were employed.

Yamaki, Y. R.↗

Hot-pressed silicon nitride with various lanthanide oxides as sintering additives

The effects of addition of various lanthanide oxides and their mixture with Y2O3 on the sintering of Si3N4 were investigated. The addition of simple and mixed lanthanide oxides promoted the densification of Si3N4 in hot-pressing at 1800 C under 300-400kg/ centimeters squared for 60 min. The crystallization of yttrium and lanthanide-silicon oxynitrides which was observed inn the sintered body containing yttrium-lanthanide mixed oxides as additives led to the formation of a highly refractory Si3N4 ceramic having a bending strength of 82 and 84 kg/millimeters squared at room temperature and 1300 C respectively. In a Y2O3+La2O3 system, a higher molar ratio of La2O3 to Y2O3 gave a higher hardness and strength at high temperatures. It was found that 90 min was an optimum sintering time for the highest strength.

Ueno, K.↗

Physical aging and its influence on the reliability of network epoxies and epoxy-matrix composites

The matrix-dominated physical and mechanical properties of a carbon fiber reinforced epoxy composite and a neat epoxy resin were found to be affected by sub-Tg annealing in nitrogen and dark atmosphere. Postcured specimens of Thornel 300 carbon-fiber/Fiberite 934 epoxy as well as Fiberite 934 epoxy resin were quenched from above Tg and given annealing at 140 C, 110 C, or 80 C, for time up to one-hundred thousand minutes. No weight loss was observed during annealing at these temperatures. Significant variations were found in density, modulus, hardness, damping, moisture absorption ability, thermal expansivity. Moisture-epoxy interactious were also studied. The kinetics of aging as well as the molecular aggregation during this densification process were monitored by differential scanning calorimetry, dynamic mechanical analysis, density gradient column, microhardness tester, Instron, and solid-state nuclear magnetic resonance spectroscopy.

Heinemann, K.↗

Analysis of grain boundary phase devitrification of Y2O3- and Al2O3-doped Si3N4

The present study has the objective to show that a Fourier Transform IR (FTIR) spectrometer in a single-beam reflection mode can be used for direct comparison of fractured vs nonfractured Si3N4 surfaces. This can be done because the FTIR method permits a digital summation of nearly 1000 scans of the fracture surface. Commercial-grade Si3N4, Y2O3, and Al2O3 were used in the study. The samples were heat treated in a vacuum induction heating furnace at either 1000 C for 10 h or 1200 C for 10 h each. Use of Fourier transform IR reflection spectroscopic analysis and X-ray diffraction shows that 10 h at 1200 C is sufficient to devitrify the amorphous grain boundary phase of Si3N4 containing 15 percent Y2O3 + 2 percent Al2O3 densification aids.

Hench, L. L.↗

Shock experiments on maskelynite-bearing anorthosite

A series of shock recovery experiments over 9.9-60.4 GPa have been carried out on naturally shocked anorthosite from the Mistastin impact structure in Labrador consisting primarily of diaplectic plagioclase glass or maskelynite, An(50), and pyroxene. Petrographic observations of the experimental products indicate that the component minerals and diaplectic glasses generally retained their initial character throughout, the only exception being the increase in fracturing which occurred in the 9.9 GPa shot. Reshocking at pressures higher than the initial shock tends to lower the refractive index of maskelynite. The increase in refractive index of maskelynite reshocked to pressures lower than the initial pressure is interpreted as due to shock densification of the diaplectic glass above the Hugoniot elastic limit and below the mixed phase regime. The data suggest that the low-high-low density transition of maskelynite occurs about 8 GPa below that of the crystal of corresponding composition.

Lambert, P.↗

Structure of ices on satellites

The pressure densification of ices, in combination with density changes induced by pore migration in a thermal gradient and the phase transitions of water due to meteoritic bombardment (into either high pressure polymorphs or an amorphous phase) create a complex situation, which is not easily evaluated in either satellites or cometary nuclei. Accordingly, the present findings concerning solar system satellites and comets cannot be rendered quantitative. In general, due to insolation, icy satellites may have slightly warmer surfaces than their interiors. If there are CO2 ice inclusions in satellite water ices, they would have diffused as vapor along pores toward the cold interiors or, if near the surface, would have evaporated. The presence of pores and amorphous ice in cometary nuclei has an important effect on their flare-up and the size of the comas and tails.

Smoluchowski, R.↗

Evolution of density in solar system ices

Pores present in ices in the solar system do not remain unchanged. In isothermal conditions they shrink, while in a thermal gradient they migrate towards the higher temperature and escape so that the ice densifies. This motion has been investigated for pure H2O- and CO2-ices in a very simple one-dimensional model assuming uniform thermal conductivity and temperature gradient. The results indicate that the densification of H2O-ice is so slow that it could be significant only for icy satellites having an internal heat source. On the other hand, CO2-ice densifies orders of magnitude faster and the effect should be important for the CO2 component of cometary nuclei. No effect is expected for icy planetary rings.

Smoluchowski, R.↗

Reactive sintering of SiC

Investigation of the sintering processes involved in the sintering of SiC revealed a connection between the types and quantities of sintering additives or catalysts and densification, initial shrinkage, and weight loss of the sintered SiC material. By sintering processes, is meant the methods of mass transport, namely solid vapor transport and grain boundary diffusion.

Kim, Y. W.↗

Blade tip geometry - A factor in abrading sintered seal material

Experimental results are presented for the case of titanium blade tip specimens of various geometrical configurations rubbing at 100 m/s against specimens of nickel-chromium sintered powder metal seal material, the latter being fed toward the rotating blades at an incursion rate of 0.0254 mm/s. Blade tips in the form of orthogonal cutting tools with about 85 deg negative rake angles exhibited desirable abrading capabilities, as measured by the tear-free appearance of the grooves they generated in the seal material, little wear of blade tips, low forces of interaction and low seal densification. Similar results have been obtained for blade specimens with tips of small radius of curvature, as well as for square-ended and slanted blade tips that are plasma-sprayed with abrasive particles. The relationship between the size of these particles and their abrading effectiveness is considered.

Wolak, J.↗

Frictional and morphological properties of Au-MoS2 films sputtered from a compact target

AuMoS2 films 0.02 to 1.2 microns thick were sputtered from target compacted from 5 wt percent Au + 95 wt percent MoS2, to investigate the frictional and morphological film growth characteristics. The gold dispersion effects in MoS2 films are of interest to increase the densification and strengthening of the film structure. Three microstructural growth stages were identified on the nano-micro-macrostructural level. During sliding both sputtered Au-MoS2 and MoS2 films have a tendency to break within the columner region. The remaining or effective film, about 0.2 microns thick, performs the lubrication. The Au-MoS2 films displayed a lower friction coefficient with a high degree of frictional stability and less wear debris generation as compared to pure MoS2 films. The more favorable frictional characteristics of the Au-MoS2 films are attributed to the effective film thickness and the high density packed columner zone which has a reduced effect on the fragmentation of the tapered crystallites during fracture.

Spalvins, T.↗

Evaluation of alpha-SiC sintering using statistical methods

The effect of time and temperature on the density and strength of alpha-SiC was studied and mathematically modeled using a central composite experimental design. A sintering temperature of 2150 C for 1.7 h maximized the flexural strength and densification values. However, temperatures above 2200 C promoted abnormal grain growth, with resulting appreciable decreases in strength. Flexural strength increased exponentially with increasing density for specimens with densities less than or equal to 92 percent of theoretical.

Hurst, J. B.↗

Processing of laser formed SiC powder

Superior SiC characteristics can be achieved through the use of ideal constituent powders and careful post-synthesis processing steps. High purity SiC powders of approx. 1000 A uniform diameter, nonagglomerated and spherical were produced. This required major revision of the particle formation and growth model from one based on classical nucleation and growth to one based on collision and coalescence of Si particles followed by their carburization. Dispersions based on pure organic solvents as well as steric stabilization were investigated. Although stable dispersions were formed by both, subsequent part fabrication emphasized the pure solvents since fewer problems with drying and residuals of the high purity particles were anticipated. Test parts were made by the colloidal pressing technique; both liquid filtration and consolidation (rearrangement) stages were modeled. Green densities corresponding to a random close packed structure (approx. 63%) were achieved; this highly perfect structure has a high, uniform coordination number (greater than 11) approaching the quality of an ordered structure without introducing domain boundary effects. After drying, parts were densified at temperatures ranging from 1800 to 2100 C. Optimum densification temperatures will probably be in the 1900 to 2000 C range based on these preliminary results which showed that 2050 C samples had experienced substantial grain growth. Although overfired, the 2050 C samples exhibited excellent mechanical properties. Biaxial tensile strengths up to 714 MPa and Vickers hardness values of 2430 kg/sq mm 2 were both more typical of hot pressed than sintered SiC. Both result from the absence of large defects and the confinement of residual porosity (less than 2.5%) to small diameter, uniformly distributed pores.

Haggerty, J. S.↗

Brightness curve and porosity of cometary nuclei

The brightness curve of a comet is analyzed in terms of porosity and nature of volatiles in its nucleus. Mobility of pores, densification, phase changes, differential thermal expansion and heat flow into and out of the nucleus are discussed leading to a method for estimating the effective heat conductivity and porosity of the nucleus. The method is applied to comets P/Giacobini-Zinner, P/Halley, P/Kopff, P/Encke, P/Tempel 2 and P/d'Arrest.

Smoluchowski, R.↗

Sintering, microstructural, radiographic, and strength characterization of a high-purity Si3N4-based composition

A commercially available high purity alpha-Si3N4 powder (UBE SN-E10) was characterized, milled with additives, and sintered in a high-pressure nitrogen atmosphere at temperatures ranging from 1750 to 2140 C. The composition selected for this study has been previously examined using a different alpha-Si3N4 powder. Densification behavior, microstructure characteristics, X-radiographic appearance, room- and high-temperatures flexural strength, and fracture-initiating flaw sites were determined. The high-temperature flexural strengths significantly exceeded those observed in the earlier studies using an identical composition (different alpha-Si3N4 powder) and similar processing techniques.

Kiser, J. D.↗

Effect of composition and grain size on slow plastic flow properties of NiAl between 1200 and 1400 K

A series of about 15-micron diameter polycrystalline B2 crystal structure NiAl alloys ranging in composition from 43.9 to 52.7 Al (at. pct) have been compression tested at constant velocities in air between 1200 and 1400 K. All materials were fabricated via powder metallurgy techniques with hot extrusion as the densification process. Seven intermediate compositions were produced by blending various amounts of two master heats of prealloyed powder; in addition, a tenth alloy of identical composition, 48.25 Al, as one of the blended materials, was produced from a third master heat. Comparison of the flow stress-strain rate behavior for the two 48.25 Al alloys revealed that their properties were identical. The creep strength of materials for Al/Ni not above 1.03 was essentially equal, and deformation could be described by a single stress exponent and activation energy. Creep at low temperatures and faster strain rates is independent of grain sizes and appears to be controlled by a subgrain mechanism. However, at higher temperatures and slower strain rates, diffusional creep seems to contribute to the overall deformation rate.

Whittenberger, J. Daniel↗

Effect of thermal history on mechanical properties of polyetheretherketone below the glass transition temperature

The effect of thermal history on the tensile properties of polyetheretherketone neat resin films was investigated at different test temperatures (125, 25, and -100) using four samples: fast-quenched amorphous (Q); quenched, then crystallized at 180 C (C180); slowly cooled (for about 16 h) from the melt (SC); and air-cooled (2-3 h) from the melt (AC). It was found that thermal history significantly affects the tensile properties of the material below the glass transition. Fast quenched amorphous films were most tough, could be drawn to greatest strain before rupture, and undergo densification during necking; at the test temperature of -100 C, these films had the best ultimate mechanical properties. At higher temperatures, the semicrystalline films AC and C180 had properties that compared favorably with the Q films. The SC films exhibited poor mechanical properties at all test temperatures.

Cebe, Peggy↗

Powder processing of nickel and other aluminides by hot consolidation

Alloys based on FeAl, NiAl, and Ni3Al have been processed by extrusion of powders over a range of compositions, powder characteristics, and extrusion parameters. It is found that extrusion leads to dynamic recrystallization and that the grain size of the extrusions depends on the powder size, extrusion temperature, and extrusion ratio. Prior particle boundary oxides play an important role in controlling the grain size and uniformity by acting as obstacles to grain growth. Hot isostatic pressing and vacuum hot pressing can be used for powder densification, but prior particle oxides are not effectively broken up due to insufficient shearing deformation.

Vedula, K.↗

Properties of silicon carbide fiber-reinforced silicon nitride matrix composites

The mechanical properties of NASA Lewis developed SiC/RBSN composites and their thermal and environmental stability havd been studied. The composites consist of nearly 30 vol pct of aligned 142 micron diameter chemically vapor-deposited SiC fibers in a relatively porous silicon nitride matrix. In the as-fabricated condition, the unidirectional and 2-D composites exhibited metal-like stress-strain behavior, graceful failure, and showed improved properties when compared with unreinforced matrix of comparable density. Furthermore, the measured room temperature tensile properties were relativley independent of tested volume and were unaffected by artifical notches normal to the loading direction or by thermal shocking from temperatures up to 800 C. The four-point bend strength data measured as a function of temperature to 1400 C in air showed that as-fabricated strength was maintained to 1200 C. At 1400 C, however, nearly 15 pct loss in strength was observed. Measurement of room temperature tensile strength after 100 hr exposure at temperatures to 1400 C in a nitrogen environment indicated no loss from the as-fabricated composite strength. On the other hand, after 100 hr exposure in flowing oxygen at 1200 and 1400 C, the composites showed approximately 40 pct loss from their as-fabricated ultimate tensile strength. Those exposed between 400 to 1200 C showed nearly 60 pct strength loss. Oxidation of the fiber/matrix interface as well as internal oxidation of the porous Si3N4 matrix are likely mechanisms for strength degradation. The excellent strength reproducibility, notch insensitivity, and high temperature strength of the composite makes it an ideal candidate for advanced heat engine applications provided coating or densification methods are developed to avoid internal oxidation attack.

Bhatt, Ramakrishna T.↗