Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “tantalum”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 775 records · Page 43

Materials technology programs in support of a mercury Rankine space power system

A large portion of the materials technology is summarized that was generated in support of the development of a mercury-rankine space power system (SNAP-8). The primary areas of investigation are: (1) the compatibility of various construction materials with the liquid metals mercury and NaK, (2) the mechanical properties of unalloyed tantalum, and (3) the development of refractory metal/austenitic stainless steel tubing and transition joints. The primary results, conclusions, and state of technology at the completion of this effort for each of these areas are summarized. Results of possible significance to other applications are highlighted.

Stone, P. L.↗

Generation of long time creep data on refractory alloys at elevated temperatures

Four separate studies of various aspects of the vacuum creep behavior of two tantalum alloys (T-111 and ASTAR 811C) and of pure CVD tungsten are reported. The first part of the program involved a study of the influence of high temperature pre-exposure to vacuum or to liquid lithium on the subsequent creep behavior T-111 alloy. Results of this study revealed significant effects of pre-exposure on the 1% creep life of T-111, with life reductions of about 3 orders of magnitude being observed in extreme cases. The second part of this study involved an investigation of the creep behavior of T-111 under conditions of continuously increasing stress and decreasing temperature which simulated the conditions anticipated in radioisotope capsule service. Results of this study showed that such test conditions produced a creep curve having a very unusual shape, and led to the identification of a new creep design parameter for this type of service. The third area of investigation was a study of the influence of heat treatment on the microstructure and creep behavior of ASTAR 811C. The fourth part of the program was directed toward a preliminary characterization of the 1% creep life of CVD tungsten as obtained from two different sources.

Sheffler, K. D.↗

Irradiation of three T-111 clad uranium nitride fuel pins for 8070 hours at 990 C (1815 F)

The design and successful operation of three tantalum alloy (Ta-8W-2Hf) clad uranium mononitride (UN) fuel pins irradiated for 8070 hr at 990 C (1815 F) is described. Two pin diameters having measured burnups of 0.47 and 0.90 uranium atom percent were tested. No clad failures or swelling was detected; however, postirradiation clad samples tested failed with 1 percent strain. The fuel density decrease was 2 percent, and the fission gas release was less than 0.05 percent. Isotropic fuel swelling, which averaged about 0.5 percent, was less than fuel pin assembly clearances. Thus the clad was not strained. Thermocouples with a modified hot zone operated at average temperatures to 1100 C (2012 F) without failure. Factors that influence the ability to maintain uniform clad temperature as well as the results of the heat transfer calculations are discussed.

Slaby, J. G.↗

Recent materials compatibility studies in refractory metal-alkali metal systems for space power applications.

Advanced Rankine and other proposed space power systems utilize refractory metals in contact with both single-phase and two-phase alkali metals at elevated temperatures. A number of recent compatibility experiments are described which emphasize the excellent compatibility of refractory metals with the alkali metals, lithium, sodium, and potassium, under a variety of environmental conditions. The alkali metal compatibilities of tantalum-, columbium-, molybdenum-, and tungsten-base alloys are discussed.

Harrison, R. W.↗

Ultrasonic measurement of elastic moduli in slender specimens using extensional and torsional wave pulses.

The pulse-echo method using extensional and torsional waves is described relative to determining elastic properties and other characteristics of specimens which are slender acoustically. Several applications are reviewed, including: glass fibers of diameter 16 to 42 microns; glass rods of diameter about 1 mm, tested to 700 C; iron-base alloys of diameter 3.2 mm, tested from nearly -200 up to +200 C; titanium specimens of rectangular cross section, 1.5 by 3 mm; and tantalum-base alloys of diameter 6.4 mm, tested up to 1400 C. Limitations are pointed out regarding dispersive materials and geometry.

Lynnworth, L. C.↗

Determination of work functions near melting points of refractory metals by using a direct-current arc.

A direct-current arc in argon at atmospheric pressure was used to determine effective work functions of refractory metals, including tantalum, tungsten, molybdenum, and niobium. The procedure is experimentally advantageous, because surface cleanliness of the specimen is not critical, high vacuum is not required, and the anode-cathode spacing is not critical. The experimental procedure involves striking an arc to a metal wire cathode to form a melted ball having an emitting area defined by its diameter. The literature melting point of the metal is taken as the emitting temperature. By using these parameters and the known arc current, effective work functions were calculated from the Richardson-Dushman equation. The calculated work functions agree with recommended handbook values to within about 0.1 V and have typical repeatabilities of 0.02 V.

Gordon, W. A.↗

Studies of the performance of W-Re type thermocouples.

The effect of exposure of bare-wire and BeO-insulated commercial W-Re thermocouple materials to high temperatures in gaseous environments was investigated. The temperature range of interest was primarily 2000 to 2400 K, and the investigations were confined to thermocouple wires of 0.25 mm diameter. Thermoelements were examined for metallurgical structural changes and chemical changes by conventional methods. In the temperature range of interest, grain growth was inhibited in the chemically doped W-3% Re alloy, and excellent room-temperature ductility was retained subsequent to the exposure. The compatibility of high purity (in excess of 99.8%), sintered BeO insulators with the thermoelements differed, depending upon whether the BeO-insulated thermoelement assemblies were self-heated electrically or heated in a furnace; in tests in argon environments, highly reliable performance occurred when the assemblies were heated in a furnace. BeO-insulated W-3% Re vs W-25% Re thermocouples, constructed with degassed and aged materials, exhibited drifts equivalent to about 3 mK/hr during 1000 hours of exposure at 2073 K in argon while in the presence of tantalum.

Burns, G. W.↗

Measured drift of irradiated and unirradiated W3%Re/W25%Re thermocouples at a nominal 2000 K.

Seven tantalum sheathed, BeO insulated, 0.157-cm-diam, grounded-junction W-3%Re/W-25%Re thermocouples were irradiated in a helium-argon environment at a temperature of 1900 to 2100 K. Six other thermocouples from the same lot were operated out-of-pile with the same temperature history as the in-pile thermocouples. Drift-in-pile was determined by periodically replacing a 'reference' thermocouple in the irradiation capsule. Drift out-of-pile was determined with an optical pyrometer. After 8000 hours irradiation, the estimated neutron fluence was 4 x 10 to the 21st power thermal neutrons/sq cm and 0.9 x 10 to the 21st power fast neutrons/sq cm (E greater than 0.18 MeV). At this time the in-pile group had decreased in output the equivalent of 340 K at 2073 K, while the out-of-pile group had decreased in output the equivalent of 54 K at 2073 K. The maximum deviation in drift between thermocouples of the in-pile group and between thermocouples of the out-of-pile group was less than plus or minus 15 K and less than plus or minus 10 K, respectively.

Heckelman, J. D.↗

Preparation of refractory cermet structures for lithium compatibility testing

High-purity nitride and carbide cermets were synthesized for compatability testing in liquid lithium. A process was developed for the preparation of high-purity hafnium nitride powder, which was subsequently blended with tungsten powder or tantalum nitride and tungsten powders and fabricated into 3 in diameter billets by uniaxial hot pressing. Specimens were then cut from the billets for compatability testing. Similar processing techniques were applied to produce hafnium carbide and zirconium carbide cermets for use in the testing program. All billets produced were characterized with respect to chemistry, structure, density, and strength properties.

Heestand, R. L.↗

Study of photoemission and work function of large surface areas, phase 3, phase 4

The photoemission of materials which might be used in probe measurements of the exo-atmospheric electric field is considered by evaluating the wavelength dependence of their photoelectric yield for eleven elements over the range 800 to 3200 A. Yield data for zinc, copper beryllium, platinum, cadmium, graphite, carbon, gold, silver, tantalum, and tungsten show that copper-beryllium is a preferred material. Silver has one of the highest photoemissions when exposed to solar radiation.

Source record↗

Examination of T-111 clad uranium nitride fuel pins irradiated up to 13,000 hours at a clad temperature of 990 C

The examination of 27 fuel pins irradiated for up to 13,000 hours at 990 C is described. The fuel pin clad was a tantalum alloy with uranium nitride as the nuclear fuel. Two nominal fuel pin diameters were tested with a maximum burnup of 2.34 atom percent. Twenty-two fuel pins were tested for fission gas leaks; thirteen pins leaked. Clad ductility tests indicated clad embrittlement. The embrittlement is attributed to hydrogen from an n,p reaction in the fuel. Fuel swelling was burnup dependent, and the amount of fission gas release was low, generally less than 0.5 percent. No incompatibilities between fuel, liner, and clad were in evidence.

Slaby, J. G.↗

Use of thin film light detector

A photovoltaic cell device with a trapezoidal barrier is described. An aluminum, magnesium, or tantalum base is vapor deposited on a quartz substrate. An oxide or nitride film of the base metal is produced as an insulator by reaction in a glow discharge plasma to a thickness of less than 100 Angstroms. A metal, preferably gold, conter-electrode is vapor deposited on the insulating layer. A bias generator of high impedance is used to set and shift or modulate the spectral response of the device.

Lewicki, G. W.↗

SNAP-8 refractory boiler development program

Performance and endurance tests of the SNAP-8, SN-1 refractory metal boiler are described. The tests were successful and indicated that the boiler heat transfer area could be reduced significantly primarily because of the wetting characteristics of mercury on tantalum in a contaminant-free environment. A continuous endurance test of more than 10,000 hours was conducted without noticeable change in the thermal performance of the boiler. A conclusion of the metallographic examination of the boiler following the endurance test was that expected boiler life would be of the order of 40,000 hours at observed corrosion rates.

Fuller, R. A.↗

Skylab M551 Metals Melting Experiment

The objectives of the M551 Metals Melting Experiment are to (a) study behavior of molten metal, (b) characterize metals melted and solidified in the low gravity space environment compared to one-gravity of earth, and (c) determine feasibility of joining metals in space. The experiment used the electron beam (EB) and chamber of the M512 apparatus to make a dwell puddle and a melt in a rotating disc of varying thickness. Hence, the EB performed cut-through, full and partial penetration melts, in addition to a re-solidified button. The three disc materials were aluminum 2219-T87, 304 stainless steel and pure tantalum to provide a wide range of density and melting conditions. Observations to date include (a) the proof that EB welding, cutting and melting can be done successfully in low gravity. Earlier, some welding authorities had postulated that without gravity the EB would force the molten puddle out of contact. However, the experiment proved that surface tension forces predominate. (b) From the view-point of cast-solidification, small, equiaxed grains in Skylab specimens compared to large, elongated grains in ground-based specimens were observed. The former are thought to be associated with constitutional supercooling and nucleation where the latter are associated with dendritic solidification. In further support of the more equiaxed grain growth in Skylab, symmetric sub-grain patterns were frequently observed where there was much less symmetry in ground-based specimens. Further work is being done to explain the differences in solidification.

E C Mckannan↗

Eight cm technology thruster development

A structural integrated ion thruster with 8-cm beam diameter (SIT-8) was developed for attitude control and stationkeeping of synchronous satellites. As optimized, the system demonstrates a thrust T=1.14 mlb (not corrected for beam V sub B = 1200 V (I sub sp = 2200 sec) total propellant utilization efficiency nu sub u = 59.8% (is approximately 72% without auxiliary pulse-igniter electrode), and electrical efficiency n sub E 61.9%. The thruster incorporates a wire-mesh anode and tantalum cover surfaces to control discharge chamber flake formation and employs an auxiliary pulse-igniter electrode for hollow-cathode ignition. When the SIT-8 is integrated with the compatible SIT-5 propellant tankage, the system envelope is 35 cm long by 13 cm flange bolt circle with a mass of 9.8 kg including 6.8 kg of mercury propellant. Two thrust vectoring systems which generate beam deflections in two orthogonal directions were also developed under the program and tested with the 8-cm thruster. One system vectors the beam over + or - 10 degrees by gimbaling of the entire thruster (not including tankage), while the other system vectors the beam over + or - 7 degrees by translating the accel electrode relative to the screen electrode.

Hyman, J., Jr.↗

Effect of solutes in binary columbium /Nb/ alloys on creep strength

The effect of seven different solutes in binary columbium (Nb) alloys on creep strength was determined from 1400 to 3400 F for solute concentrations to 20 at.%, using a new method of creep-strength measurement. The technique permits rapid determination of approximate creep strength over a large temperature span. All of the elements were found to increase the creep strength of columbium except tantalum. This element did not strengthen columbium until the concentration exceeded 10 at.%. Hafnium, zirconium, and vanadium strengthed columbium most at low temperatures and concentrations, whereas tungsten, molybdenum, and rhenium contributed more to creep strength at high temperatures and concentrations.

Klein, M. J.↗

Thermal fatigue behavior of T-111 and ASTAR 811C in ultrahigh vacuum

The thermal fatigue behavior of the tantalum alloys T-111 (Ta-8W-2Hf) and ASTAR 811C (Ta-8W-1Re-0.7Hf-0.025C) has been evaluated using completely reversed push-pull fatigue tests conducted in ultrahigh vacuum with independently programmed temperature and strain cycles. Test results showed that cycling of the test temperature simultaneously with the mechanical strain in most cases significantly reduced the cycles to failure of both alloys compared to isothermal testing. Notched specimens had reduced lives under isothermal conditions, but the presence of a notch or use of a 1-h holdtime provided only a small further decrease in life for the temperature cycled tests. Compressive stress at the maximum temperature produced longer lives than tensile stress. ASTAR 811C was more fatigue resistant than T-111 isothermally and did not have as great a decrease in life with thermal cycling. Results are analyzed by partition of plastic strains into creep and creep-independent components and considering where each component was active in the hysteresis cycle.

Sheffler, K. D.↗

Evaluation of several additional dry lubricants for spacecraft applications

Four transfer-film ball-bearing retainer materials were evaluated for their lubricating ability and wear capability under conditions of 120-gram radial load, 450-gram axial load, 3600-rpm unidirectional rotation, 23 C ambient temperature, and less than .1 microtorr pressure, using R-2 sized unshielded ball bearings. The 'stop-test' criterion was a total of one billion revolutions or a torque buildup greater than 18 gm-cm per bearing pair. A PTFE-fiberglass-MoS2 composite, a PTFE-bronze composite, and a tantalum-molybdenum-MoS2 composite operated for one billion revolutions without reaching the 18-gram torque limit. A p-oxybenzoyl polymer-MoS2 composite operated sixteen million revolutions before reaching the 18-gm cm stop-test torque. The first three materials are considered as suitable lubricants under the test conditions employed.

Vest, C. E.↗