Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “alloy solidification”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 775 records · Page 43

Directional Solidification of Bi-Sn on USMP-4

The experiments used MEPHISTO hardware to study the solidification and melting behavior of bismuth alloyed with 1 at% tin. Three samples, each approximately 900 mm long and 6mm in diameter, were used. A portion of each sample also included a 2 mm diameter growth capillary, to assist in the formation of a single grain. One sample provided the Seebeck voltage generated during melting and freezing processes. Another provided temperature data and Peltier pulsed demarcation of the interface shape for post flight analysis. The third sample provided resistance and growth velocity measurements, as well as additional thermal data. The third sample was also quenched at the end of the mission to preserve the composition of the liquid near the interface for post flight determination. A total of 450mm of directionally solidified samples were preserved for post mission structural and compositional characterization. Substantial differences were observed in the Seebeck signal between the ground-based experiments and the space-based experiments. The temperature gradient in the liquid for the ground-based experiments was significantly lower than the temperature gradient in the liquid for the space-based experiments.

Abbaschian, Reza↗

Morphological Stability of Faceted Interfaces

The major focus of this investigation is to study the fundamentals of layer spreading mechanisms during growth of doped Ge (a facet forming material), and to determine the conditions for morphological instability of vicinal solid-liquid interfaces. The investigation will also lead to the determination of the effect of dopants on the layer growth kinetics, step free energy, and dopant capture by the advancing ledges. The theoretical treatment of growth of faceted interfaces indicates that the kinetics of a step on a growing vicinal interface considerably depends on its angle of inclination, the melt concentration, and characteristics of flow currents in the melt. The morphological stability of the interface also depends on these parameters, as well as on the density and spreading velocity of the steps. However, the treatment of the instability of the interface by the layer growth mechanism is rather difficult because it requires exact knowledge of the thermal and solutal fields, hydrodynamics of the melt, and supercooling at the interface. The results of recent space experiments of the principal investigator involving directional solidification of faceted Bi-Sn alloys have shown that the morphological stability of various crystallographic orientations is significantly affected by the anistropy in interfacial properties of the faceted alloy in general, and the interface kinetics in particular. These findings have also raised many important and fundamental questions, particularly with respect to the behavior of interfacial steps, which need to be addressed via additional groundbased and microgravity experiments. For the present investigation we will use a novel crystal growth technique which provides axial heat flux close to the solid-liquid boundary. The Axial Heat Processing (AHP) technique allows for precise control and determination of the heat and mass transfer close to the crystallization front, and the establishment of a planar interface over the entire cross-section of the growing crystal.

Abbaschian, Reza↗

Orbital Processing of Eutectic Rod-Like Arrays

The eutectic is one of only three solidification classes that exist. The others are isostructural and peritectic-class reactions, respectively. Simplistically, in a binaryeutectic phase diagram, a single liquid phase isothermally decomposes to two solid phases in a cooperative manner. The melting point minimum at the eutectic composition, isothermal solidification temperature, near-isocompositional solidification and refined solidification microstructure lend themselves naturally to such applications as brazing and soldering; industries that eutectic alloys dominate. Interest in direct process control of microstructures has led, more recently, to in-situ eutectic directional solidification with applications in electro-magnetics and electro-optics. In these cases, controlled structural refinement and the high aspect ratio and regularity of the distributed eutectic phases is highly significant to the fabrication and application of these in-situ natural composites. The natural pattern formation and scaling of the dispersed phase on a sub-micron scale has enormous potential application, since fabricating bulk materials on this scale mechanically has proven to be particularly difficult. It is thus of obvious importance to understand the solidification of eutectic materials since they are of great commercial significance. The dominant theory that describes eutectic solidification was derived for diffusion-controlled growth of alloys where both solid eutectic phases solidify metallically, i.e. without faceting at the solidification interface. Both high volume fraction (lamellar) and low volume fraction (rod-like) regular metallic arrays are treated by this theory. Many of the useful solders and brazements, however, and most of the regular in-situ composites are characterized by solidification reactions that are faceted/non-faceted in nature, rather than doubly non-faceted (metallic). Further, diffusion-controlled growth conditions are atypical terrestrially since gravitationally-driven convection is pervasive. As a consequence, it is important to determine whether these faceted/non-faceted composites behave in the same manner as their doubly non-faceted counterparts, particularly in the presence of convection. Prior analytical convective sensitivity testing of this theory predicted insensitivity. Prior experimental testing of this theory offered broad-based agreement between theory and experiment, though most results were for high volume fraction lamellar eutectics that solidified without faceting at the solidification interface. Directional solidification experiments of low volume fraction rod eutectics under damped (microgravity or magnetic field) conditions, however, have demonstrated significant sensitivity, challenging this fundamental theory. More recent theories have been proposed which introduce kinetic undercooling, faceting, fluid shear of the solute redistribution zone and the possibility that the interface composition is not the same as the bulk liquid composition. This program tests the established and proposed analytical theories and addresses the origins of discrepancies between the experimental and analytical results.

Larson, David J., Jr.↗

Growth of Solid Solution Single Crystals

The solidification of a solid solution semiconductor, having a wide separation between liquidus and serious has been extensively studied in ground based, high magnetic field and Spacelab experiments. Two alloys of mercury cadmium telluride have been studied; mercury cadmium telluride with 80.0 mole percent of HgTe and 84.8 mole percent respectively. These alloys are extremely difficult to grow by directional solidification on earth due to high solutal and thermal density differences that give rise to fluid flow and consequent loss of interface shape and composition. Diffusion controlled growth is therefore impossible to achieve in conventional directional solidification. The ground based experiments consisted of growing crystals in several different configurations of heat pipe furnaces, NASA's Advanced Automated Directional Solidification Furnace (AADSF), and a similar furnace incorporated in a superconducting magnet capable of operating at up to 5T. The first microgravity experiment took place during the flight of STS-62 in March 1994, with the AADSF installed on the second United States Microgravity Payload (USMP-2). The alloy was solidified at 3/4 inch per day over a 9 day period, and for the first time a detailed evaluation was performed of residual acceleration effects. The second flight experiment took place in the fourth United States Microgravity Payload Mission (USMP-4) in November 1997. Due to contamination of the furnace system by a previously processed sample, the sample was not received until May 1998, and the preliminary analysis shows that the conditions prevailing during the experiment were quite different from the requirements requested prior to the mission. Early results are indicating that the sample may not accomplish the desired objectives. As with the USMP-2 mission, the results of the ground based experiments were compared with the crystal grown in orbit under microgravity conditions. On the earth, it has been demonstrated that the application of the magnetic field leads to a significant reduction in fluid flow, with improved homogeneity of composition. The field strength required to suppress flow increases with diameter of the material. The 8 mm diameter sample used here was less than the upper diameter limit for a ST magnet. The configuration for USMP-4 was changed so that the material was seeded and other processing techniques were also modified. It was decided to examine the effects of a strong magnetic field under the modified configuration and parameters. A further change from USMP-2 was that a different composition of material was grown, namely with 0.152 mole fraction of cadmium telluride rather than the 0.200 of the USMP-2 experiment. The objective was to grow highly homogeneous, low defect density material of a composition at which the conduction band and the valence band of the material impinge against each other. As indicated, the furnace was contaminated during the mission. As a result of solid debris remaining in the furnace bore, the cartridge in this experiment, denoted as SL1-417, was significantly bent during the insertion phase. During translation the cartridge scraped against the plate which isolates the hot and cold zones of the furnace. Thermocouples indicated that a thermal assymetry resulted. The scraping in the slow translation or crystal growth part of the processing was not smooth and it is probable that the jitter was sufficient to give rise to convection in the melt. Early measurements of composition from the surface of the sample have shown that the composition varies in an oscillatory manner.

Lehoczky, Sandor L.↗

Growth of Solid Solution Single Crystals

The solidification of a solid solution semiconductor, having a wide separation between liquidus and solidus has been extensively studied in ground based, high magnetic field and Spacelab experiments. Two alloys of mercury cadmium telluride have been studied; with 80.0 mole percent of HgTe and 84.8 mole percent of HgTe respectively, the remainder being cadmium telluride. Such alloys are extremely difficult to grow by directional solidification on earth due to high solutal and thermal density differences that give rise to fluid flow and consequent loss of interface shape and composition. Diffusion controlled growth is therefore impossible to achieve in conventional directional solidification. The ground based experiments consisted of growing crystals in several different configurations of heat pipe furnaces, NASA's Advanced Automated Directional Solidification Furnace (AADSF), and a similar furnace incorporated in a superconducting magnet capable of operating at up to 5T. The first microgravity experiment took place during the flight of STS-62 in March 1994, with the AADSF installed on the second United States Microgravity Payload (USMP-2). The alloy was solidified at 3/4 inch per day over a 9 day period, and for the first time a detailed evaluation was performed correlating composition variations to measured residual acceleration. The second flight experiment took place in the fourth United States Microgravity Payload Mission (USMP-4) in November 1997. Due to contamination of the furnace system, analysis shows that the conditions prevailing during the experiment were quite different from the requirements requested prior to the mission. The results indicate that the sample did accomplish the desired objectives.

Lehoczky, Sandor L.↗

Joining of superalloy Inconel 600 by diffusion induced isothermal solidification of a liquated insert metal

The effect of process variables on the microstructure of transient liquid phase bonded IN 600 using a commercial filler alloy was studied. Microstructural examination of bonded specimens showed that isothermal solidification of the liquated insert occurred during holding at the joining temperatures. In cases where the holding time was insufficient for complete isothermal solidification, the residual liquid transformed on cooling into a centerline eutectic product. The width of the eutectic decreased with increased holding time and an increase in initial gap width resulted in thicker eutectic width in specimens bonded at the same temperature and for equivalent holding times. In addition to the centerline eutectic microconstituent, precipitation of boron-rich particles was observed within the base metal region adjacent to the substrate-joint interface. Formation of these particles appeared to have influenced the rate of solidification of the liquated interlayer during bonding. In contrast to the conventional expectation of an increase in the rate of isothermal solidification with an increase in temperature, a decrease in the rate was observed with an increase in temperatures above 1160 deg. C. This could be related to a decrease in solubility of boron in nickel above the Ni-B eutectic temperature.

36 MATERIALS SCIENCE↗

Microstructure Evolution of Gas Atomized Iron Based ODS Alloys

In a simplified process to produce precursor powders for oxide dispersion-strength- ened (ODS) alloys, gas-atomization reaction synthesis (GARS) was used to induce a surface oxide layer on molten droplets of three differing erritic stainless steel alloys during break-up and rapid solidification. The chemistry of the surface oxide was identified using auger electron spectroscopy (AES) and scanning electron microscopy (SEM) with energy dispersive spectroscopy (EDS). The precursor iron-base powders were consolidated at 850 C and 1,300 C using hot isostatic pressing (HIPing). Consolidation at the lower temperature resulted in a fully dense microstructure, while preventing substantial prior particle-boundary-oxide dissociation. Microstructural analysis of the alloys consolidated at the higher temperature confirmed a significant reduction in prior-particle-boundary-oxide volume fraction, in comparison with the lower-temperature-consolidated sample. This provided evidence that a high-temperature internal oxygen-exchange reaction occurred between the metastable prior particle-boundary-oxide phase (chromium oxide) and the yttrium contained within each prior particle. This internal oxygen-exchange reaction is shown to result in the formation of yttrium-enriched oxide dispersoids throughout the alloy microstructure. The evolving microstructure was characterized using transmission electron microscopy (TEM) and high-energy X-ray diffraction (HE-XRD).

36 MATERIALS SCIENCE↗

Microstructure Evolution of Gas Atomized Iron Based ODS Alloys

In a simplified process to produce precursor powders for oxide dispersion-strengthened (ODS) alloys, gas-atomization reaction synthesis (GARS) was used to induce a surface oxide layer on molten droplets of three differing erritic stainless steel alloys during break-up and rapid solidification. The chemistry of the surface oxide was identified using auger electron spectroscopy (AES) and scanning electron microscopy (SEM) with energy dispersive spectroscopy (EDS). The precursor iron-base powders were consolidated at 850 C and 1,300 C using hot isostatic pressing (HIPing). Consolidation at the lower temperature resulted in a fully dense microstructure, while preventing substantial prior particle-boundary-oxide dissociation. Microstructural analysis of the alloys consolidated at the higher temperature confirmed a significant reduction in prior-particle-boundary-oxide volume fraction, in comparison with the lower-temperature-consolidated sample. This provided evidence that a high-temperature internal oxygen-exchange reaction occurred between the metastable prior particle-boundary-oxide phase (chromium oxide) and the yttrium contained within each prior particle. This internal oxygen-exchange reaction is shown to result in the formation of yttrium-enriched oxide dispersoids throughout the alloy microstructure. The evolving microstructure was characterized using transmission electron microscopy (TEM) and high-energy X-ray diffraction (HE-XRD).

36 MATERIALS SCIENCE↗

Ordering in liquid and its heredity impact on phase transformation of Mg-Al-Ca alloys

It is a long-sought goal to achieve desired mechanical properties through tailoring phase formation in alloys, especially for complicated multi-phase alloys. In fact, unveiling nucleation of competitive crystalline phases during solidification hinges on the nature of liquid. Here we employ ab initio molecular dynamics simulations (AIMD) to reveal liquid configuration of the Mg-Al-Ca alloys and explore its effect on the transformation of Ca-containing Laves phase from Al 2 Ca to Mg 2 Ca with increasing Ca/Al ratio (r Ca/Al ). There is structural similarity between liquid and crystalline phase in terms of the local arrangement environment, and the connection schemes of polyhedras. The forming signature of Mg 2 Ca, as hinted by the topological and chemical short-range order originating from liquid, ascends monotonically with increasing r Ca/Al . However, Al 2 Ca crystal-like order increase at first and then decrease at the crossover of r Ca/Al = 0.74, corresponding to experimental composition of phase transition from Al 2 Ca to Mg 2 Ca. The origin of phase transformation across different compositions lies in the dense packing of atomic configurations and preferential bonding of chemical species in both liquid and solid. The present finding provides a feasible scenario for manipulating phase formation to achieve high performance alloys by tailoring the crystal-like order in liquid.

36 MATERIALS SCIENCE↗

Eutectic nucleation in hypoeutectic Al-Si alloys

The nucleation mechanism of eutectic grains in hypoeutectic Al-Si foundry alloys has been investigated by examining deep etched specimens in high-resolution field emission gun scanning electron microscope (FEG-SEM) and by using in-situ Focused Ion Beam (FIB) milling and microscopy. Both unmodified and Sr-modified alloys were studied to characterize the nucleation mechanism of eutectic silicon flakes and fibers. It is proposed that following nucleation of eutectic Al on the primary {alpha}-Al dendrites, fine Si particles form at the solidification front upon which the eutectic Si flakes and fibers could develop. The formation of small Si particles is attributed to Si enrichment of the remaining melt due to the formation of eutectic Al (aluminum spikes) at the eutectic temperature. A hypothesis is then proposed to explain the mechanism of eutectic grains formation with main emphasis on the eutectic Si phase.

36 MATERIALS SCIENCE↗

High-Performance MnBi Alloy Prepared Using Profiled Heat Treatment

The profiled heat treatment (PHT) method has been used to synthesize MnBi alloys with high-purity low-temperature phase (LTP). In the PHT method, the arc-melted MnBi alloy was remelted then slowly cooled by a pseudo-equilibrium solidification process to promote the formation of LTP phase. The PHT-treated MnBi alloys had an LTP phase up to 94 wt.% and a magnetization of 73 emu/g under a field of 9 T. Scanning electron microscopy showed that there exist some micrometer-sized Mn-rich inclusions in the LTP matrix of the PHT MnBi alloy. The PHT MnBi alloys were crushed into powders with an average size of ~3 μm by low-energy ball milling. These MnBi powders were aligned in an 18 kOe field and warm compacted into a bulk magnet at 300 °C for 30 min. The magnet had a density of 8.2 g/cm3 and magnetic properties of Ms = 6.7 kG, Mr = 5.3 kGs, i Hc = 5 kOe, and (BH)max = 6.1 MGOe

MnBi↗

Multiphase Model of Semisolid Slurry Generation and Isothermal Holding During Cooling Slope Rheoprocessing of A356 Al Alloy

In the present paper, we present an experimentally validated 3D multiphase and multiscale solidification model to understand the transport processes involved during slurry generation with a cooling slope. In this process, superheated liquid alloy is poured at the top of the cooling slope and allowed to flow along the slope under the influence of gravity. As the melt flows down the slope, it progressively loses its superheat, starts solidifying at the melt/slope interface with formation of solid crystals, and eventually exits the slope as semisolid slurry. In the present simulation, the three phases considered are the parent melt as the primary phase, and the solid grains and air as secondary phases. The air phase forms a definable air/liquid melt interface as the free surface. After exiting the slope, the slurry fills an isothermal holding bath maintained at the slope exit temperature, which promotes further globularization of microstructure. The outcomes of the present model include prediction of volume fractions of the three different phases considered, grain evolution, grain growth, size, sphericity and distribution of solid grains, temperature field, velocity field, macrosegregation and microsegregation. In addition, the model is found to be capable of making predictions of morphological evolution of primary grains at the onset of isothermal coarsening. The results obtained from the present simulations are validated by performing quantitative image analysis of micrographs of the rapidly oil-quenched semisolid slurry samples, collected from strategic locations along the slope and from the isothermal slurry holding bath.

36 MATERIALS SCIENCE↗

Effect of Undercooling in a Low-Gravity Containerless Environment on the Structure and Properties of Alloys

The 30 meter and 100 meter drop tubes at the Marshall Space Flight Center offer a unique opportunity to study solidification in a containerless, microgravity environment. Samples are melted in a furnace at the top of the drop tube and solidify during a 4.5 second free fall in the 100 meter drop tube or a 2.6 second free fall in the 30 meter drop tube. The cooling rate obtained in the drop tubes is lower than cooling rates in atomization and splat-quenching processes. Decoupling the rapid solidification process allows the study of the effects of undercooling and recalescence on alloy morphologies. The research therefore has a three-fold purpose. The first is examination of the limits of undercooling of niobium and niobium-base alloys in the drop tube. The second purpose is the observation of microstructures resulting from the solidification of samples at large undercoolings and moderate cooling rates. The third purpose is the observation of metastable phase formation in highly undercooled samples.

Bayuzick, R. J.↗

Iron rich low cost superalloys

An iron-rich low-cost superalloy was developed. The alloy, when processed by conventional chill casting, has physical and mechanical properties that compare favorably with existing nickel and cobalt based superalloys while containing significantly lower amounts of strategic elements. Studies were also made on the properties of Cr(20)-Mn(10)-C(3.4)-Fe(bal.), a eutectic alloy processed by chill casting and directional solidification which produced an aligned microstructure consisting of M7C3 fibers in a gamma-Fe matrix. Thermal expansion of the M7C3 (M = Fe, Cr, Mn) carbide lattice was measured up to 800 C and found to be highly anisotropic, with the a-axis being the predominant mode of expansion. Repetitive impact sliding wear experiments performed with the Fe rich eutectic alloy showed that the directionally solidified microstructure greatly improved the alloy's wear resistance as compared to the chill cast microstructure and conventional nickel base superalloys. Studies on the molybdenum cementite phase prove that the crystal structure of the xi phase is not orthorhombic. The crystal structure of the xi phase is made up of octahedra building elements consisting of four Mo and two Fe atoms and trigonal prisms consisting of four Fe and two Mo atoms. The voids are occupied by carbon atoms. The previous chemical formula for the molybdenum cementite MoFe2C is now clearly seen to be Mo12Fe22C10.

Wayne, S. F.↗

Liquid Phase Miscibility Gap Materials

The manner in which the microstructural features of liquid-phase miscibility gap alloys develop was determined. This will allow control of the microstructures and the resultant properties of these alloys. The long-duration low gravity afforded by the shuttle will allow experiments supporting this research to be conducted with minimal interference from buoyancy effects and gravitationally driven convection currents. Ground base studies were conducted on Al-In, Cu-Pb, and Te-Tl alloys to determine the effect of cooling rate, composition, and interfacial energies on the phase separation and solidification processes that influence the development of microstructure in these alloys. Isothermal and directional cooling experiments and simulations are conducted. The ground based activities are used as a technological base from which flight experiments formulated and to which these flight experiments are compared.

Gelles, S. H.↗

Skylab Experiment M552: Exothermic Brazing

The M552 Skylab experiment reveals that brazing in space is feasible. It successfully demonstrated the ability to retain molten metal within a braze tube joint system. Surface energy was the dominant operative force system controlling liquid metal for this experiment. The zero gravity environment for brazing resulted in several differences; increased solubility, increased liquid spreading, more uniform menisci (liquid/vapor interface) and a reduction of braze alloy shrinkage defects. The residual radioactive intensity and location of the redistributed isotope was interpreted to provide a sequential history of braze alloy movement during the melt-flow-solidification stages of the process. Convection theory applied to M552 was validated but some results were not explainable by it, i.e., increased nickel transport and the radial mixing of the silver isotope on samples SLN-2 and SLN-4. All characteristics of thermal analysis appeared to react as expected but heat conduction rates increased because of increased extent, rate and uniformity of braze alloy spreading.

J R Williams↗

FNAS modify matric and transparent experiments

Monotectic alloy materials are created by rapid melt/rapid solidification processing on the NASA KC-135. Separation of the uniform liquid into two liquids may occur by either of two processes; spinodal decomposition or nucleation followed by growth. In the first case, the liquid is unstable to composition waves, which form and grow, giving liquids of two different compositions. In the latter process discrete particles of the second liquid phase form via thermal fluctuations and then grow by diffusion. The two processes are very different, with the determining process being dictated by temperature, composition, and thermodynamic characteristics of the alloy. The first two quantities are process variables, while the third is determined by electronic interactions between the atoms in the alloy. In either case the initial alloy decomposition is followed by coarsening, resulting in growth of the particle size at nearly constant volume fraction. In particular, reduced gravity experiments on monotectic solutions have shown a number of interesting results in the KC-135. Monotectic solutions exhibit a miscibility gap in the liquid state, and consequently, gravity driven forces can dominate the solidification parameters at 1 g. In reduced gravity however, the distribution of the phases is different, resulting in new and interesting microstructures. The Rapid Melt/Rapid Quench Furnace allows one to melt a sample and resolidify it in one parabola of the KC-135's flight path, thus eliminating any accumulative influence of multiple parabolas to affect the microstructure of the material.

Smith, Guy A.↗

Processing of High-Entropy AlCoCr{sub 0.75}Cu{sub 0.5}FeNi Alloy by Spray Forming

Compositionally complex AlCoCrCuFeNi alloy system is one of the extensively studied high-entropy alloys (HEA). Most of these studies have been carried out on as-cast materials that witness slow cooling rate during solidification. In the present investigation, HEA based on AlCoCrCuFeNi system was processed employing spray forming so as to realize its inherent rapid solidification effect and unique microstructural evolution mechanism. The spray formed as well as the as-cast alloys were compared in terms of their microstructural features, phase constitution and hardness. These microstructural features were also compared with that of the overspray powders (< 250 µm) obtained as a by-product of spray forming. Both the as-cast and spray formed alloys showed a mixture of mainly two phases, i.e., face-centered and body-centered cubic (BCC) phases, in contrast to a single BCC phase in overspray powders. However, the spray formed alloy revealed unidentified phases, as against the as-cast material, which disappeared after heat treatment at 1473 K for 3 h. The grain size of the as-cast alloy was around 600-1000 μm compared to a highly refined grain size of 25-30 μm in the as-spray formed alloy. It was found that the hardness of the regions dominated by the constituent phases as well as the bulk of the spray formed material was higher than that of the as-cast alloy. The results validate the efficacy of the process in achieving drastic refinement in grain size, in a single step of large-scale spray forming. The characteristic microstructural features and the phase constitutions have been discussed in light of the prevailing mechanisms of structural evolution and possible solidification phenomena during spray atomization and deposition. This study gives a new direction in processing of these alloys and understanding their solidification behavior under the conditions of layer-by-layer deposition of semi-solid/liquid droplets.

36 MATERIALS SCIENCE↗