Preferred orientation in experimentally deformed stishovite: implications for deformation mechanisms
Abstract not provided
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Abstract not provided
The flow characteristics of polypropylene filled with high percentages of wood flour (50 and 70 wt%) are investigated at a feasible processing temperature (195 °C). Rotational rheometry in oscillatory mode in conjunction with the Cox–Merz rule is ineffective at this temperature due to insufficient linear viscoelastic region (LVR) size and ease of fibres degradation. An in-line rheometer, directly attached to a single screw extruder, is used to avoid these problems: this method allows measurements in real processing conditions with no LVR issues and with reduced degradation risks. The 70 wt% displays plug flow, thus it has been impossible to obtain the flow curve but only the slip velocity as a function of shear stress. The 50 wt% could be corrected for slip using the Mooney procedure. Comparing the flow curve of this material with the ones of the 30 wt% and the unfilled polypropylene matrix, a single master-curve can be obtained and modelled with a Carreau–Yasuda equation.
Grain boundaries (GBs) in polycrystalline materials act as impediments to dislocation motion and result in strengthening. Understanding slip transmission through GBs, specifically twin boundaries, is essential to understand the plastic deformation behavior of polycrystalline fcc materials. Here the interaction between a glide dislocation and Σ3{112} incoherent twin boundary (ITB) in copper is investigated using a combined atomistic and mesoscale approach. The material parameters and structure of the GB in the mesoscale phase field dislocation dynamics (PFDD) model are informed from Molecular Statics (MS) simulations. The structural unit of the ITB consists of an array of three partial dislocations. The interaction between a glide dislocation impinging on each of the GB partial dislocations is investigated using both PFDD and Molecular Dynamics (MD) with two boundary conditions. Transmission planes predicted by both PFDD and MD (NVT) are in agreement, and show that not all transmission events are direct. Critical transmission stresses predicted by PFDD are in the range of 276 MPa to 1380 MPa, while MD predictions are in the range from 100 MPa to 700 MPa. The PFDD and MD predictions of slip transmission are explained using dislocation theory based on isotropic linear elasticity.
Highlights: • C-(A-)S-H samples under stress were characterized at the bond and grain level. • Small angle scattering showed that 720 MPa reduced grain thickness by 30%. • In-situ Raman showed that cross-linked C-A-S-H slips along its intralayer. • However, in-situ Raman showed that C-S-H slips along the interlayer. • In-situ Raman also showed a growth in CaCO{sub 3}, indicating fracture in both samples. Creep of the cement matrix affects the structural stability of concrete. In Portland cements, the creep is largely controlled by the binding phase calcium-(aluminum-)silicate-hydrate, or C-(A-)S-H. This phase has a lamellar structure and under deviatoric stress aligns its c-axis with the principal stress. However, the limiting resistance to this reorientation is unknown at the nanocrystalline level. Small-angle X-ray scattering shows that the lamellae thickness decreases under 100's MPa deviatoric stress. Deviatoric stress Raman spectroscopy shows that there are two ways that this break-up can occur. If the material's silicate chains are cross-linked, then strain in SiO bonds does not increase above certain stresses, indicating a relaxation adjacent to the SiO bond. If the chains are not cross-linked, then the silicate chains are broken up by rastering against each other, introducing defects. These results show that the plastic deformation of C-(A-)S-H is relevant for Portland cement creep.
Two-phase flow measurements were carried out using a resistive void fraction meter coupled to a venturi or orifice plate. The measurement system used to estimate the liquid and gas mass flow rates was evaluated using an air-water experimental facility. Experiments included upward vertical and horizontal flow, annular, bubbly, churn and slug patterns, void fraction ranging from 2% to 85%, water flow rate up to 4000 kg/h, air flow rate up to 50 kg/h, and quality up to almost 10%. The fractional root mean square (RMS) deviation of the two-phase mass flow rate in upward vertical flow through a venturi plate is 6.8% using the correlation of Chisholm (D. Chisholm, Pressure gradients during the flow of incompressible two-phase mixtures through pipes, venturis and orifice plates, British Chemical Engineering 12 (9) (1967) 454-457). For the orifice plate, the RMS deviation of the vertical flow is 5.5% using the correlation of Zhang et al. (H.J. Zhang, W.T. Yue, Z.Y. Huang, Investigation of oil-air two-phase mass flow rate measurement using venturi and void fraction sensor, Journal of Zhejiang University Science 6A (6) (2005) 601-606). The results show that the flow direction has no significant influence on the meters in relation to the pressure drop in the experimental operation range. Quality and slip ratio analyses were also performed. The results show a mean slip ratio lower than 1.1, when bubbly and slug flow patterns are encountered for mean void fractions lower than 70%. (author)
Natural gas-powered engines play a critical role in gas drilling, compression, and transmission sectors, but methane (CH 4 ) from engine combustion slip can be significant over their lifespan, contributing to atmospheric pollution and signaling reduced engine efficiency. Here, to address this challenge, computational fluid dynamics (CFD) simulations offer valuable insights into the in-cylinder combustion process, enabling the optimization of combustion strategies and engine designs to minimize unburned CH 4 slip. This study aims to evaluate and improve combustion models for simulating the combustion process and predicting unburned CH 4 concentrations in natural gas spark-ignition (SI) engines, including engines that are part of combined reformer-engine systems. Specifically, the performance of two flamelet-based combustion models—the Extended Coherent Flame Model (ECFM) and the G-equation model—was assessed using experimental engine data collected under varying excess-air ratio (λ) conditions and fuel compositions, including natural gas and syngas blends. In addition, to enhance the predictive capabilities of the G-equation model, a flame-wall interaction (FWI) sub-model was integrated into its framework. The effects of its model parameters, such as quenching and influence distance, on combustion behavior and unburned methane predictions were analyzed in detail. The ECFM tended to predict delayed combustion phasing under diluted mixture conditions, resulting in overprediction of unburned CH 4 concentrations. In contrast, the G-equation model provided reasonable predictions of combustion pressure, while representing higher the CH 4 reduction rate across the operating condition compared to experimental data. Incorporating the FWI sub-model—with the quenching distance calculated based on a pressure-dependent relation (P -0.48 ) and a fixed influence distance of 1.5 mm—further improved the G-equation model’s accuracy in predicting CH 4 reduction rates without compromising its ability to simulate the combustion process.
In this paper, coupled reservoir-geomechanical (TOUGH-FLAC) modeling is applied for the first time to the St. Lawrence Lowlands region to evaluate the potential for shear failure along pre-existing high-angle normal faults, as well as the potential for tensile failure in the caprock units (Utica Shale and Lorraine Group). This activity is part of a general assessment of the potential for safe CO 2 injection into a sandstone reservoir (the Covey Hill Formation) within an Early Paleozoic sedimentary basin. Field and subsurface data are used to estimate the sealing properties of two reservoir-bounding faults (Yamaska and Champlain faults). The spatial variations in fluid pressure, effective minimum horizontal stress, and shear strain are calculated for different injection rates, using a simplified 2D geological model of the Becancour area, located ~110 km southwest of Quebec City. The simulation results show that initial fault permeability affects the timing, localization, rate, and length of fault shear slip. Contrary to the conventional view, our results suggest that shear failure may start earlier for a permeable fault than for a sealing fault, depending on the site-specific geologic setting. In simulations of a permeable fault, shear slip is nucleated along a 60 m long fault segment in a thin and brittle caprock unit (Utica Shale) trapped below a thicker and more ductile caprock unit (Lorraine Group) – and then subsequently progresses up to the surface. In the case of a sealing fault, shear failure occurs later in time and is localized along a fault segment (300 m) below the caprock units. The presence of the inclined low-permeable Yamaska Fault close to the injection well causes asymmetric fluid-pressure buildup and lateral migration of the CO 2 plume away from the fault, reducing the overall risk of CO 2 leakage along faults. Finally, fluid-pressure-induced tensile fracturing occurs only under extremely high injection rates and is localized below the caprock units, which remain intact, preventing upward CO 2 migration.
Hydrogen embrittlement of a nickel-based superalloy IN718 was investigated using slow strain rate tensile tests. Post-mortem observation of fractured samples was performed to explore hydrogen-assisted failure mechanisms of the alloy. The results reveal that hydrogen charging reduces yield strength, tensile strength, fracture strain and work hardening rate. With increasing current density, yield strength and tensile strength reduce linearly and fracture strain decreases exponentially. Furthermore, the crack initiation and propagation in hydrogen-charged region depends on the distribution of δ phase in the alloy. For needle-shaped δ phase within the grains, the nucleation of voids takes place at the intersections between dislocation slip bands and δ phase due to the hydrogen-enhanced localized plasticity (HELP)-assisted shear localization and possible hydrogen agglomeration. For δ phase along the grain boundaries, the impingement of slip bands and local hydrogen accumulation at γ-matrix/δ phase interfaces as well as hydrogen-enhanced decohesion (HEDE)-assisted decohesion lead to the void nucleation at the interfaces. Because of the decoration of δ phase at the grain boundaries, hydrogen-assisted cracking preferentially propagates along the grain boundaries. It is therefore suggested that the synergistic interplay of HELP mechanism and HEDE mechanism can be used to explain the embrittlement of the alloy.
Instrumented nanoindentation techniques have been widely used to characterize the small-scale mechanical behavior of materials. The elastic-plastic transition during nanoindentation is often indicated by a sudden displacement burst (pop-in) in the measured load-displacement curve. In defect-free single crystals, the pop-in is believed to be the result of homogeneous dislocation nucleation because the maximum shear stress corresponding to the pop-in load approaches the theoretical strength of the materials and because the statistical distribution of pop-in stresses is consistent with what is expected for a thermally activated process of homogeneous dislocation nucleation. This paper investigates whether this process is affected by crystallography and stress components other than the resolved shear stress. A Stroh formalism coupled with the two-dimensional Fourier transformation is used to derive the analytical stress fields in elastically anisotropic solids under Hertzian contact, which allows the determination of an indentation Schmid factor, namely, the ratio of maximum resolved shear stress to the maximum contact pressure. Nanoindentation tests were conducted on B2-structured NiAl single crystals with different surface normal directions. This material was chosen because it deforms at room temperature by {110}<001> slip and thus avoids the complexity of partial dislocation nucleation. Good agreement is obtained between the experimental data and the theoretically predicted orientation dependence of pop-in loads based on the indentation Schmid factor. Pop-in load is lowest for indentation directions close to <111> and highest for those close to <001>. In nanoindentation, since the stress component normal to the slip plane is typically comparable in magnitude to the resolved shear stress, we find that the pressure sensitivity of homogeneous dislocation nucleation cannot be determined from pop-in tests. Our statistical measurements generally confirm the thermal activation model of homogeneous dislocation nucleation. That is, the extracted dependence of activation energy on resolved shear stress is almost the same for all the indentation directions considered in this study, except for those close to <001>. Because very high pop-in loads are measured for orientations close to <001>, which implies a large contact area at pop-in, there is a higher probability of activating pre-existing dislocations in these orientations, which may explain the discrepancy near <001>.
The evolution of the cementite phase during wet wire drawing of a pearlitic steel wire has been followed as a function of strain. Particular attention has been given to a quantitative characterization of changes in the alignment and in the dimensions of the cementite phase. Scanning electron microscope observations show that cementite plates become increasingly aligned with the wire axis as the drawing strain is increased. Measurements in the transmission electron microscope show that the cementite deforms plastically during wire drawing , with the average thickness of the cementite plates decreasing from 19 nm ({epsilon} = 0) to 2 nm ({epsilon} = 3.7) in correspondence with the reduction in wire diameter. The deformation of the cementite is strongly related to plastic deformation in the ferrite, with coarse slip steps, shear bands and cracks in the cementite plates/particles observed parallel to either {l_brace}110{r_brace}{sub {alpha}} or {l_brace}112{r_brace}{sub {alpha}} slip plane traces in the ferrite.
Recovered pipe bomb fragments, exploded under controlled conditions, have been characterized using scanning electron microscopy, optical microscopy and microhardness. Specifically, this paper examines the microstructural changes in plain carbon-steel fragments collected after the controlled explosion of galvanized, schedule 40, continuously welded, steel pipes filled with various smokeless powders. A number of microstructural changes were observed in the recovered pipe fragments: deformation of the soft alpha-ferrite grains, deformation of pearlite colonies, twin formation, bands of distorted pearlite colonies, slip bands, and cross-slip bands. These microstructural changes were correlated with the relative energy of the smokeless powder fillers. The energy of the smokeless powder was reflected in a reduction in thickness of the pipe fragments (due to plastic strain prior to fracture) and an increase in microhardness. Moreover, within fragments from a single pipe, there was a radial variation in microhardness, with the microhardness at the outer wall being greater than that at the inner wall. These findings were consistent with the premise that, with the high energy fillers, extensive plastic deformation and wall thinning occurred prior to pipe fracture. Ultimately, the information collected from this investigation will be used to develop a database, where the fragment microstructure and microhardness will be correlated with type of explosive filler and bomb design. Some analyses, specifically wall thinning and microhardness, may aid in field characterization of explosive devices.
This paper presents a three dimensional image processing strategy that has been developed to quantitatively analyze and correlate the path of a fatigue crack with the lamellar microstructure found in Ti-6246. The analysis is carried out on X-ray microtomography images acquired in situ during uniaxial fatigue testing. The crack, the primary β-grain boundaries and the α lamellae have been segmented separately and merged for the first time to allow a better characterization and understanding of their mutual interaction. This has particularly emphasized the role of translamellar crack growth at a very high propagation angle with regard to the lamellar orientation, supporting the central role of colonies favorably oriented for basal 〈a〉 slip to guide the crack in the fully lamellar microstructure of Ti alloy. - Highlights: • 3D tomography images reveal strong short fatigue crack interaction with α lamellae. • Proposed 3D image processing methodology makes their segmentation possible. • Crack-lamellae orientation maps show prevalence of translamellar cracking. • Angle study comforts the influence of basal/prismatic slip on crack path.
A nanocrystalline surface layer was produced on Mg-3 wt.% Li-6 wt.% Al alloy by means of surface mechanical attrition treatment (SMAT). Microstructure features of various sections were systematically characterized by transmission electron microscopy. The results indicate that grain refinement induced by SMAT is dominated mainly by dislocation slip. Twinning is active at the early stage of grain refinement process when the grain size is large. The dislocation-dominated deformation mechanism is attributed to the change of c/a ratio due to the alloying of Li in Mg matrix and the suppression of twinning due to grain refinement. Nanoindentation results show that the hardness of the surface is enhanced by SMAT. - Highlights: •Nanocrystalline surface layer was produced on Mg-3 wt.%Li-6 wt.%Al alloy by SMAT. •Grain refinement induced by SMAT is dominated mainly by dislocation slip. •Twinning is active at the early stage of grain refinement process. •The hardness of the surface was enhanced by SMAT.
The tensile deformation behavior of laser welded Ti{sub 2}AlNb joints was investigated using in situ analysis methods. The fracture mode of the single-B2-phase fusion zone was quasi-cleavage at room temperature and intergranular at 650 °C, while that of base metal was microvoid coalescence at both room temperature and 650 °C. Tensile deformation at room temperature was observed using in situ SEM tensile testing. In base metal, microcracks nucleated and propagated mainly within the O phase or along O/B2 phase boundaries. While both the cross- and multi-slips were found in the single-B2-phase fusion zone, a confocal laser scanning microscopy was used to observe the crack initiation and propagation process in situ at 650 °C. Cracks mainly formed along the B2/O phase boundaries in base metal, along the fragile grain boundaries of B2 phase in the fusion zone. The thermal simulation experiment and following TEM analysis indicated that the precipitation of continuous O-phase films along the B2 grain boundaries resulted in the high temperature brittleness of laser welded Ti{sub 2}AlNb joints. - Highlights: •Cracks formed within O phase or along B2/O boundaries in the base metal. •Cross- and multi-slips relieved stress in the fusion zone at room temperature. •Cracks mainly formed along the B2/O boundaries at 650 °C. •In the fusion zone, intergranular cracks were in situ observed at 650 °C. •O-phase films along B2 grain boundaries caused the high temperature brittleness.
Highlights: • Nano-scale lamellar Al-Al{sub 2}Cu eutectic was synthesized by laser surface remelting. • Orientation relationship (OR) is {211}{sub Al2Cu}||{111}{sub Al} and <120>{sub Al2Cu}||<110>{sub Al.} • The OR has two variants, I has (001){sub Al2Cu}||{001}{sub Al} and II has (001){sub Al2Cu}||{111}{sub Al.} • Variant I is associated with low energy interfaces. - Abstract: A fully lamellar Al-Al{sub 2}Cu eutectic comprising alternate nano-scale α-Al and θ-Al{sub 2}Cu phases was synthesized through laser surface remelting of a cast Al-32.7 wt% Cu alloy. The orientation relationship between α-Al and θ-Al{sub 2}Cu phases was investigated from Kikuchi patterns obtained using electron backscattered diffraction (EBSD) and t-EBSD techniques. The characteristic orientation relationship (OR), {211}{sub Al2Cu}||{111}{sub Al} and <120>{sub Al2Cu}||<110>{sub Al}, was observed independent of interlamellar spacing. This OR has two variants where, besides the two parallel planes, the variant I exhibits (001){sub Al2Cu}||{001}{sub Al} and the variant II exhibits (001){sub Al2Cu}||{111}{sub Al}. Variant I prevails over variant II in laser-processed α-Al and θ-Al{sub 2}Cu nano-laminates, and atomistic modeling indicates that this is due to the low energy interfaces associated with variant I, i.e., {211}{sub Al2Cu}||{111}{sub Al} or (001){sub Al2Cu}||{001}{sub Al}. A comprehensive understanding of the crystallographic orientation relationships between two phases may help predict or explain the active slip systems in fine-scale Al-Al{sub 2}Cu eutectic and other cubic-tetragonal two-phase materials.
Graphical abstract: FESEM micrographs of the fresh fracture surfaces for the La{sub 0.80}Sr{sub 0.20}Cr{sub 0.92}Co{sub 0.08}O{sub 3} sintered specimens cast from optimised suspensions with 13.5, 15 and 17.5 vol.% solids loading. Aqueous suspensions were prepared using ammonium polyacrylate (PAA) as dispersant and tetramethylammonium hydroxide (TMAH) to assure a basic pH and providing stabilization. Sintering of the green discs was performed in air at 1600 {sup o}C for 4 h. Highlights: {yields} Optimum casting slips were achieved with 3 wt.% of ammonium polyacrylate and 1 wt.% of tetramethylammonium hydroxide. -- Abstract: Many studies have been performed dealing with the processing conditions of electrodes and electrolytes in solid oxide fuel cells (SOFCs). However, the processing of the interconnector material has received less attention. Lanthanum chromite (LaCrO{sub 3}) is probably the most studied material as SOFCs interconnector. This paper deals with the rheology and casting behaviour of lanthanum chromite based materials to produce interconnectors for SOFCs. A powder with the composition La{sub 0.80}Sr{sub 0.20}Cr{sub 0.92}Co{sub 0.08}O{sub 3} was obtained by combustion synthesis. Aqueous suspensions were prepared to solids loading ranging from 8 to 17.5 vol.%, using ammonium polyacrylate (PAA) as dispersant and tetramethylammonium hydroxide (TMAH) to assure a basic pH and providing stabilization. The influence of the additives concentrations and suspension ball milling time were studied. Suspensions prepared with 24 h ball milling, with 3 wt.% and 1 wt.% of PAA and TMAH, respectively, yielded the best conditions for successful slip casting. Sintering of the green discs was performed in air at 1600 {sup o}C for 4 h leading to relatively dense materials.
Small-diameter carbon nanotubes (CNTs) have outstanding mass-transport properties, especially enhanced water flow. Here, we report on water transport through the first macroscopic membranes with vertically oriented, subnanometer (0.8 nm) CNT pores, made by a scalable, solution-based method with electric-field alignment of bulk-grown single-wall CNTs (SWCNTs). After plasma etching to open pores, vertically aligned CNTs served as the primary pathway for liquid-water transport. The CNT membranes showed fast pressure-driven water transport, with up to 105-fold enhancement compared to no-slip Hagen–Poiseuille flow. Comparing 0.8 and 3 nm CNTs, we found that the hydrodynamic slip lengths increased with decreasing nanotube diameter, reaching 8.5 μm for the smaller-diameter CNTs. Here, the results suggest that pressure-driven water transport in small-diameter CNTs is increasingly dominated by entrance resistance, thus becoming independent of nanotube length. Scalably fabricated membranes incorporating vertically aligned subnanometer CNT pores could have applications in water filtration, desalination, and energy harvesting.