A microstructure-based modeling approach to predict the mechanical properties of Zr alloy with hydride precipitates

In nuclear reactors, hydrides can form in fuel cladding due to hydrogen absorption in ZIrcaloy and cause embrittlement. This work presents a microstructure-based finite element model to predict the stress-strain response of Zircaloy containing hydrides. Quantitative microstructural details extracted from scanning electron microscopy (SEM) images were used to generate heterogeneous microstructures including the morphology and spatial distribution of hydrides. The constitutive material model for zircaloy in this study is based on crystal plasticity theory which considers the hexagonal close-packed (HCP) atomic structure of Zircaloy material. The hydrides were modeled as brittle material along with a damage model. Hydride formation inside the zircoloy matrix results in residual stress. This phenomenon is also captured in this model. A parametric study has been conducted to understand the effect of volume fraction, orientation, and lamellae thickness of the hydride phase on the mechanical properties of the overall material.

Kulkarni, Shank S.↗

Transverse impact by RCCs on S-glass and Kevlar® FRC strips

This study aims to isolate interactions between plies and tows and reveal fundamental physics involved in transverse impact on fiber-reinforced composite (FRC) structures. Composite strips were sectioned from large panels and characterized by optical photography, three-dimensional synchrotron X-ray computed tomography, and scanning electron microscopy (SEM). Each strip was impacted perpendicularly by a right circular cylinder (RCC) projectile at a velocity ranging from ~ 150 to 600 m/s. The global strip behavior, as well as localized deformation and failure of the strip near the projectile corner, were both captured by high-speed optical imaging. S-Glass FRC strips were observed to fail in tension ahead of the RCC projectiles’ flat surfaces while Kevlar® FRC strips fractured at the projectile corners. The concept of critical velocity region previously used for impact on yarns was introduced to define different failure modes of each composite strip type. The strip damage extent was found to increase with the impact velocity and reach the maximum at the upper limit of the critical velocity region. Above the critical velocity region, the damage extent decreased with impact velocity. Wave propagations and load histories in the composite strips during impact were quantified and compared with Smith’s theory. Finally, critical velocities of single fibers, yarns, and composite strips and ballistic limits of single-ply and multi-ply composite panels were compared to provide insight into the design of impact-resistant fabrics and composites.

42 ENGINEERING↗

Sizing comingled CF/PA 6 fibers with cellulose nanofibrils for enhanced performance properties

Compatibility between the reinforcing phase and the polymer matrix is critical to achieving the desired mechanical and thermal performance of composite materials. Several mechanisms can enhance this interfacial interaction, including surface treatments (e.g., oxidation, plasma, or irradiation), in-situ nanoparticle deposition, and fiber sizing. Here, in this study, cellulose nanofibrils (CNF) were employed as a sustainable sizing agent to modify the interface in commingled carbon fiber (CF)/polyamide 6 (PA 6) yarns, in which CF and PA6 filaments are intimately blended to enable simultaneous consolidation. A 0.25 wt% CNF aqueous suspension was applied under bath sonication to ensure uniform dispersion and minimize agglomeration. CNF-sized and unsized yarns were used to fabricate unidirectional composite plates via filament winding on a flat mandrel, followed by compression molding. Scanning electron microscopy confirmed CNF presence on both CF and PA6 filaments. CNF-sized composites exhibited increments in interlaminar shear strength (ILSS) by 50%, flexural strength by 11%, and tensile strength by 2.5% compared to unsized composites. Thermal analysis showed minimal changes in degradation temperature and crystallinity. These findings demonstrate that CNF sizing enhances interfacial bonding and mechanical performance, offering a scalable and environmentally friendly strategy for thermoplastic composite manufacturing along with yarn/tow handleability.

Cellulose nanofibrils (CNF)↗

Influence of plasticizers on thermal and mechanical properties of biocomposite filaments made from lignin and polylactic acid for 3D printing

Polylactic acid (PLA) and organosolv lignin were mixed at different ratios and extruded to obtain PLA-lignin composite filaments. PLA was replaced with lignin up to 20 wt%. Two plasticizers (polyethylene glycol (PEG) 2000 and struktol TR451) were added in varying concentrations to enhance the properties of PLA_L20 (20% lignin in PLA) composite filaments. Furthermore, the effect of lignin in PLA, and PEG, and struktol in PLA_L20 composites was investigated via tensile test, differential scanning calorimetry, thermogravimetric analysis, scanning electron microscopy, Fourier transform infrared spectroscopy of the filaments, and dynamic mechanical analysis of 3D printed samples. A 2 wt% PEG was able to enhance both tensile stress and elongation at maximum load of PLA_L20 composite by 19% and 35%, respectively, whereas struktol TR451 was able to improve elongation at maximum load by 24%.

3D printing↗

Processing and mechanical characterization of short carbon fiber-reinforced epoxy composites for material extrusion additive manufacturing

Fiber-reinforced polymer composites have been extensively utilized in recent years as feedstock materials for material extrusion additive manufacturing (AM) processes to improve strength, stiffness, and functionality of printed parts over unfilled printed polymers. However, the widespread adoption of AM of fiber-reinforced polymer composites requires a deeper understanding of the process-structure-property relationships in printed components, and such relationships are not well understood yet. Fiber length is critically important to the mechanical performance of short fiber composites, but very few studies to-date have focused on how the fiber length distribution (FLD) evolves during processing of composite feedstocks and how this evolution affects printing behavior and mechanical properties in 3D-printed composites. Here, FLD is measured for carbon fiber reinforced epoxy composites over a wide range of ink compositions and shear mixing times, and the distributions are fit with a Weibull-type distribution function. The effects of FLD on the tradeoff between ink processability, ink rheology, printing behavior and mechanical properties are investigated. Furthermore, the effects of printing parameters (nozzle size and print speed) on mechanical anisotropy and fiber orientation distribution (FOD) in printed composites are explored. Mechanical properties of printed composites are characterized via 3 pt-flexural testing, and microstructure is investigated using optical and scanning electron microscopy (SEM), and x-ray computed tomography. Finally, the fitted Weibull parameters are fed into a composite model that incorporates FLD and FOD, and model predictions are found to be in excellent agreement with experimental observations.

3D printing↗

Degradation mechanism of blended cement pastes in sulfate-bearing environments under applied electric fields: Sulfate attack vs. decalcification

Applied electric fields, the reason behind stray currents, accelerate the ingress of sulfate into cementitious materials. To identify mitigation approaches, this study investigates the effects of slag and fly ash on sodium sulfate attacks of cement pastes under a constant electric current. The mineralogical alterations induced by the attacks were analyzed using X-ray diffractometry, thermogravimetric analysis, scanning electron microscopy, and thermodynamic modeling. The dissolution of aluminates in the slag and fly ash induced a monosulfate-rich area (>~20 mm from the cathode surface) to form next to the ettringite-rich area on the sample surface (<~20 mm). This effect reduced the availability of SO 4 2– in the pore solution, thereby hindering the penetration of sulfate. Meanwhile, the consumption of portlandite by the pozzolanic reaction lowered the decalcification resistance of the materials. This produced a wide area that endured the decomposition of portlandite and carbonate-AFm. Altogether, blending 30% fly ash did not improve the resistance of the material to either sulfate attacks or decalcification; blending 50% slag can effectively mitigate sulfate ingress, though decalcification may become a governing mechanism in the degradation process.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effects of graphene surface functionalities towards controlled reinforcement of a lignin based renewable thermoplastic rubber

In this report, we describe methods to enhance mechanical properties of a renewable thermoplastic rubber by incorporating functional graphene platelets into an equal-mass mixture of lignin, a feedstock from plant biomass, and a nitrile-butadiene rubber having 41 mol % acrylonitrile content (NBR41) that form a nanocomposite. Not all lignins yield mechanically strong material when they are combined with NBR41, and thus, limit its use for such rubbery products. Here, we evaluate different graphene oxides (GO) and reduced graphene oxides (rGO) dry-powders with different surface areas, functionality, and wettability in the synthesis of performance-enhanced nanocomposites of soft lignin/NBR41 matrix via a solvent-free, high shear reactive process. High surface area GO (HSGO) platelets with strong hydrophilicity exhibit good dispersion in the multiphase lignin/NBR41 composites with lignin dispersion varying from 200 to 2000 nm, resulting in superior reinforcement over other graphene derivatives. The addition of 1–4 wt % HSGO increased the tensile stress of the lignin/NBR41 thermoplastic rubber matrix by 60–160% (15–24 MPa) and the modulus by 200–700% (60–140 MPa). Scanning electron microscopy and small angle X-ray scattering results show that the well-dispersed HSGO platelets effectively disrupt the lignin-rich aggregates in NBR41 matrix, resulting in both strength and stiffness enhancements in the formed nanocomposites. This report on performance enhancement of lignin-based renewable polymers via the production of nanocomposite would increase potential for ‘finding the value of lignin’—a grand challenge associated with modern biorefineries.

36 MATERIALS SCIENCE↗

Internal arcing and lightning strike damage in short carbon fiber reinforced thermoplastic composites

Short carbon fiber reinforced thermoplastic composites (S-CFRTP) are currently used in interior parts of aircraft such as electronic circuitry and assemblies, and their usage in aircraft's exterior is also being studied. In this paper, we present a lightning strike study on S-CFRTPs. High performance thermoplastics such as a polyphenylene sulfide (PPS) reinforced with 50% weight (wt.) short carbon fiber (CF), a polyphenyl sulfone (PPSU) reinforced with 25 % wt. Short CF and a acrylonitrile butadiene styrene (ABS) with 20 % wt. short CF were tested against artificial lightning strikes. All samples were prepared using an extrusion compression molding (ECM) technique. A modified component A (100 kA) of lightning waveform, as defined by SAE ARP 5412-B, was applied. High speed imaging, thermography, scanning electron microscopy (SEM) and ultrasonic non-destructive evaluation were performed to understand the effect of lightning strikes on the thermoplastic panels. The results show that electrical conductivity of the composite, thermal stability of the polymers, and CF orientation significantly affected the damage from artificial lightning strikes. PPS composite had the highest resilience against lightning strike damage, retaining 95% and 89% residual flexural strength and modulus, respectively. CF exfoliation due to internal arcing was observed in the carbon fiber-reinforced ABS polymer (CF-ABS) composite. CF exfoliation damage has been reported for the first time.

36 MATERIALS SCIENCE↗

High-speed synchrotron X-ray phase-contrast imaging for evaluating microscale damage mechanisms and tracking cracking behaviors inside cross-ply GFRCs

In this study, we integrated the high-speed synchrotron X-ray phase-contrast imaging (PCI) with a modified Kolsky compression bar loading platform to visualize the dynamic failure processes of cross-ply glass fiber reinforced composites (GFRCs). Four S-2 glass/SC-15 composite specimens were prepared, having similar thicknesses but different stacking sequences, namely as [0 12 /90 12 ], [90 12 /0 12 ], [0 8 /90 8 /0 8 ], and [90 8 /0 8 /90 8 ]. Three-dimensional synchrotron X-ray computed tomography and scanning electron microscopy (SEM) were employed to examine the microstructures and quantify the fiber volume fractions. Each specimen was notched and subjected to a dynamic three-point flexural loading. The onset of cracking close to the notch tip, crack propagation in 0° or 90° plies and their interface, crack opening, and ultimately failure of the specimen were captured by high-speed synchrotron X-ray PCI. Additional dynamic experiments were performed to determine the average time when the stress wave propagated through the specimen and correlate the X-ray images with the specimen&#x27;s force-deflection response. Finally, the surface morphology of each specimen after the dynamic loading was imaged by SEM. Comparison between real-time X-ray images and post-fracture SEM images demonstrated the capability of the X-ray method to record damage evolution inside composites. Furthermore, the high spatial and temporal resolutions of the X-ray setup and edge enhancement by PCI enabled the identification of microscale damage features within 1 μs. Two damaging processes were identified, crack growth was quantified, and fracture toughness of the composites was evaluated. The method is deemed useful to reveal microscale damage mechanisms and track cracking behaviors inside cross-ply GFRCs under dynamic loading in real time.

42 ENGINEERING↗

Degradation in interfacial shear strength of carbon fiber/ vinyl ester composites due to long-term exposure to seawater using push-out tests

Here, in this study, single fiber (~7-μm diameter) push-out tests are conducted to evaluate hygrothermal effects on the interfacial shear strength (IFSS) of carbon fiber/vinyl ester (CF/VE) composites. Hygrothermal conditioning is achieved by saturating samples in simulated seawater at 40 °C for two years. An investigation has been conducted on the preparation, validity, and interpretation of the push-out test results. First, the authors present a polishing methodology that results in thin films of CF/VE composites in the thickness range of 15–120 μm and produces an average 41.2% drop in IFSS due to long-term hygrothermal exposure. Using scanning electron microscopy (SEM), we show that during the push-out tests, the failure initiates locally at the zone of minimum bond strength at the bottom (away from the indenter), then propagates along the length of the interface. The influence of radial tensile stresses originating due to bending is found to be negligible. Using the SEM imaging of the pushed-out fibers, we validate the failure of the interface to be the primary source of failure. The associated results are found to depend on the thickness of the interface. We then reevaluate the results using the Weibull distribution, knowing that the failure mechanism is analogous to the weakest link theory. The results show a 25.5% drop in the IFSS of the CFVE composite, measured at an infinitesimal scale due to long-term to hygrothermal conditioning at 40 °C. A significant drop in IFSS was observed after reheating above glass transition temperature (T g ) and cooling.

36 MATERIALS SCIENCE↗

Microstructure and corrosion of CrFeMnV multi-principal element alloy

In this study, a multi-principal element alloy consisting of equiatomic concentrations of Cr, Fe, Mn, and V was produced by arc melting. The combination of X-ray diffraction, scanning electron microscopy and energy-dispersive X-ray spectroscopy indicated that the CrFeMnV MPEA was comprised of a BCC matrix with a dispersion of a secondary phase. Cyclic potentiodynamic polarization tests in 0.6M NaCl revealed high corrosion resistance – superior to that of stainless steel 304L, as evident from high breakdown and repassivation potentials. X-ray photoelectron spectroscopy and time-of-flight secondary ion mass spectrometry provided insight into the formed multi-layer surface film after constant immersion and potentiostatic conditioning.

36 MATERIALS SCIENCE↗

Reverse martensitic transformation on the corrosion behavior of a 2304 lean duplex stainless steel

This study investigates the influence of the reverse martensitic transformation on the corrosion behavior of 2304 lean duplex stainless steel (LDSS) at low temperatures (400–600°C). The steel underwent cold rolling, followed by isochronal annealing for 0.5 h. Phase transformations and microstructures were analyzed using X-ray diffraction, scanning electron microscopy, and transmission electron microscopy. Corrosion resistance was evaluated using a syringe cell with cyclic potentiodynamic polarization in 0.6 M NaCl solution and double-loop electrochemical potentiokinetic reactivation in 0.5 M H 2 SO 4 + 0.001 M KSCN solution. A bimodal breakdown potential behavior, associated with either pitting or transpassivity, was observed in the as-received (AR) and samples annealed at 400°C. Pitting in the AR sample was associated with Al–Mg–Si–Ca–O inclusions, while pitting on the samples annealed at 400°C was linked to local reduced passive film resistance. Severe cold rolling enhanced the pitting resistance of 2304 LDSS. Selective electrochemical etching revealed preferential corrosion at phase interfaces and within the austenite phase. Additionally, annealing at 500°C to 600°C led to a marked decrease in pitting resistance and increased sensitization. Electron backscatter diffraction analysis of the corroded pits in the annealed specimens indicated that pits tend to nucleate and grow in α'-martensite/austenite regions. Furthermore, the nanostructure formed during low-temperature reversion, characterized by dislocation-cell martensite with high dislocation density and stacking faults, may adversely affect corrosion resistance due to heterogeneities associated with alloying element redistribution.

36 MATERIALS SCIENCE↗

Mechanistic transition of stainless steel 304L corrosion in MgCl 2 phase change material under thermal cycling

Magnesium chloride (MgCl 2 )-based molten salt phase change materials (PCMs) are promising candidates for thermal energy storage (TES) owing to their advantageous thermophysical properties, however, their high corrosivity in the molten state limits material compatibility. In this study, the corrosion behavior of 304?L stainless steel (SS304L) exposed to MgCl2 PCM was investigated as a function of thermal cycling (up to 9000 cycles) relevant to PCM-based TES systems. Microstructural changes and elemental redistribution at the alloy-salt interface under thermal cycling conditions were characterized using synchrotron-based X-ray fluorescence (XRF) and scanning electron microscopy coupled with energy dispersive X-ray spectroscopy (SEM-EDS). Results show that corrosion is governed by selective Cr-dissolution and elemental diffusion near the interface and grain boundaries. A clear transition in the dominant corrosion mechanism is observed with increasing thermal cycles. Surface corrosion is the dominant mechanism up to 1000 cycles, whereas intergranular corrosion becomes the primary degradation mode beyond 2000 cycles. These mechanistic changes are interpreted in terms of evolving interfacial chemistry, microstructure and the diffusion-driven redistribution of alloying elements.

36 MATERIALS SCIENCE↗

Adaptations for gas exchange enabled the elongation of lepidopteran proboscises

The extensive biodiversification of butterflies and moths (Lepidoptera) is partly attributed to their unique mouthparts (proboscis [Pr]) that can span in length from less than 1 mm to over 280mm in Darwin's sphinx moths. Lepi-doptera, similar to other insects, are believed to inhale and exhale respiratory gases only through valve-like spi-racles on their thorax and abdomen, making gas exchange through the narrow tracheae (Tr) challenging for the elongated Pr. How Lepidoptera overcome distance effects for gas transport to the Pr is an open question that is important to understanding how the Pr elongated over evolutionary time. Here, we show with scanning electron microscopy and X-ray imaging that distance effects on gas exchange are overcome by previously unreported micropores on the Pr surface and by superhydrophobic Tr that prevent water loss and entry. We find that the density of micropores decreases monotonically along the Pr length with the maxima proportional to the Pr length and that micropore diameters produce a Knudsen number at the boundary between the slip and transition flow regimes. By numerical estimation, we further show that the respiratory gas exchange for the Pr predominantly occurs via diffusion through the micropores. In conclusion, these adaptations are key innovations vital to Pr elongation, which likely facilitated lepidopteran biodiversification and the radiation of angiosperms by coevolutionary processes.

59 BASIC BIOLOGICAL SCIENCES↗

Characterization of thermally heat-treated polyacrylonitrile carbon fibers

This study investigates the graphitization process of polyacrylonitrile (PAN) carbon fibers by subjecting commercial fibers to thermal heat treatment at temperatures ranging from 1400 to 2100 °C in 100 °C increments, using either argon or nitrogen gas atmospheres. Changes in crystallinity, surface morphology, and lattice parameters were analyzed for two commercial carbon fibers using X-ray diffraction, scanning electron microscopy, and Raman spectroscopy. Results indicated minimal changes in surface morphology with increasing heat-treatment temperature; however, crystallinity significantly increased. Crystallinity changes were more strongly dependent on temperature rather than gas atmosphere or fiber type. At intermediate heat-treatment temperatures (1600–1800 °C), fibers treated in argon showed a slight preference for graphitization. The highest level of graphitization was measured at 2100 °C. Crystallite size increased as the intensity ratio of the D1 to G Raman peaks increased, reaching a peak around ~1800 °C, after which the ratio started to decrease. This behavior aligns with Ferrari's three-stage model of carbon crystallization and is consistent with both the Marie-Mering degree of graphitization and Brubaker's Integrated Absolute Differential models, all of which describe the transformation from an amorphous to a more graphitic structure. At the higher heat-treatment temperatures, the changes between atmospheres and fiber types were measured to converge to similar levels of graphitization. In conclusion, this study evaluates the progressive change in commercial grade carbon fibers when heat-treated.

Characterization↗

Electrolytic recovery of metals from lithium battery cathodes in moisture-tolerant molten hydroxide salt

Lithium-ion battery recycling offers an opportunity to develop innovative technologies to close the loop on the battery materials cycle and increase the resilience of the battery supply chain. Here, in this study, we demonstrate a two-step pyroelectrochemical method for producing mixed-metals from lithium-ion cathodes in a molten hydroxide salt. Mixed metal oxides in the form of insoluble lithium-ion cathode materials of LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) and spent lithium-ion battery materials (black mass) were electrochemically reduced to a soluble form and dissolved into a molten hydroxide salt bath. Electrochemical characterization of the process salt indicated accumulation of dissolved transition metals in the salt. A separate cathode was used to produce alloys of Ni, Mn, and Co electrochemically from the dissolved lithium-ion cathode materials. Characterization by scanning electron microscopy fitted with an energy dispersive X-ray spectrometer showed transition metals present in the cathode materials were recovered at the separate cathode. This approach represents a scalable, low temperature pyroelectrochemical process that can potentially reduce the cost and close the loop of battery cathode recycling.

25 ENERGY STORAGE↗

Effect of temperature and aging duration on ethylene propylene diene monomer (EPDM) nonmetallic components used in caustic liquid waste transfer lines

Nonmetallic materials are used in waste transfer lines at the United States Department of Energy’s Hanford Site Tank Farm in Benton County, Washington, USA. During use, the ethylene propylene diene monomer (EPDM) inner hose of the hose-in-hose transfer lines (HIHTLs) are exposed to β and γ radiation, caustic solutions as well as high temperatures and high pressures. Aging behavior of specimens of EPDM HIHTLs and dog-bone shaped specimens were evaluated by exposing to a solution of 25% sodium hydroxide (NaOH) at 38 °C, 54 °C and 77 °C for 6 and 12-months as well as water only at 77 °C for 12-months. Tensile strength and burst pressure of the specimens were characterized and compared with the unexposed (baseline) specimens. Both the tensile strength of the EPDM material and the burst pressure of the HIHTLs significantly decreased with the higher temperatures and longer exposure times. Analyses using scanning electron microscopy with energy dispersive X-ray spectroscopy (SEM-EDS) of the HIHTLs and the dog-bone specimens were conducted. Our results show that the surface degradation increased with increasing exposure temperature. Penetration of NaOH into the EPDM material also increased with increasing temperature and exposure duration.

36 MATERIALS SCIENCE↗

Effect of solution concentration on ethylene propylene diene monomer (EPDM) nonmetallic components used in caustic liquid waste transfer lines

The hose-in-hose transfer lines (HIHTL) used to transfer waste at the United States Department of Energy’s Hanford Site Tank Farm are fabricated from an ethylene propylene diene monomer (EPDM) synthetic rubber. During waste transport, these hoses are exposed to several stressors including caustic solutions at high temperatures and high pressures, as well as β and γ radiation. The aging behavior of HIHTL and dog-bone shaped EPDM specimens were evaluated by exposure to solutions at 77 °C containing 0.00, 6.25, 12.50, and 25.00 % (v/v) sodium hydroxide (NaOH) for 12-months. After the exposure, the material properties of the specimens were measured and compared to the unaged samples. The material properties evaluated included the tensile strength of the EPDM dog-bone samples and the burst pressure of the HIHTL. Both the tensile strength of the EPDM dog-bone samples and the burst pressure of the HIHTL specimens exposed to the 6.25 % NaOH solution exhibited the most significant deterioration and those exposed to 25.00 % NaOH solution had the least deterioration. Finally, examination of the HIHTL and the EPDM dog-bone specimens with scanning electron microscopy showed that the deterioration for the specimens exposed to 6.25 % NaOH solution were the most severe and the samples exposed to 25.00 % NaOH solution had the least deterioration.

42 ENGINEERING↗