Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ROLLING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 775 records · Page 43

Hot Forging Options for Thick Castings

Uranium alloyed with 10 wt% molybdenum (U-10Mo) is a monolithic nuclear fuel relevant to the National Nuclear Security Administration’s nonproliferation efforts. Research has been underway to optimize processing techniques for the U-10Mo fuel. This study investigated the use of hot compression or “hot forging” on a thick (~1") cast and homogenized U-10Mo plate before standard hot and cold rolling procedures. After plates were cast and homogenized, six samples were cut and forged at 700°C at a strain rate of either 0.10 s –1 or 0.01 s –1 at six levels of reduction. After forging, all samples underwent hot and cold rolling followed by annealing to achieve a final foil thickness of about 0.0085". Samples were taken at each stage of the casting and thermomechanical processing to assess the microstructural evolution. Chemical composition, microstructure, and uranium carbide morphology are presented and assessed in this study. Upon hot forging, dislocations accumulate along the grain boundaries, which serve as nucleation sites for randomly oriented, strain-free grains during subsequent annealing steps. Hot forging and subsequent annealing produced very heterogeneous grain sizes. However, no molybdenum segregation was observed after forging. No obvious trend was observed between forging conditions (strain rate and reduction percentage) and the microstructure after final thermomechanical processing. Upon hot rolling to 0.04" and annealing (700°C for 45 min), the average grain diameters from OM was 17 ± 2 µm across the six different forged samples. The subsequent cold rolling to 0.0085" and then annealing (700°C for 45 min) resulted in an average of 13 ± 2 µm between the six samples. Thus, the starting, as-forged microstructure did not appear to significantly influence the final microstructure of the cold-rolled foil. These results will help with understanding and expanding hot working capabilities for thicker U-10Mo castings. They also provide useful information on the effects of hot forging and its potential use to minimize defects that can arise during subsequent hot and cold rolling procedures.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

PNNL's Intermediate Characterization Summary for the MP-1 Experiment

Characterization of the as-fabricated fuel is being performed at Pacific Northwest National Laboratory (PNNL) in accordance with Characterization Plan for the Fabrication of U-10Mo for the MP-1 Experiment, hereinafter the MP-1 Characterization Plan. Similar characterization work is also being performed at two other organizations, INL and Los Alamos National Laboratory, to provide a detailed understanding of the as-fabricated fuel that would be irradiated in the MP-1 experiment. Under the MP 1 Characterization Plan, fuel foils with different fabrication parameters (such as rolling condition, rolling thickness reduction, co-rolling with Zr layers) are being studied. Similar samples from master foils were sent to each of the three organizations, so that testing and analysis can be performed independently using similar equipment and a standardized set of measurement and analysis procedures. A final consolidated report will be prepared based on this work and it will summarize all of the information obtained from different labs. The MP-1 experiment will provide an opportunity to understand the effects of processing conditions on the final fuel microstructure, to compare results obtained independently, and achieve a three-way validation. Currently, PNNL characterized 28 U-10Mo samples, by sectioning six pieces/specimens from each sample/foil, in accordance with the MP-1 Characterization Plan. These 28 samples consist of six types of MP-1 characterization foils from BWXT: 0.047 in. thick hot-rolled samples with and without Zr layers; 0.02 in. thick cold-rolled and annealed samples with and without Zr layers, and 0.01 in. thick cold-rolled and annealed samples with and without Zr layers. During the first year, PNNL completed sectioning of two subsamples per sample/foil and performed the necessary characterization on all 28 U-10Mo samples. This report covers the results of the first year’s analyses of PNNL’s MP-1 fuel characterization samples. Microstructure, chemical composition, carbide morphology, U-10Mo foil thickness, Zr thickness, mechanical properties (microhardness), and density were evaluated in both longitudinal and transverse directions for foils of the three different thicknesses.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Low-Cost Flexible Electrochromic Film for Energy Efficient Buildings

Broad Funding Opportunity Announcement Project: ITN is addressing the high cost of electrochromic windows with a new manufacturing process: roll-to-roll deposition of the film onto flexible plastic surfaces. Production of electrochromic films on plastic requires low processing temperatures and uniform film quality over large surface areas. ITN is overcoming these challenges using its previous experience in growing flexible thin-film solar cells and batteries. By developing sensor-based controls, ITN’s roll-to-roll manufacturing process yields more film over a larger area than traditional film deposition methods. Evaluating deposition processes from a control standpoint ultimately strengthens the ability for ITN to handle unanticipated deviations quickly and efficiently, enabling more consistent large-volume production. The team is currently moving from small-scale prototypes into pilot-scale production to validate roll-to-roll manufacturability and produce scaled prototypes that can be proven in simulated operating conditions. Electrochromic plastic films could also open new markets in building retrofit applications, vastly expanding the potential energy savings.

ARPA-E↗

High Volume Production of Nanoscale Elements

The utility of nanoscale elements spans numerous potential markets including healthcare, communications, energy, optics, and structures. The energy market in particular will require large volumes and is price sensitive. In this talk we will discuss strategies to scale nanoscale elements, including nanoparticle inks and nanoscale thin films, for the large area deposition (hundreds of square meters) using high through put processes. Historically, roll-to-roll production of thin films has been carried out at very high speeds over large areas using solution phase inks. Nanoparticles are produced in a bottom-up approach in solution phase that simplifies the processing and is amenable to ink formulations. Sintering and annealing of the thin films can be increased by using radiation thermal processing that integrates easily into roll-to-roll manufacturing. Results of printed films on the order of tens of nanometers to hundreds of nanometers are presented including studies of morphologies and uniformity over large areas. Solar cells devices using the roll-to-roll setup are demonstrated and a techno-economic analysis of the manufacturing is proposed. These results are presented with a comparison to the current photovoltaic technologies in production.

Druffel, Thad↗

CRACK GROWTH RESPONSE OF ALLOY 690 IN SIMULATED PWR PRIMARY WATER

The stress corrosion crack growth response of three extruded alloy 690 CRDM tube heats was investigated in several thermomechanical conditions. Extremely low propagation rates (< 1 x 10{sup -9} mm/s) were observed under constant stress intensity factor (K) loading at 325-350 C in the as-received, thermally treated (TT) materials despite using a variety of transitioning techniques. Post-test observation of the crack-growth surfaces revealed only isolated intergranular (IG) cracking. One-dimensional cold rolling to 17% reduction and testing in the S-L orientation did not promote enhanced stress corrosion rates. However, somewhat higher propagation rates were observed in a 30% cold-rolled alloy 690TT specimen tested in the T-L orientation. Cracking of the cold-rolled material was promoted on grain boundaries oriented parallel to the rolling plane with the % IG increasing with the amount of cold rolling.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

The Effect of Homogenization Heat Treatment on the Texture Evolution in U-10Mo Alloy

Uranium alloyed with 10 wt% Mo (U-10Mo) undergoes discontinuous precipitation (DP) when subjected to sub-eutectoid heat-treatment. It is hypothesized that the crystallographic texture of the U-10Mo can be modified to minimize the degree of DP, however the evolution of texture throughout the manufacturing process is not well understood. Crystallographic textures of two U-10Mo samples homogenized at 900°C and 1000°C were studied after uniaxial rolling and annealing. A total of 6 samples were analyzed upon rolling using a combination of hot and cold rolling conditions to strains of 83%, 90% and 97% and subsequently annealed at 700°C for one hour. Microstructures and textures were analyzed via electron backscatter diffraction (EBSD) for each homogenization, strain and post-annealed states. Results show that the U-10Mo exhibits typical rolling textures seen in body-centered cubic materials with increasing intensities of both a- and ?-fibers with increasing strain. After recrystallization, the texture appeared to be effectively randomized in all samples. Homogenization temperature showed no effect on the rolling and recrystallization behavior. Potential factors leading to the randomization of texture are discussed along with the implications of textures on the minimization of DP.

nuclear fuel, texture, rolling↗

Effect of Wear on Surface Crack Propagation in Rail–Wheel Wet Contact

The interaction between wear and rolling contact fatigue in wet contact was investigated by means of experiments on a two-disk test bench. Specimens of various railway wheel steels were coupled with specimens of the same rail steel, subjected to rolling and sliding wet contact with varying sliding/rolling ratio. Some tests with a dry rolling–sliding contact phase preceding wet contact were carried out as well (dry–wet tests). The pressurization of the fluid entrapped in the surface cracks was the cause of a rapid and severe damage in the dry–wet tests, due to the nucleation of surface cracks by ratcheting in the dry phase, which subsequently propagate in the wet phase. In the wet tests, the fluid pressurization effect was much mitigated due to the absence of initial surface cracks; the specimens subjected to higher sliding/rolling ratio showed the best performance against rolling contact fatigue, due to the effect of wear in reducing the length of surface cracks. A model for assessing the interaction between wear and rolling contact fatigue was proposed, based on the correction of the classical Paris law for crack propagation by taking into account the effect of wear on crack length reduction. The application of the model to the experimental tests allowed finding a correlation between the model predictions and the occurrence of fatigue failure.

36 MATERIALS SCIENCE↗

Influence of Local Inhomogeneity of Thermomechanical Treatment Conditions on Microstructure Evolution in Aluminum Alloys

The influence of local inhomogeneity of the stress–strain condition on structure and texture evolution during thermomechanical treatment of aluminum alloys is studied in this work. For this purpose, laboratory rolling and plane strain tests that simulated roughing mill thermomechanical modes were performed. For all processes, the local inhomogeneity of structure evolution was estimated. For this purpose, x-ray texture analysis, EBSD and optical microscopy were used. Additionally, the calculations which allow to evaluate local inhomogeneity of stress–strain conditions for the each process were performed. The experimental results were compared with mathematical simulation output. They indicated structure and texture evolution inhomogeneities, especially during the plane strain and industrial rolling processes. In the plane strain test, typical local deformation zones occurred with different resulting grain size and texture effects than those observed in both rolling processes. This difference was mainly associated with different stress states, strain intensity and strain rate distribution throughout the deformation zone. This study demonstrated that the inhomogeneity of these parameters has a strong impact on structure and texture evolution in the first stage of thermomechanical treatment. In the center layer, laboratory rolling could adequately generate the structure and texture effects observed during rolling of ingots in a commercial mill. Plane strain tests can generate useful results only in the case of adequate choice of sample geometry.

36 MATERIALS SCIENCE↗

The Evolution of Deformation-Induced Carbides during Divorced Eutectoid Transformation in GCr15 Steels

A series of rolling experiments were carried out using GCr15 steel to investigate the effect of initial microstructure on the spheroidizing process, and especially the effect of deformation-induced carbides (DIC) on the divorced eutectoid transformation (DET). The results indicated that the existence of DIC was beneficial to the spheroidizing process, the optimal initial microstructure for DET was lamellar pearlite, and DIC precipitated at grain boundaries. The average thickness of the cementite lamella and the size of DIC decreased with a decrease in rolling temperature in the critical temperature region. When the specimen was rolled at 1053 K, a small amount of DIC of size ~ 1 μm precipitated at grain boundaries. In contrast, the amount of DIC was increased when the rolling temperature was decreased to 1023 K, whereas the size of DIC was reduced to ~ 0.5 μm. Interrupted quenching experiments indicated that DIC (M{sub 7}C{sub 3}) were transformed to M{sub 3}C during the process of partial austenitization, and the evolution of spheroidization was influenced by the variation in the initial microstructure. For the specimens rolled at 1023 K, only ~ 60 min was needed to achieve the dissolution of DIC, which was the minimum, and the total time needed to achieve spheroidization was reduced to ~ 90 min.

36 MATERIALS SCIENCE↗

Microstructure, texture evolution and magnetic properties of strip-casting non-oriented 6.5 wt.% Si electrical steel doped with cerium

A 0.3 mm thick non-oriented 6.5 wt.% Si electrical steel sheet doped with cerium is produced by twin-roll strip casting, hot rolling, warm rolling and annealing. A detailed study of the cerium precipitates in the as-cast strip, microstructure and texture evolution at different processing stages is carried out by electron probe micro-analysis, optical microscopy, X-ray diffraction and electron backscattered diffraction analysis. Grain interior distributing precipitates identified as Ce-oxides, Ce-oxysulfides and Ce-phosphides, and boundary distributing Ce-oxides and Ce-phosphides are observed in the as-cast strip. The initial as-cast strip is characterized by a much finer solidification microstructure and dominated by obvious < 001 >//ND texture through the strip thickness. After hot and warm rolling, inhomogeneous microstructure containing large amounts of in-grain shear bands is characterized by mixed < 110 >//RD and < 111 >//ND textures. The texture of the annealed sheet with a relatively large average grain size is far more optimized by the domination of the beneficial cube, rotated cube, (001)< 120 > to (001)< 130 > and Goss texture components, and the elimination of the detrimental γ-fiber texture, leading to a superior magnetic induction and improved iron loss. - Highlights: • An Fe–6.5 wt.% Si as-cast strip doped with cerium was produced. • A thin warm rolled sheet with limited edge cracks was obtained. • Microstructure and texture evolution at each stage were investigated. • Strong λ-fiber and Goss recrystallization textures were formed. • The magnetic properties of the annealed sheet were significantly improved.

36 MATERIALS SCIENCE↗

Annealing texture of nanostructured IF steel

In the present work, the evolution of annealing texture in nanostructured interstitial free steel fabricated via accumulative roll bonding (ARB) process was investigated. Textural evolution after post-annealing of ARB-processed samples was evaluated using X-ray diffraction. There were several texture transitions in the γ-fiber and ζ-fiber during ARB and post-annealing treatment. It was found that with increasing the number of ARB cycles, the volume fraction of the low angle grain boundary decreased and the high angle grain boundary fraction increased. Also, the shear texture was dominant after the first cycle, while for other samples, the rolling texture was dominant. The one-cycle sample clearly indicated a weak α-fiber and γ-fiber and a relatively strong ζ-fiber. In addition, during the recrystallization and before the grain growth, the intensity of α-fiber and γ-fiber decreased, the intensity of ζ-fiber increased, and the intensity of (011)〈100〉 orientation in the ε-fiber and η-fiber increased. Moreover, it was concluded that the transition from the rolling texture to the shear one was a sign of occurrence of the recrystallization (before the grain growth). Finally, with increasing the number of ARB cycles, the intensity of rolling and shear textures saturated and a stable texture formed. - Highlights: • There were texture transitions in the γ-fiber and ζ-fiber. • When the number of cycles increased, the low angle grain boundaries decreased. • The shear texture was dominant after the first cycle. • Transition from rolling texture to shear one was a sign of recrystallization. • With increasing the number of ARB cycles, a stable texture formed.

36 MATERIALS SCIENCE↗

Microstructure and texture evolution of duplex stainless steels with different molybdenum contents

Highlights: • The 3.05Mo steel has higher resistance to strain-induced transformation than the 0.28Mo steel. • The increased Mo content affects the grain growth of austenite and ferrite due to the effects of segregation and anchoring. • At high annealing temperatures, this Mo retarding effect is weakened. • The suppression of γ-fiber development in the ferrite texture is associated with the increased Mo content. • High amounts of Mo generate unfavorable conditions for the formation of CSL boundaries. - Abstract: The microstructure and texture evolution of duplex stainless steels with different molybdenum contents were studied. For this purpose, hot-rolled 2205 and 2304 samples were solution-annealed at 1100 °C for 1800 s and then cold-rolled to a 75% thickness reduction. This was followed by an isothermal annealing at 900 and 1100 °C for 180 s. The EBSD technique was used to determine the phase ratio, crystallographic texture, and microstructural characteristics. The hot-rolled steel had a work hardened microstructure and the samples submitted to intermediate annealing presented mainly deformation-free grains. Cold rolling resulted in a substantial reduction in the phase spacing with the formation of the strain-induced α′-martensite (SIM) from the metastable austenite. After annealing at 900 °C, the ferrite grains retained the elongated shape of the cold-rolled condition and the primary recrystallization progressed in the austenite phase. Increasing the Mo content increased the resistance to strain-induced martensitic transformation and inhibited the grain growth of austenite phase during annealing at 900 °C. Increasing annealing temperature to 1100 °C promoted the coarsening of both bcc and fcc structures with the formation of annealing twins in the austenitic grains. The recrystallization kinetics and subsequent grain growth occur earlier in ferrite than in austenite phase. Differences in Mo content did not significantly alter the evolution of austenite texture, whereas in the ferrite phase the increase in Mo content suppressed the γ-fiber development. Oriented nucleation was the predominant mechanism observed during the recrystallization of ferritic grains in the 2205 samples. The development of ∑19a boundaries was associated with the selected growth of {554}<225>{sub α} grains in the annealed 2304 samples. Annealing twins were associated with the formation of Σ3 boundaries after the heat treatments. Grain coarsening resulted in a larger fraction of the special boundaries in ferrite phase but inhibited the CSL formation in the austenite phase.

36 MATERIALS SCIENCE↗

ROTATING MOTIONS AND MODELING OF THE ERUPTING SOLAR POLAR-CROWN PROMINENCE ON 2010 DECEMBER 6

A large polar-crown prominence composed of different segments spanning nearly the entire solar disk erupted on 2010 December 6. Prior to the eruption, the filament in the active region part split into two layers: a lower layer and an elevated layer. The eruption occurs in several episodes. Around 14:12 UT, the lower layer of the active region filament breaks apart: One part ejects toward the west, while the other part ejects toward the east, which leads to the explosive eruption of the eastern quiescent filament. During the early rise phase, part of the quiescent filament sheet displays strong rolling motion (observed by STEREO-B) in the clockwise direction (viewed from east to west) around the filament axis. This rolling motion appears to start from the border of the active region, then propagates toward the east. The Atmospheric Imaging Assembly (AIA) observes another type of rotating motion: In some other parts of the erupting quiescent prominence, the vertical threads turn horizontal, then turn upside down. The elevated active region filament does not erupt until 18:00 UT, when the erupting quiescent filament has already reached a very large height. We develop two simplified three-dimensional models that qualitatively reproduce the observed rolling and rotating motions. The prominence in the models is assumed to consist of a collection of discrete blobs that are tied to particular field lines of a helical flux rope. The observed rolling motion is reproduced by continuous twist injection into the flux rope in Model 1 from the active region side. Asymmetric reconnection induced by the asymmetric distribution of the magnetic fields on the two sides of the filament may cause the observed rolling motion. The rotating motion of the prominence threads observed by AIA is consistent with the removal of the field line dips in Model 2 from the top down during the eruption.

79 ASTRONOMY AND ASTROPHYSICS↗

SQA(TM): Surface Quality Assured Steel Bar Program

OG Technologies, Inc. (OGT) has led this SQA (Surface Quality Assured Steel Bar) program to solve the major surface quality problems plaguing the US special quality steel bars and rods industry and their customers, based on crosscutting sensors and controls technologies. Surface defects in steel formed in a hot rolling process are one of the most common quality issues faced by the American steel industry, accounting for roughly 50% of the rejects or 2.5% of the total shipment. Unlike other problems such as the mechanical properties of the steel product, most surface defects are sporadic and cannot be addressed based on sampling techniques. This issue hurts the rolling industry and their customers in their process efficiency and operational costs. The goal of this program is to develop and demonstrate an SQA prototype, with synergy of HotEye® and other innovations, that enables effective rolling process control and efficient quality control. HotEye®, OGT’s invention, delivers high definition images of workpieces at or exceeding 1,450°C while the workpieces travel at 100 m/s. The elimination of surface defect rejects will be achieved through the integration of imaging-based quality assessment, advanced signal processing, predictive process controls and the integration with other quality control tools. The SQA program team, composed of entities capable of and experienced in (1) research, (2) technology manufacturing, (3) technology sales and marketing, and (4) technology end users, is very strong. There were 5 core participants: OGT, Georgia Institute of Technology (GIT), University of Wisconsin (UW), Charter Steel (Charter) and ArcelorMittal Indiana Harbor (Inland). OGT served as the project coordinator. OGT participated in both research and commercialization. GIT and UW provided significant technical inputs to this SQA project. The steel mills provided access to their rolling lines for data collection, design of experiments, host of technology test and verification, and first-hand knowledge of the most advanced rolling line operation in the US. This project lasted 5 years with 5 major tasks. The team successfully worked through the tasks with deliverables in detection, data analysis and process control. Technologies developed in this project were commercialized as soon as they were ready. For instance, the advanced surface defect detection algorithms were integrated into OGT’s HotEye® RSB systems late 2005, resulting in a more matured product serving the steel industry. In addition to the commercialization results, the SQA team delivered 7 papers and 1 patent. OGT was also recognized by two prestigious awards, including the R&D100 Award in 2006. To date, this SQA project has started to make an impact in the special bar quality industry. The resulted product, HotEye® RSB systems have been accepted by quality steel mills worldwide. Over 16 installations were completed, including 1 in Argentina, 2 in Canada, 2 in China, 2 in Germany, 2 in Japan, and 7 in the U.S. Documented savings in reduced internal rejects, improved customer satisfaction and simplified processes were reported from various mills. In one case, the mill reported over 50% reduction in its scrap, reflecting a significant saving in energy and reduction in emission. There exist additional applications in the steel industry where the developed technologies can be used. OGT is working toward bringing the developed technologies to more applications. Examples are: in-line inspection and process control for continuous casting, steel rails, and seamless tube manufacturing.

47 OTHER INSTRUMENTATION↗

Hardening of A6111-T4 Aluminum Alloy at Large Strains and Its Effect on Sheet Forming Operations

In a number of sheet metal stamping and joining processes, the material undergoes large plastic deformation exceeding the range of plastic strain achievable in a standard tensile test prior to material plastic instability. In order to extend the range of effective strains, the multistep rolling process was employed which enabled prestraining of aluminum sheet above 2.0 of true strain. Tensile testing of rolled samples was used to identify the flow stress corresponding to the level of prestrain: By varying the prestrain level, several data points were obtained for the studied flow curve. The numerical simulation using Abaqus software for the cold rolling process of aluminum strips confirmed that majority of the strip is deformed in plane strain compression condition. Performed simulation of the LDH test determined that earlier fracture might occur if the curve obtained via rolling–tensile testing approach is used versus traditional power law approximation and Voce law approximation. The results of simulation for the multistep drawing of a cylindrical cup revealed possible wrinkling in the die entry area during redrawing stage of the process if the rolling–tensile testing flow curve is employed.

36 MATERIALS SCIENCE↗

AZ61 and AZ61-La Alloys as Anodes for Mg-Air Battery

AZ61 and AZ61-0.5La (wt.%) alloys are prepared by the conventional casting method and then, AZ61 and AZ61-0.5La alloy sheets are obtained with multi-pass hot rolling. Microstructures and electrochemical properties of four alloys are investigated, and discharge properties are tested by an assembled Mg-air battery using alloy anode sheets with a dimension of 70 × 100 × 2.5 mm. Results show that Al{sub 11}La{sub 3} phases are formed in as-cast AZ61-0.5La alloy and promote the grain refinement and the formation of uniform microstructure in as-rolled AZ61-0.5La alloy. As-rolled AZ61-0.5La alloy exhibits a weak self-corrosion tendency but a strong discharge activity. After discharge test for 5 h, the Mg-air battery based on the as-rolled AZ61-0.5La sheet can provide the maximum power output of 1.625 W, and as-rolled AZ61-0.5La anode can supply the maximum energy density of 1417 mWhg{sup −1}. In addition, the relationship between microstructures and discharge properties is sufficiently described and discussed in this paper.

36 MATERIALS SCIENCE↗

Deformation Strengthening of Uranium and Dilute Uranium Alloys

The strength and ductility of uranium and dilute uranium alloys can be substantially improved by deformation strengthening. The yield strength of unalloyed uranium can be nearly doubled by rolling in the vicinity of 250°C. The embrittling effect of hydrogen is also overcome, eliminating the need for vacuum outgassing to obtain good ductility. Significant differences in longitudinal versus transverse tensile properties result, in part, from texture introduced by unidirectional rolling. Warm rolling of U-2.3%Nb results in both traditional strain hardening and a significant Bauschinger effect, resulting in differences between tensile and compressive yield strength. A similar combination of strain hardening and Bauschinger effect also occurs in deformation strengthened U-0.75%Ti. Warm rolling of U-0.75%Ti results in significantly better combinations of tensile yield strength and ductility than can be obtained by conventional age hardening. Warm rolling prior to aging also reduces the loss of ductility which typically accompanies conventional age hardening. Here, an approach is developed in which the effects of prior deformation on tensile and compressive yield strengths are analyzed in terms of texture, long-range dislocation, and Bauschinger effects. The Bauschinger effect is shown to vary in sign with the type of deformation, thus providing opportunities to tailor tensile and compressive properties.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗