DOE OSTI2010
TaN is a potential candidate for metal gates. BCl{sub 3}-based plasma is used to pattern metal gates because it has a high selectivity over Si substrate and capable of etching metal oxides (native oxides on metal gates and high-k dielectrics). During metal gate etch in inductively coupled plasma reactor, the authors found that the TaN metal gate profile depends on the composition of BCl{sub 3}-based plasma. Pure BCl{sub 3} results in an undercut of TaN. The undercut can be avoided by addition of 5%O{sub 2}, further increase in O{sub 2} concentration (until 10%) does not change the TaN profile. When N{sub 2} is added to BCl{sub 3} plasma, first the undercut disappears (at about 6% of N{sub 2}) and then a slope appears as N{sub 2} concentration increases further (toward 10%). It was found that the profile is controlled by a film deposited from BCl{sub 3}-based plasma. In the case of pure BCl{sub 3} plasma, the film consists of B (50%), Cl (30%), and O (20%). When 5% of O{sub 2} is added, no film is observed, but strong BO and BO{sub 2} peaks appear in the plasma emission spectra. When 5%N{sub 2} is added to the BCl{sub 3} plasma, again a film is deposited, but it contains less Cl (18%). Based on our research, the authors propose the following etch mechanism to explain the observed profile notching/footing. In pure BCl{sub 3} plasma, a B- and Cl-containing film is deposited on the sidewalls of the gate. Cl from this film will react with TaN producing an undercut. When O{sub 2} is added, no film is formed and the TaN profile is straight as B apparently reacts with O in the gas phase, forming volatile BO{sub x} species. Further increase of O{sub 2} content does not change the profile as no film is formed. When N{sub 2} is added to BCl{sub 3}, a film is formed but in this case N replaces Cl and the film becomes passivating leading to a straight TaN profile. As more N{sub 2} is added, the film passivates TaN more efficiently leading to a sloped profile.