Crosslinked functional binders and their use in silicon-containing anodes of lithium-ion batteries

A crosslinked polymer composition comprising: (i) a base polymer containing a multiplicity of at least one type of functional group selected from amino, amido, thiol, carboxylic acid, carboxylic acid ester, and epoxy groups; (ii) a multiplicity of hydroxylated benzene rings covalently linked to the base polymer, wherein each hydroxylated benzene ring contains at least two hydroxy groups, and with at least two of the hydroxy groups on said hydroxylated benzene rings being free as OH groups; and (iii) a multiplicity of crosslinking groups that crosslink at least two of said functional groups in the base polymer. The invention is also directed to lithium-ion batteries in which the above-described composition is incorporated in an electrode of the battery, and also directed to methods of operating a lithium-ion battery in which the above-described crosslinked polymer composition is incorporated in an electrode thereof.

Saito, Tsuguyuki↗

An In-Depth Analysis of the Transformation of Tin Foil Anodes during Electrochemical Cycling in Lithium-Ion Batteries

Tin foils have an impressive lithium-storage capacity more than triple that of graphite anodes, and their adoption could facilitate a drastic improvement in battery energy density. However, implementation of a dense foil electrode architecture represents a significant departure from the standard blade-cast geometry with a distinct electrochemical environment, and this has led to confusion with regards to the first cycle efficiency of the system. In this work, we investigate the unique behavior of a tin active material in a foil architecture to understand its performance as an anode. We find shallow cycling of the foil results in an irreversible formation (< 40%) due to diffusional trapping, but intermediate and complete utilization allows for a remarkably reversible formation reaction (> 90%). This striking nonlinearity stems from an in situ transformation from bulk metal to porous electrode that occurs during formation cycles and defines electrode-level lithium-transport on subsequent cycles. As a result, an alternative cycling procedure for assessing the stability of foils is proposed to account for this chemomechanical effect.

25 ENERGY STORAGE↗

Understanding the Role of SEI Layer in Low-Temperature Performance of Lithium-Ion Batteries

Low-temperature electrolytes (LTEs) have been considered as one of the most challenging aspects for the wide adoption of lithium-ion batteries (LIBs) since the SOA electrolytes cannot sufficiently support the redox reactions at LT resulting in dramatic performance degradation. Although many attempts have been taken by employing various noncarbonate solvent electrolytes, there was a lack of fundamental understanding of the limiting factors for low-temperature operations (e.g., -20 to -40 degrees C). Here, the crucial role of the solid-electrolyte-interface (SEI) in LIB performance at low temperature using a butyronitrile (BN)-based electrolyte was demonstrated. These results suggested that an additive formed SEI with low resistance and low charge transfer dictates the LT performance in terms of capacity and cycle life, presenting a useful guideline in designing new electrolytes to address the LT issue.

25 ENERGY STORAGE↗

Atomic-scale tuned interface of nickel-rich cathode for enhanced electrochemical performance in lithium-ion batteries

The Ni-rich layered LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC6 22 ) is one promising cathode for lithium-ion batteries (LIBs), but suffers from poor cycling stability under high cutoff potentials. The performance degradation was reflected as capacity fading and voltage drop, having their roots in instable interface of NMC622. Aimed at improving interfacial stability, in this study, we deposited nanoscale ZrO 2 coatings conformally over NMC622 cathodes using atomic layer deposition (ALD). We found that, under a high cutoff voltage (4.5 V), the ALD ZrO 2 coatings evidently improved the performance of NMC622 cathode, showing better cyclability and higher sustainable capacity. In addition, the ALD coatings dramatically boosted the rate capability of NMC622. All these compelling performance results are ascribed to the atomic-scale tunable ZrO 2 coatings via ALD, which create stable interface and thereby inhibit unfavorable evolutions. In the study, we utilize a suite of characterization tools and various analyses to clarify the effects of ALD ZrO 2 coatings. This study will be helpful for improving the performance of nickel-rich cathodes via interfacial engineering using ALD.

25 ENERGY STORAGE↗

Alloying Interlayers for Anode‐Less Lithium‐Metal Polymer Batteries

Anode‐less lithium‐metal batteries potentially offer further increased energy densities. However, the Coulombic efficiency (CE) of lithium plating and stripping, as a classical measure of Li inventory reversibility, is commonly still insufficient for achieving long‐lasting rechargeable batteries. Herein, the potential benefits of employing thin (20 nm) metal interlayers of Ag, Pt, and Au on Cu to alloy with Li in Cu||Li half‐cells and induce homogeneous Li plating with poly(ethylene oxide)‐based electrolytes are investigated. Interestingly, not all alloying interlayers enable a higher CE compared to neat Cu foil with 84%—specifically Ag@Cu with only 81%, while the best performing one, Au@Cu, provides a substantially increased CE of 91%. While generally the formation of “dead lithium” is found to be the major source of CE, this appears to be less pronounced in the case of Au@Cu, indeed. Further improvement can be achieved by carefully adjusting the cell voltage to a region in which the continuous de‐/alloying is suppressed, yielding a further enhanced CE of 94%, thus highlighting the need for a comprehensive approach to design suitable electrode chemistries and designs beyond a “simple” material improvement.

anode-less battery↗

Influence of Electrolyte Additives on Interfacial Stability of Manganese-Rich Lithium-Ion Battery Cathodes

Affordable, long-lasting energy storage has become critical to support increased electricity demand in recent years. Cobalt-free, lithium- and manganese-rich lithium nickel manganese oxide (LMR-NM) cathodes stand to reduce cost and supply-chain concerns associated with traditional cobalt-containing cathodes for lithium-ion batteries by leveraging more earth-abundant materials; however, they have shown issues with long-term cycling stability. Here, we investigate lithium difluoro(oxalate)borate (LiDFOB), tris(trimethylsilyl) phosphite (TMSPi), and vinylene carbonate (VC) electrolyte additives for their ability to improve cycling performance of LMR-NM (0.3 Li 2 MnO 3 + 0.7 LiMn 0.5 Ni 0.5 0 2 ) cells. Cryogenic scanning transmission electron microscopy (cryo-STEM) with electron energy loss spectroscopy enables the construction of a structure–function relationship between cathode electrolyte interphase (CEI) characteristics and the electrochemical performance of cells aged with these additives. We find the combination of 2 wt % TMSPi + 1 wt % LiDFOB performs better than any single additive, achieving a 28% improvement in specific capacity over the baseline electrolyte after long-term cycling. We attribute this to LiDFOB mitigating Mn ion dissolution, with cryo-STEM showing Mn stabilized up to the CEI surface, coupled with improved CEI structure and chemistry enabled by TMSPi, evidenced by a moderately thick (∼7–15 nm) CEI that appears to protect against further electrolyte reactions with the particle. These results, achieved through site-specific nanoscale characterization, directly reveal mechanisms through which electrolyte engineering can improve the performance of earth-abundant cathodes, enabling informed development of more affordable and reliable batteries to meet future energy storage needs.

25 ENERGY STORAGE↗

Resolving Graphite‐Electrolyte Interphase of Lithium‐Ion Batteries using Air‐Tight Ambient Mass Spectrometry

Abstract The formation of a stable solid electrolyte interphase (SEI) at graphite electrode is necessary for lithium‐ion batteries (LIB) to prevent excessive degradation of electrolytes. Until now, the exact organic composition of SEI has not been decisively determined with lithium ethylene mono‐carbonate (LEMC) being one of the debated components. An air‐tight ambient mass spectrometry (MS) platform is developed to directly characterize the air‐sensitive organic components present in SEI. Ionization occurs via a solvent‐free field‐induced process at atmospheric pressure. Our experimental data, based on tandem MS analysis, revealed LEMC to be the major organic component in SEI. This result resolves a long‐standing mystery surrounding the composition of native SEI in LIB, where no trace of the other debated compound, lithium ethylene dicarbonate, was detected. The energetics of fragmentation of LEMC and the corresponding stabilities of various ionic species detected during the air‐tight ambient MS analysis were calculated using density functional theory (DFT). Our findings confirmed favorable protonation energies and suggested the molecular structures for many of the detected species. Solvent (i. e., ethylene carbonate)‐induced stabilization effects observed during the ionization process were also confirmed by DFT. The reported study encourages the routine use of ambient mass spectrometry to characterize both anodic and cathodic electrodes of all battery types as well as to study other air‐sensitive materials in their native state.

25 ENERGY STORAGE↗

Lithiated and passivated lithium ion battery anodes

An electrode material includes a lithium active material composition. The lithium active material composition includes lithium and an active anode material. The lithium active material composition is coated with a lithium ion conducting passivating material, such that the electrode material is lithiated and pre-passivated. An electrode and a battery are also disclosed. Methods of making an electrode material, electrode and battery that are lithiated and pre-passivated are also disclosed.

Sacci, Robert L.↗

Failure analysis and design principles of silicon-based lithium-ion batteries using micron-sized porous silicon/carbon composite

Significant progresses have been made to overcome the fundamental challenges in silicon (Si)-based lithium-ion batteries (LIBs). However, much less work have been reported on the design and failure analysis these batteries for practical applications. In this work, we analyzed various cell design parameters affecting the performance of pouch cells using micron-sized porous Si with nano-pore structure and coated by pitch-carbon (p-Si/C). The correlation among particle level, electrode level, and cell level properties, especially the effect of electrode density on the volumetric capacity density of Si anode and full batteries have been systematically investigated. It is found that the corrosion of p-Si/C particle surface is the main failure mechanisms on the eventual capacity loss, while Li plating on anode electrode surface is the main reason for the fast capacity loss in later stage of cycling. The volumetric capacity of Si anode highly depends on both electrode density and the Si content. Moreover, the prelithiation of Si anodes is found to increase energy density while decreasing cycle life of Si-based full cells. Finally, the pathways and strategies for adoption of micron-sized p-Si/C anodes in LIBs have been proposed for their practical applications.

25 ENERGY STORAGE↗

Parametric Study of Lithium-Ion Batteries using BatPaC (Final Report)

The Battery Performance and Cost Model (BatPaC) is a tool developed by Argonne National Laboratory to design lithium-ion battery (LIB) packs for automotive applications. The material demand and design specifications are used to estimate the cost of manufacturing the battery pack in a large volume production plant (5-50 GWh/year). With the option to select from various electrode chemistries and materials with their associated properties and prices, the resultant battery pack mass, volume, and cost can vary considerably. This report is the result of a parametric sensitivity study that helps identify the key parameters and prices that affect the battery metrics – the specific energy (Wh/kg) and the pack cost ($/kWh). The study was conducted with LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) and graphite (G) electrodes as the baseline materials used in a battery pack for a 300-mile range battery electric vehicle (BEV300) and a 50-mile range plug-in hybrid electric vehicle (PHEV50).

25 ENERGY STORAGE↗

Progress of 3D network binders in silicon anodes for lithium ion batteries

Prompted by its overwhelming benefits, silicon (Si) has evolved as one of the most promising anode materials for high-capacity lithium-ion batteries (LIBs). However, some of the intrinsic drawbacks such as low ionic conductivity and inevitable volume change during the alloying/dealloying process seriously hamper the commercialization of Si-based anodes in LIBs. Among the several strategies to overcome the challenges of the Si anode, the development of designed polymeric binders is imperative for enabling stable and satisfactory performance. The improved cell performance due to the designed binders is recognized as an economical and practical approach, especially from the industrial perspective. In addition to their conventional role in integrating electrode components, binders also play a significant role in alleviating the unfavorable phenomenon of volume expansion, and ultimately stabilizing the Si anode and Si-electrolyte interphase. The polymer architecture of the binders significantly influences the binder performance, and three-dimensional (3D) network binders are generally more effective at coping with the stress resulting from the huge volume change of the Si anode. To develop advanced 3D binders, substantial research efforts have been made including various crosslinking strategies in the past decade. In this review, we focus on diverse crosslinking methods including chemical-, physical-, and topological-crosslinking for rationally designing network binders for Si anodes and take a glance at dynamic interactions to construct healable binders for long-term stability.

25 ENERGY STORAGE↗

Rational Design of a Ni 3 N 0.85 Electrocatalyst to Accelerate Polysulfide Conversion in Lithium–Sulfur Batteries

Slow kinetics of polysulfide conversion reactions lead to severe issues for lithium–sulfur (Li–S) batteries, for example, low rate capability, polysulfide migration, and low Coulombic efficiencies. These challenges hinder the practical applications of Li–S batteries. Here, we proposed a rational strategy of tuning the d-band of catalysts to accelerate the conversion of polysulfides. Nitrogen vacancies were engineered in hexagonal Ni 3 N (space group P 6 3 22) to tune its d-band center, leading to the strong interaction between polysulfides and Ni 3 N. Because of the greater electron population in the lowest occupied molecular orbital of Li 2 S 4 , the terminal S–S bonds were weakened for breaking. Temperature-dependent experiments confirm that Ni 3 N 0.85 demonstrates a much low activation energy, thereby accelerating the conversion of polysulfides. A Li–S cell using Ni 3 N 0.85 can deliver a high initial discharge capacity of 1445.9 mAh g –1 (at 0.02 C) and low decay per cycle (0.039%). The Ni 3 N 0.85 cell can also demonstrate an initial capacity of 1200.4 mAh g –1 for up to 100 cycles at a high loading of 5.2 mg cm –2 . The high efficiency of rationally designed Ni 3 N 0.85 demonstrates the effectiveness of the d-band tuning strategy to develop low-activation-energy catalysts and to promote the atomic understanding of polysulfide conversion in Li–S batteries.

25 ENERGY STORAGE↗

Voltage and temperature effects on low cobalt lithium-ion battery cathode degradation

Degradation of low cobalt lithium-ion cathodes was tested using a full factorial combination of upper cut-off voltage (4.0 V and 4.3 V vs. Li/Li + ) and operating temperature (25 °C and 60 °C). Half-cell batteries were analyzed with electrochemical and microstructural characterization methods. Electrochemical performance was assessed with galvanostatic cycling, cyclic voltammetry (CV), and electrochemical impedance spectroscopy (EIS) supported by distribution of relaxation times (DRT) analysis. Electrode microstructure was characterized with scanning electron microscopy (SEM), X-ray diffraction (XRD), and X-ray absorption near edge structure (XANES) imaging. Higher cut-off voltage cycling shows presence of NiO x formation, a low diffusivity rock-salt phase, in both CV and XRD data. XRD patterns confirmed that the rock-salt phase was beginning to form at the low cut-off voltage at high temperature, but in much lower intensity than at the high cut-off voltage. Higher temperature accelerates degradation processes at both voltages. Degradation factors at high temperature include NiO x formation, cathode material dissolution, and electrolyte decomposition. SEM analysis suggests that supporting phases may isolate and disconnect active material particles reducing capacity retention and battery life cycle. DRT analysis and XANES imaging show that both high temperature samples revealed a NiO x phase based on an increased diffusive impedance and a visible shift in the XANES spectra. The low cut-off voltage, high temperature sample showed a split peak and shift to lower energies indicating early formation of the NiO x phase. The diffusive impedance, which hinders intercalation and deintercalation, is driven by the formation of the NiO x phase. While primarily driven by cut-off voltage, elevated temperature also contributes to this degradation mechanism.

electrochemical impedance spectroscopy↗

Hierarchical assembly of ZnO nanowire trunks decorated with ZnO nanosheets for lithium ion battery anodes

Hierarchical architectures composed of nanomaterials in different forms are essential to improve the performance of lithium-ion battery (LIB) anodes. Here, we systematically studied the effects of hierarchical ZnO nanostructures on the electrochemical performance of LIBs. ZnO nanowire (NW) trunks were decorated with ZnO NWs or ZnO nanosheets (NSs) by successive hydrothermal synthesis to create hierarchical three-dimensional nanostructures. The branched ZnO NSs on the ZnO NW trunk exhibited a two-fold higher specific gravimetric capacity compared to ZnO NWs and branched ZnO NWs on ZnO NW trunks after 100 cycles of charging–discharging at 0.2C (197.4 mA g –1 ). The improvement in battery anode performance is attributable to the increased interfacial area between the electrodes and electrolyte, and the void space of the branched NSs that facilitates lithium ion transport and volume changes during cycling.

25 ENERGY STORAGE↗

Enabling 4C Fast Charging of Lithium–Ion Batteries by Coating Graphite with a Solid–State Electrolyte

Enabling fast-charging (≥4C) of lithium-ion batteries is an important challenge to accelerate the adoption of electric vehicles. However, the desire to maximize energy density has driven the use of increasingly thick electrodes, which hinders rate capability. Herein, atomic layer deposition is used to coat a single-ion conducting solid electrolyte (Li 3 BO 3 -Li 2 CO 3 ) onto postcalendered graphite electrodes, forming an artificial solid-electrolyte interphase (SEI). When compared to uncoated control electrodes, the solid electrolyte coating: 1) eliminates natural SEI formation during preconditioning; 2) decreases interphase impedance by >75% compared to the natural SEI; and 3) extends cycle life under 4C charging conditions, enabling retention of 80% capacity after 500 cycles (compared to 12 cycles in the uncoated control) in pouch cells with >3 mAh cm –2 loading. Furthermore, this work demonstrates that 4C charging without Li plating can be achieved through purely interfacial modification without sacrificing energy density and sheds new light on the role of the SEI in Li plating and fast-charge performance.

25 ENERGY STORAGE↗

Microstructure and defect engineering of graphite anodes by pulsed laser annealing for enhanced performance of lithium-ion batteries

We report nanosecond pulsed laser annealing significantly improves cyclability and current carrying capacity of lithium-ion batteries (LIBs). This improvement is achieved by engineering of microstructure and defect contents present in graphite in a controlled way by using pulsed laser annealing (PLA) to increase the number density of Li + ion trapping sites. The PLA treatment causes the following changes: (1) creates surface steps and grooves between the grains to improve Li + ion charging and intercalation rates; (2) removes inactive polyvinylidene difluoride (PVDF) binder from the top of graphite grains and between the grains which otherwise tends to block the Li + migration; and (3) produces carbon vacancies in (0001) planes which can provide Li + charging sites. From X-ray diffraction data, we find upshift in diffraction peak or reduction in planar spacing, from which vacancy concentration was estimated to be about 1.0%, which is higher than the thermodynamic equilibrium concentration of vacancies. The laser treatment creates single and multiple C vacancies which provide sites for Li + ions, and it also produces steps and grooves for Li + ions to enter the intercalating sites. It is envisaged that the formation of these sites enhances Li+ ion absorption during charge and discharge cycles. The current capacity increases from an average 360 mAh/g to 430 mAh/g, and C–V shows significant reduction in SEI layer formation after the laser treatment. If the vacancy concentration is too high and charge-discharge cycles are long, then trapping of electrons by Li + may occur, which can lead to Li 0 formation and Li plating causing reduction in current capacity.

25 ENERGY STORAGE↗

The Effect of Cell Geometry and Trigger Method on the Risks Associated with Thermal Runaway of Lithium-Ion Batteries

Consideration of thermal runaway heat output variability is paramount for the development of safe lithium-ion battery assemblies. This study utilizes data gathered from fractional thermal runaway calorimetry (FTRC) experiments to conduct a comparative analysis of thermal runaway heat output for three cell formats (18650, 21700, and 33600) as a function of trigger method (heaters, internal short-circuiting device, and nail penetration). The analysis is based on comparisons for the calculated total energy yield, fractional energy yield, heat rate, and heat flux. This study reveals that nail penetration tends to result in higher thermal runaway heat output for larger cells (21700 & 33600); these experiments also tended to result in higher fractions of the total energy being released through the cell body. The smaller cells (18650) did not appear to have significant variation in heat output as a function of trigger method. This finding suggests that, for this cell type, worst-case scenario heat output could be achievable in assembly level testing regardless of the utilized trigger method. This study also demonstrates successful translation of FTRC results, as recorded in the Battery Failure Databank, into meaningful analysis that breaks down the influence of specific conditions on thermal runaway heat output.

calorimetry↗