Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “COMPRESSION BUCKLING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 775 records · Page 43

Fabric geometry distortion during composites processing

Waviness and tow misalignment are often cited as possible causes of data scatter and lower compression stiffness and strength in textile composites. Strength differences of as much as 40 percent have been seen in composites that appear to have the same basic material and structural properties -- i.e., yarn orientation, yarn size, interlacing geometry. Fabric geometry distortion has been suggested as a possible reason for this discrepancy, but little quantitative data or substantial evidence exists. The focus of this research is to contribute to the present understanding of the causes and effects of geometric distortion in textile composites. The initial part of the study was an attempt to gather qualitative information on a variety of textile structures. Existing and new samples confirmed that structures with a significant direction presence would be more susceptible to distortion due to the compaction process. Thus, uniweaves (fiber vol frac: 54-72 percent) biaxial braids (vf: 34-58 percent) demonstrated very little fabric geometry distortion. In stitched panels, only slight buckling of z-direction stitches was observed, primarily near the surface. In contrast, for structures with high compaction ratios -- e.g., large cylindrical yarns (2.5:1) orpowder towpreg (4:1) -- there were visible distortions where previously smooth and periodic undulations were transformed to abrupt changes in direction. A controlled study of the effect of forming pressure on distortion was conducted on type 162 glass plain weave fabrics. Panels (6 x 6 in) were produced via a resin infusion type setup, but with an EPON 815 epoxy resin. Pressures ranging from hand layup to 200 psi were used (vf: 34-54 percent). Photomicrographs indicated that at pressures up to 50 psi, large changes in thickness were due primarily to resin squeeze out. At higher pressures, when intimate contact was made between the layers, there was some tow flattening and in-plane shifting to optimize nesting. However, even at 200 psi the period and amplitude of the tow undulation remained constant, suggesting that for this relatively fine fabric, distortions from compaction were not a problem. Because of the interest in using larger tows (to reduce cost) and more complex structures, tests were also run on 2D triaxial glass braid (113 yd/lb at 0, 225 yd/lb at +/- 45). Forming pressures of 20, 50, 200, and 500 psi were used, and short block compression tests were run. The 500 psi specimen had a 10 percent decrease in modulus and an almost 50 percent decrease in strength (vs. 20 psi). Because the total fiber wgt/panel was kept constant, the thickness varied from 0.32 to 0.22 in (49-70 percent vf). Yet, the strength value is clearly below what would be expected, even with the decrease in thickness. Photomicrographs of these samples will be taken to determine if more fabric distortion exists in the 500 psi specimens. Finally, because the ultimate goal is to be able to predict and control distortion in a variety of textile structures, a model compaction test was developed to directly measure the deformation of the tows during compaction. Layers of dry glass fabric were placed in a mold with a clear plexiglass window. The yarn amplitude and period was then calculated using image analysis of the videotaped deformation. Preliminary tests demonstrated the feasibility of this technique for simple fabrics with large tows.

Chen, Julie↗

Minimum-weight design of laminated composite plates for postbuckling performance

Minimum-weight design of simply-supported, symmetrically laminated, thin, rectangular, specially orthotropic laminated plates for buckling and postbuckling strength is investigated. The postbuckling analysis is based on an Marguerre-type energy method. The failure load of laminates is calculated by the maximum strain failure criterion based on the in-plane strains. Design variables are individual layer thicknesses with specified fiber orientations. Optimization with discrete valued design is achieved by introducing additional penalty terms to the regular pseudoobjective function of sequential unconstrained minimization technique. The proposed optimization technique is applied to the design of rectangular laminates with various aspect ratios loaded by axial compressive loads.

Shin, Dong KU↗

Stability of the cylindrical shell of variable curvature

This report is a first attempt to devise a calculation method for representing the buckling behavior of cylindrical shells of variable curvature. The problem occurs, for instance, in dimensioning wing noses, the stability of which is decisively influenced by the variability of curvature. The calculation is made possible by simplifying the stability equations (permissible for the shell of small curvature) and by assuming that the curvature 1/R as a function of the arc lengths can be represented by a very few Fourier terms. The formulas for the special case of an ellipse-like half oval with an axis ratio 1/3 ?= e ?= 1 under compression in longitudinal direction,shear, and a combination of shear and compression were evaluated. However, the results can also be applied approximately to an unsymmetrical oval-shell segment under compression, shear, and bending so that the numerical values contained in the diagrams 10 to 12 represent directly dimensioning data for the wing nose.

LOADS AND STRESSES, STRUCTURAL - BENDING↗

Compressive strength improvements from noncircular carbon fibers: A numerical study

The benefits of high-performance unidirectional carbon fiber composites are limited in many cost-driven industries due to the high cost relative to alternative reinforcement fibers. Low-cost carbon fibers have been previously proposed, but the longitudinal compressive strength continues to be a limiting factor or studies are based on simplifications that warrant further analysis. A micromechanical model is used to (1) determine if the longitudinal compressive strength of composites can be improved with noncircular carbon fiber shapes and (2) characterize why some shapes are stronger than others in compression. In comparison to circular fibers, the results suggest that the strength can be increased by 10%–13% by using a specific six-lobe fiber shape and by 6%–9% for a three-lobe fiber shape. A slight increase is predicted in the compressive strength of the study two-lobe fiber but has the highest uncertainty and sensitivity to fiber orientation and misalignment direction. The underlying mechanism governing the compressive failure of the composites was linked to the unique stress fields created by the lobes, particularly the pressure stress in the matrix. Importantly, this work provides mechanics-based evidence of strength improvements from noncircular fiber shapes and insight on how matrix yielding is altered with alternative fiber shapes.

36 MATERIALS SCIENCE↗

Plastic buckling

The present article is concerned mainly with the post-bifurcation and imperfection-sensitivity aspects of plastic buckling. A simple two-degree-of-freedom model is used to introduce post-bifurcation behavior and a second model illustrates features of the behavior of continuous solids and structures. Hill's bifurcation criterion for a class of three-dimensional solids is applied to the Donnell-Mushtari-Vlasov (DMV) theory of plates and shells. A general treatment of the initial post-bifurcation behavior of plates and shells is given within the context of the DMV theory. This is illustrated by problems involving columns and circular plates under radial compression. Numerical results are given for a column under axial compression, a circular plate under radial compression, and spherical and cylindrical shells.

Hutchinson, J. W.↗

Experimental Study of Torsional Column Failure

Thirty-three 24ST aluminum-alloy 2- by 2- by 0.10-inch channels, with lengths ranging from 10 to 90 inches were tested at Stanford University in compression to obtain an experimental verification of the theoretical formulas for torsional failure developed by Eugene E. Lundquist of the N.A.C.A. The observed critical loads and twist-axis locations were sufficiently close to the values obtained from the formulas to establish the substantial validity of the latter. The differences between observed and computed results were small enough to be accounted for by small and mostly unavoidable differences between actual test conditions and those assumed in deriving the formulas. Some data were obtained from the shorter specimens regarding the growth of the buckles that resulted in local buckling failure.

Nile, Alfred S↗

Characterization and Modeling of Cell Wall Imperfections in Aluminum Honeycomb Cores using X-ray CT Imaging

Honeycomb cell imperfections may significantly affect the failure of sandwich composites in core crushing and shear modes. Identification and quantification of the different types of imperfections and evaluation of their effects on the mechanical response of honeycomb cores in flatwise compression is presented. X-Ray computed tomography (CT) scans of honeycomb cores in co-cured composite sandwich panels were performed. Image analysis methods are applied to characterize and quantify core cell geometry and cell wall waviness. An approach is developed for extracting cell wall mid surface planes and waviness for constructing finite element models using shell elements. Analysis results from models with the as-manufactured imperfections are compared to results from models with idealized geometries to evaluate the effect of the as-manufactured imperfections on the initiation of cell wall buckling and subsequent core crushing.

aluminum honeycomb↗

Soft elasticity optimises dissipation in 3D-printed liquid crystal elastomers

Soft-elasticity in monodomain liquid crystal elastomers (LCEs) is promising for impact-absorbing applications where strain energy is ideally absorbed at constant stress. Conventionally, compressive and impact studies on LCEs have not been performed given the notorious difficulty synthesizing sufficiently large monodomain devices. Here, we use direct-ink writing 3D printing to fabricate bulk (>cm 3 ) monodomain LCE devices and study their compressive soft-elasticity over 8 decades of strain rate. At quasi-static rates, the monodomain soft-elastic LCE dissipated 45% of strain energy while comparator materials dissipated less than 20%. At strain rates up to 3000 s –1 , our soft-elastic monodomain LCE consistently performed closest to an ideal-impact absorber. Drop testing reveals soft-elasticity as a likely mechanism for effectively reducing the severity of impacts – with soft elastic LCEs offering a Gadd Severity Index 40% lower than a comparable isotropic elastomer. Lastly, we demonstrate tailoring deformation and buckling behavior in monodomain LCEs via the printed director orientation.

36 MATERIALS SCIENCE↗

Optimization of Elastically Tailored Tow-Placed Plates with Holes

Elastic stiffness tailoring of laminated composite panels by allowing the fibers to curve within the plane of the laminate is a design concept that has been demonstrated to be both beneficial and practical. The objective of the present paper is to demonstrate the effectiveness of stiffness tailoring through the use of curvilinear fibers to reduce stress concentrations around the hole and improve the load carrying capability of panels. Preliminary panel designs that are to be manufactured and tested were determined through design studies for flat plates without holes under axial compression using an optimization program. These candidate designs were then analyzed with finite element models that accurately reflect the test conditions and geometries in order to decide upon the final designs for manufacture and testing. An advanced tow-placement machine is used to manufacture the test panels with varying fiber orientation angles. A total of six large panels measuring three feet by six feet, each of which is used to produce four specimens with or without holes, are fabricated. The panels were machined into specimens with holes and tested at NASA Langley Research Center. Buckling response and failure of panels without holes and with two different hole dimensions are presented. Buckling and failure loads of tow-steered specimens are significantly greater than the buckling and failure loads of traditional straight-fiber specimens.

Jegley, Dawn C.↗

Picosecond Optical MCPI-Based Imagers

We present the desired performance specifications for an advanced optical imager, which borrows practical concepts in high-speed microchannel plate (MCP) intensified x-ray stripline imagers and time-dilation techniques. With a four-fold speed improvement in state-of-the-art high-voltage impulse drivers, and novel atomic-layer deposition MCPs, we tender a design capable of 5 ps optical gating without the use of magnetic field confinement of the photoelectrons. We analyze the electron dispersion effects in the MCP and their implications for gating pulses shorter than the MCP transit time. We present a wideband design printed-circuit version of the Series Transmission Line Transformer (STLT) that makes use of 50-ohm coaxial 1.0 mm (110 GHz) and 1.85 mm (65 GHz) hermetically sealed vacuum feedthroughs and low-dispersion Teflon/Kapton circuit materials without the use of any vias. The STLT matches impedance at all interfaces with a 16:1 impedance (4:1 voltage) reduction, and delivers a dispersion-limited sharp impulse to the MCP strip. A comparison of microstrip design calculations is given, showing variances between method of moments, empirical codes, and finite element methods for broad, low-impedance traces. Prototype performance measurements are forthcoming.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Experimental observations and finite element analysis of the initiation of fiber microbuckling in notched composite laminates

An understanding was developed of the factors that determine the semi-circular edge-notched compressive strength and the associated failure mode(s) were identified of thermoplastic composite laminates with multidirectional stacking sequences. The experimental observations and the detailed literature review suggest at least four factors that affected the determination of the strain levels at which fiber microbuckling initiates and thus, partially control the composite's compression strength. The dependent variables studied are the compressive strength of a reduced gage section compression specimen and the compression strength of a compression specimen with two semi-circular edge notches (no opposite free edges) centered along the gage section. In this research, specimens containing two semi-circular edge notches (no opposite free edges) were loaded in compression at a relatively slow rate to provide more stable development of fiber microbuckling damage. The results indicate that the local constraints (free surfaces, supporting ply orientation, and resin-rich regions) significantly affect the strain level for the initiation of in-plane fiber microbuckling. Preliminary results at an elevated temperature, 77 C, showed the shear stress yield strength of the resin was reduced and consequently, the resistance to fiber microbuckling was also reduced. The finite element analysis of the perfectly straight fiber problem indicates that the free surface effect causes a 10 percent reduction in the critical buckling strain. However, the experimentally measured reduction for fibers with an initial fiber curvature, was 35 percent.

Guynn, E. Gail↗

Test and Analyses of a Composite Multi-Bay Fuselage Panel Under Uni-Axial Compression

A composite panel containing three stringers and two frames cut from a vacuum-assisted resin transfer molded (VaRTM) stitched fuselage article was tested under uni-axial compression loading. The stringers and frames divided the panel into six bays with two columns of three bays each along the compressive loading direction. The two frames were supported at the ends with pins to restrict the out-of-plane translation. The free edges of the panel were constrained by knife-edges. The panel was modeled with shell finite elements and analyzed with ABAQUS nonlinear solver. The nonlinear predictions were compared with the test results in out-of-plane displacements, back-to-back surface strains on stringer flanges and back-to-back surface strains at the centers of the skin-bays. The analysis predictions were in good agreement with the test data up to post-buckling.

Li, Jian↗

Structural Concepts Study of Non-circular Fuselage Configurations

A preliminary study of structural concepts for noncircular fuselage configurations is presented. For an unconventional flying-wing type aircraft, in which the fuselage is inside the wing, multiple fuselage bays with non-circular sections need to be considered. In a conventional circular fuselage section, internal pressure is carried efficiently by a thin skin via hoop tension. If the section is non-circular, internal pressure loads also induce large bending stresses. The structure must also withstand additional bending and compression loads from aerodynamic and gravitational forces. Flat and vaulted shell structural configurations for such an unconventional, non-circular pressurized fuselage of a large flying-wing were studied. A deep honeycomb sandwich-shell and a ribbed double-wall shell construction were considered. Combinations of these structural concepts were analyzed using both analytical and simple finite element models of isolated sections for a comparative conceptual study. Weight, stress, and deflection results were compared to identify a suitable configuration for detailed analyses. The flat sandwich-shell concept was found preferable to the vaulted shell concept due to its superior buckling stiffness. Vaulted double-skin ribbed shell configurations were found to be superior due to their weight savings, load diffusion, and fail-safe features. The vaulted double-skin ribbed shell structure concept was also analyzed for an integrated wing-fuselage finite element model. Additional problem areas such as wing-fuselage junction and pressure-bearing spar were identified.

Mukhopadhyay, Vivel↗

ANATOMY OF THE BAR INSTABILITY IN CUSPY DARK MATTER HALOS

We examine the bar instability in galactic models with an exponential disk and a cuspy dark matter (DM) halo with a Navarro-Frenk-White cosmological density profile. The equilibrium models are constructed from a three-integral composite distribution function but subject to the bar instability. We generate a sequence of models with a range of mass resolution from 1.8 K to 18 M particles in the disk and 10 K to 100 M particles in the halo along with a multimass model with an effective resolution of {approx}10{sup 10} particles. We describe how mass resolution affects the bar instability, including its linear growth phase, the buckling instability, pattern speed decay through the resonant transfer of angular momentum to the DM halo, and the possible destruction of the halo cusp. Our higher resolution simulations show a converging spectrum of discrete resonance interactions between the bar and DM halo orbits. As the pattern speed decays, orbital resonances sweep through most of the DM halo phase space and widely distribute angular momentum among the halo particles. The halo does not develop a flat density core and preserves the cusp, except in the region dominated by gravitational softening. The formation of the bar increases the central stellar density and the DM is compressed adiabatically increasing the halo central density by 1.7 times. Overall, the evolution of the bar displays a convergent behavior for halo particle numbers between 1 M and 10 M particles, when comparing bar growth, pattern speed evolution, the DM halo density profile and a nonlinear analysis of the orbital resonances. Higher resolution simulations clearly illustrate the importance of discrete resonances in transporting the angular momentum from the bar to the halo.

79 ASTRONOMY AND ASTROPHYSICS↗

Effect of impact damage on the compression fatigue behavior of composite tubes

Experimental results are presented from an exploratory study to assess the effect of barely visible impact damage on the fatigue behavior of thin walled composite tubes. Undamaged composite tubes and tubes containing barely visible impact damage were tested in compression-compression fatigue. All tubes were inspected ultrasonically prior to testing. Tubes were outfitted with strain gages both in the damaged and far-field regions and an extensometer was utilized to measure axial displacements across the damaged region. Periodically, testing was halted and tubes were inspected ultrasonically and statically tested. In general, the impact damaged tubes exhibited a significantly shorter life than the undamaged tubes; however, there were considerable differences in the lives of the individual impact damaged tubes. No damage growth or stiffness loss was observed prior to failure. Failure of the impact damaged tubes was observed to occur in a combination of delamination buckling and shear crippling modes.

Krafchak, T. M.↗

Flaw criticality of circular disbond defects in compressive laminates

The compressive behavior of T300/5208 graphite-epoxy laminates containing circular delaminations was studied to determine the flaw criticality of two types of implanted defect, Kapton bag and Teflon film, on several laminate configurations. Defect size was varied. Results, presented in the form of residual strength curves, indicate that the Teflon film defect reduced strength more than the Kapton bad defect in 12-ply samples, but that two laminates (+ or - 45) sub 2s and (90/+ or - 45) sub s were insensitive to any implanted defect. A clear thickness effect was shown to exist for the (o/+ pr 45) sub ns laminate and was attributed to failure mode transition. The analytically predicted buckling loads show excellent agreement with experimental results and are useful in predicting failure mode transition.

Webster, J. D.↗

Cytherean crustal bending at Salme Dorsa

The Salme ridge belt can be interpreted as being the leading edge of a venusian crustal unit that moved against the highland foreland unit. It is indicative of a compressional zone, with a thrust front facing west. The Salme ridge belt with adjoining structures is an evident indication of lateral stresses and adjoining crustal movements on Venus. It supports the idea of southeast compression against and over the foreland planitia, which has bent under the load and/or lateral stress, resulting in trough and bulge formation in front of the ridge belt. The origin of the driving force for the movements remains masked. Laima Tessera is located in the direction from which the thrust is thought to apply but there are no appropriate candidates for a rift zone although a thrust from the southeast would be in good agreement with structures of Laima Tessera. The temperature gradient suggests that the lithosphere is approximately 12 km thick, while its elastic layer is approximately 3 km thick based either on the load-induced flexure model or on the compressional buckling model.

Raitala, J.↗

Effect of Tritium-Induced Damage on Plastic Targets from High-Density DT Permeation

Direct-drive inertial fusion experiments conducted at the Laboratory for Laser Energetics implode 860-μm-diam, 8-μm-thick glow-discharge polymer (GDP) capsules that have a solid, uniform, 60- to 80-μm-thick layer of an equimolar mixture of deuterium and tritium (DT) on their interior. The DT is permeated through the capsule’s wall up to pressures of 1000 atm in small pressure steps to prevent buckling; this occurs over many hours. The capsule is then cooled, the DT is solidified, and the uniform layer is formed using thermal gradients produced by heat deposited from beta decay of the tritium. Thermal contraction of the capsule from cooling is expected to be ~1% of the diameter. Capsules permeated with DT do not exhibit this contraction and retain their room-temperature diameter after cooling. Sources of error in the imaging system were explored, and a systematic 3 μm over measurement of the diameter was revealed and corrected. However, both GDP capsules permeated with only deuterium and polystyrene capsules permeated with DT do exhibit thermal contraction. The highly cross-linked GDP shell is under compressive stress after fabrication and experiences bond breakage when exposed to high-density DT during permeation. It is speculated that some of this compressive stress is relieved during bond cleavage and the capsule’s wall swells, which counteracts contraction during cooling. In addition, mass spectrometry of the DT gas in the permeation system has revealed the presence of hydrocarbons and other carbon-containing species that increase with time, confirming the radio-degradation of the polymer.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗