Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “AGGLOMERATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 775 records · Page 43

Characterization, sintering and dielectric properties of nanocrystalline barium titanate synthesized through a modified combustion process

Nanocrystalline barium titanate has been synthesized through a modified combustion process in a single step for the first time. The as-prepared barium titanate powder is cubic perovskite with lattice constant a = 4.018 A. The phase purity of the nanopowder was examined using thermo gravimetric analysis, differential thermal analysis and Fourier transform infrared spectroscopy. Transmission electron microscopic investigations have shown that the particle size of the as-prepared powder is in the range 20-40 nm. The agglomerate size distribution of the as-prepared powder was studied using atomic force microscopy. The nanoparticles of barium titanate were sintered to 97% of the theoretical density at a temperature of 1350 deg. C for 3 h. The microstructure of the sintered surface was examined using scanning electron microscopy. The dielectric constant and loss factor of the sintered pellets at 1 MHz measured at room temperature were 1223 and 3.5 x 10{sup -3} respectively.

36 MATERIALS SCIENCE↗

Preparation and characterization of {alpha}-Fe{sub 2}O{sub 3}-CeO{sub 2} composite

In our previous study we attempted to see the effect of cerium doping (Ce/Fe ratio 0.015 to 0.074) on goethite matrix and conversion of doped goethite to hematite. In the present communication, nano-structured {alpha}-Fe{sub 2}O{sub 3}-CeO{sub 2} composite with Fe/Ce weight ratio as 1.1 has been synthesized by calcination of goethite-cerium hydroxide precursor prepared by co-precipitation method. It was observed that co-precipitation of cerium along with iron in hydroxide medium resulted in hindering the formation of crystalline order as the precursor formed showed poorly crystallized goethite and almost no crystallinity in Ce(OH){sub 4}. Calcination of the precursor at 400 deg. C showed the formation of hematite together with a broad peak corresponding to cerium oxide whereas at 800 deg. C, two distinct phases of {alpha}-Fe{sub 2}O{sub 3} and CeO{sub 2} were observed. The Moessbauer spectra showed the presence of a paramagnetic component both for the precursor as well as for the sample calcined at 400 deg. C but on raising the calcination temperature to 800 deg. C, the paramagnetic component disappeared and the spectrum corresponding to pure {alpha}-Fe{sub 2}O{sub 3} phase was observed. The microstructure of the product obtained by calcining at 800 deg. C showed rod like structure (30 to 50 nm width and 300 to 500 nm length) of {alpha}-Fe{sub 2}O{sub 3} having equi-dimensional CeO{sub 2} particles on and around the surface. Besides the rods, equi-dimensional particles and agglomerates corresponding to CeO{sub 2} were also observed. The results show that co-precipitation followed by calcinations gives nanorods hematite with CeO{sub 2} particles bonded to its surface.

36 MATERIALS SCIENCE↗

On the role of processing parameters in producing Cu/SiC metal matrix composites via friction stir processing: Investigating microstructure, microhardness, wear and tensile behavior

The main aim of this study is to produce copper reinforced metal matrix composite (MMC) layers using micron sized SiC particles via friction stir processing (FSP) in order to enhance surface mechanical properties. Microstructural evaluation using optical microscopy (OM) and scanning electron microscopy (SEM) indicated that an increase in traverse speed and a decrease in rotational speed cause a reduction in the grain size of stir zone (SZ) for the specimens friction stir processed (FSPed) without SiC particles. With the aim of determining the optimum processing parameters, the effect of traverse speed as the main processing variable on microstructure and microhardness of MMC layers was investigated. Higher traverse speeds resulted in poor dispersion of SiC particles and consequently reduced the microhardness values of MMC layers. It was found that upon addition of SiC particles, wear properties were improved. This behavior was further supported by SEM images of wear surfaces. Results demonstrated that the microcomposite produced by FSP exhibited enhanced wear resistance and higher average friction coefficient in comparison with pure copper. Tensile properties and fracture characteristics of the specimens FSPed with and without SiC particles and pure copper were also evaluated. According to the results, the MMC layer produced by FSP showed lower strength and elongation than pure copper while a remarkable elongation was observed for FSPed specimen without SiC particles. Research Highlights: {yields} Decrease in traverse speed leads to good dispersion of SiC particles in composites. {yields} No distinct TMAZ in side regions of SZ of FSPed specimens with SiC particles. {yields} Microhardness of FSPed specimens with SiC particles shows a remarkable increase. {yields} Reinforcement of Cu with SiC particles improves wear and friction behavior of surface. {yields} A weak bonding in tensile due to probable agglomeration for SiC containing samples.

36 MATERIALS SCIENCE↗

Morphology and composition of Ni-Co electrodeposited powders

The morphology, phase and chemical composition of Ni-Co alloy powders electrodeposited from an ammonium sulfate-boric acid containing electrolyte with different ratio of Ni/Co ions were investigated. The ratios of Ni/Co ions were 1/1, 1/2 and 1/3. The morphology, chemical composition and phase composition of the electrodeposited alloy powders were investigated using AES, SEM, EDS and XRD analysis. Composition of the electrolyte, i.e. the ratio of Ni/Co concentrations was found to influence both, the alloy phase composition and the morphology of Ni-Co alloy powders. At the highest ratio of Ni/Co = 1/1 concentrations typical 2D fern-like dendritic particles were obtained. With a decrease of Ni/Co ions ratio among 2D fern-like dendrites, 3D dendrites and different agglomerates were obtained. X-ray diffraction studies showed that the alloy powders mainly consisted of the face-centered cubic {alpha}-nickel phase and hexagonal close-packed {epsilon}-cobalt phase and minor proportions of face-centered cubic {alpha}-cobalt phase. The occurrence of the latter phase was observed only in the alloy powder with the higher cobalt concentration in electrolyte. The electrodeposition of Ni-Co powders occurred in an anomalous manner. - Highlights: Black-Right-Pointing-Pointer Ni-Co alloys powders were successfully electrodeposited. Black-Right-Pointing-Pointer Composition of the electrolyte (Ni/Co ions ratio) was found to influence on morphology of powders. Black-Right-Pointing-Pointer The electrodeposition of Ni-Co powders occurred in an anomalous manner.

36 MATERIALS SCIENCE↗

Nanostructured cobalt powders synthesised by polyol process and consolidated by Spark Plasma Sintering: Microstructure and mechanical properties

Bulk nanostructured cobalt was processed using a bottom-up strategy. Nanostructured particle agglomerates of about 50 and 240 nm in diameter were synthesised using a polyol route and subsequently consolidated by Spark Plasma Sintering (SPS). The microstructure of the starting powders and of the processed bulk samples was studied and characterised by X-ray diffraction (XRD) and transmission electron microscopy (TEM). The XRD patterns of the as-prepared powders showed predominantly a face centred cubic (fcc) crystalline phase, whereas both fcc and hexagonal close packed (hcp) phases were found within the consolidated samples. A sample with the highest relative mass density (94.5%) was obtained from the small powder particles. TEM observations revealed a lamellar substructure with a high density of nanotwins and stacking faults in every grain in the sample with the highest density. Brillouin light scattering (BLS) and quasistatic compression tests were used to investigate the mechanical properties of the consolidated samples. The two techniques yielded Young modulus values of 168 GPa and 130 GPa, respectively, in the sample with the highest density. This sample also exhibited a yield stress higher than 1 GPa after the compression test, which is mainly attributed to the lamellar-like structure occurring in almost every grain of the polycrystalline aggregate. - Highlights: Black-Right-Pointing-Pointer Cobalt nanoparticles produced by the polyol process present mainly the fcc metastable phase. Black-Right-Pointing-Pointer Bulk nanostructured cobalt is obtained from the nano-particles by Spark Plasma Sintering consolidation. Black-Right-Pointing-Pointer Nanotwins and stacking faults are present in every grain of the more dense sample. Black-Right-Pointing-Pointer Yield strength and plastic domain may be varied depending on the nanoparticle size and the porosity of the consolidated material.

36 MATERIALS SCIENCE↗

CoTiO{sub 3} via cobalt oxalate-TiO{sub 2} precursor. Synthesis and characterization

Purely trigonal ilmenite type powder; CoTiO{sub 3} was successfully synthesized through the thermal decomposition of CoC{sub 2}O{sub 4}{center_dot}2H{sub 2}O-TiO{sub 2} precursor. The decomposition course was followed using differential thermal analysis-thermogravimetry measurements and the intermediate decomposition products as well as the titanate product were characterized using X-ray diffraction, Fourier transform infrared, transmission electron microscopy techniques. Thermal analysis study indicated that, the intermediate decomposition product; Co{sub 3}O{sub 4} decomposed endothermically into CoO at 963 Degree-Sign C with instantaneous formation of CoTiO{sub 3}. X-ray diffraction of the powder calcined at 950 Degree-Sign C showed characteristic lines for Co{sub 2}TiO{sub 4} besides secondary phase of rutile-TiO{sub 2}, which are disappeared by rising the calcination temperature to 1000 Degree-Sign C. Transmission electron microscopy image of CoTiO{sub 3} powder exhibit weak agglomerated particles with heterogeneous morphology in both shape and dimensions. Type II adsorption isotherm estimated using Brunauer-Emmett-Teller procedure indicated a very high specific surface area of 29.7 m{sup 2} g{sup -1}. Electrical properties of CoTiO{sub 3} measured as a function of temperature and frequency showed a semiconducting behavior at high temperatures with conduction activation energy of 0.73 eV. Kinetic analysis of the non-isothermal thermogravimetry curves, using different computational methods, illustrated that the random nucleation and growth mechanisms are the predominant one. - Graphical Abstract: The figure showed the variation of dielectric constant ({epsilon} Prime ) for CoTiO{sub 3} with temperature at different frequencies. {epsilon} Prime appeared to be temperature and frequency independent at low temperatures. By increasing the temperature, the orientation polarization plays a significant role and a gradual increase of {epsilon} Prime occurred. Highlights: Black-Right-Pointing-Pointer CoTiO{sub 3} was synthesized through decomposition of CoC{sub 2}O{sub 4}{center_dot}2H{sub 2}O-TiO{sub 2} precursor. Black-Right-Pointing-Pointer XRD, FT-IR, TEM techniques are used to characterize decomposition course. Black-Right-Pointing-Pointer Specific surface area of 29.7 m{sup 2} g{sup -1} was obtained. Black-Right-Pointing-Pointer The prepared titanate showed semiconducting behavior.

36 MATERIALS SCIENCE↗

Characterisation of titanium-titanium boride composites processed by powder metallurgy techniques

In this work, a detailed characterisation of titanium-titanium boride composites processed by three powder metallurgy techniques, namely, hot isostatic pressing, spark plasma sintering and vacuum sintering, was conducted. Two composites with different volume percents of titanium boride reinforcement were used for the investigation. One was titanium with 20% titanium boride, and the other was titanium with 40% titanium boride (by volume). Characterisation was performed using X-ray diffraction, electron probe micro analysis - energy dispersive spectroscopy and wavelength dispersive spectroscopy, image analysis and scanning electron microscopy. The characterisation results confirm the completion of the titanium boride reaction. The results reveal the presence of titanium boride reinforcement in different morphologies such as needle-shaped whiskers, short agglomerated whiskers and fine plates. The paper also discusses how mechanical properties such as microhardness, elastic modulus and Poisson's ratio are influenced by the processing techniques as well as the volume fraction of the titanium boride reinforcement. - Highlights: Black-Right-Pointing-Pointer Ti-TiB composites were processed by HIP, SPS and vacuum sintering. Black-Right-Pointing-Pointer The completion of Ti-TiB{sub 2} reaction was confirmed by XRD, SEM and EPMA studies. Black-Right-Pointing-Pointer Hardness and elastic properties of Ti-TiB composites were discussed. Black-Right-Pointing-Pointer Processing techniques were compared with respect to their microstructure.

36 MATERIALS SCIENCE↗

Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4} nanoparticles dispersed in a SiO{sub 2} matrix synthesized by sol-gel processing

(Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4})x/(SiO{sub 2})(100 - x) (x = 5, 20 and 50 wt.%) nanocomposites are synthesized by a sol-gel method using tetraethylorthosilicate (TEOS) and metallic nitrates as precursors, and by further annealing the powders for 1 h at 1273 K. X-ray diffraction (XRD), transmission electron microscopy (TEM), room temperature vibrating sample magnetometry (VSM) and SQUID measurements are employed for structural, morphological and magnetic sample characterization. For all the concentrations analyzed, the powder nanocomposites actually consist of spinel NiZn ferrite nanoparticles, dispersed in an amorphous silica matrix. TEM studies reveal different particle size distributions and particle morphologies for the three ferrite contents. The 20 wt.%-NiZn ferrite samples consist of nearly spherical nanoparticles, of about 8 nm, mainly superparamagnetic, well-dispersed in the amorphous silica matrix, while the 5 wt.%-NiZn ferrite samples exhibit a bimodal particle size distribution (5 and 30 nm) of single-domain nanoparticles embedded in the silica. In the 50 wt.%-NiZn ferrite samples, two particle families are observed: small round superparamagnetic nanoparticles of about 8 nm embedded in the amorphous silica matrix and large, non-spherical, ferrimagnetic ones, forming agglomerates outside the matrix. In all the synthesized samples, thickness fringes are observed inside some of the ferrite nanoparticles in dark field images. This contrast is explained using the theory of electron diffraction in a weak beam dark field (WBDF) condition and considering spherical ferrite nanoparticles. A large range of tailored magnetic properties varying the fraction, dispersion and mean size of the ferrimagnetic NiZn ferrite particles is obtained. Room temperature saturation magnetization values are found in the range 3.0-30.4 Am{sup 2}/kg for the different concentration samples. Coercivity values, between 1.9 and 7.6 mT, are more than 50% higher than those measured in powders of pure stoichiometric NiZn ferrite nanoparticles and somewhat higher than those reported for similar NiZn ferrite/SiO{sub 2} nanocomposites also synthesized by sol-gel processes. A correlation between the nanocomposite microstructure and the observed magnetic properties is established. - Highlights: Black-Right-Pointing-Pointer NiZn ferrite/SiO{sub 2} nanocomposites are successfully synthesized by a sol-gel route. Black-Right-Pointing-Pointer Depending on the NiZn ferrite content single or bimodal size distributions result. Black-Right-Pointing-Pointer Coercivity (1.9-7.6 mT) is 50% higher than in stoichiometric NiZn ferrite powders. Black-Right-Pointing-Pointer Microstructure and magnetic properties are correlated.

36 MATERIALS SCIENCE↗

Synthesis and characterization of barium ferrite–silica nanocomposites

In this work, we prepared barium ferrite-silica (BaM-SiO{sub 2}) nanocomposites of different molar ratios by high-energy ball milling, followed by heat-treatment at different temperatures. The microstructure, morphology and magnetic properties were characterized for different synthesis conditions by using X-ray diffraction (XRD), scanning electron microscopy (SEM) and vibrating sample magnetometry (VSM). The results indicate that 15 h of milling was enough to avoid the generation of hematite phase and to get a good dispersion of barium ferrite particles in the ceramic matrix. For milling periods beyond 15 h and heat treatment above 900 °C, the XRD patterns showed the presence of hematite phase caused by the decomposition of BaM. The agglomerate size observed through SEM analysis was around 150 nm with a good BaM dispersion into the SiO{sub 2} matrix. The highest saturation magnetization (Ms) value obtained was 43 emu/g and the corresponding coercivity (Hc) value of 3.4 kOe for the composition 60BaM-40SiO{sub 2} milled for 15 h and heat treated at 900 °C. This coercivity value is acceptable for the application in magnetic recording media. Highlights: • Barium ferrite–silica nanocomposites were prepared by high energy ball milling. • Optimal processing time is 15 h milling and heat treatment at 900 °C. • This is enough to avoid the generation of hematite phase. • Obtain good dispersion of barium ferrite particles in the ceramic matrix • Above this processing time shows the presence of increased amount of hematite.

36 MATERIALS SCIENCE↗

Morphological effects on the electrochemical performance of lithium-rich layered oxide cathodes, prepared by electrospinning technique, for lithium-ion battery applications

Li-rich Li{sub 1.2}Ni{sub 0.17}Co{sub 0.17}Mn{sub 0.5}O{sub 2} cathode materials were synthesized by electrospinning technique with different polymers, and their structural, morphological, and electrochemical performances were investigated. It was found that the electrospinning process leads to the formation of a fiber and flower-like morphology, by using different polymers and heat treatment conditions. The nanostructured morphology provided these materials with high initial discharge capacity. The cycling stability was improved with agglomerated nano-particles, as compared with porous materials. - Highlights: • Fiber and flower-like Li-rich cathode was synthesized by simple electrospinning. • Polymer dependent morphology and electrochemical performance was investigated. • Well-organized porous structure facilitates the diffusion of lithium ions. • Technique could be applicable to other cathode materials as well.

36 MATERIALS SCIENCE↗

Tapioca starch: An efficient fuel in gel-combustion synthesis of photocatalytically and anti-microbially active ZnO nanoparticles

Zinc oxide nanoparticles were synthesized by gel-combustion method using novel bio-fuel tapioca starch pearls, derived from the tubers of Manihotesculenta. The product is characterized using various techniques. The X-ray diffraction pattern correspond to a hexagonal zincite structure. Fourier transform infrared spectrum showed main absorption peaks at 394 and 508 cm{sup −} {sup 1} due to stretching vibration of Zn–O. Ultravoilet–visible spectrum of zinc oxide nanoparticles showed absorption maximum at 373 nm whereas the maximum of the bulk zinc oxide was 377 nm. The morphology of the product was studied using scanning electron microscopy and transmission electron microscopy. The scanning electron microscopic images showed that the products are agglomerated and porous in nature. The transmission electron microscopic images revealed spherical particles of 40–50 nm in diameter. The photocatalytic degradation of methylene blue was examined using zinc oxide nanoparticles and found more efficient in sunlight than ultra-violet light due to reduced band gap. The antibacterial properties of zinc oxide nanoparticles were investigated against four bacterial strains Klebsiella aerogenes, Escherichia coli, Pseudomonas aeruginosa and Staphylococcus aereus, where Pseudomonas aeruginosa and Staphylococcus aereus exhibited significant antibacterial activity in agar well diffusion method when compared to positive control. - Highlights: • ZnO nanoparticles have been prepared from a new bio-fuel, tapioca starch by gel combustion method. • XRD pattern revealed hexagonal zincite crystal structure with crystallite size 33 nm. • ZnO nanoparticles exhibited a band gap of 2.70 eV. • The ZnO nanoparticles exhibited superior degradation in sunlight in comparison with UV light. • The product showed a good anti-bacterial activity against two bacterial strains.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Role of intensive milling in the processing of barium ferrite/magnetite/iron hybrid magnetic nano-composites via partial reduction of barium ferrite

In this research a mixture of barium ferrite and graphite was milled for different periods of time and then heat treated at different temperatures. The effects of milling time and heat treatment temperature on the phase composition, thermal behavior, morphology and magnetic properties of the samples have been investigated using X-ray diffraction, differential thermal analysis, high resolution transmission electron microscopy and vibrating sample magnetometer techniques, respectively. X-ray diffraction results revealed that BaFe{sub 12}O{sub 19}/Fe{sub 3}O{sub 4} nanocomposites form after a 20 h milling due to the partial reduction of BaFe{sub 12}O{sub 19}. High resolution transmission electron microscope images of a 40 h milled sample showed agglomerated structure consisting of nanoparticles with a mean particle size of 30 nm. Thermal analysis of the samples via differential thermal analysis indicated that for un-milled samples, heat treatment up to 900 °C did not result in α-Fe formation, while for a 20 h milled sample heat treatment at 700 °C resulted in reduction process progress to the formation of α-Fe. Wustite was disappeared in an X-ray diffraction pattern of a heat treated sample at 850 °C, by increasing the milling time from 20 to 40 h. By increasing the milling time, the structure of heat treated samples becomes magnetically softer due to an increase in saturation magnetization and a decrease in coercivity. Saturation magnetization and coercivity of a sample milled for 20 h and heat treated at 850 °C were 126.3 emu/g and 149.5 Oe which by increasing the milling time to 40 h, alter to 169.1 emu/g and 24.3 Oe, respectively. High coercivity values of milled and heat treated samples were attributed to the nano-scale formed iron particles. - Graphical abstract: Display Omitted - Highlights: • Barium ferrite and graphite were treated mechano-thermally. • Increasing milling time increases reduction progress after heat treatment. • Composites including iron nano-crystals forms by milling and heat treatment. • Shorter milling time results in higher H{sub C} of the milled and heat treated samples.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Study of morphology and magnetic properties of the HoNi{sub 3} crystalline and ball-milled compound

The morphology and magnetic properties of the HoNi{sub 3} crystalline and ball-milled intermetallic compounds are presented. The polycrystalline HoNi{sub 3} bulk compound crystallizes in the rhombohedral PuNi{sub 3} — type of crystal structure and indicates ferrimagnetic arrangement with the Curie temperature of T{sub C} = 57 ± 2 K, the helimagnetic temperature T{sub h} = 23 ± 2 K with the total saturation magnetic moment of 6.84 μ{sub B}/f.u. at 2 K. The use of the ball-milling method leads to the formation of HoNi{sub 3} nanoflakes with typical thickness of less than 100 nm prone to agglomeration upon milling. The increase of grinding duration leads to the reduction in crystallite size, which was confirmed by various complementary microscopical and diffraction studies. Moreover, the increase in milling duration results in the emergence of the relatively small coercivity (H{sub C}), remanence (M{sub r}) and a variation of the saturation magnetization (M{sub S}). - Graphical abstract: Display Omitted - Highlights: • The ball-milling method exhibits significant potential for producing RT{sub 3} nanopowders. • The AFM method was used for the first time in analysis of R–T nanoflakes morphology. • HoNi{sub 3} compound forms polycrystalline and textured nanoflakes evolving upon milling. • The decrease in crystallite size via grinding is confirmed by XRD, TEM and AFM. • The magnetic parameters were sensitive to the extension of pulverization b.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structural and electrical properties of TiO{sub 2}/ZnO core–shell nanoparticles synthesized by hydrothermal method

TiO{sub 2}/ZnO core–shell nanoparticles were successfully synthesized by hydrothermal method in two stages: first stage is the hydrothermal synthesis of ZnO nanoparticles and second stage the obtained ZnO nanoparticles are encapsulated in TiO{sub 2}. The obtained ZnO, TiO{sub 2} and TiO{sub 2}/ZnO core–shell nanoparticles were investigated by means of X-ray diffraction, transmission electron microscopy, Brunauer, Emmett, Teller and resistance measurements. X-ray diffraction analysis revealed the presence of both, TiO{sub 2} and ZnO phases in TiO{sub 2}/ZnO core–shell nanoparticles. According to transmission electron microscopy images, ZnO nanoparticles have hexagonal shapes, TiO{sub 2} nanoparticles have a spherical shape, and TiO{sub 2}/ZnO core–shell nanoparticles present agglomerates and the shape of particles is not well defined. The activation energy of TiO{sub 2}/ZnO core–shell nanoparticles was about 101 meV. - Graphical abstract: Display Omitted - Highlights: • TiO{sub 2}/ZnO core–shell nanoparticles were synthesized by hydrothermal method. • TiO{sub 2}/ZnO core–shell nanoparticles were investigated by means of XRD, TEM and BET. • Electrical properties of TiO{sub 2}/ZnO core–shell nanoparticles were investigated. • The activation energy of TiO{sub 2}/ZnO core–shell nanoparticles was about E{sub a} = 101 meV.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

PVA and PEG functionalised LSMO nanoparticles for magnetic fluid hyperthermia application

La{sub 0.7}Sr{sub 0.3}MnO{sub 3} magnetic nanoparticles are synthesized by a solution combustion method and functionalised with polyvinyl alcohol and polyethylene glycol. The induction heating characteristics of coated magnetic nanoparticles (42 °C) were observed at a reasonably low concentration (5 mg/mL). Remarkably, coated magnetic nanoparticles exhibited a promisingly high specific absorption rate with varying magnetic field and constant frequency. The surface analysis is carried out by X-ray photoelectron spectroscopy. A reduction in the agglomeration of the particles was observed when the magnetic nanoparticles were functionalised with polyvinyl alcohol or polyethylene glycol and can be confirmed by transmission electron microscopy and dynamic light scattering studies. Vibrating sample magnetometer measurements indicate superparamagnetic behaviour at room temperature before and after coating. Colloidal stability revealed a considerably higher zeta potential value for coated system. In vitro cytotoxicity test of the magnetic nanoparticles indicates that coated nanoparticles have no significant effect on cell viability within the tested concentrations (1–5 mg mL{sup -1}) as compared to uncoated La{sub 0.7}Sr{sub 0.3}MnO{sub 3}. All these findings explore the potentiality of La{sub 0.7}Sr{sub 0.3}MnO{sub 3} nanoparticles for magnetic fluid hyperthermia. - Highlights: • Surface functionalization of LSMO nanoparticles — first time with PVA • Surface functionalization of LSMO nanoparticles — first time with PEG • BSA protein — first time used as dispersion medium for stability of LSMO nanoparticles • The heating ability observed at low concentration • Improved efficiency of magnetic fluid hyperthermia treatment with surfactants.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Characterization of mechano-thermally synthesized Curie temperature-adjusted La{sub 0.8}Sr{sub 0.2}MnO{sub 3} nanoparticles coated with (3-aminopropyl) triethoxysilane

This research aimed to synthesize nanostructured strontium-doped lanthanum manganite, La{sub 0.8}Sr{sub 0.2}MnO{sub 3} (LSMO), with its Curie temperature (T{sub c}) adjusted to the therapeutic range, through a mechanothermal route. In order to investigate the effect of heat treatment temperature and duration on the resulting crystallite size, morphology, magnetic behavior and Curie temperature, the starting powder mixture was milled in a planetary ball mill before being subsequently heat treated at distinct temperatures for different time lengths. The composition, morphology, and magnetic behavior were characterized using X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), high resolution transmission electron microscopy (HRTEM), selected area electron diffraction (SAED) and vibrating sample magnetometer (VSM). In addition, magnetic properties were further investigated using an alternating current (AC) susceptometer and thermo-magnetic analyzer. 20 h of milling produced a crystallite size reduction leading to a decrease in the heat treatment temperature of LSMO synthesis to 800 °C. Moreover, SEM analysis has shown the morphology of a strong agglomeration of fine nanoparticles. HRTEM showed clear lattice fringes of high crystallinity. The mean crystallite and particle size of 20-hour milled sample heat treated at 1100 °C for 10 h are relatively 69 and 100 nm, respectively. The VSM data at room temperature, indicated a paramagnetic behavior for samples heat treated at 800 °C. However, by increasing heat treatment temperature to 1100 °C, LSMO indicates a ferromagnetic behavior with well-adjusted Curie temperature of 320 K, suitable for hyperthermia applications. Also, reentrant spin glass (RSG) behavior has been found in heat treated samples. The particles are coated with (3-aminopropyl) triethoxysilane (APTES) for biocompatibility purposes; Fourier transform infrared spectroscopy (FTIR) and thermo-gravimetric analysis (TGA) are used for further confirmation of APTES coating. - Highlights: • La{sub 0.8}Sr{sub 0.2}MnO{sub 3} nanoparticles were synthesized via a mechanothermal route. • We report a significant reduction in the heat treatment temperature. • The Curie temperature was tuned within the therapeutic range. • The particles were coated with (3-aminopropyl) triethoxysilane for biocompatibility purposes.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Exothermic low temperature sintering of Cu nanoparticles

Sintering of the Cu nanoparticle at low temperatures resulted in exothermic behavior after its initiation. The calorimetry study of the heating of a 20 nm copper nanoparticles agglomerate revealed the evolution of 41.17 J/g of heat between 170 °C and 270 °C. High resolution transmission electron microscopy (HRTEM) images indicated that the heat generation was accompanied by sintering. The surface energy of the 20 nm copper nanoparticles was estimated to be 1.23 × 10{sup 3} erg/cm{sup 2} based on the heat released during sintering. The in situ high resolution transmission electron microscope (HRTEM) investigation showed that vigorous sintering occurred between 217 and 234 °C, which took place through the dislocation sintering mechanism. - Highlights: • Calorimetry showed exothermic behavior during heating of Cu nanoparticles between 170 and 270 °C. • Heat released due to the sintering of Cu nanoparticles was demonstrated by HRTEM. • Surface energy of 20 nm copper nanoparticles was estimated to be 1.23 × 10{sup 3} erg/cm{sup 2} during sintering. • Growth in crystallite sizes during sintering is disclosed by X-ray diffraction. • In situ HRTEM heating study showed occurrence of sintering through dislocation mechanism.

36 MATERIALS SCIENCE↗

Structural phase transformation of as-prepared Mg–Mn nanoferrites by annealing temperature

As-prepared Mg{sub 0.2}Mn{sub 0.8}Fe{sub 2}O{sub 4} nanoferrite samples by coprecipitation method were annealed at different temperatures T. XRD, TEM, IR, VSM and Mössbauer techniques were used to characterize the samples. This study proved the transformation of the sample structure from cubic spinel to Z-type hexagonal phase at 700 °C. This transformation was assigned to Jahn–Teller effect of the Mn{sup 3+} and Fe{sup 2+} ions and/or atomic disorder in the crystal lattice. All the deduced structural parameters were affected by the transformation process. The infrared and structural parameters showed dependence on T, whereas tetrahedral band position did not. TEM images showed agglomeration of the nanoparticles, where the average particle size ranged 25–55 nm and was a little higher than R. Study on the elastic properties proved the weakening of inter-atomic bonds inside the crystal lattice as T increases. The magnetic properties were affected by the transformation process and showed T dependence, whereas M{sub s} and H{sub c} proved dependence on porosity. Hyperfine interaction parameters, area ratio (B/A) and spontaneous magnetization were discussed as functions of T. - Graphical abstract: The XRD patterns of as-prepared (AP) and annealed Mg{sub 0.2}Mn{sub 0.8}Fe{sub 2}O{sub 4} nanoparticles. - Highlights: • As-prepared Mg–Mn nanoferrites were annealed at different temperatures T. • Sample structure was transformed from cubic to Z-type hexagonal with T. • This transformation was attributed to Jahn–Teller effect and atomic disorder. • The deduced parameters were affected by annealing and transformation process. • The porosity was affected the saturation magnetization and coercivity.

36 MATERIALS SCIENCE↗