Sodium Chemistry Assessment and Initiation of Sodium Exposure Experiment on A709 Commercial Heats and LPBF 316H SS
This report documents sodium chemistry characterization and the initiation of forced‑convection sodium exposure experiments for two structural materials for sodium‑cooled fast reactors (SFRs): Alloy 709 (solution‑annealed and with an additional 775 °C/10 h precipitation treatment) and laser powder bed fusion (LPBF) 316H stainless steel tensile specimens printed with an as‑built surface condition. The sodium exposure experiment was conducted in a forced‑convection sodium loop with two vessels operated at 550 °C and 600 °C, and a cold trap maintained at <130 °C. Carbon activity in sodium was quantified using a nickel‑foil equilibration method. Initial post‑exposure evaluation after ~1,000 h indicates negligible thickness change for Alloy 709 and a small but measurable mass decrease. To isolate thermal effects from sodium effects, parallel thermal‑aging experiments were performed on Alloy 709 at 550 °C and 600 °C. Baseline tensile tests at room temperature, 550 °C, and 600 °C show expected reduction in strength with increasing temperature and serration tensile curves at elevated temperatures, consistent with dynamic strain aging. After 3,000 h thermal aging, Alloy 709 exhibits modest strengthening and reduced ductility at 550 °C. Together, these results establish the loop chemistry conditions and provide the initial corrosion and mechanical property results for ongoing long‑duration sodium exposure of Alloy 709 and LPBF 316H stainless steel.