Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “materials aging”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 757 records · Page 42

Constitutive Model Development for Aging Polymer Encapsulants (ASC P&EM FY2021 L2 Milestone 7836)

This SAND report fulfills the completion requirements for the ASC Physics and Engineering Modeling Level 2 Milestone 7836 during Fiscal Year 2021. The Sandia Simplified potential energy clock (SPEC) non-linear viscoelastic constitutive model was developed to predict a whole host of polymer glass physical behaviors in order to provide a tool to assess the effects of stress on these materials over their lifecycle. Polymer glasses are used extensively in applications such as electronics packaging, where encapsulants and adhesives can be critical to device performance. In this work, the focus is on assessing the performance of the model in predicting material evolution associated with long-term physical aging, an area that the model has not been fully vetted in. These predictions are key to utilizing models to help demonstrate electronics packaging component reliability over decades long service lives, a task that is very costly and time consuming to execute experimentally. The initiating hypothesis for the work was that a model calibration process can be defined that enables confidence in physical aging predictions under ND relevant environments and timescales without sacrificing other predictive capabilities. To test the hypothesis, an extensive suite of calibration and aging data was assembled from a combination of prior work and collaborating projects (Aging and Lifetimes as well as the DoD Joint Munitions Program) for two mission relevant epoxy encapsulants, 828DGEBA/DEA and 828DGEBA/T403. Multiple model calibration processes were developed and evaluated against the entire set of data for each material. A qualitative assessment of each calibration's ability to predict the wide range of aging responses was key to ranking the calibrations against each other. During this evaluation, predictions that were identified as non-physical, i.e., demonstrated something that was qualitatively different than known material behavior, were heavily weighted against the calibration performance. Thus, unphysical predictions for one aspect of aging response could generate a lower overall rating for a calibration process even if that process generated better quantitative predictions for another aspect of aging response. This insurance that all predictions are qualitatively correct is important to the overall aim of utilizing the model to predict residual stress evolution, which will depend on the interplay amongst the different material aging responses. The DSC-focused calibration procedure generated the best all-around aging predictions for both materials, demonstrating material models that can qualitatively predict the whole host of different physical aging responses that have been measured. This step forward in predictive capability comes from an unanticipated source, utilization of calorimetry measurements to specify model parameters. The DSC-focused calibration technique performed better than compression-focused techniques that more heavily weigh measurements more closely related to the structural responses to be predicted. Indeed, the DSC-focused calibration procedure was only possible due to recent incorporation of the enthalpy and heat capacity features into SPEC that was newly verified during this L2 milestone. Fundamentally similar aspects of the two material model calibrations as well as parametric studies to assess sensitives of the aging predictions are discussed within the report. A perspective on the next steps to the overall goal of residual stress evolution predictions under stockpile conditions closes the report.

36 MATERIALS SCIENCE↗

Aging effects on the mechanical properties of alumina-forming austenitic stainless steels

Isothermal aging and tensile evaluation were conducted for recently developed alumina-forming austenitic stainless steels (AFAs). Microstructural observation reveals that NiAl-type B2 and Fe{sub 2}(Mo,Nb)-type Laves phase precipitates form as dominant second phases in the austenitic matrix during aging at 750 C. At room temperature these precipitates increase the strength but decrease the ductility of the AFA alloys. However, when tested at 750 C, the AFA alloys did not show strong precipitation hardening by these phases, moreover, the elongation to fracture was not affected by aging. Fracture surface and cross-sectional microstructure analysis after tensile testing suggests that the difference of mechanical behaviors between room temperature and 750 C results from the ductile-brittle transition of the B2 precipitates. At room temperature, B2 precipitates are strong but brittle, whereas they become weak but ductile above the ductile-brittle transition temperature (DBTT).

36 MATERIALS SCIENCE↗

Proposed Mars Surveyor Landing Sites in Northern Meridiani Sinus, Southern Elysium Planitia, and Argyre Planitia

Our objective is to propose two landing sites that the Mars Surveyor 2001 Lander and Athena Rover could go to on Mars that should meet the safety requirements of the spacecraft landing system and optimize surface operations (chiefly driven by power and communications requirements). An additional site within Argyre Planitia, initially proposed by Parker to the Mars Surveyor Landing Site program, is also proposed for potential consideration for post-2001 missions to Mars, as it is well outside the current latitude limits for the Athena Rover. All three sites are designed to be situated as close to a diversity of geologic units within a few kilometers of the landing site so that diversity can be placed in a geologic context. This objective is very different from the Mars Pathfinder requirement to land at a site with a maximum chance for containing a diversity of rocks within a few tens of meters of the lander. That requirement was driven by the Sojourner mobility limit of a few tens of meters. It can be argued that the Athena project, with its much larger mobility capability, might actually want to avoid such a site, because placing collected samples in geologic context would be difficult. While it has been argued, both before and after the Mars Pathfinder landing, that the provenance for local blocks may be determined by orbiter spectra, primarily from the MGS TES instrument, our ability to do so has yet to be demonstrated. Indeed, several months after conclusion of the Pathfinder mission, we have yet to reach a consensus on the composition of local materials. Our primary data set for selecting a landing site within the latitude and elevation constraints of the 2001 mission is the Viking Orbiter image archive. The site must be selected to place the landing ellipse so as to avoid obvious hazards, such as steep slopes, large or numerous craters, or abundant large knobs. For this purpose, we chose a resolution limit of better than 50 m/pixel. This necessarily excludes from the present study images from current and future orbiter spacecraft, until such data does become readily available. Within each proposed region, it may be possible to identify additional sites once these data become available. Second, the fine-component thermal inertia data, should be greater than about 5 or 6 cgs Units (10(exp -3) cal/sq cm s(exp -0.5)/K). Low thermal inertias imply dusty environments, which could pose a mobility hazard. Similarly, the albedo of the site should not be particularly high, which would also suggest dusty surfaces. Low albedos are preferred, as they often coincide with low Viking red:violet ratios and indicate less dusty surfaces. Next, the Modeled Block Abundance should also not be too high or too low. Based on the Viking Lander and Mars Pathfinder experiences, percentages of blocks should be on the order of 5-25%. Too many blocks could pose a hazard to the landing and mobility. Too few blocks could also indicate a dusty surface. Primary Landing Site: Northern Meridiani Sinus (Proposed by T. J. Parker and K., S. Edgett) Vital Statistics: (1) Latitude, Longitude: 0-3 N, 350-2 W. *Elevation (Viking): about0.5-1.5 Ian. (2) Viking Orbiter Image coverage: Excellent coverage by 15 - 25 m/pixel images (orbits 709A and 410B). Possible stereo coverage in region where two orbits overlap (probably small parallax angle, as these orbits are not listed in NASA Contractor Report 3501) (3) Albedo: about .18 -.26 (4) Block Abundance: 5-26% (5)Fine-Component Thermal Inertia: 5-9 cgs units This region consists of bright deposits similar to those described by Edgett et al, that also lie within a prominent dark albedo region. These deposits are flat-lying, to such a degree that they ramp against topography rather than draping over it. This led Edgett and Parker to suggest that they may be subaqueous sediments, possibly lacustrine or marine evaporites, laid down sometime from the late Noachian to middle Hesperian (age determination pending crater counts). A contact between this material and elevated, dissected highlands to the south was identified , and is described by Edgett et al. Our desire in proposing this landing site is to sample the edge of this deposit where it has been exposed through etching, presumably eolian deflation (the deposit, though in the highlands, is itself only lightly to moderately cratered). This should enable access to in situ stratigraphy. The actual landing site will be selected where slopes are not expected to be steep, such that the rover itself should be able to traverse them and sample layered materials on the way, either up or down the slope. Perhaps due to uncertainties at this time as to the friability or meter-scale roughness of the deposit, it might make sense to place the landing ellipse on the exhumed highland surface adjacent to the deflated margin of the deposit and plan on driving to the deposit rather than landing on it and driving downslope. This should also enable imaging the margin for evidence of layering should it prove too difficult to climb. A target ellipse on the highland surface should also allow Athena access to ancient Noachian highland materials, particularly if placed near crater ejecta or an inlier of knobby material. Secondary Landing Site: Southern Elysium Planitia (Proposed by T. J. Parker) Vital Statistics: (1) Latitude, Longitude: 1.5-3.5 S, 195-198 W. (2) Elevation (Viking): -1.0 km. (3) Viking Orbiter Image coverage: Excellent coverage by 15 - 25 m/pixel images (orbit 725). Possible stereo coverage between images from beginning and end of orbit that overlap (probably small parallax angle) (4) Albedo: about .27-.28 (5) Block Abundance: 4-7% (6) Fine-Component Thermal Inertia: about 3 cgs units This region consists of eroded knobby material, probably of Noachian age, though much of the crater population has been destroyed, that is onlapped at a sharp contact by an extensive plains unit in southern Elysium Planitia that is Amazonian in age. The plains materials have been attributed to unusually low-viscosity flood lavas from fissures south of the Elysium volcanic rise, or to lacustrine materials associated with a large, Amazonian lake at the source of Marte Vallis. Parker and Schenk presented evidence in support of the latter interpretation, though they attributed the putative shore morphology to an embayment of a northern plains ocean into the southern Elysium region. Detailed examination of the margin of the deposit, showing erosion, not simply burial, of small crater rims and fluidized ejecta blankets, also points to lacustrine or marine sedimentation rather than volcanic plains burial. The plains surface exhibits a "crusty" appearance that many researchers have attributed to pressure ridges in lava flows. In a lacustrine context, they also resemble pressure ridges in desiccated evaporite deposits and salt-rimmed pools (now dry) similar in scale and morphology to spectacular, hundred meter-scale pool rims in alkaline Lake Natron, East African Rift. The eroded highland margin surface adjacent to these plains appears to be fairly smooth, even at 15 m/pixel. Isolated knob inliers are scattered from a few kilometers to several tens of "kilometers apart. Heights of the knobs have not been measured yet but, based on experience with similar features in the Pathfinder landing ellipse, are probably typically on the order of several tens of meters high and smaller, though some of the largest knobs in the region are probably up to a few hundred meters high. Two craters larger than a kilometer in diameter, with fluidized deposits, lie nearby the proposed landing site. Very high-resolution images from MOC should help to determine whether a landing site navigable by the Athena rover could be placed in this region. The space between knobs and craters is large enough to enable placement of a target landing ellipse between them but still provide access to one or more of them and to the margin of the Elysium plains material. Post-2001 Mars Surveyor Landing Site: Argyre Planitia (Proposed by T. J. Parker) Vital Statistics: (1) Latitude, Longitude: 55-56 S, 41-43 W. (2) Elevation (Viking): 1.0 km. (3) Viking Orbiter Image coverage: Excellent coverage by 40 m/pixel images (orbits 567B, 568B, and 569B). Excellent stereo coverage with large parallax angles over the entire landing site region, and much of central and southern Argyre. (4) Albedo: about .23-.24 (5) Block Abundance: No data (6) Fine-Component Thermal Inertia: No data The floors of both the Argyre and Hellas basins contain etched layered materials that are probably thick accumulations of channel or lacustrine sediments. The deposits in Hellas are much more eroded than those in Argyre, and Hellas lacks a channel outlet. Argyre is unique in that Uzboi Vallis flowed out of the basin, requiring overflow of a standing body of water within Argyre. This makes it the largest impact basin on Mars with channels both draining into it and flowing out from it. Hellas' channels may be catastrophic flood channels, whereas Argyre was fed by modest-scale valley networks, though the outlet at Uzboi Vallis was a catastrophic flood Highland craters and basins of this kind should be high-priority landing targets for missions intended to focus on the search for either prebiotic organic materials or even simple fossil microorganisms. Basins with internally-draining valley networks should be preferred over flood channels, as they could have provided the long-term influx of water favorable to the origin of life. (Catastrophic floods are not conducive to fossil preservation, due to their very short durations and high transportation energies). They also afford an opportunity to study the evolution of the planet's climate and volatiles during the period of time between the late Noachian and early Hesperian, when a drastic change from a proposed early warm, wet climate to one more closely resembling the modern environment is thought to have occurred. Large basin

Parker, T. J.↗

Study of PBAT Photostabilization with Ultraviolet Absorber in Combination with Hindered Amine Light Stabilizer and Vitamin E, Aiming Mulching Film Application

This work evaluated two combinations of additives, i.e. “carbon black and hindered amine light stabilizer (HALS)” and “carbon black and vitamin E” to prevent photodegradation of poly(butylene adipate-co-terephthalate) (PBAT) aiming its application as mulch films. A 2{sup 2} factorial rotatable central composite design (α = 1.414) with three central points was conducted. Five different concentrations for each additive were used (0.1, 0.5, 1.0, 1.5 and 2.0% in mass). The formulations were exposed in an environmental simulator to radiation and condensation cycles. The both combination did not avoid the gel formation but its action reduced PBAT chain scission process during photodegradation. Nevertheless, comparing the two different combinations with carbon black, HALS additive was more efficient than vitamin E to minimize the reduction on tensile strength and elongation. The chain scission and crosslinking processes were evaluated by chain scission distribution function. The chain scission was the predominant process during photodegradation of pure PBAT and it was possibly favored by hydrolysis during condensation cycles in the accelerated aging test. It was verified that higher concentrations of carbon black in the formulations led to a reduction on light transmission in both experimental designs. Considering the responses of studied factors on mechanical properties and light transmission it was possible to identify the most promising formulations for application in mulch films, which correspond to 1.5% (weight) for each additive.

36 MATERIALS SCIENCE↗

Aging behavior of an in-situ TiB{sub 2}/Al-Cu-Li-x matrix composite

Transmission electron microscopy, differential scanning calorimetry and hardness tests have been performed on an in-situ TiB{sub 2}/Al-3.3Cu-1.0Li-0.60Mg-0.40Ag-0.14Zr-0.13Si composite to study its aging behavior at 175 °C. A cubic phase suspected to be the σ (Al{sub 5}Cu{sub 6}Mg{sub 2}) phase or its variant is precipitated at all aging stages studied, and this phase is not typically observed in the Al-Cu-Li alloys. The primary hardening (aging for 3 h) phases consist of δ′ (Al{sub 3}Li), β′ (Al{sub 3}Zr) and the cubic phase. After aging for 18 h, all precipitates including T{sub 1} (Al{sub 2}CuLi), S (Al{sub 2}CuMg), θ′ (Al{sub 2}Cu), δ′, β′ and the cubic phase have appeared, and the formation of T{sub 1} and S results in a rapid increase in hardness. With prolonging of aging time, the apparent coarsening of T{sub 1} and S results in a decline in hardness. - Highlights: •The aging behavior of an in-situ TiB{sub 2}/Al-Cu-Li-x composite was studied. •A cubic phase suspected to be σ (Al{sub 5}Cu{sub 6}Mg{sub 2}) or its variant was precipitated. •The hardness change was dominated by the evolution of T{sub 1} (Al{sub 2}CuLi) and S (Al{sub 2}CuMg).

36 MATERIALS SCIENCE↗

Experimental quantification of “hardenability” of 2195 and 2050 Al-Li alloys by using cold-rolled sheets

Highlights: • An experimental simulation method for intuitive “hardenability” evaluation. • With increasing the distance from the quenching end, the strength of 2050 alloy lowers more slowly than that of 2195 alloy, indicating its better “hardenability”. • At the location far away from the quenching end, lenticular-shaped phases form within grains, which impede T1 precipitation at the same local location during the following aging process. • More intra-granular lenticular-shaped phases in 2195 Al-Li alloy corresponds to its lower “hardenability”. - Abstract: To effectively and intuitively evaluate the “hardenability” during the design of new heat-treatable Al alloys, an experimental evaluation method by using cold-rolled thin sheets was proposed, which combined end-quenching with tensile test after aging, and eliminated the effect of different original structure of thick plate through-thickness. The “hardenability” of 2050 and 2195 Al-Li alloys was then intuitively characterized by their strength lowering as a function of distance away from the quenching end after T8-aging following end-quenching. As the distance is increased, the strength of the 2050 Al-Li alloy lowers more slowly than that of the 2195 Al-Li alloy, indicating a better “hardenability” of the 2050 Al-Li alloy. At the location with a certain distance away from the quenching end, in addition to the Cu-rich secondary phases at the grain boundary, lenticular-shaped Cu-containing secondary phases also form within grains during the end quenching process, which impede the precipitation of T1 (Al{sub 2}CuLi) phase at the same local location during the following aging process. More importantly, the number of the intra-granular lenticular-shaped phases in the 2195 Al-Li alloy is much more than that in the 2050 Al-Li alloy, which contributes to a less “hardenability” of the 2195 Al-Li alloy.

36 MATERIALS SCIENCE↗

Ultrasonic inspection of carbon fiber reinforced plastic by means of sample-recognition methods

In the case of carbon fiber reinforced plastic (CFRP), it has not yet been possible to detect nonlocal defects and material degradation related to aging with the aid of nondestructive inspection method. An approach for overcoming difficulties regarding such an inspection involves an extension of the ultrasonic inspection procedure on the basis of a use of signal processing and sample recognition methods. The basic concept involved in this approach is related to the realization that the ultrasonic signal contains information regarding the medium which is not utilized in conventional ultrasonic inspection. However, the analytical study of the phyiscal processes involved is very complex. For this reason, an empirical approach is employed to make use of the information which has not been utilized before. This approach uses reference signals which can be obtained with material specimens of different quality. The implementation of these concepts for the supersonic inspection of CFRP laminates is discussed.

Bilgram, R.↗

The Effect of Casting Speed on Microstructure, Microsegregation, and Mechanical Properties of High-Strength Mg-Nd-Zn-Zr Alloy

High-quality Mg-Nd-Zn-Zr magnesium alloy billets were successfully prepared by direct chill casting. The effect of casting speed on microstructure, microsegregation, and mechanical properties of the Mg-Nd-Zn-Zr alloy was systematically investigated. The results show that the as-cast microstructure is composed of equiaxed α-Mg and Mg{sub 12}Nd. Optimum values of mechanical properties were obtained corresponding to the casting speed of 90 mm/min. An age hardening at 200 °C took a remarkable effect on the mechanical properties of billets. The maximum ultimate tensile strength ~ 323.4 MPa was obtained in the billet undergoing T6 heat treatment. The shapes of concentration curves of various alloying elements (e.g., Nd and Zn) in Mg-Nd-Zn-Zr, as predicted by the Gulliver–Scheil model, resemble reasonably with the shapes measured by electron probe microanalysis.

36 MATERIALS SCIENCE↗

Shelf life of alkali activated cement: Effects of storage condition and duration

Hydraulic cements based on the alkali aluminosilicate chemistry tend to be more reactive than Type I Portland cement. An experimental investigation was conducted in order to evaluate the effects of storage in air and in sealed condition on the properties and performance of alkali aluminosilicate cements. Different storage durations up to 28 days were considered in this experimental study. Hydraulic cements were evaluated based on their morphology, chemistry and mineralogy, hydration kinetics, strength development characteristics, and microstructure of the resultant hydration products. The early-age hydration kinetics and strength development characteristics of the alkali aluminosilicate cement were found to be altered by storage, especially when the cement was exposed to air. Older cements also produced hydration products that were more susceptible to microcracking when dried under vacuum. Longer-term strength development characteristics of cements were less influenced than their shorter-term strength development characteristics with duration of storage in sealed or exposed condition.

36 MATERIALS SCIENCE↗

Effects of various Mg/Si ratios on microstructure and performance property of Al-Mg-Si alloy cables

High quality AA6101 aluminum cables are critical to electrical industry to meet the energy consumption requests. In the present work, the influence of Mg/Si ratios on the electrical conductivity and mechanical properties of AA6101 aluminum alloy was investigated. Wheatstone Bridge method and tensile test were employed to characterize the mechanical properties. X-ray Diffraction (XRD), Scanning Electron Microscope (SEM) and Transmission Electron Microscope (TEM) were used to understand the morphology of the precipitation and the mechanism of age hardening. It is found that excessive Si benefits high strength and high conductivity while excessive Mg plays a negative role in the strength and the conductivity of AA6101 cables. Excessive Si elements promote both the precipitating rate and quantity of β″ phase therefore increase the tensile strength. Excessive Si elements also help with decreasing the lattice distortion, which contributes to the enhancement of the conductivity. Excessive Mg elements lead to more dissolved Mg after aging treatment, therefore increase lattice distortion of the matrix and promote the deposit of coarse Mg-enriched secondary phase. - Highlights: •A new available method to improve the mechanical and electrical properties of Al-Mg-Si alloy •Investigation on the role of various Mg/Si ratios in the changes of comprehensive performances •Discussions on the morphology of the precipitation phases and the mechanism of hardening.

36 MATERIALS SCIENCE↗

Irradiation Programs and Test Plans to Assess High-Fluence Irradiation Assisted Stress Corrosion Cracking Susceptibility.

. Irradiation assisted stress corrosion cracking (IASCC) is a known issue in current reactors. In a 60 year lifetime, reactor core internals may experience fluence levels up to 15 dpa for boiling water reactors (BWR) and 100+ dpa for pressurized water reactors (PWR). To support a safe operation of our fleet of reactors and maintain their economic viability it is important to be able to predict any evolution of material behaviors as reactors age and therefore fluence accumulated by reactor core component increases. For PWR reactors, the difficulty to predict high fluence behavior comes from the fact that there is not a consensus of the mechanism of IASCC and that little data is available. It is however possible to use the current state of knowledge on the evolution of irradiated microstructure and on the processes that influences IASCC to emit hypotheses. This report identifies several potential changes in microstructure and proposes to identify their potential impact of IASCC. The susceptibility of a component to high fluence IASCC is considered to not only depends on the intrinsic IASCC susceptibility of the component due to radiation effects on the material but to also be related to the evolution of the loading history of the material and interaction with the environment as total fluence increases. Single variation type experiments are proposed to be performed with materials that are representative of PWR condition and with materials irradiated in other conditions. To address the lack of IASCC propagation and initiation data generated with material irradiated in PWR condition, it is proposed to investigate the effect of spectrum and flux rate on the evolution of microstructure. A long term irradiation, aimed to generate a well-controlled irradiation history on a set on selected materials is also proposed for consideration. For BWR, the study of available data permitted to identify an area of concern for long term performance of component. The efficiency of hydrogen water chemistry mitigation technology may decrease as fluence increases for high-stress intensity factors. This report describes a program plan to determine the efficiency of hydrogen water chemistry as a function of the stress intensity factor applied and fluence. The use of existing, available, materials and the generation of additional materials via irradiation in a research reactor are considered.

36 MATERIALS SCIENCE↗

Effects of Nd Addition on the Microstructure and Mechanical Properties of Extruded Mg-6Gd-2.5Y-0.5Zr Alloy

The microstructure, age-hardening behavior, mechanical properties and texture of extruded Mg-6Gd-2.5Y-0.5Zr alloys with various additions of Nd have been investigated through optical microscopy, x-ray diffraction, scanning electron microscopy, transmission electron microscopy, electron back-scattered diffraction, hardness and tensile tests. The results indicate that the number of second-phase particles in the as-extruded alloys increases (especially with the addition of 1.5 wt.% Nd), and the amount of the strengthening β′ phase in the peak-aged sample initially increases, and then decreases when the content of Nd increases above 1.0 wt.%. The precipitation of second-phase particles in the extrusion process weakens the age strengthening. The peak-aged Mg-6Gd-2.5Y-1Nd-0.5Zr alloy shows a maximum yield strength of 259 MPa and an ultimate tensile strength of 350 MPa, which can be attributed to the finely dispersed strengthening β′ phase. All as-extruded alloys exhibit that (0001) planes are aligned perpendicular to the extrusion direction, and the maximum intensity of the texture increases gradually with Nd addition.

36 MATERIALS SCIENCE↗

Alkali-silica reaction products: Comparison between samples from concrete structures and laboratory test specimens

Alkali-silica gels (ASG) were investigated in concrete from bridge structures (constructed from the 1920s to 2000), as well as in experimental specimens; employing optical microscopy, petrographic image analysis, and scanning electron microscopy combined with energy dispersive spectroscopy (SEM/EDS). The main differences were found in the chemical composition and morphology of the ASGs. ASGs which had formed in older concrete samples (50-80 years old) show a partly crystalline structure and higher Ca{sup 2+} content, indicating their aging and maturation. Younger concrete samples and experimental test specimens exhibit the presence of amorphous ASG. The chemistry of ASG from experimental specimens reflects the chemical composition of accelerating solutions. - Research Highlights: {yields} Quantitative analysis of alkali-silica gels {yields} Comparison of ASR in experimental conditions with ASR in bridge structures {yields} Investigation of factors affecting alkali-silica reaction {yields} Investigation of ASR of different types of aggregates.

36 MATERIALS SCIENCE↗

Microstructural evolution of ω assisted α precipitates in β-CEZ alloy during ageing process

Highlights: • Ultrafine Athermal ω precipitates were formed in β-CEZ alloy by quenching from above the β transus temperature. • In the ageing process, these ω precipitates coarsen, accompanied by the form of needle-like α phase. • ω precipitates were formed by {111}β planes shift 0.5d222 along the direction. • The superfine α particles are formed in close proximity of the ω/β interface. - Abstract: The microstructural evolution in β-CEZ (Ti-5Al-2Sn-4Zr-4Mo-2Cr-1Fe wt%) alloy, after quenching and ageing, has been investigated by combining results from orientation imaging microscopy, transmission electron microscopy, high-resolution TEM (HRTEM). Ultrafine Athermal ω precipitates (about 1 nm) are formed in this alloy by quenching from above the β transus temperature. In the ageing process, these ω precipitates coarsen, accompanied by the form of needle-like α phase. The scale of ω assisted α increased from 5 to 10 nm in width and about 50 nm in length to 10 nm in width and 100–300 nm in length while extending ageing time from 2 h to 5 h at 350 °C. However, when going on extending the ageing time from 5 h to 20 h at 350 °C, the scale of α didn't grow dramatically but the density of α increased clearly. When increasing the ageing temperature from 350 °C to 450 °C, the scale of ω assisted α grow dramatically. Furthermore, the structural relationship of ω and α is observed by HRTEM images. It can be found that ω precipitates were formed by {111}β planes shift 0.5d222 along the <111> direction, and the superfine α particles are formed in close proximity of the ω/β interface.

36 MATERIALS SCIENCE↗

Observation of Precipitation Evolution in Fe-Ni-Mn-Ti-Al Maraging Steel using Atom Probe Tomography

We describe the full decomposition sequence in an Fe-Ni-Mn-Ti-Al maraging steel during isothermal annealing at 550 C. Following significant pre-precipitation clustering reactions within the supersaturated martensitic solid solution, (Ni,Fe){sub 3}Ti and (Ni,Fe){sub 3}(Al,Mn) precipitates eventually form after isothermal aging for {approx}60 seconds. The morphology of the (Ni,Fe){sub 3}Ti particles changes gradually during aging from predominantly plate-like to rod-like, and, importantly, Mn and Al were observed to segregate to these precipitate/matrix interfaces. The (Ni,Fe){sub 3}(Al,Mn) precipitates occurred at two main locations: uniformly within the matrix and at the periphery of the (Ni,Fe){sub 3}Ti particles. We relate this latter mode of precipitation to the Mn-Al segregation.

36 MATERIALS SCIENCE↗

Influence of recrystallization on phase separation kinetics of oxide dispersion strengthened Fe Cr Al alloy

The effect of different starting microstructures on the kinetics of Fe-rich ({alpha}) and Cr-rich ({alpha}') phase separation during aging of Fe-Cr-Al oxide dispersion strengthened (ODS) alloys has been analyzed with a combination of atom probe tomography and thermoelectric power measurements. The results revealed that the high recrystallization temperature necessary to produce a coarse grained microstructure in Fe-base ODS alloys affects the randomness of Cr-atom distributions and defect density, which consequently affect the phase separation kinetics at low annealing temperatures.

36 MATERIALS SCIENCE↗

EVALUATION OF LOCAL STRAIN EVOLUTION FROM METALLIC WHISKER FORMATION

Evolution of local strain on electrodeposited tin films upon aging has been monitored by digital image correlation (DIC) for the first time. Maps of principal strains adjacent to whisker locations were constructed via comparing pre- and post-growth scanning electron microscopy (SEM) images. Results showed that the magnitude of the strain gradient plays an important role in whisker growth. DIC visualized the dynamic growth process in which the alteration of strain field has been identified to cause growth of subsequent whiskers.

36 MATERIALS SCIENCE↗

Microstructure and mechanical behavior of direct metal laser sintered Inconel alloy 718

In this paper, we investigate microstructure and quasi-static mechanical behavior of the direct metal laser sintered Inconel 718 superalloy as a function of build direction (BD). The printed material was further processed by annealing and double-aging, hot isostatic pressing (HIP), and machining. We characterize porosity fraction and distribution using micro X-ray computed tomography (μXCT), grain structure and crystallographic texture using electron backscattered diffraction (EBSD), and mechanical response in quasi-static tension and compression using standard mechanical testing at room temperature. Analysis of the μXCT imaging shows that majority of porosity develops in the outer layer of the printed material. However, porosity inside the material is also present. The EBSD measurements reveal formation of columnar grains, which favor < 001 > fiber texture components along the BD. These measurements also show evidence of coarse-grained microstructure present in the samples treated by HIP. Finally, analysis of grain boundaries reveal that HIP results in a large number of annealing twins compared to that in samples that underwent annealing and double-aging. The yield strength varies with the testing direction by approximately 7%, which is governed by a combination of grain morphology and crystallographic texture. In particular, we determine tension–compression asymmetry in the yield stress as well as anisotropy of the material flow during compression. We find that HIP lowers yield stress but improves ductility relative to the annealed and aged material. These results are discussed and critically compared with the data reported for wrought material in the same condition. - Highlights: • Microstructure and mechanical properties of DMLS Inconel 718 are studied in function of build direction. • Inhomogeneity of microstructure in the material in several conditions is quantified by μXCT and EBSD. • Anisotropy and asymmetry in the mechanical response are determined by tension and compression testing.