Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “cracks”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 757 records · Page 42

Crystallographic effects on transgranular chloride-induced stress corrosion crack propagation of arc welded austenitic stainless steel

Abstract The effect of crystallography on transgranular chloride-induced stress corrosion cracking (TGCISCC) of arc welded 304L austenitic stainless steel is studied on >300 grains along crack paths. Schmid and Taylor factor mismatches across grain boundaries (GBs) reveal that cracks propagate either from a hard to soft grain, which can be explained merely by mechanical arguments, or soft to hard grain. In the latter case, finite element analysis reveals that TGCISCC will arrest at GBs without sufficient mechanical stress, favorable crystallographic orientations, or crack tip corrosion. GB type does not play a significant role in determining TGCISCC cracking behavior nor susceptibility. TGCISCC crack behaviors at GBs are discussed in the context of the competition between mechanical, crystallographic, and corrosion factors.

36 MATERIALS SCIENCE↗

Statistical study of ductility-dip cracking induced plastic deformation in polycrystalline laser 3D printed Ni-based superalloy

Ductility-dip cracking in Ni-based superalloy, resulting from heat treatment, is known to cause disastrous failure, but its mechanism is still not completely clear. A statistical study of the cracking behavior as a function of crystal orientation in a laser 3D-printed DL125L Ni-based superalloy polycrystal is investigated here using the synchrotron X-ray microdiffraction. The dislocation slip system in each of the forty crystal grains adjacent to the 300 μm long crack has been analyzed through Laue diffraction peak shapes. In all these grains, edge-type geometrically necessary dislocations (GNDs) dominate, and their dislocation line directions are almost parallel to the crack plane. Based on Schmid's law, the equivalent uniaxial tensile force direction is revealed normal to the trace of the crack. A qualitative mechanism is thus proposed. Thermal tensile stress perpendicular to the laser scanning direction is elevated due to a significant temperature gradient, and thus locations in the materials where the thermal stress exceeds the yield stress undergo plastic deformation mediated by GND activations. As the dislocations slip inside the crystal grains and pile up at the grain boundaries, local strain/stress keeps increasing, until the materials in these regions fail to sustain further deformation, leading to voids formation and cracks propagation.

36 MATERIALS SCIENCE↗

Redox oxidative cracking of n -hexane with Fe-substituted barium hexaaluminates as redox catalysts

Light olefins such as ethylene and propylene are critical building blocks in the chemical industry and are currently produced mainly from steam cracking of naphtha. However, the highly endothermic nature of steam generation and the cracking reactions make this process highly energy- and CO 2 -intensive. Coke formation in the steam cracker tubes represents another obstacle. To address these challenges, we proposed a chemical looping approach to convert naphtha into olefins via a redox oxidative cracking (ROC) process. In the present work, Fe-substituted barium hexaaluminates (BaFe x Al 12– x O 19 ) were investigated as oxygen carriers, or redox catalysts, to convert n -hexane to olefins via ROC. The cyclic redox scheme facilitated by the Fe-substituted hexaaluminates allows autothermal operation and higher olefin yields relative to the endothermic steam-cracking process. While base BaFe x Al 12– x O 19 ( x = 1, 2, 3, 4, 6) oxides showed high CO x yields (8.4–55.2%) in ROC of n -hexane, 20 wt% Na 2 WO 4 promotion of BaFe 6 Al 6 O 19 (20-NaW/BaFe6) significantly inhibited CO x formation (0.6–1.2% CO x yield) while oxidizing all the H 2 produced during cracking within a temperature range of 600–700 °C and GHSV of 9000 h –1 . Benefiting from the donation of selective lattice oxygen, we report 20-NaW/BaFe6 more than doubled the olefin yield when compared to that from thermal cracking (26.0% vs. 12.8%). Moreover, decreasing the GHSV from 9000 h –1 to 2250 h –1 resulted in 8.5% increase in n -hexane conversion on an absolute basis, while maintaining nearly the same olefin selectivity. Long-term stability of the 20-NaW/BaFe6 oxygen carrier was also demonstrated within 30 cycles at 700 °C and 2250 h –1 , achieving an olefin yield in the range of 31.3–32.4% and low CO x yield of 0.6–0.7%. XPS analysis of cycled BaFe6 revealed a shift towards near-surface Ba enrichment upon redox cycling. In comparison, both as-prepared and cycled 20-NaW/BaFe6 showed suppression of near surface Ba content, indicating that Na 2 WO 4 inhibited the migration of Ba into the near-surface region during n -hexane ROC and effectively suppressed non-selective oxidation reactions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The Release of Trapped Gases from Amorphous Solid Water Films: I. “Top-Down” Crystallization-Induced Crack Propagation Probed using the Molecular Volcano

In this (Paper I) and the companion paper (Paper II) we investigate the mechanisms for the release of trapped gases from underneath of amorphous solid water (ASW) films. In prior work, we reported the episodic release of trapped gases in concert with the crystallization ASW, a phenomenon that we termed the "molecular volcano". The observed abrupt desorption is due to the formation of cracks that span the film to form a connected pathway for release. In this paper we utilize the "molecular volcano" desorption peak to characterize the formation of crystallization-induced cracks. We find that the crack length and distribution are independent of the trapped gas (Ar, Kr, Xe, CH4, N2, O2 or CO). Selective placement of the inert gas layer is used to show that cracks form near the top of the film and propagate downward into the film. Isothermal experiments reveal that, after some induction time, cracks propagate linearly in time with an Arrhenius dependent velocity corresponding to an activation energy of 54 kJ/mol. This value is consistent with the crystallization growth rate reported by others and establishes a direct connection between crystallization growth rate and the crack propagation rate. A two-step model in which nucleation and crystallization occurs in an induction zone near the top of the film followed by the propagation of a crystallization/crack front into the film is in good agreement with the temperature programmed desorption results.

Environmental Molecular Sciences Laboratory↗

Crack Front Segmentation and Facet Coarsening in Mixed-Mode Fracture

A planar crack generically segments into an array of “daughter cracks” shaped as tilted facets when loaded with both a tensile stress normal to the crack plane (mode I) and a shear stress parallel to the crack front (mode III). We investigate facet propagation and coarsening using in situ microscopy observations of fracture surfaces at different stages of quasistatic mixed-mode crack propagation and phase-field simulations. The results demonstrate that the bifurcation from propagating a planar to segmented crack front is strongly subcritical, reconciling previous theoretical predictions of linear stability analysis with experimental observations. As a result, they further show that facet coarsening is a self-similar process driven by a spatial period-doubling instability of facet arrays.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Ultraviolet Fluorescence Bleaching Rates for New Cell Cracks

Ultraviolet Fluorescence (UVF) is an inspection tool that can be used to identify cell cracks in some photovoltaic (PV) modules. Cell cracks can also be identified with electroluminescence (EL) and similar techniques, but it is generally not possible to differentiate new cracks from old ones with EL. UVF has a unique property of taking time for the cracks to show up, which could be used to differentiate new cracks (e.g., from a recent storm) from old ones (e.g., from installation damage). We perform tests on several different modules, some the same make and model but with different bill of materials (BOMs), to characterize the amount of time that it takes for crack signatures to progress in UVF.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Crack tip microplasticity mediated by microstructure gradients

Abstract Traditional fracture theories infer damage at cracks (local field) by surveying loading conditions away from cracks (far field). This approach has been successful in predicting ductile fracture, but it normally assumes isotropic and homogeneous materials. However, myriads of manufacturing procedures induce heterogeneous microstructural gradients that can affect the accuracy of traditional fracture models. This work presents a microstructure‐sensitive finite element approach to explore the shielding effects of grain size and crystallographic orientation gradients on crack tip microplasticity and blunting. A dislocation density‐based crystal plasticity model conveys texture evolution, grain size effects, and directional hardening by computing the constraint from dislocation structures. The results demonstrate that the microstructure can act as a buffer between the local and far fields that affects the crack tip microplasticity variability. For nominal opening loading, grain size and texture affect the local ductility and induce a non‐negligible multiaxial plastic deformation. Furthermore, driving forces based on measuring displacements away from the crack tip are less affected by the microstructure, which suggests that traditional experimental methods smear out important crack tip variability.

Castelluccio, Gustavo M.↗

Effect of Indenter Elastic Modulus on Hertzian Ring Crack Initiation in Silicon Carbide

The effect of spherical indenter stiffness on Hertzian-contact-induced fracture initiation was examined in hot-pressed silicon carbides (SiCs). Hertzian ring crack initiation forces were measured using zirconia, steel, silicon nitride, alumina, or tungsten carbide spherical indenters (elastic moduli ranging between 213 and 630 GPa). The two (flat target) SiCs were fully dense, and had equivalent elastic moduli (~450 GPa) and fracture toughnesses; however, about 20% of the grains in one SiC were larger than the largest grains in the other. Decreasing the indenter elastic modulus consistently resulted in lower ring crack initiation forces and those differences were statistically significant. Such a decrease in Hertzian ring crack initiation force with decreased indenter elastic modulus indicates the presence of a non-zero friction coefficient. Additionally, independent of the indenter material, ring crack initiation occurred at lower Hertzian indentation forces in the SiC containing larger grains suggesting that the grains in that tail of the grain-size-distribution acted as Griffith-type flaws. Lastly, selecting a spherical indenter material that has the same or similar elastic modulus as the target material provides simpler interpretation, and estimates of ring crack initiation stresses with greater usefulness and fidelity. Such a "matched" condition serves to circumvent the complexities that a ubiquitously unknown coefficient of friction introduces in the estimation of Hertzian ring crack initiation stress.

36 MATERIALS SCIENCE↗

Crack propagation in silica from reactive classical molecular dynamics simulations

Mechanistic insight into the process of crack growth can be obtained through molecular dynamics (MD) simulations. In this investigation of fracture propagation, a slit crack was introduced into an atomistic amorphous silica model and mode I stress was applied through far–field loading until the crack propagates. Atomic displacements and forces and an Irving–Kirkwood method with a Lagrangian kernel estimator were used to calculate the J –integral of classical fracture mechanics around the crack tip. The resulting fracture toughness (K IC ), 0.76 ± 0.16 MPa√m, agrees with experimental values. In addition, the stress fields and dissipation energies around the slit crack indicate the development of an inelastic region ~30Å in diameter. This is one of the first reports of KIC values obtained from up–scaled atomic–level energies and stresses through the J –integral. In conclusion, the application of the ReaxFF classical MD force field in this study provides the basis for future research into crack growth in multicomponent oxides in a variety of environmental conditions.

36 MATERIALS SCIENCE↗

In situ observations of cracking in constrained sintering

Here in this article, we examine the long-standing problem of cracking during constrained sintering of a powder aggregate. Using binder jet 3D printing, we prepare ceramic green bodies in the form of center-notched panels, then use in situ imaging to observe how cracks nucleate and grow from the notch as the material sinters under restraint. Quantitative image analysis allows us to identify important characteristics of the sinter-cracking process, indicating a framework for analyzing the problem and developing methods for avoiding it, including representation of sinter-cracking as a creep crack growth process, use of fracture mechanics parameters to design specimen geometries that do not exceed critical stress intensities, and the possibility of exploiting the inherently ductile nature of sinter-cracking to mitigate damage.

36 MATERIALS SCIENCE↗

Role of slip in hydrogen-assisted crack initiation in Ni-based alloy 725

We conduct in situ tensile straining experiments to investigate the role of hydrogen and slip in crack initiation in nickel-based alloy 725. Our experiments reveal no tendency for hydrogen to enhance localized slip and no necessity of slip for crack initiation. We use electrochemical charging to introduce hydrogen into samples, melt extraction to measure hydrogen content, and digital image correlation to analyze localized plastic strains during in situ tensile tests in a scanning electron microscope. Cracks initiate both in regions with and without nearby localized slip. Moreover, the fraction of cracks initiating with no nearby slip is greater at higher hydrogen content. Slip-assisted crack initiation generally occurs at locations where intergranular slip is arrested, especially at intersections of slipping coherent twin boundaries with thin twin lamellae. Cracks that initiate without nearby slip occur at a wider variety of microstructural features, including inclusions, triple junctions, and surface flaws.

36 MATERIALS SCIENCE↗

Phase-field modeling of orientation-dependent crack growth in ductile single crystals with anisotropic elasticity

Crack growth in ductile single crystals (DuSCs) is orientation dependent due to the anisotropies of crystal plasticity and elastic tensor. This study develops a phase-field model incorporating both crystal plasticity and crack growth and proposes a general method to decompose the elastic energy into compressive and tensile parts to prevent crack growth under compression in the phase-field description. The phase-field model, in combination with three Euler angles, is employed to simulate orientation-dependent crack growth in DuSCs. The contributions from crystal plasticity and anisotropic elasticity are compared, and the former is found to dominate in the anisotropy of crack growth in copper single crystals. Furthermore, the simulation results demonstrate that crystal orientation strongly affects the heterogeneous distribution of plastic strain and the interaction between plastic strain and crack growth. High-throughput phase-field simulations are performed with exhaustive crystal orientations, and the results are explained based on the anisotropy of the Taylor factor.

Computational Solid Mechanics↗

Analysis of fatigue crack propagation

The correlation between fatigue crack propagation and stress intensity factor is analyzed. When determining fatigue crack propagation rate, a crack increment, delta a, and its corresponding increment in load cycles, delta N, are measured. Fatigue crack propagation must be caused by a shear and/or a normal separation mode. Both of these two processes are discrete if one looks at the atomic level. If the average deformation and fracture properties over the crack increments, delta a, can be considered as homogeneous, if the characteristic discrete lengths of sigma a, if the plastic zone size is small, and if a plate is thick enough to insure a plane strain case, da/dN is proportional to delta K squared. Any deviation of empirical data from this relation must be caused by the fact that one or more of these conditions are not satisfied. The effects of plate thickness and material inhomogeneity are discussed in detail. A shear separation mode of fatigue crack propagation is described and is used to illustrate the effects of material inhomogeneity.

Liu, H. W.↗

Hydrogen-enhanced fatigue crack growth in Ti-6Al-4V ELI weldments.

The effects of a hydrogen environment on the fatigue crack growth rates in Ti-6Al-4V ELI (STA) and weld material were determined in the temperature range of ambient to -200 F. The hydrogen environment resulted in an acceleration of the crack growth rate and a change in the fracture mode for both materials in the temperature range of ambient to -100 F. At -200 F, there was no significant difference between the crack growth rates obtained in helium and hydrogen gas. The degree of hydrogen-enhanced crack growth was found to be dependent on the crack tip stress-intensity range, temperature, and microstructure of the material. The data are consistent with an embrittlement mechanism involving hydrogen diffusing ahead of the crack front.

Pittinato, G. F.↗

The influence of temperature on fatigue crack growth in a mill annealed Ti-6Al-4V alloy.

To study the influence of temperature on the rate of fatigue crack growth in high strength metal alloys, constant load amplitude fatigue crack growth experiments were carried out using a .25-in.-thick mill annealed Ti-6Al-4V alloy plate. The rates of fatigue crack growth were determined as a function of temperature, ranging from room temperature to about 290 C, and as a function of the crack tip stress intensity factor in a dehumidified high purity argon environment. Limited correlative experiments were carried out in distilled water, dehumidified oxygen and hydrogen, and in vacuum. The results indicate that the rate of fatigue crack growth is essentially independent of test temperature in this alloy, and is affected by residual moisture in very small concentrations. Companion fractographic examinations suggest that the mechanims for fatigue crack growth in the various environments are essentially the same.

Wei, R. P.↗

Stresses in bonded materials with a crack perpendicular to the interface.

The problem of two elastic bonded half planes containing a crack perpendicular to the interface is considered. First the solution for the semi-infinite crack under concentrated wedge loading is given. Then the problem of a finite crack fully imbedded in one of the half planes of terminating at the interface is considered. The Mellin transform in conjunction with the dislocations is used to formulate the problem and to derive the integral equation. The integral equation is solved; the stress intensity factors, the crack surface displacement, and the stresses around the crack tip terminating at the interface are obtained. Noting that the power of the singularity for the interface tip of the crack is not -1/2, a tentative fracture criterion dealing with the initiation of fracture propagation is proposed.

Cook, T. S.↗

An Experimental Investigation of the Effects of Vacuum Environment on the Fatigue Life, Fatigue-Crack-Growth Behavior, and Fracture Toughness of 7075-T6 Aluminum Alloy

Axial load fatigue life, fatigue-crack propagation, and fracture toughness tests were conducted on 0.090-inch thick specimens made of 7075-T6 aluminum alloy. The fatigue life and fatigue-crack propagation experiments were conducted at a stress ratio of 0.02. Maximum stresses ranged from 33 to 60 ksi in the fatigue life experiments, and from 10 to 40 ksi in the fatigue-crack propagation experiments, and fatigue life experiments were conducted at gas pressures of 760, 0.5, 0.05, and 0.00000005 torr. Fatigue-crack-growth and fracture toughness experiments were conducted at gas pressures of 760 and 5 x 10 to the minus 8th power torr. Residual stress measurements were made on selected fatigue life specimens to determine the effect of such stresses on fatigue life. Analysis of the results from the fatigue life experiments indicated that fatigue life progressively increased as the gas pressure decreased. Analysis of the results from the fatigue-crack-growth experiments indicates that at low values of stress-intensity range, the fatigue crack growth rates were approximately twice as high in air as in vacuum. Fracture toughness data showed there was essentially no difference in the fracture toughness of 7075-T6 in vacuum and in air.

Hudson, C. M.↗

Effect of specimen thickness of fatigue-crack-growth behavior and fracture toughness of 7075-T6 and 7178-T6 aluminum alloys

A study was made to determine the effects of specimen thickness on fatigue crack growth and fracture behavior of 7075-T6 and 7178-T6 aluminum alloy sheet and plate. Specimen thicknesses ranged from 5.1 to 12.7 mm (0.20 to 0.50 in.) for 7075-T6 and from 1.3 to 6.4 mm (0.05 to 0.25 in.) for 7178-T6. The stress ratios R used in the crack growth experiments were 0.02 and 0.50. For 7075-T6, specimen thickness had relatively little effect on fatigue-crack growth. However, the fracture toughness of the thickness of the thickest gage of 7075-T6 was about two-thirds of the fracture toughness of the thinner gages of 7075-T6. For 7178-T6, fatigue cracks generally grew somewhat faster in the thicker gages than in the thinnest gage. The fracture toughness of the thickest gage of 7178-T6 was about two-thirds of the fracture toughness of the thinner gages of 7178-T6. Stress intensity methods were used to analyze the experimental results. For a given thickness and value of R, the rate of fatigue crack growth was essentially a single-valued function of the stress intensity range for 7075-T6 and 7178-T6. An empirical equation developed by Forman, Kearney, and Engle fit the 7075-T6 and 7178-T6 crack growth data reasonably well.

Hudson, C. M.↗