Electrolyte Study for High-Nickel LiNi 0.9 Mn 0.05 Co 0.05 O 2 Cathodes

With an increasing demand for intermittent renewable energy and electric vehicles, it is imperative to develop lithium-ion batteries with Earth-abundant cathode materials. Cobalt (Co) is preferred to be kept at a minimum because of its high cost and limited mining options, yet it has played an essential role in the high-performance transition metal oxides (TMOs). Herein, we report work from Argonne National Laboratory, conducted under the U.S. DoE's Vehicle Technologies Office, Deep Dive consortium on Next-Generation Cathodes, to optimize electrolytes for LiNi 0.9 Mn 0.05 Co 0.05 O 2 . LiNi 0.9 Mn 0.05 Co 0.05 O 2 is a high-Ni TMO benchmark as it outperforms most other TMOs under standard cycling conditions. In this study, we use the figure-of-merit approach to optimize electrolytes for this novel cathode material. Dual-salt carbonate electrolytes containing lithium difluorooxyphosphate and hexafluorophosphates were found to be the best for capacity retention and slowing the impedance rise. Importantly, transition metal dissolution and lithium inventory losses in the solid electrolyte interface were found to be the major causes for capacity fade.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Modelling of cracking during beam oscillation laser welding of a creep-resistant nickel alloy

During high power laser welding of Inconel 740H, horizontal solidification cracks form at locations between approximately 70–80% of the weld depth. With the integration of circular beam oscillation, the laser energy density distribution and underlying thermo-mechanical conditions were altered. By coupling three-dimensional heat transfer, fluid flow, and stress modelling tools, the role that circular beam oscillation plays in the formation of the strain rates and stresses driving this cracking phenomenon was identified. While the addition of a circular oscillation pattern appeared to lower the stress levels along the solidification front, it did not eliminate the appearance of horizontal cracking. Only when the beam amplitudes reached 1.6 mm did solidification cracking disappear, but the weld depths were also significantly reduced.

Gao, Mingze↗

Maximizing Calendering Effects Through the Mechanical Pulverization of Co-Free Nickel-Rich Cathodes in Lithium-Ion Cells

Calendering is a technique used to maximize the volumetric energy density of battery electrodes. However, higher amounts of calendering result in increased tortuosity and particle cracking. We propose a novel packing structure of electrode particles to maximize calendering benefits while minimizing particle fracture. Cobalt-free layered oxide cathode LiNi0.92Mn0.04Al0.04O2 (NMA) particles are pulverized through ball-milling and coated with lithium phosphate. Pulverized and pristine NMA are fabricated into “bimodal” electrodes, whereas “unimodal” electrodes consist of only pristine NMA. Each electrode type was made into 30% porosity, 40% porosity, and uncalendered coin cell samples. X-ray diffraction suggests that the unimodal samples suffer from more particle fracture than the bimodal samples when calendered to the same porosity of 30%. Electrochemical impedance spectroscopy suggests that the bimodal electrodes exhibit lower surface film resistance. This is supported by enhanced capacity retention for the bimodal samples after 100 cycles.

25 ENERGY STORAGE↗

Process design for calcination of nickel-based cathode materials by in situ characterization and multiscale modeling

Developing battery materials towards commercial use, from the early discovery through synthesis, processing, scaling up, and eventually to industrial production, may take decades. A notable example is Ni-based layered oxides, which were discovered as early as 1950s and intensively pursued as cathode active materials (CAMs) since the early 90s but have yet to realize their full commercial potential. Significant efforts have been devoted to materials development aiming at improving performance, far less to process development for large-scale synthesis and processing of CAMs. In this paper, we present a rational design of calcination for scalable production of Ni-based CAMs. We start with an overview of the current understanding and knowledge gaps hindering rational process design and scaling-up of the calcination process. Then with specific examples, we demonstrate how to tackle those fundamental challenges through in situ characterization and multiscale modeling. Finally, we conclude by providing perspectives on the remaining challenges and emerging opportunities in commercial development of Ni-based cathodes, calling for more endeavors in this field.

25 ENERGY STORAGE↗

Oxygen Reduction on Platinum-Nickel and Platinum-Cobalt Alloy Based Catalysts for High Temperature Proton Exchange Membrane Fuel Cells

Catalyst layers, with commercial PtNi/TKK (TECNiE52; platinum 46.5 wt%), PtCo/TKK (TEC36E52; platinum 45.8 wt%) catalysts, and an in-house catalyst PtNi-NC (platinum 38.4 wt%), synthesised using acoustic mixer and a tube furnace, are prepared using three different ionomers: 20 wt% Nafion®, 60 wt% polytetrafluoroethylene (PTFE), and an in-house 5 wt% ionomer (‘Ionomer X’). These inks are bar-coated onto carbon paper gas diffusion layers (GDLs), which are cut into 3 cm × 5 cm pieces. The coated layers are tested for oxygen reduction in a commercial gas diffusion electrode (GDE) test cell, FlexCell® (Gaskatel GmbH, Germany), using 85 wt% phosphoric acid at both room temperature and at 155°C. This study evaluates the polynorbornene (PNB)-based in-house ionomer performance as binder and in-house catalyst oxygen reduction reaction (ORR) activity in comparison to commercial products. The catalyst layers are characterised using X-ray diffraction (XRD) analysis, X-ray photoelectron spectroscopy (XPS), and high-angle annular dark-field scanning transmission electron microscopy (HAADF-STEM). Among the catalyst layers prepared with PTFE ionomer and tested at 155°C, the in-house catalyst demonstrates the highest ORR activity. Ionomer X proves to be a good candidate to be used as a per- and polyfluoroalkyl-free binder for high-temperature (HT) proton exchange membrane fuel cell (PEMFC) applications.

85 wt% phosphoric acid↗

Distribution of nickel(II) ions adsorbed at the muscovite mica (001)-water interface determined by in-situ resonant anomalous X-ray reflectivity

Mineral-water interfaces mediate adsorption, ion exchange, and secondary mineral formation that control element mobility in natural and engineered systems. Reliable prediction and control of these processes require a fundamental understanding of the interfacial structure that links adsorbed ion speciation to macroscopic sorption capacity and strength. Here, we determine atomic-scale changes in hydration and distribution of Ni(II) at the muscovite mica (001)-water interface using in situ high-resolution X-ray reflectivity (XR) and resonant anomalous X-ray reflectivity (RAXR) at 1 mM NiCl2 and pH 5.7. XR reveals reorganization of the primary hydration structure relative to that in deionized water: the water layer adsorbed in the cavity sites at a height of ~1.3 Å disappears, while distinct solution layers emerge at ~2.3, ~4.1, and ~5.6 Å above the basal oxygen plane. RAXR resolves three interfacial Ni(II) species: a dominant outer-sphere complex at 3.65 Å (~80% of the total coverage), a minor inner-sphere complex at 0.75 Å, and a low-coverage, more distant outer-sphere species at 5.63 Å. These three adsorbed Ni(II) species account for a total Ni(II) coverage of 0.54 ± 0.02 ion per unit cell area that compensates for the surface charge. These results highlight the role of interfacial hydration in controlling the speciation and stability of adsorbate cations on the negatively charged mica surface, providing quantitative insight into predicting the geochemical behavior of divalent metal cations in the aqueous environments.

Lee, Sang Soo↗