Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Glasses”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 757 records · Page 42

In-Situ Crystallization of a Lithium Disilicate Glass--Effect of Pressure on Crystal Growth Rate

Crystallization of a Li2O.2SiO2 (LS2) glass subjected to a uniform hydrostatic pressure of 4.5 GPa and 6 GPa was investigated up to a temperature of 750 C. The density of the compressed glass is about 2% greater at 4.5 GPa than at 1 atm and, depending upon the processing temperature, up to 10% greater at 6 GPa. Crystal growth rates investigated as a function of temperature and pressure show that lithium disilicate crystal growth is an order of magnitude slower at 4.5 GPa than 1 atm resulting in a shift of +45 C (plus or minus 10 C) in the growth rate curve at high pressure compared to 1 atm condition. At 6 GPa lithium disilicate crystallization is suppressed entirely, while a new high pressure lithium metasilicate crystallizes at temperatures 95 C (plus or minus 10 C) higher than those reported for lithium disilicate crystallization at 1 atm. The decrease in crystal growth rate with increasing pressure for lithium disilicate glass up to 750 C is related to an increase in viscosity with pressure associated with fundamental changes in glass structure accommodating densification.

Fuss, T.↗

FE-SEM, FIB and TEM Study of Surface Deposits of Apollo 15 Green Glass Volcanic Spherules

Surface deposits on lunar pyroclastic green (Apollo 15) and orange (Apollo 17) glass spherules have been attributed to condensation from the gas clouds that accompanied fire-fountain eruptions. The fire fountains cast molten lava high above the lunar surface and the silicate melt droplets quenched before landing producing the glass beads. Early investigations showed that these deposits are rich in sulfur and zinc. The deposits are extremely fine-grained and thin, so that it was never possible to determine their chemical compositions cleanly by SEM/EDX or electron probe x-ray analysis because most of the excited volume was in the under-lying silicate glass. We are investigating the surface deposits by TEM, using focused ion beam (FIB) microscopy to extract and thin the surface deposits. Here we report on chemical mapping of a FIB section of surface deposits of an Apollo green glass bead 15401using the ultra-high resolution JEOL 2500 STEM located at NASA Johnson Space Center.

Ross, Daniel K.↗

Vibration Considerations for Cryogenic Tanks Using Glass Bubbles Insulation

The use of glass bubbles as an efficient and practical thermal insulation system has been previously demonstrated in cryogenic storage tanks. One such example is a spherical, vacuum-jacketed liquid hydrogen vessel of 218,000 liter capacity where the boiloff rate has been reduced by approximately 50 percent. Further applications may include non-stationary tanks such as mobile tankers and tanks with extreme duty cycles or exposed to significant vibration environments. Space rocket launch events and mobile tanker life cycles represent two harsh cases of mechanical vibration exposure. A number of bulk fill insulation materials including glass bubbles, perlite powders, and aerogel granules were tested for vibration effects and mechanical behavior using a custom design holding fixture subjected to random vibration on an Electrodynamic Shaker. The settling effects for mixtures of insulation materials were also investigated. The vibration test results and granular particle analysis are presented with considerations and implications for future cryogenic tank applications. A thermal performance update on field demonstration testing of a 218,000 L liquid hydrogen storage tank, retrofitted with glass bubbles, is presented. KEYWORDS: Glass bubble, perlite, aerogel, insulation, liquid hydrogen, storage tank, mobile tanker, vibration.

Werlink, Rudolph J.↗

Adhesion Between Volcanic Glass and Spacecraft Materials in an Airless Body Environment

The successful exploration of airless bodies, such as the Earth s moon, many smaller moons of the outer planets (including those of Mars) and asteroids, will depend on the development and implementation of effective dust mitigation strategies. The ultrahigh vacuum environment (UHV) on the surfaces of these bodies, coupled with constant ion and photon bombardment from the Sun and micrometeorite impacts (space weathering), makes dust adhesion to critical spacecraft systems a severe problem. As a result, the performance of thermal control surfaces, photovoltaics and mechanical systems can be seriously degraded even to the point of failure. The severe dust adhesion experienced in these environments is thought to be primarily due to two physical mechanisms, electrostatic attraction and high surface energies, but the dominant of these has yet to be determined. The experiments presented here aim to address which of these two mechanisms is dominant by quantifying the adhesion between common spacecraft materials (polycarbonate, FEP and PTFE Teflon, (DuPont) Ti-6-4) and a synthetic noritic volcanic glass, as a function of surface cleanliness and triboelectric charge transfer in a UHV environment. Adhesion force has been measured between pins of spacecraft materials and a plate of synthetic volcanic glass by determining the pull-off force with a torsion balance. Although no significant adhesion is observed directly as a result of high surface energies, the adhesion due to induced electrostatic charge is observed to increase with spacecraft material cleanliness, in some cases by over a factor of 10, although the increase is dependent on the particular material pair. The knowledge gained by these studies is envisioned to aid the development of new dust mitigation strategies and improve existing strategies by helping to identify and characterize mechanisms of glass to spacecraft adhesion for norite volcanic glass particles. Furthermore, the experience of the Apollo missions revealed that dust mitigation strategies must be subjected to high fidelity tests. To facilitate the effectiveness of ground-based testing of mitigation strategies, the issue of a pressure limit for high fidelity tests will be addressed.

Berkebile, Stephen↗

Shock Experiments on Basalt - Ferric Sulfate Mixes at 21 GPa & 49 GPa and their Relevance to Martian Meteorite Impact Glasses

Large abundance of Martian atmospheric gases and neutron-induced isotopic excesses as well as Rb-Sr isotopic variations determined in some impact glasses in basaltic shergottites (e.g., Shergotty #DBS, Zagami #H1 and EET79001 #27, #8 and #104) provide definitive evidence for the occurrence of a Martian regolith component in their constituent mineral assemblages. Some of these glass-es, known as gas-rich impact-melts (GRIM), contain numerous micron-sized iron sulfide blebs along with minor amounts of iron sulfate particulates. As these GRIM glasses contain a Martian regolith component and as iron sulfates (but not sulfides) are found to occur abundantly on the Mars surface, we suggested that the sulfide blebs in GRIMs were likely generated by shock-reduction of the parental iron sulfate bearing regolith material that had been incorporated into the cavities/crevices of basaltic host rock prior to the impact event on Mars. To test whether the sulfates could be reduced to sulfides by impact shock, we carried out laboratory shock experiments on a basalt plus ferric sulfate mixture at 49 GPa at the Caltech Shock Wave Laboratory and at 21 GPa at Johnson Space Center (JSC) Experimental Impact Laboratory. The experimental details and the preliminary results for the Caltech 49 GPa experiment were presented at LPSC last year. Here, we report the results for the 21 GPa experiment at JSC and compare these results to obtain further insight into the mechanism of the bleb formation in the GRIM glasses.

Rao, M. N.↗

Tracking the Depleted Mantle Signature in Melt Inclusions and Residual Glass of Basaltic Martian Shergottites using Secondary Ionization Mass Spectrometry

Trace element abundances of depleted shergottite magmas recorded by olivine-hosted melt inclusions (MI) and interstitial mesostasis glass were measured using the Cameca ims-1270 ion microprobe. Two meteorites: Tissint, an olivine-­phyric basaltic shergottite which fell over Morocco July 18th 2001; and the Antarctic meteorite Yamato 980459 (Y98), an olivine-phyric basaltic shergottite with abundant glassy mesostasis have been studied. Chondrite-­normalized REE patterns for MI in Tissint and Y98 are characteristically LREE depleted and, within analytical uncertainty, parallel those of their respective whole rock composition; supporting each meteorite to represent a melt composition that has experienced closed-­system crystallization. REE profiles for mesostasis glass in Y98 lie about an order of magnitude higher than those from the MI; with REE profiles for Tissint MI falling in between. Y98 MI have the highest average Sm/Nd and Y/Ce ratios, reflecting their LREE depletion and further supporting Y98 as one of our best samples to probe the depleted shergotitte mantle. In general, Zr/Nb ratios overlap between Y98 and Tissint MI, Ce/Nb ratios overlap between Y98 MI and mesostasis glass, and Sm/Nd ratios overlap between Y98 mesostasis glass and Tissint MI. These features support similar sources for both, but with subtle geochemical differences that may reflect different melting conditions or fractionation paths during ascent from the mantle. Interestingly, the REE patterns for both Y98 bulk and MI analyses display a flattening of the LREE that suggests a crustal contribution to the Y98 parent melt. This observation has important implications for the origins of depleted and enriched shergottites.

Peters, Timothy J.↗

Fractal Loop Heat Pipe Performance Comparisons of a Soda Lime Glass and Compressed Carbon Foam Wick

This study compares heat flux performance of a Loop Heat Pipe (LHP) wick structure fabricated from compressed carbon foam with that of a wick structure fabricated from sintered soda lime glass. Each wick was used in an LHP containing a fractal based evaporator. The Fractal Loop Heat Pipe (FLHP) was designed and manufactured by Mikros Manufacturing Inc. The compressed carbon foam wick structure was manufactured by ERG Aerospace Inc., and machined to specifications comparable to that of the initial soda lime glass wick structure. Machining of the compressed foam as well as performance testing was conducted at the United States Naval Academy. Performance testing with the sintered soda lime glass wick structures was conducted at NASA Goddard Space Flight Center. Heat input for both wick structures was supplied via cartridge heaters mounted in a copper block. The copper heater block was placed in contact with the FLHP evaporator which had a circular cross-sectional area of 0.88 cm(sup 2). Twice distilled, deionized water was used as the working fluid in both sets of experiments. Thermal performance data was obtained for three different Condenser/Subcooler temperatures under degassed conditions. Both wicks demonstrated comparable heat flux performance with a maximum of 75 W/cm observed for the soda lime glass wick and 70 W /cm(sup 2) for the compressed carbon foam wick.

Myre, David↗

Systems and Methods for Implementing Bulk Metallic Glass-Based Macroscale Compliant Mechanisms

Systems and methods in accordance with embodiments of the invention implement bulk metallic glass-based macroscale compliant mechanisms. In one embodiment, a bulk metallic glass-based macroscale compliant mechanism includes: a flexible member that is strained during the normal operation of the compliant mechanism; where the flexible member has a thickness of 0.5 mm; where the flexible member comprises a bulk metallic glass-based material; and where the bulk metallic glass-based material can survive a fatigue test that includes 1000 cycles under a bending loading mode at an applied stress to ultimate strength ratio of 0.25.

Hofmann, Douglas C.↗

Apollo Sample 64455: Petrologic and Geochemical Characterization of a Glass-Coated Impact Melt Rock

Introduction and Background: Impact melts are a key product of the impact cratering process. Impact melts can turbulently entrain pre-existing rock fragments, and melt part of those entrained materials until thermal equilibrium is achieved [1–3]. Lunar impact melt rocks are valuable for determining the precise ages of basin-forming and cratering events, which anchor the cratering chronology and dynamics of the entire solar system [4, and references therein]. Additionally, entrained clasts can inform on the petrology and age of crustal materials that predate the melt-forming impact. In lithologies where no pristine samples are available, entrained materials may hold the record of endogenous lunar volatiles, provided we can untangle their impact histories as high temperature impact melt can heat the clasts and may alter their native volatiles or isotopic signatures [5–6]. Here, we characterize an Apollo 16 sample, 64455,70B, in an effort to understand the physical, microstructural, and geochemical consequences of impact melt contact metamorphism. We acquired optical light and x-ray maps of the sample, as well as quantitative analyses via electron probe microanalysis (EPMA). These tasks allow us to better understand the interaction between impact melts and entrained clasts, ultimately closing knowledge gaps in high-temperature impact processing on planetary surfaces. Sample Description: Sample 64455 is an oblong crystalline rock encased in glass to form an egg-like shape [7–8]. The impact melt coating has altered the outer (1 to 2 mm) rind of the crystalline rock and has preserved schlieren. The interior crystalline rock is likely a crystalline impact melt rock based on its bulk Ir content of 2.25 parts per billion [9]. The composition of the impact melt glass rind cannot be solely derived from the crystalline interior, the glassy rind is more aluminous and less magnesian [10]. Neither the crystalline interior nor the glassy rind were radiometrically age dated, although several studies investigated its cosmogenic isotopes and exposure ages, which reveal the sample was exposed on the lunar surface for ~1–2 Ma [11–13]. Preliminary Results: The interior crystalline rock consists primarily of plagioclase with interstitial pyroxene and olivine. Plagioclase grains are zoned and compositions range from An97–89, while pyroxene compositions generally range from En68Fs19Wo13 to En82Fs15Wo3 and olivine are Fo77 to Fo85. Minor phases include Fe-Ni metal, Ca-phosphates, a K- and Si-rich phase, sulfides, and Fe-phosphides. The glass rind contains approximately 44 wt.% SiO2, 25 wt.% Al2O3, 6 wt.% FeO, 8 wt.% MgO, and 14 wt.% CaO, with other oxides at <1 wt.% each, although the composition of the glass becomes more variable closest to the crystalline rock. The rind consists of rounded plagioclase, pyroxene, and olivine crystals with interstitial melt. In some locations, the rounded crystals are surrounded by closely-packed, blade-like crystals, <5 µm in width. These results indicate that the crystalline interior has partially melted where in contact with the high-temperature impact melt and while further investigation is needed, pyroxene may have preferentially melted relative to olivine and plagioclase. Future Work: We plan to conduct electron backscatter diffraction (EBSD) mapping in order to determine crystallinity and crystal orientation. Next using transmission electron microscopy (TEM) data in conjunction with EBSD and EPMA information, we will model the diffusion of moderately volatile elements between the melt and remnant crystals.

A C Stadermann↗

Sulfur outgassing and in-gassing in lunar orange glass beads and implications for 33S “Anomaly” in the Moon

Our recent investigations have discovered inward diffusion (in-gassing) of moderately volatile elements (MVEs; e.g., Na, K and Cu) from volcanic gas into volcanic beads/droplets. In this work, we examine the distribution of sulfur in lunar orange glass beads. Our analyses reveal that sulfur exhibits a non-uniform distribution across the beads, forming “U” or “W” shaped profiles typical of in-gassing. A model developed to assess sulfur contributions from different sources (original magmatic sulfur versus atmospheric in-gassed sulfur) in the orange beads indicates that atmospheric sulfur in-gassed during eruption contributes approximately 9–24 % to the total sulfur content of an orange bead, averaging around 16 %. This in-gassed sulfur is derived from the eruption plume, where atmospheric sulfur could undergo photochemical reactions induced by UV light, leading to mass independent fractionation and a distinct sulfur isotope signature. Interestingly, a recent study discovered a small mass independent isotope fractionation of sulfur in lunar orange glass beads in drive tube 74002/1 and a lack of such mass independent isotope fractionation in black glass beads in the same lunar sample. This finding contrasts with sulfur in lunar basalts, which typically exhibit mass dependent fractionation. With our work, the observed mass independent fractionation signal in sulfur isotopes of orange beads can be attributed to the in-gassing of photolytic sulfur in the optically thin part of the eruption plume where UV light can penetrate. Using the sulfur isotope data of lunar orange beads, we estimate that the Δ33S value of atmospheric sulfur is approximately −0.18 ‰. Our study provides new insights into the complex dynamics of volatile elements in lunar volcanic processes, highlighting the role of in-gassing in shaping sulfur isotope signatures in volcanic glass beads.

Xue Su↗

Encapsulated sulfide glass solid electrolytes and solid-state laminate electrode assemblies

Nanofilm-encapsulated sulfide glass solid electrolyte structures and methods for making the encapsulated glass structures involve a lithium ion conducting sulfide glass sheet encapsulated on its opposing major surfaces by a continuous and conformal nanofilm made by atomic layer deposition (ALD). During manufacture, the reactive surfaces of the sulfide glass sheet are protected from deleterious reaction with ambient moisture, and the nanofilm can be configured to provide additional performance advantages, including enhanced mechanical strength and improved chemical resistance.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Computationally-Aided Design of a Small-Scale Radioactive Waste Glass Melter

To provide mission support to the Hanford Waste Immobilization and Treatment Plant for the vitrification of legacy nuclear tank waste, a reduced-scale vitrification pilot system is being designed to process simulated and actual radioactive tank wastes. The tank waste will be separated into high-level waste (HLW) and low-activity waste (LAW) fractions, where the majority by mass (~90%) is LAW and by activity (>95%) is HLW. The first tank waste to be processed at the WTP will be LAW. Since Hanford tank waste and the resultant melter feed compositions are known to vary widely, pilot-scale operations are essential to identify potential problems, provide needed data, confirm assumptions, and determine impacts to full-scale melters and off-gas systems from these different feeds. In addition, the reduced-scale melter system must be capable of quickly providing results to operations without the typically high costs of radioactive operations and provide an engineering platform in close proximity to local operations staff. The objective is to produce similar process conditions to those encountered in the full-scale LAW melters and minimize the volume of radioactive waste necessary for the evaluations. To this end, melter design features are being explored to increase production without significantly increasing surface area, melter glass volumes or compromising data quality. In support of these objectives, a set of computational fluid dynamic models have been developed to provide insight into the flow patterns within these small melters and evaluate design features to increase production without significantly increasing glass inventory. Computed velocities were evaluated at the interface between the cold cap and the molten glass pool and within the bulk glass pool. A method was developed to correlate results to an estimated melt rate and down-select design features that produce the highest gains.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Encapsulated sulfide glass solid electrolytes and solid-state laminate electrode assemblies

Nanofilm-encapsulated sulfide glass solid electrolyte structures and methods for making the encapsulated glass structures involve a lithium ion conducting sulfide glass sheet encapsulated on its opposing major surfaces by a continuous and conformal nanofilm made by atomic layer deposition (ALD). During manufacture, the reactive surfaces of the sulfide glass sheet are protected from deleterious reaction with ambient moisture, and the nanofilm can be configured to provide additional performance advantages, including enhanced mechanical strength and improved chemical resistance.

Visco, Steven J.↗

Encapsulated sulfide glass solid electrolytes and solid-state laminate electrode assemblies

Nanofilm-encapsulated sulfide glass solid electrolyte structures and methods for making the encapsulated glass structures involve a lithium ion conducting sulfide glass sheet encapsulated on its opposing major surfaces by a continuous and conformal nanofilm made by atomic layer deposition (ALD). During manufacture, the reactive surfaces of the sulfide glass sheet are protected from deleterious reaction with ambient moisture, and the nanofilm can be configured to provide additional performance advantages, including enhanced mechanical strength and improved chemical resistance.

Visco, Steven J.↗

Determination of the structure of lithium niobosilicate glasses by molecular dynamics simulation with a new Nb-O potential

A partial charge empirical potential for the Nb-O pair has been developed based on existing parameters of other pairs in a Teter potential to enable molecular dynamics simulations of both lithium niobate crystal and lithium niobosilicate glasses. The developed potential is capable of describing structural features of lithium niobosilicate glasses in a wide composition range, including niobium coordination number and bond length, density, bond angle distribution, polyhedral distribution and fraction of bridging oxygen. Furthermore, the results obtained using this new potential show good agreement with experimental data of density and structure from Raman spectroscopy of lithium niobosilicate glasses and X-ray absorption spectroscopy near Nb K-edge.

36 MATERIALS SCIENCE↗

Anomalous fast atomic dynamics in bulk metallic glasses

It is believed that the strong glass formers tend to be dense packing and have rather slow atomic dynamics. Here, we report that the anomalous fast atomic dynamics exist in an Au 55 Cu 20 Ag 5 Si 20 metallic glass (MG) with good glass forming ability (GFA) by combining X-ray photon correlation spectroscopy measurements with ab initio molecular dynamics simulations. The fast dynamics are mainly originated from the increased mobility of Cu atoms by Ag addition. Ag atoms are inclined to locate at Cu-centered <0, 2, 8, 1> motifs, which slow or accelerate the dynamics of shell Cu atoms, depending on whether Ag atoms appear at the first shells or not, leading to the formation of structural heterogeneity at the atomic level. The results enrich the understanding of atomic dynamics in Cue-Ag-containing MGs and will trigger more studies on the dynamics-GFA relationship in MGs.

74 ATOMIC AND MOLECULAR PHYSICS↗

Predicting the location of shear band initiation in a metallic glass

We report atomistic simulation results which indicate that the location of shear banding in a metallic glass (MG) can be ascertained with reasonably high accuracy solely from the undeformed static structure. Correlation is observed between the location of the initiation of shear bands in a simulated MG and the initial distribution of the density of fertile sites (DFS) for stress-driven shear transformations identified a priori based on a deep learning model devised in our recent work. In addition, we demonstrated that one can judge whether a glass is brittle or ductile solely based upon its initial DFS distribution. These validate that shear bands in MG arise from nonlinear instabilities and that the as-quenched glass structure contains inhomogeneities that influence these instabilities. In this study, we also reveal an important subtlety regarding the nondeterministic nature of athermal quasistatic shear simulations.

36 MATERIALS SCIENCE↗

Hybrid Li-S pouch cell with a reinforced sulfide glass solid-state electrolyte film separator

Here, in this paper, sulfide glass electrolyte powder with a nominal composition of (Li 2 S) 60 (SiS 2 ) 28 (P 2 S 5 ) 12 is hot pressed at a 330°C and 12 MPa into separator films using non-woven fiberglass reinforcement. The reinforced separator films are 93% dense, bendable, and have an ionic conductivity of 0.7 mS/cm at room temperature. When integrated into hybrid Li-S coin cells with liquid electrolyte, these reinforced glass separators blocked the parasitic polysulfide shuttle sufficiently to enable reversible cycling without LiNO 3 co-salt. Furthermore, the scalability of the reinforced glass separator technology is demonstrated by assembling and testing a hybrid single-layer pouch cell.

25 ENERGY STORAGE↗