Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Disordered alloys”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

745 records · Page 42

Tuneable magnetic patterning of paramagnetic Fe{sub 60}Al{sub 40} (at. %) by consecutive ion irradiation through pre-lithographed shadow masks

Arrays of ferromagnetic circular dots (with diameters ranging from 225 to 420 nm) have been prepared at the surface of atomically ordered paramagnetic Fe{sub 60}Al{sub 40} (at. %) sheets by means of ion irradiation through prelithographed poly(methyl methacrylate) (PMMA) masks. The cumulative effects of consecutive ion irradiation (using Ar{sup +} ions at 1.2 x 10{sup 14} ions/cm{sup 2} with 10, 13, 16, 19 and 22 keV incident energies) on the properties of the patterned dots have been investigated. A progressive increase in the overall magneto-optical Kerr signal is observed for increasingly larger irradiation energies, an effect which is ascribed to accumulation of atomic disorder. Conversely, the coercivity, H{sub C}, shows a maximum after irradiating at 16-19 keV and it decreases for larger irradiation energies. Such a decrease in H{sub C} is ascribed to the formation of vortex states during magnetization reversal, in agreement with results obtained from micromagnetic simulations. At the same time, the PMMA layer, with an initial thickness of 90 nm, becomes progressively thinned during the successive irradiation processes. After irradiation at 22 keV, the remaining PMMA layer is too thin to stop the incoming ions and, consequently, ferromagnetism starts to be generated underneath the nominally masked areas. These experimental results are in agreement with calculations using the Monte-Carlo simulation Stopping Range of Ions in Matter software, which show that for exceedingly thin PMMA layers Ar{sup +} ions can reach the Fe{sub 60}Al{sub 40} layer despite the presence of the mask.

36 MATERIALS SCIENCE↗

High-entropy induced a glass-to-glass transition in a metallic glass

Glass-to-glass transitions are useful for us to understand the glass nature, but it remains difficult to tune the metallic glass into significantly different glass states. Here, we have demonstrated that the high-entropy can enhance the degree of disorder in an equiatomic high-entropy metallic glass NbNiZrTiCo and elevate it to a high-energy glass state. An unusual glass-to-glass phase transition is discovered during heating with an enormous heat release even larger than that of the following crystallization at higher temperatures. Dramatic atomic rearrangement with a short- and medium-range ordering is revealed by in-situ synchrotron X-ray diffraction analyses. This glass-to-glass transition leads to a significant improvement in the modulus, hardness, and thermal stability, all of which could promote their applications. Based on the proposed high-entropy effect, two high-entropy metallic glasses are developed and they show similar glass-to-glass transitions. These findings uncover a high-entropy effect in metallic glasses and create a pathway for tuning the glass states and properties.

36 MATERIALS SCIENCE↗

Nanoscale magnetic phase competition throughout the Ni 50– x Co x Mn 40 Sn 10 phase diagram: Insights from small-angle neutron scattering

The Ni 2 MnSn-derived Ni 50– x Co x Mn 25+ y Sn 25– y alloys are premier examples of a class of off-stoichiometric Heusler alloys recently discovered to exhibit attractive magnetic properties in tandem with extraordinarily reversible martensitic phase transformations. Multiferroicity, magnetic phase competition and separation, field-induced martensitic transformations, magnetic shape memory behavior, and sizable magneto-, elasto-, and barocaloric effects result, generating substantial interest and application potential. In this work we expand on a prior small-angle neutron scattering (SANS) study at a single composition (Ni 44 Co 6 Mn 40 Sn 10 ) by exploring all three main regions of the recently established Ni 50–x Co x Mn 40 Sn 10 phase diagram, i.e., at the representative y = 15 composition. Wide temperature and scattering wave-vector range (20–500K, 0.004–0.2Å –1 ) SANS data on x = 2, 6, and 14 polycrystals provide a detailed picture of the evolution in magnetic order and inhomogeneity. Consistent with recent studies with a variety of techniques, phase separation into short-range coexisting ferromagnetic and antiferromagnetic regions is deduced below the martensitic transformation at x = 2 and 6, with average ferromagnetic cluster spacing of ~13 nm. Remarkably, at x = 14, where the martensitic transformation is suppressed and ferromagnetic austenite is stabilized to low temperatures, nanoscopic magnetic inhomogeneity nevertheless persists. Further, distinct ferromagnetic clusters (~36-nm average spacing) in a ferromagnetic matrix are observed at intermediate temperatures, homogenizing into a uniform long-range ordered ferromagnet only at low temperatures. This unusual ferromagnet cluster/ferromagnet matrix inhomogeneity, as well as x -dependent subtleties of the superparamagnetic freezing of ferromagnetic clusters, are discussed in light of 55 Mn nuclear magnetic resonance data, and the recent observation of annealing-induced core/shell nanoprecipitates. The origins of nanoscalemagnetic inhomogeneity are discussed in terms of statistical variations in local composition and structure, tendency to chemical phase separation, and other forms of disorder.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Co{sub 2}FeAl Heusler thin films grown on Si and MgO substrates: Annealing temperature effect

10 nm and 50 nm Co{sub 2}FeAl (CFA) thin films have been deposited on MgO(001) and Si(001) substrates by magnetron sputtering and annealed at different temperatures. X-rays diffraction revealed polycrystalline or epitaxial growth (according to CFA(001)[110]//MgO(001)[100] epitaxial relation) for CFA films grown on a Si and on a MgO substrate, respectively. For these later, the chemical order varies from the A2 phase to the B2 phase when increasing the annealing temperature (T{sub a}), while only the A2 disorder type has been observed for CFA grown on Si. Microstrip ferromagnetic resonance (MS-FMR) measurements revealed that the in-plane anisotropy results from the superposition of a uniaxial and a fourfold symmetry term for CFA grown on MgO substrates. This fourfold anisotropy, which disappears completely for samples grown on Si, is in accord with the crystal structure of the samples. The fourfold anisotropy field decreases when increasing T{sub a}, while the uniaxial anisotropy field is nearly unaffected by T{sub a} within the investigated range. The MS-FMR data also allow for concluding that the gyromagnetic factor remains constant and that the exchange stiffness constant increases with T{sub a}. Finally, the FMR linewidth decreases when increasing T{sub a}, due to the enhancement of the chemical order. We derive a very low intrinsic damping parameter (1.1×10{sup −3} and 1.3×10{sup −3} for films of 50 nm thickness annealed at 615 °C grown on MgO and on Si, respectively)

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Evidence for boron diffusion into sub-stoichiometric MgO (001) barriers in CoFeB/MgO-based magnetic tunnel junctions

Evidence of boron diffusion into the MgO barrier of a CoFeB/MgO based magnetic tunnel junction has been identified using analytical scanning transmission electron microscopy (STEM) and X-ray photoelectron spectroscopy. Structures were deposited by DC/RF-magnetron sputtering, where defective, sub-stoichiometric MgO barriers degrading device performance have been previously mitigated against by deposition of thin Mg layers prior to MgO deposition. We show that despite the protection offered by the Mg layer, disorder in the MgO barrier is still evident by STEM analysis and is a consequence of the oxidation of the Co{sub 40}Fe{sub 40}B{sub 20} surface during MgO deposition. Evidence of boron diffusion from CoFeB into the MgO barrier in the as-deposited and annealed structure is also presented, which in the as-deposited case we suggest results from the defective structures at the barrier interfaces. Annealing at 375 Degree-Sign C results in the presence of B in the trigonal coordination of [BO{sub 3}]{sup 3-} in the MgO barrier and partial crystallization of the top electrode (we presume there is also some boron diffusion into the Ta capping layer). The bottom electrode, however, fails to crystallize and much of the boron is retained in this thicker electrode. A higher annealing temperature or lower initial boron content is required to crystallize the bottom electrode.

36 MATERIALS SCIENCE↗

New FCC Mg–Zr and Mg–Zr–ti deuterides obtained by reactive milling

Results for binary Mg–Zr and ternary Mg–Zr–Ti mixtures ball milled at room temperature under reactive deuterium atmosphere (5.6–6.7 MPa) are reported. X-ray and neutron powder diffraction combined with Rietveld refinements show that two new cubic phases were formed during milling. Mg{sub 0.40}Zr{sub 0.60}D{sub 1.78} and Mg{sub 0.40}Zr{sub 0.26}Ti{sub 0.34}D{sub 1.98} crystallize with disordered face centered cubic metal atom arrangements. Results of differential scanning calorimetry and termogravimetric measurements demonstrate that both deuterides desorb deuterium at lower temperatures than MgD{sub 2}, ZrD{sub 2} or TiD{sub 2}; 528 and 575 K in the Mg–Zr–D and Mg–Zr–Ti–D system, respectively. Interestingly, Mg{sub 0.40}Zr{sub 0.26}Ti{sub 0.34}D{sub 1.98} stores deuterium reversibly at 673 K and 10 MPa of D{sub 2}. - Graphical abstract: High resolution SR-PXD patterns obtained for Mg{sub 0.40}Zr{sub 0.60}D{sub 1.78} and first time reported Mg{sub 0.40}Zr{sub 0.26}Ti{sub 0.34}D{sub 1.98}. - Highlights: • Synthesis and characterization of Mg{sub 0.40}Zr{sub 0.60}D{sub 1.78} and Mg{sub 0.40}Zr{sub 0.26}Ti{sub 0.34}D{sub 1.98}. • New deuterides obtained by milling under H{sub 2} gas pressure in the order of a few MPa. • Phases desorb deuterium at temperature lower than corresponding binary deuterides. • Mg{sub 0.40}Zr{sub 0.26}Ti{sub 0.34}D{sub 1.98} stores hydrogen reversibly at 673 K and 10 MPa of D{sub 2}.

36 MATERIALS SCIENCE↗

Crystal growth and properties of Ln{sub 2}Ag{sub 1-x}Ga{sub 10-y} (Ln=La, Ce), a disordered variant of the Ce{sub 2}NiGa{sub 10}-structure type

We report the flux growth and characterization of Ln{sub 2}Ag{sub 1-x}Ga{sub 10-y} (Ln=La, Ce), a disordered variant of the Ce{sub 2}NiGa{sub 10} structure type. Single crystals of La{sub 2}Ag{sub 1-x}Ga{sub 10-y} (x{approx}0.3; y{approx}0.6) and Ce{sub 2}Ag{sub 1-x}Ga{sub 10-y} (x{approx}0.3; y{approx}0.9) were grown by the self-flux method and characterized using single-crystal X-ray diffraction. Transport measurements of Ce{sub 2}Ag{sub 1-x}Ga{sub 10-y} (x{approx}0.3; y{approx}0.9) reveal metallic behavior with a transition at 3 K. Magnetic measurements indicate antiferromagnetic ordering at 3 K of localized Ce{sup 3+} moments for Ce{sub 2}Ag{sub 1-x}Ga{sub 10-y}. Magnetoresistance is positive with a maximum value of 16% at 9 T. La{sub 2}Ag{sub 1-x}Ga{sub 10-y} exhibits metallic behavior with magnetic susceptibility showing temperature independent paramagnetism. We will compare Ce{sub 2}Ag{sub 1-x}Ga{sub 10-y} (x{approx}0.3; y{approx}0.9) to Ce{sub 2}NiGa{sub 10} to examine the effects of transition metal substitution and to the related Ce(Ag,Ga){sub 4} phase to examine the effects of crystal structure on the physical properties. - Graphical abstract: The figure illustrates the structure of Ce{sub 2}Ag{sub 0.7(1)}Ga{sub 9.1(1)}, which can be described as a distorted variant of the Ce{sub 2}NiGa{sub 10} structure. The distorted gallium segments are best described as variants of CeGa{sub 6} (PuGa{sub 6}-structure type), and the distorted Ce(Ag,Ga){sub 4}-type segments are built of layers of face-sharing tetragonal antiprisms. Here M=Ag+Ga and the shaded atoms are partially occupied.

36 MATERIALS SCIENCE↗