Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “materials aging”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 739 records · Page 41

Precipitation kinetics during aging of an alumina-forming austenitic stainless steel

The microstructural evolution of DAFA26, an alumina-forming austenitic (AFA) stainless steel, was investigated during aging. The effect of aging at 750 °C and 800 °C on the growth of spherical γ’-Ni 3 (Al, Ti) particles present in the as-processed state was studied extensively using X-ray diffraction, microhardness testing, scanning electron microscopy, transmission electron microscopy, and atom probe tomography. The γ’ particles had a cube-on-cube orientation relationship with the matrix (i.e. ((010)(010) m //(010)(010) p , [100][100] m //[100][100] p )). The coarsening kinetics of γ’-Ni 3 Al particles were in agreement with the Lifshitz, Slyozof-Wagner theory. Coarse Laves phase particles were also present in the as-processed state, and during the aging process both smaller Laves phase precipitates and B2-NiAl precipitates formed on both the grain boundaries and in the matrix. As a result, the γ’ precipitates were determined to have the most impact on the room temperature hardness.

36 MATERIALS SCIENCE↗

Photoinduced aging and viscosity evolution in Se-rich Ge-Se glasses

We propose here to investigate the non-equilibrium viscosity of Ge-Se glasses under and after light irradiation. Ge{sub 10}Se{sub 90} and Ge{sub 20}Se{sub 80} fibers have been aged in the dark and under ambient light, over months. During aging, both the relaxation of enthalpy and the viscosity have been investigated. The viscosity was measured by shear relaxation-recovery tests allowing the measurement of non-equilibrium viscosity. When Ge{sub 10}Se{sub 90} glass fibers are aged under irradiation, a relatively fast fictive temperature decrease is observed. Concomitantly, during aging under irradiation, the non-equilibrium viscosity increases and reaches an equilibrium after two months of aging. This viscosity increase is also observed in Ge{sub 20}Se{sub 80} fibers. Nevertheless, this equilibrium viscosity is far below the viscosity expected at the configurational equilibrium. As soon as the irradiation ceases, the viscosity increases almost instantaneously by about one order of magnitude. Then, if the fibers are kept in the dark, their viscosity slowly increases over months. The analysis of the shear relaxation functions shows that the aging is thermorheologically simple. On the other side, there is no simple relaxation between the shear relaxation functions measured under irradiation and those measured in the dark. These results clearly suggest that a very specific photoinduced aging process occurs under irradiation. This aging is due to photorelaxation. Nevertheless, the viscosity changes are not solely correlated to photoaging and photorelaxation. A scenario is proposed to explain all the observed viscosity evolutions under and after irradiation, on the basis of photoinduced transient defects.

36 MATERIALS SCIENCE↗

Mechanical Properties and Corrosion Behavior of Spray-Formed 7075 Alloy with One-Stage Aging

The mechanical properties, corrosion resistance and microstructure of the spray-formed 7075 alloy after one-stage aging treatments were studied by using a tensile tester, hardness tester, slow strain rate test, electrical test, intergranular corrosion test, electrochemical corrosion test, scanning electron microscope and transmission electron microscope. The results show that the strength and hardness of the alloy have double peaks with the one-stage aging treatments. With aging at 120 °C for 24 h (first peak), abundant tiny η′ phases and η phases precipitate in the matrix. The tensile strength of the alloy increases to 760 MPa, and the elongation is 4.8%. After aging at 120 °C for 132 h (second peak), blocky η phases appear. The tensile strength and elongation of the alloy are 757 MPa and 5.9%, respectively. The grain boundary precipitates dissociate, and the precipitate-free zones are widened. The corrosion resistance of the alloy increases.

36 MATERIALS SCIENCE↗

Room Temperature Stamping of High-Strength Aluminum for Lightweight Structural Automotive Components

The use of aluminum (Al) 7xxx series in automobile structural applications is limited by factors such as its low room-temperature formability in T6 temper and the need for off-line artificial aging to regain high strength if it is formed in soft temper. In this study, two tempers were established that enable Al 7075 blanks to be room temperature stamped to create side impact beams that achieve near-T6 strength without post-forming artificial aging. It is shown that natural aging at room temperature, after solution treatment and before stamping, provides an alternative to high temperature pre-aging and hot stamping techniques in 7xxx alloys. Both tempers enabled room temperature stamping of the beams without cracking, indicating good formability. The Al beams were ~38% lighter than the benchmark boron steel beam. Further, the hardness in the low-deformation regions of the stamped Al beams were within 88% of a conventional 7075-T6 sheet. Paint-bake treatment of the beams appeared to cause over aging, lowering the ultimate tensile strength and ductility. Finite element three point bending simulations of the beams showed higher bending force and energy absorption before failure for the Al 7075 showing good promise for 7xxx series Al as a light-weight alternative to steel beams.

36 MATERIALS SCIENCE↗

Model ages of three uranium metal CRMs and implications for radiochronometry data interpretation

In this study, we report 230 Th/ 234 U and 231 Pa/ 235 U model ages in three uranium metal certified reference materials with distinct production histories and isotopic compositions ranging from depleted to highly enriched (CRMs 112-A, 115, and 116-A). Here, our results provide the first model age values for these materials using multiple radiochronometers, which can be used as reference values for quality control of radiochronometry measurements performed during nuclear forensic investigations. Furthermore, we evaluate the model ages in the context of available production records for the materials, which provides insight into the processes that may impact radiochronometry systems during uranium metal production.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Thermal aging of traditional and additively manufactured foams: analysis by time-temperature-superposition, constitutive, and finite-element models

Cellular solids or foams are a very important class of materials with diverse applications ranging from thermal insulation and shock absorbing support cushions, to light-weight structural and floatation components, and constitute crucial components in a large number of industries including automotive, aerospace, electronics, marine, biomedical, packaging, and defense. In many of these applications the foam material is subjected to long periods of continuous stress, which can, over time, lead to a permanent change in structure and a degradation in performance. In this report we summarize our modeling efforts to date on polysiloxane foam materials that form an important component in our systems. Aging of the materials was characterized by two measured quantities, i.e., compression set and load retention. Results of accelerated aging experiments were analyzed by an automated time-temperaturesuperposition (TTS) approach, which creates a master curve that can be used for long-term predictions (over decades) under ambient conditions. When comparing such master curves for traditional (stochastic) foams with those for recently 3D-printed (i.e., additively manufactured, or AM) foams, it became clear that AM foams have superior aging behavior. To gain deeper understanding, we imaged the microstructure of both foams using X-ray computed tomography, and performed finite-element analysis of the mechanical response within these microstructures. This indicates a wider stress variation in the stochastic foam with points of more extreme local stress as compared to the 3D printed material.

36 MATERIALS SCIENCE↗

Structural and compositional evolution of Al{sub 3}(Zr,Y) precipitates in Al-Zr-Y alloy

Structural and compositional evolution of Al{sub 3}(Zr,Y) precipitates in aged Al-Zr-Y alloy was investigated through atom probe tomography (APT) and transmission electron microscope (TEM) analysis and first principles calculations. The results show that short-bar-shaped D0{sub 19}-Al{sub 3}Y with some Zr atoms dissolved in precipitated at the very beginning of decomposition and worked as heterogeneous nuclei for L1{sub 2}-Al{sub 3}Zr with spherical morphology after being aged at 400 °C for 2 h. Quasi-static coarsening happened as the aging treatment lasted from 2 h to 200 h. However, distribution of Zr and Y atoms in Al{sub 3}(Zr,Y) is nearly uniform and Al{sub 3}(Zr,Y) do not have the typical “Al{sub 3}RE core-Al{sub 3}Zr shell” structure which observed in other RE containing Al-Zr-RE alloys with L1{sub 2}-Al{sub 3}RE as nuclei. First principles calculations revealed that binding energy between Y and Zr is strong during the growth of Al{sub 3}(Zr,Y), which led to the co-precipitation of Y and Zr atoms and attribute to the evolution of Al{sub 3}(Zr,Y). - Highlights: •Al{sub 3}Y precipitated firstly and then became nuclei for Al{sub 3}Zr during aging of Al-Zr-Y. •Al{sub 3}(Zr,Y) precipitates do not have the typical “Al{sub 3}Y core-Al{sub 3}Zr shell” structure. •Strong binding between Y and Zr led to the co-precipitation of Y and Zr atoms.

36 MATERIALS SCIENCE↗

Phase transformation sequence and magnetic properties of melt-spun SmCo-based alloy after isochronal heat treatment

The phase transformation sequence, microstructure and compositions, and magnetic properties for a melt-spun Sm(Co{sub 0.68}Fe{sub 0.2}Cu{sub 0.1}Zr{sub 0.02}){sub 7.5} alloy after isochronal heat treatments have been studied by using x-ray diffraction, transmission electron microscopy, three-dimensional atom probe (3DAP), and magnetometry. The as-spun ribbons had a single phase with the Cu{sub 7}Tb structure. After being aged at 720 deg. C, the single phase decomposed into two major phases: 2:17R and 1:5H, and one minor CoFeZr-rich phase. The formation of the Z-phase happened after the cellular structure, requiring a higher temperature than that for the cellular structure. The 3DAP analysis showed that Zr was depleted from the 2:17R and 1:5H phases by a half while the other elements remained almost unchanged when the aging temperature increased from 720 to 840 deg. C. In contrast to the sintered permanent magnets, Cu was enriched in the 1:5H phase with a much higher concentration (>40 at. %). The Cu enrichment also occurred at the boundary of the Z-phase. The coercivity achieved was H{sub c}=4.34 kOe following aging at 720 deg. C. The highest maximum energy product, (BH){sub max}, was 6.48 MG Oe after aging at 800 deg. C and the remanence to saturation magnetization ratio, M{sub r}/M{sub s}, was 0.69. This relatively low H{sub c} and high M{sub r}/M{sub s} ratio may be a consequence of the formation of a significant volume fraction of the CoFeZr-rich nanocrystalline phase.

36 MATERIALS SCIENCE↗

The Effect of Multistage Aging on Mechanical Properties and Microstructure of Forged 7050 Aluminum Alloys

A new four-stage aging treatment, which is composed of pre-aging, retrogression, natural aging (NA) and re-aging, is designed to increase the tensile properties and the fatigue life of forged 7050 aluminum alloy in this work. As compared to traditional T74 and RRA treatments, the four-stage aging-treated sample exhibits the highest tensile properties and ductility. The tensile strength and yield strength are 627 and 608 MPa, respectively, and the elongation is 11.3%. The results of TEM and DSC show that an increased G.P zones and fine η′ phase distributed in the matrix of the alloy are subjected by this new aging processing as compared with T74 and RRA treatments. The natural aging in four-stage aging treatment accelerates the diffusion of Mg vacancies, and promotes the precipitation of G.P zones in grain interior during re-aging stage. On the basis of dislocation shearing mechanism, more dense and fine G.P zones of four-stage aging temper result in the superior tensile strength as compared to T74 and RRA temper. In addition, a combination of shearable precipitates, fine GBPs and narrow PFZs is beneficial to the slip reversibility in the plastic zone at the crack tip, thereby reducing fatigue damage accumulation and increasing the fatigue life.

36 MATERIALS SCIENCE↗

Microscopic ergodicity breaking governs the emergence and evolution of elasticity in glass-forming nanoclay suspensions

We report a study combining x-ray photon correlation spectroscopy (XPCS) with in situ rheology to investigate the microscopic dynamics and mechanical properties of aqueous suspensions of the synthetic hectorite clay Laponite, which is composed of charged, nanometer-scale, disk-shaped particles. The suspensions, with particle concentrations ranging from 3.25 to 3.75 wt%, evolve over time from a fluid to a soft glass that displays aging behavior. The XPCS measurements characterize the localization of the particles during the formation and aging of the soft-glass state. The fraction of localized particles f 0 increases rapidly during the early formation stage and grows more slowly during subsequent aging, while the characteristic localization length r loc steadily de- creases. Despite the strongly varying rates of aging at different concentrations, both f 0 and r loc scale with the elastic shear modulus G' in a manner independent of concentration. During the later aging stage, the scaling between r loc and G' agrees quantitatively with a prediction of naive mode coupling theory. Breakdown of agreement with the theory during the early formation stage indi- cates the prevalence of dynamic heterogeneity, suggesting the soft solid forms through precursors of dynamically localized clusters.

36 MATERIALS SCIENCE↗

A Comparison of Emerging Nonfluoropolymer-Based Coextruded PV Backsheets to Industry-Benchmark Technologies

As the photovoltaic (PV) industry is rapidly expanding around the world, there has been an increasing interest in extending the lifespan of PV modules. Concern has also emerged regarding the recyclability of modules and their component materials, including fluoropolymer-based backsheets. Laminated polyethylene-terephthalate (PET) core backsheets have traditionally been used in the PV industry, but new, coextruded polyolefin (PO) backsheets show promise as an improved alternative. In this work, minimodule and coupon samples of seven different backsheets (made of layers including contemporary PET and fluoropolymers, novel PO, and polyamide materials) were run through hygrometric- or UV photolytic-accelerated aging to identify and better understand each material's degradation modes and the backsheets' field reliability. In addition to the artificial aging, the natural weathering methods used in this article are described. The comprehensive set of chemical, mechanical, and structural characterizations at intermittent read points in this article is presented, including: visual appearance and color; gloss; mechanical tensile testing; I-V performance; electroluminescence (EL) imaging; dielectric breakdown; Fourier-transform infrared-chemical structure; X-ray-polymer structure; and differential scanning calorimetry-crystalline content. After 4000 h of aging, a strong correlation occurs between initial physical characteristics (mechanical tensile test) and operating performance (EL and I-V characteristics).

14 SOLAR ENERGY↗

BACKFLIP: A Comparison of Emerging Non-Fluoropolymer-Based, Co-Extruded PV Backsheets to Industry-Benchmark Technologies

As the photovoltaic (PV) industry is rapidly expanding around the world, there has been an increasing interest in extending the lifespan of PV modules. Concern has also emerged regarding the recyclability of modules and their component materials, including fluoropolymer-based backsheets. Laminated polyethylene-terephthalate (PET) core backsheets have traditionally been used in the PV industry, but new, co-extruded polyolefin (PO) backsheets show promise as an improved alternative. Mini-module and coupon samples of seven different backsheets (made of layers including contemporary PET and fluoropolymers, novel PO, and polyamide (PA) materials) were run through hygrometric- or UV photolytic-accelerated aging to identify and better understand each material’s degradation modes and the backsheets’ field reliability. In addition to the artificial aging, the natural weathering methods used in this study are described. The comprehensive set of chemical, mechanical, and structural characterizations at intermittent read points in this study is presented, including: visual appearance and color; gloss; mechanical tensile testing; I-V performance; electroluminescence (EL) imaging; dielectric breakdown; FTIR-chemical structure; X-ray-polymer structure (WAXS); and DSC-crystalline content. After 4000 h of aging, a strong correlation occurs between initial physical characteristics (mechanical tensile test) and operating performance (EL and I-V characteristics).

41 EE - Solar Energy Technologies Office (EE-4S)↗

BACKFLIP: A Comparison of Emerging Non-Fluoropolymer-Based, Co-Extruded PV Backsheets to Industry-Benchmark Technologies

As the photovoltaic (PV) industry is rapidly expanding around the world, there has been an increasing interest in extending the lifespan of PV modules. Concern has also emerged regarding the recyclability of modules and their component materials, including fluoropolymer-based backsheets. Laminated polyethylene-terephthalate (PET) core backsheets have traditionally been used in the PV industry, but new, co-extruded polyolefin (PO) backsheets show promise as an improved alternative. Mini-module and coupon samples of seven different backsheets (made of layers including contemporary PET and fluoropolymers, novel PO, and polyamide (PA) materials) were run through hygrometric- or UV photolytic-accelerated aging to identify and better understand each material's degradation modes and the backsheets' field reliability. In addition to the artificial aging, the natural weathering methods used in this study are described. The comprehensive set of chemical, mechanical, and structural characterizations at intermittent read points in this study is presented, including: visual appearance and color; gloss; mechanical tensile testing; I-V performance; electroluminescence (EL) imaging; dielectric breakdown; FTIR-chemical structure; X-ray-polymer structure (WAXS); and DSC-crystalline content. After 4000 h of aging, a strong correlation occurs between initial physical characteristics (mechanical tensile test) and operating performance (EL and I-V characteristics). This presentation focuses on gloss, FTIR, and breakdown voltage measurements. Results for MiMo power, grayness from EL imaging, optical micrscopy, and specimen morphology (on extraction when cut from MiMos) is also presented.

backsheet↗

Residual stress stability in fiber textured stoichiometric AlN film grown using rf magnetron sputtering

The authors report on the stability of mechanical stress with aging and thermal cycling for columnar structured stoichiometric and homogeneous aluminum nitride thin films grown using radio frequency magnetron sputtering technique. The set of deposition parameters were optimized for the best possible orientation of crystallites in the c axis of compositionally stoichiometric films. The as-grown stress in the slightly nitrogen-rich film does not change when exposed to the atmosphere following deposition, while that in the nitrogen-deficient film, it changes due to oxidation. Additionally, the magnitude of as-grown stress has been found to depend on the substrate material in addition to the deposition parameters. The stress in the film grown on a Si(001) substrate was more tensile than in the film grown on a semi-insulating (si) GaAs(001) substrate for a given set of deposition parameters. Furthermore, the stress in the film grown on Si decreased with temperature, while that on si GaAs increased, indicating the thermally induced stress component to be the major component in the residual stress. Upon subsequent cooling the stress changes in both substrates followed the same path as of heating, thus exhibiting no hysteresis with thermal cycles between room temperature and 400 deg. C.

36 MATERIALS SCIENCE↗

Titanium dioxide nanoparticles: Impact of increasing ionic strength during synthesis, reflux, and hydrothermal aging

This work investigates the role of ionic strength during synthesis, reflux, and hydrothermal aging of sol-gel synthesized titanium dioxide. Research presented here uses X-ray diffraction data and Rietveld refinements to quantify anatase, brookite, and rutile phases as functions of synthetic and aging variables. In addition, the Scherrer equation is used to obtain average crystallite sizes for each phase quantified. Results presented in this work demonstrate that the most control over the sol-gel products can be obtained by modifying the pH during hydrolysis. In addition, while varying the ionic strength during reflux and hydrothermal aging can result in enhanced control over the crystalline phase and crystallite size, the most control can be achieved by varying the ionic strength during synthesis. Finally, sol-gel synthesis at low pH (-0.6) and high-chloride concentration (3 M NaCl) produced a heterogeneous sample composed of nanocrystalline anatase (3.8 nm) and rutile (2.9 nm)

36 MATERIALS SCIENCE↗

The Microstructure, and Mechanical and Corrosion Properties of As-Cast and As-Extruded Mg-2%Zn-x%Cu Alloys After Solution and Aging Heat Treatments

The effects of different Cu concentrations and heat treatment on the microstructure, mechanical and corrosion properties of the as-cast and hot-extruded Mg-2%Zn alloys were studied. The results showed that T6 heat treatment led to the dissolution of intermetallics and breaking the continuous networks of intermetallics. Also, the grain size of the base alloy decreased with further Cu additions after solution and aging heat treatments. Microstructural characterization indicated that Mg(Zn,Cu) and Mg(Zn,Cu){sub 2} intermetallics were formed which their volume fractions increased with exceeding Cu additions. Moreover, the addition of 3 wt.% Cu and T6 heat treatment increased the Brinell hardness of both as-cast and hot-extruded specimens reached to 94 HBN and 116 HBN, respectively. The optimum amounts of the ultimate tensile strength and elongation values obtained from 0.1 wt.% Cu addition for both conditions after T6 treatment which were 253 MPa, 11.5% and 263 MPa, 14.7%, respectively. However, more Cu addition (> 0.5 wt.%) deteriorated the tensile properties of the alloy due to the high volume fraction of intermetallics. The yield tensile strength increased continuously with different Cu additions for the cast and extruded alloys after solution and aging heat treatments. After T6 heat treatment, extruded alloys showed better anti-corrosion properties than those of the cast alloys, while the extruded Mg-2%Zn-0.1%Cu alloy exhibited the best anti-corrosion property. Further Cu addition increased the volume fraction of intermetallics and enhanced the corrosion rate which was due to the galvanic couple effect.

36 MATERIALS SCIENCE↗

Intergranular corrosion resistance of Zn modified 5××× series Al alloy during retrogression and re-aging treatment

Highlights: • Increase the strength due to precipitation hardening of T-Mg{sub 32}(AlZn){sub 49} phase in the Zn modified Al-Mg alloy. • Both high corrosion resistance and high strength are achieved by retrogression and re-aging treatment in Al-5Mg-3Zn alloy. • Large Mg and Zn content difference between GBP and PFZ results in relatively high IGC susceptibility. • The intergranular corrosion mechanism of Zn modified Al-Mg alloy during retrogression and re-aging treatment is clarified. - Abstract: The effects of retrogression and re-aging treatment on the intergranular corrosion behavior of Al-5.0Mg-3.0Zn alloys are systematically studied. The alloy's strength increases when retrogression temperature increases from 390 °C to 420 °C. Samples retrogressed at 390 °C then re-aged are very susceptible to intergranular corrosion and those retrogressed at 405 °C and 420 °C express good corrosion resistance. Then the alloy's corrosion susceptibility rises with increasing retrogression temperature. Grain boundary precipitates are coarsened and distributed discontinuously with decreasing retrogression temperature. Higher retrogression temperature results in higher Mg and Zn content difference and intergranular corrosion susceptibility.

36 MATERIALS SCIENCE↗

Influence of quenching agent on microstructure, properties and thermal stress of SiC{sub p}/2009 composites

15% vol. SiC{sub p}/2009 composites prepared by powder metallurgy were quenched in room temperature water and 20% polyethylene glycol (PEG) solution respectively, then aged naturally. The influence of quenching agent on microstructure, properties and thermal stress of SiC{sub p}/2009 composites were investigated by means of scanning/transmission electron microscope, hardness and tensile test. The results showed that the number of precipitated phase in water quenched composites increased, with much finer in size and more homogeneous in distribution compared with 20% PEG quenched one. Meanwhile, the density of dislocation in composites by water quenching was also much higher. Intergranular corrosion did not occur with the two quenching agents. The 20% PEG quenched composites exhibited slight lower hardness and higher electrical conductivity than that of water quenched one. The two quenched composites showed same level in tensile strength, but the yield strength of water-quenched composites was higher (8 MPa, 3%). The usage of 20% PEG reduced thermal stress and minimized warping deformation of the parts, it is a more suitable quenching agent for SiC{sub p}/2009 composites in engineering application fields. - Highlights: •SiC{sub p}/2009 composites quenched by water and 20% PEG solution were investigated. •Aging precipitation behavior of SiC{sub p}/2009 composites is sensitive to quenchant. •Influence of quenching agent on properties of SiC{sub p}/2009 composites are minimal. •Quenching with 20% PEG reduces thermal stress of SiC{sub p}/2009 composites remarkably. •20% PEG is a more suitable quenching agent for SiC{sub p}/2009 composites than water.

36 MATERIALS SCIENCE↗