Shape memory alloys: New materials for future engineering

Shape memory is a new material property. An alloy which experiences relative severe plastic deformation resumes its original shape again after heating by 10 to 100 C. Besides simple shape memory, in similar alloys there is the second effect where the change in shape is caused exclusively by little temperature change. In pseudo-elasticity, the alloy exhibits a rubber-like behavior, i.e., large, reversible deformation at little change in tension. Beta Cu and beta NiTi alloys have been used in practice. The probability is that soon alloys based on Fe will become available. Recently increasing applications for this alloy were found in various areas of technology, even medical technology. A review with 24 references is given, including properties, production, applications and fundamental principles of the shape memory effect.

Hornbogen, E.↗

Precipitation strengthened high strength, high conductivity Cu-Cr-Nb alloys produced by chill block melt spinning

A series of Cu-based alloys containing 2 to 10 a/o Cr and 1 to 5 a/o Nb were produced by chill block melt spinning (CBMS). The melt spun ribbons were consolidated and hot rolled to sheet to produce a supersaturated Cu-Cr-Nb solid solution from which the high melting point intermetallic compound Cr2Nb could be precipitated to strengthen the Cu matrix. The results show that the materials possess electrical conductivities in excess of 90 percent that of pure Cu at 200 C and above. The strengths of the Cu-Cr-Nb alloys were much greater than Cu, Cu-0.6 Cr, NARloy-A, and NARloy-Z in the as-melt spun condition. The strengths of the consolidated materials were less than Cu-Cr and Cu-Cr-Zr below 500 C and 600 C respectively, but were significantly better above these temperatures. The strengths of the consolidated materials were greater than NARloy-Z, at all temperatures. The GLIDCOP possessed similar strength levels up to 750 C when the strength of the Cu-Cr-Nb alloys begins to degrade. The long term stability of the Cu-Cr-Nb alloys was measured by the microhardness of aged samples and the growth of precipitates. The microhardness measurements indicate that the alloys overage rapidly, but do not suffer much loss in strength between 10 and 100 hours which confirms the results of the electrical resistivity measurements taken during the aging of the alloys at 500 C. The loss in strength from peak strength levels is significant, but the strength remains exceptionally good. Transmission electron microscopy (TEM) of the as-melt spun samples revealed that Cr2Nb precipitates formed in the liquid Cu during the chill block melt spinning, indicating a very strong driving force for the formation of the precipitates. The TEM of the aged and consolidated materials indicates that the precipitates coarsen considerably, but remain in the submicron range.

Ellis, David L.↗

Determination of the gaseous hydrogen ductile-brittle transition in copper-nickel alloys

A series of copper-nickel alloys were fabricated, notched tensile specimens machined for each alloy, and the specimens tested in 34.5 MPa hydrogen and in air. A notched tensile ratio was determined for each alloy and the hydrogen environment embrittlement (HEE) determined for the alloys of 47.7 weight percent nickel to 73.5 weight percent nickel. Stacking fault probability and stacking fault energies were determined for each alloy using the x ray diffraction line shift and line profiles technique. Hydrogen environment embrittlement was determined to be influenced by stacking fault energies; however, the correlation is believed to be indirect and only partially responsible for the HEE behavior of these alloys.

Parr, R. A.↗

Superplastic forming and diffusion bonding of rapidly solidified, dispersion strengthened aluminum alloys for elevated temperature structural applications

Rapidly solidified alloys, based upon the Al-Fe-V-Si system and designed for elevated temperature applications, were evaluated for superplasticity and diffusion bonding behavior. Alloys with 8, 16, 27, and 36 volume percent silicide dispersoids were produced; dispersoid condition was varied by rolling at 300, 400, and 500 C (572, 752, and 932 F). Superplastic behavior was evaluated at strain rates from 1 x 10(exp -6)/s to 8.5/s at elevated temperatures. The results indicate that there was a significant increase in elongation at higher strain rates and at temperatures above 600 C (1112 F). However, the exposure of the alloys to temperatures greater than 600 C (1112 F) resulted in the coarsening of the strengthening dispersoid and the degradation of mechanical properties. Diffusion bonding was possible using low gas pressure at temperatures greater than 600 C (1112 F) which also resulted in degraded properties. The bonding of Al-Fe-V-Si alloys to 7475 aluminum alloy was performed at 516 C (960 F) without significant degradation in microstructure. Bond strengths equal to 90 percent that of the base metal shear strength were achieved. The mechanical properties and microstructural characteristics of the alloys were investigated.

Ting, E. Y.↗

Elevated temperature crack growth in advanced powder metallurgy aluminum alloys

Rapidly solidified Al-Fe-V-Si powder metallurgy alloy FVS0812 is among the most promising of the elevated temperature aluminum alloys developed in recent years. The ultra fine grain size and high volume fraction of thermally stable dispersoids enable the alloy to maintain tensile properties at elevated temperatures. In contrast, this alloy displays complex and potentially deleterious damage tolerant and time dependent fracture behavior that varies with temperature. J-Integral fracture mechanics were used to determine fracture toughness (K sub IC) and crack growth resistance (tearing modulus, T) of extruded FVS0812 as a function of temperature. The alloy exhibits high fracture properties at room temperature when tested in the LT orientation, due to extensive delamination of prior ribbon particle boundaries perpendicular to the crack front. Delamination results in a loss of through thickness constraint along the crack front, raising the critical stress intensity necessary for precrack initiation. The fracture toughness and tensile ductility of this alloy decrease with increasing temperature, with minima observed at 200 C. This behavior results from minima in the intrinsic toughness of the material, due to dynamic strain aging, and in the extent of prior particle boundary delaminations. At 200 C FVS0812 fails at K levels that are insufficient to cause through thickness delamination. As temperature increases beyond the minimum, strain aging is reduced and delamination returns. For the TL orientation, K (sub IC) decreased and T increased slightly with increasing temperature from 25 to 316 C. Fracture in the TL orientation is governed by prior particle boundary toughness; increased strain localization at these boundaries may result in lower toughness with increasing temperature. Preliminary results demonstrate a complex effect of loading rate on K (sub IC) and T at 175 C, and indicate that the combined effects of time dependent deformation, environment, and strain aging may play a role. Fractography showed that microvoid coalescence was the microscopic mode of fracture in FVS0812 under all testing conditions. However, the nature of the microvoids varied with test temperature and loading rate, and is complex for the fine grain and dipersoid sizes of FVS0812.

Porr, William C., Jr.↗

The effects of zinc addition on the environmental stability of Al-Li alloys

It was found that relatively small addition of Zn can improve the stress corrosion cracking (SCC) resistance of Al-Li alloys. However, the mechanism by which this is accomplished is unclear. The role that Zn plays in altering the behavior of Alloy 8090 is investigated. Early results suggest that Zn additions increase the volume fraction of delta(Al3Li) precipitation and differential scanning calorimetry (DSC) on these alloys confirms this. The four alloys studied each had initial compositions lying in the 8090 window and had varying amounts of Zn added to them. Alloy 8090, like other Al-Li alloys, displays a delta' precipitate free zone (PFZ) upon artificial aging along the grain and subgrain boundaries. However Zn additions greatly decreased or eliminated a delta' PFZ after 100 hours at 160 C. This implies that the subgrain boundary precipitation kinetics are being altered and suppressed. Furthermore, there appears to be a window of Zn concentration above which a delta ' PFZ can reappear with the nucleation and growth of a currently unidentified precipitate on the boundaries. Polarization experiments were performed and the results presented. The experiments were performed in deaerated 3.5 w/o NaCl in both as received (T3) condition and at peak aging of 100 hours at 160 C. The aging profile was determined via Vickers Hardness tests.

Kilmer, Raymond J.↗

An x ray photoelectron spectroscopy study of Au(x)In(y) alloys

Four gold-indium alloys were studied by x ray photoelectron spectroscopy. The binding energies and intensity ratios of the Au 4f7/2 and In 3d5/2 core levels were determined for the bulk alloy compositions of Au(10 percent In), Au3In, AuIn, and AuIn2. These values were determined for the native oxides on the materials, for the surfaces prepared by ion bombardment to remove the oxide and for surfaces scraped in-situ with a ceramic tool to expose the bulk composition. These results furnish calibration values that allow determination of the composition of thin films of this alloy system. In addition the binding energies add to the data base for understanding the effect of alloying on core level binding energies. As an illustration, these results are used to determine the composition of a series of alloy films formed by incongruent evaporation of an alloy charge.

Jayne, Douglas T.↗

Electrochemical impedance spectroscopy of metal alloys in the space transportation system launch environment

AC impedance measurements were performed to investigate the corrosion resistance of 18 alloys under conditions similar to the Space Transportation System (STS) launch environment. The alloys were: (1) zirconium 702; (2) Hastelloy C-22, C-276, C-4, and B-2; (3) Inconel 600 and 825; (4) Ferralium 255; (5) Inco Alloy G-3; (6) 20Cb-3; (7) SS 904L, 304LN, 316L, 317L, and 304L; (8) ES 2205; and (9) Monel 400. AC impedance data were gathered for each alloy at various immersion times in 3.55 percent NaCl-0.1N HCl. Polarization resistance values were obtained for the Nyguist plots at each immersion time using the EQUIVALENT CIRCUIT software package available with the 388 electrochemical impedance software. Hastelloy C-22 showed the highest overall values for polarization resistance while Monel 400 and Inconel 600 had the lowest overall values. There was good general correlation between the corrosion performance of the alloys at the beach corrosion testing site, and the expected rate of corrosion as predicted based on the polarization resistance values obtained. The data indicate that electrochemical impedance spectroscopy can be used to predict the corrosion performance of metal alloys.

Calle, Luz↗

Superplastic formability of Al-Cu-Li alloy Weldalite (TM) 049

Extensive research during the past decade shows that several aluminum lithium alloys can be processed to attain a microstructure that enables superplasticity. The high tensile stress of Al-Cu-Li alloy Weldalite (TM) 049 in the T4 and T6 tempers offers tremendous potential for attaining exceptional post-SPF (superplastic formability) properties. The used SPF material is Weldalite, which was shown to induce SPF behavior in other Al-Cu-Li alloys. The superplastic behavior and resulting post-SPF mechanical properties of this alloy, which was designed to be the next major structural alloy for space applications, were evaluated. The results indicate that Weldalite alloy does indeed exhibit excellent superplasticity over a wide range of temperatures and strain rates and excellent post-SPF tensile strength at various potential service temperatures.

Ma, Bao-Tong↗

Hydrogen and sliding at alpha/beta interfaces of titanium alloys

Emerging evidence that the sliding between alpha and beta interfaces reported in both Ti-Mn alloys and the Ti-4.5Al-5Mo-1.5Cr ('Corona 5') alloy at room temperature is associated with hydrogen suggests that this may be a general problem contributing to Ti alloys' room-temperature creep. The present evaluation of experimental data indicates that while the hydrogen is concentrated at the Ti-Mn alloys' beta phase, no hydride formation at the alpha/beta interfaces has been reported for either the Ti-Mn alloys or Corona 5. If a hydrogen flux is needed, sliding at the alpha-beta interfaces should be a function of total hydrogen content in the alloy.

Margolin, Harold↗

Fatigue crack propagation in aluminum-lithium alloys

The principal mechanisms which govern the fatigue crack propagation resistance of aluminum-lithium alloys are investigated, with emphasis on their behavior in controlled gaseous and aqueous environments. Extensive data describe the growth kinetics of fatigue cracks in ingot metallurgy Al-Li alloys 2090, 2091, 8090, and 8091 and in powder metallurgy alloys exposed to moist air. Results are compared with data for traditional aluminum alloys 2024, 2124, 2618, 7075, and 7150. Crack growth is found to be dominated by shielding from tortuous crack paths and resultant asperity wedging. Beneficial shielding is minimized for small cracks, for high stress ratios, and for certain loading spectra. While water vapor and aqueous chloride environments enhance crack propagation, Al-Li-Cu alloys behave similarly to 2000-series aluminum alloys. Cracking in water vapor is controlled by hydrogen embrittlement, with surface films having little influence on cyclic plasticity.

Rao, K. T. V.↗

Reaction of beta-phase Ni-Al alloys with CrB2

Reaction of Ni-Al alloys within the beta-NiAl phase with CrB2 was studied at 1473 K as a function of Al concentration in the alloy. Reaction of 49-50 at. pct Al alloys with CrB2 occurred by interdiffusion of Ni into CrB2 and Cr into the alloy without forming a new product phase. On the other hand, a new product phase, rich in Ni and B, formed by the reaction of alloys having Al concentrations 48 at. pct or lower with CrB2. The reaction product was observed both at the CrB2/alloy interface and along the alloy grain boundaries.

Misra, Ajay K.↗

Development and characterization of Powder Metallurgy (PM) 2XXX series Al alloy products and Metal Matrix Composite (MMC) 2XXX Al/SiC materials for high temperature aircraft structural applications

The results of a series of material studies performed by the Lockheed Aeronautical Systems Company over the time period from 1980 to 1991 are discussed. The technical objective of these evaluations was to develop and characterize advanced aluminum alloy materials with temperature capabilities extending to 350 F. An overview is given of the first five alloy development efforts under this contract. Prior work conducted during the first five modifications of the alloy development program are listed. Recent developments based on the addition of high Zr levels to an optimum Al-Cu-Mg alloy composition by powder metallurgy processing are discussed. Both reinforced and SiC or B4C ceramic reinforced alloys were explored to achieve specific target goals for high temperature aluminum alloy applications.

Chellman, D. J.↗

The fracture resistance of 1420 and 1421 Al-Mg-Li alloys

The resistance to stable crack growth in 1420-T6 (Al-5Mg-2.1Li-0.1Zr-0.01Sc, less than 0.06Fe, in wt pct) and 1421-T6 (Al-4.7Mg-1.9Li-0.09Zr-0.2Sc, less than 0.06Fe) Al-Mg-Li alloys was investigated, based on the R curves generated in accordance with ASTM E561-86 and fractography analyses. The crack resistance of 1420 and 1421 alloys was found to be comparable to that of the conventional Space Shuttle External Tank Al alloy, 2219-T87. The main differences in the fracture behaviors arose from differences in the alloys' microstructures. In the case of 1420 alloy, a slightly enhanced toughness behavior was observed, due to the T-phase precipitates, which may have promoted more homogeneous deformation and enhanced microvoid coalescence. In the case of 1421 alloy, the addition of Sc led to a refined grain size and resulted in slightly reduced toughness.

Birt, M. J.↗

Capacity retention in hydrogen storage alloys

Results of our examination of the properties of several candidate materials for hydrogen storage electrodes and their relation to the decrease in H-storage capacity upon open-circuit storage over time are reported. In some of the alloy samples examined to date, only about 10 percent of the hydrogen capacity was lost upon storage for 20 days, while in others, this number was as high as 30 percent for the same period of time. This loss in capacity is attributed to two separate mechanisms: (1) hydrogen desorbed from the electrode due to pressure differences between the cell and the electrode sample; and (2) chemical and/or electrochemical degradation of the alloy electrode upon exposure to the cell environment. The former process is a direct consequence of the equilibrium dissociation pressure of the hydride alloy phase and the partial pressure of hydrogen in the hydride phase in equilibrium with that in the electrolyte environment, while the latter is related to the stability of the alloy phase in the cell environment. Comparison of the equilibrium gas-phase dissociation pressures of these alloys indicate that reversible loss of hydrogen capacity is higher in alloys with P(eqm) greater than 1 atm than in those with P(eqm) less than 1 atm.

Anani, A.↗

Organometallic chemical vapor deposition and characterization of ZnGe(1-x)Si(x)P2-Ge alloys on GaP substrates

In this paper, we report the epitaxial growth of ZnGe(1-x)Si(x)P2-Ge alloys on GaP substrates by open tube OMCVD. The chemical composition of the alloys characterized by energy dispersive X-ray spectroscopy shows that alloys with x up to 0.13 can be deposited on (001) GaP. Epitaxial growth with mirror smooth surface morphology has been achieved for x less than or equals to 0.05. Selected area electron diffraction pattern of the alloy shows that the epitaxial layer crystallizes in the chalcopyrite structure with relatively weak superlattice reflections indicating certain degree of randomness in the cation sublattice. Hall measurements show that the alloys are p-type, like the unalloyed films; the carrier concentration, however, dropped about 10 times from 2 x 10 exp 18 to 2 x 10 exp 17/cu cm. Absorption measurements indicate that the band tailing in the absorption spectra of the alloy has been shifted about 0.04 eV towards shorter wavelength as compared to the unalloyed material.

Xing, G. C.↗

Predicting the oxidative lifetime of beta NiAl-Zr alloys

Nickel aluminides containing 40 to 50 at. pct Al and 0.1 at. pct Zr were studied following cyclic oxidation at 1400 C. The selective oxidation of Al resulted in the formation of protective Al2O3 scales on each alloy composition. However, repeated cycling eventually resulted in the gradual formation of less-protective NiAl2O4, first appearing on the 40Al alloys followed at longer times on the 45Al alloys. The appearance of the NiAl2O4, signaling the end of the protective scale-forming capability of the alloy, was related to the presence of gamma-prime (Ni3Al) which formed as a result of the loss of Al from the sample. A diffusion model, based on finite-difference techniques, was developed to predict the protective life of beta Ni-Al alloys. This model predicts Ni and Al concentration profiles after various oxidation exposures. The model can predict the oxidative lifetime due to Al depletion when the Al concentration decreases to a critical concentration. Measured Al concentration profiles on two alloys after various oxidation exposures are compared to those predicted by the diffusion model. The time to the appearance of the NiAl2O4 and that predicted by the diffusion model are compared and discussed.

Nesbitt, J. A.↗

Tensile and stress-rupture behavior of hafnium carbide dispersed molybdenum and tungsten base alloy wires

The tensile strain rate sensitivity and the stress-rupture strength of Mo-base and W-base alloy wires, 380 microns in diameter, were determined over the temperature range from 1200 K to 1600 K. Three molybdenum alloy wires; Mo + 1.1w/o hafnium carbide (MoHfC), Mo + 25w/o W + 1.1w/o hafnium carbide (MoHfC+25W) and Mo + 45w/o W + 1.1w/o hafnium carbide (MoHfC+45W), and a W + 0.4w/o hafnium carbide (WHfC) tungsten alloy wire were evaluated. The tensile strength of all wires studied was found to have a positive strain rate sensitivity. The strain rate dependency increased with increasing temperature and is associated with grain broadening of the initial fibrous structures. The hafnium carbide dispersed W-base and Mo-base alloys have superior tensile and stress-rupture properties than those without HfC. On a density compensated basis the MoHfC wires exhibit superior tensile and stress-rupture strengths to the WHfC wires up to approximately 1400 K. Addition of tungsten in the Mo-alloy wires was found to increase the long-term stress rupture strength at temperatures above 1400 K. Theoretical calculations indicate that the strength and ductility advantage of the HfC dispersed alloy wires is due to the resistance to recrystallization imparted by the dispersoid.

Yun, Hee Mann↗