Facile Electrochemical Mg-Ion Transport in a Defect-Free Spinel Oxide
Explore the source record for details and available documents.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
A process for charging a discharged electrochemical cell includes applying a voltage bias to the discharged electrochemical cell; and illuminating the cathode with a light source.
Introduction: Calcium-aluminum inclusions (CAIs) are cm- to mm-sized intergrowths of refractory phases found in chondritic meteorites [1]. Their mineral compositions closely match the compositions of the solids thought to condense from an extremely hot (>1500K) gas with a bulk solar composition [2-4], suggesting that CAIs were the earliest solids within the Solar System [2-4]. These inclusions provide invaluable insights into the conditions and dynamics of the early Solar System. CAIs must be transported from their formation region near the protosun to the chondrite parent-body accretion region. The nature of their journey could affect how, when, and where the secondary processes recorded in these CAIs occurred [4]. Did these secondary processes occur in the solar nebula or during accretion with the parent body, or both? How were the CAIs affected by varying thermochemical processes? To better answer these questions, we have undertaken an in-depth, textural study of the secondary alteration of select CAI samples. Methods: We chose three CAIs that experienced a range of post-formation processing to gain better understanding of secondary alteration based on previous preliminary examination [5]. Representative CAIs were chosen from NWA 5508 (CV3), NWA 12772 (CV3), and Coolidge (CL4) carbonaceous chondrites. We used scanning electron microscopy (SEM) and electron backscatter diffraction (EBSD) techniques for detailed chemical, mineralogical, and textural analysis of the CAIs. Backscattered electron (BSE) images and X-ray elemental maps were taken of Coolidge and NWA 5508 using the Lunar and Planetary Institute (LPI) Phenom SEM. The JEOL 7900F SEM at NASA Johnson Space Center (JSC) was used to obtain energy dispersive spectroscopy (EDS) chemical maps of all samples. High resolution EBSD analysis identified the mineral phases and textures, providing key information on their nature. Based on the SEM and EBSD data, minerals of interest were selected for quantitative chemical electron probe micro-analysis (EPMA) using the JEOL JXA-8530F at NASA JSC. Results and Discussion: The EDS maps show that the NWA 5508 and NWA 12772 CAIs designated “Saguaro” and “Hoopoe” respectively [5] are enriched in calcium while the Coolidge CAI designated “Cottonwood” is aluminum and magnesium rich. Saguaro. A ~1.5cm diameter igneous Type B CAI with a rounded shape. The dominant phases are melilite, spinel, and Al-Ti pyroxene with minor anorthite. Spinel is subhedral and occurs in clusters. Some of these clusters have a circular geometry which encloses other minerals, known as a palisade structure [6] (Fig. 1). Some palisades form near perfect circles while others are more irregular in shape. Melilite in Saguaro ranges in size from coarse (>250m) to fine-grained (5-7m) and forms intergrown laths. A third of the melilite grains exhibit simple twinning about their <001> axis. The spinel palisades and twinned melilite in Saguaro suggest an igneous history, and the lack of secondary minerals suggests minimal aqueous alteration. At some point in time after the initial condensation of the minerals and formation of the inclusion, the sample was remelted and quickly solidified. The formation of the palisades is still heavily debated. One hypothesis is that the palisades are the rims of smaller CAIs that accreted early on, essentially acting as xenoliths within the larger CAIs [7]. Another hypothesis suggests an igneous origin for palisade structures [6-8] wherein the melt traps gas bubbles, and the spinel nucleates on the surface of this bubble. Based on the WDS spot analyses of 41 melilite grains using EPMA, the data suggest that the composition inside and outside the palisades is nearly identical. This finding indicates that these palisades are likely not exogenous but rather formed from melt-vapor reactions. Our results are consistent with studies by Simon and Grossman,1997 [6] and Zhang et al. (2019) [8]. Hoopoe. A ~0.5cm compact Type A CAI with an irregular shape. The dominant mineral phases are melilite, spinel, and hibonite with minor amounts of anorthite, augite, and perovskite. The melilite ranges in size from ~500 to 50µm. The larger melilite grains have simple twinning along the <001> axis like melilite in Saguaro. Melilite in Hoopoe exhibits crystal-plastic strain with misorientation dominantly about the <010> and <110> axes. Spinel shows subhedral to euhedral morphology and appears in clusters. Hibonite grains are similar to spinel in habit and size but show more plastic strain. The two minerals are often found together with one appearing to replace the other. Perovskite appears in fine grained recrystallized regions alongside fine augite and spinel. The abundant strain and deformation features in the melilite and hibonite suggest that Hoopoe experienced shock. This shock could have occurred in the nebula [9] or from an impact of another body on the parent body asteroid. The appearance of fine-grained (<10m) areas of augite, perovskite, and spinel in the dominantly coarse-grained inclusion suggest recrystallization, possibly due to the sudden increase in pressure and temperature. Cottonwood. This ~0.5cm CAI exhibits distinct mineralogy and textures suggesting a high degree of alteration. It is irregular in shape. The dominant mineral phases are spinel and anorthite with minor amounts of augite and rutile. The two main texture types can be seen in Fig. 2. The first type consists of coarse euhedral to subhedral spinel and anorthite. The second includes fine grained spinel, anorthite, rutile, and iron sulfides. Within these fine-grained regions, the anorthite grains are clustered into domains exhibiting the same crystallographic orientation. Rutile exclusively occurs with fine anorthite indicating a potential relationship between the two. Cottonwood has a clear and unbroken Wark-Lovering [10] rim (Fig. 2) on one side that consists of a sequence of spinel followed by anorthite and an outer layer of augite. The abundance of the fine-grained regions containing iron oxides and iron sulfides, secondary phases such as rutile, and oriented anorthite grains is evidence for recrystallization associated with a high degree of thermal metamorphism. The EPMA analyses on both coarse- and fine-grained spinel show that the fine spinel grains are more enriched in Cr (1-2 wt. %) than their coarse counterparts (0.1-0.5 wt. %). The data suggest thermal metamorphism drove chemical exchange of the previously refractory inclusion, introducing chromium and iron as well as sulfur, which is moderately volatile. Conclusions: The three CAIs analyzed record distinct secondary nebular and parent body processes. Saguaro melted in the nebula as seen by the twinned melilite and spinel palisades. Hoopoe experienced intense shock which deformed its melilite and recrystallized perovskite, augite, and spinel in fine-grained regions. Cottonwood shows evidence of recrystallization and chemical changes consistent with thermal metamorphism occurring after accretion into the parent-body.
Ca- Al-rich inclusions (CAIs) are commonly surrounded by Wark-Lovering (WL) rims - thin (approx. 50 micrometers) multilayered sequences - whose mineralogy is dominated by high temperature minerals similar to those that occur in the cores of CAIs [1]. The origins of these WL rims involved high temperature events in the early nebula such as condensation, flashheating or reaction with a nebular reservoir, or combinations of these processes. These rims formed after CAI formation but prior to accretion into their parent bodies. We have undertaken a coordinated mineralogical and isotopic study of WL rims to determine the formation conditions of the individual layers and to constrain the isotopic reservoirs they interacted with during their history. We focus here on the spinel layer, the first-formed highest- temperature layer in the WL rim sequence. Results and Discussion: We have performed mineralogical, chemical and isotopic analyses of an unusual ultrarefractory inclusion from the Allende CV3 chondrite (SHAL) consisting of an approx. 500 micrometers long single crystal of hibonite and co-existing coarsegrained perovskite. SHAL is partially surrounded by WL rim. We previously reported on the mineralogy, isotopic compositions and trace elements in SHAL [2-4]. The spinel layer in the WL rim is present only on the hibonite and terminates abruptly at the contact with the coarse perovskite. This simple observation shows that the spinel layer is not a condensate in this case (otherwise spinel would have condensed on the perovskite as well). The spinel layer appears to have formed by gas-phase corrosion of the hibonite by Mg-rich vapors such that the spinel layer grew at the expense of the hibonite. We also found that the spinel layer has the same 16Orich composition as the hibonite. The spinel layer is polycrystalline and individual crystals do not show a crystallographic relationship with the hibonite. An Al-diopside layer overlies the spinel layer, and is present on both the hibonite and perovskite. While the spinel is 16O-rich, WL-rim perovskite and pyroxene are 16O-poor. This isotopic heterogeneity likely reflects O isotopic equilibration of WL-rim perovskite and pyroxene with a planetary O isotopic reservoir after the WL rim formation. The hibonite is zoned and contains wt.% levels of Ti, Mg and Fe in contact with the Fe-bearing spinel (Sp60Hc40) in the WL rim. The Fe enrichment in spinel is likely related to the Na-Fe metasomatism that is ubiquitous in Allende. Conclusions: The petrography and microstructure of the spinel layer in a WL rim sequence shows that it formed by gas phase reactions at high temperature in the nebula. The oxygen isotopic composition of the spinel indicates that this WL rim layer formed in the same (or similar) nebular gas reservoir as the host CAI.
Introduction: Calcium-aluminum-rich inclusions (CAIs), are the first formed solids that define the age of the Solar System [1,2]. CAIs are thought to have condensed from nebular gas [3,4] within the first <1 Ma of Solar System formation [5,6]. CAIs have experienced numerous early Solar System processes including condensation, evaporation, melting, recrystallization, and aqueous alteration [e.g., 7]. The chemical, mineralogical, and textural diversity among CAIs results from a range of chemical and physical processes recorded during nebular and parent body epoch. This study aims to explore the mineralogical, textural, and chemical compositions of CAIs including the trace elemental abundances in CAI phases to determine the early Solar System processes recorded in them. Samples and Analytical Methods: We analyzed one CAI each from CV3 chondrites Northwest Africa (NWA) 5508 designated as ‘Saguaro’, and Northwest Africa (NWA) 12772 designated as ‘Hoopoe’. Back-scatter electron (BSE) images were collected using a Phenom XL scanning electron microscope (SEM) at the Lunar and Planetary Institute (LPI) and the JEOL JXA-8530F electron probe microanalyzer (EPMA) at Johnson Space Center (JSC)-NASA. Additionally, energy dispersive X-ray spectrometry (EDS) elemental maps of select areas for these samples were collected using a 15.0kV beam energy and a 40µA emission current. Using the EPMA, wavelength-dispersive X-ray spectroscopy (WDS) quantitative data were collected. In-situ trace element measurements for both CAIs were determined at JSC-NASA using a Photon Machines 193nm laser ablation system and a Thermo-Scientific Element-XR inductively coupled plasma mass spectrometer (ICP-MS). Analyses consisted of 30s ablations at 10Hz, spot sizes of 20-25µm, and a fluence of 6.0 J/cm2 for anorthite and melilite, and a 3.5 J/cm2 fluence for all other phases. NIST612 was used to correct for instrument drift, while BHVO-2g was used as a primary calibration standard. BCR-2g and in-house mineral standards were regularly measured as unknowns to ensure accuracy. Results: Saguaro is a coarse-grained CAI, ~11 x 6 mm in dimensions. Saguaro contains spinel, Al-rich pyroxene, anorthite, Mg-rich melilite, and minor perovskite in its interior and is therefore classified as a Type B CAI. Individual melilite grains shows normal compositional zoning with an Ak content ranging from ~24 to 54 with no apparent trend from the core to the edge of the CAI. The spinel appears euhedral and occurs both as clusters and as spinel palisades [8]. Two rim sequences surround most of the sample: the inner rim being a Wark-Lovering (WL) rim (~10-35 µm) containing pyroxene, spinel, and melilite (or anorthite), and the outer rim is a finer-grained, thicker (~100 µm), accretionary rim (Fig. 1). The mineral phases in Saguaro record an overall flat REE pattern with an average negative Eu anomaly in pyroxene, and an average positive Eu anomaly in anorthite and melilite respectively. Anorthite, melilite, and pyroxene have a minor depletion in Tm (Fig. 2). The Hoopoe CAI is a compact, coarse-grained ~6 × 4 mm in size. The major mineralogy includes hibonite, spinel, melilite, anorthite, and perovskite. Therefore, it is classified as a compact transitional type A and B. (?)zoning was observed in some hibonites. Individual melilite grains show both reverse and normal zoning, where the Ak content ranges from ~6- to 28. Melilite shows two distinct textures. One texture consisted of smooth melilite that appeared homogenous, while the second appeared to consist of many fine fractures. The spinel also often appears clustered. The WL-rim sequence surrounding Hoopoe is ~25 µm thick and composed of spinel, perovskite, hibonite, and melilite/anorthite. It is then partially surrounded by an outer accretionary rim (~75µm). Like before, refractory metal nuggets appeared concentrated near the WL rims. Other metal assemblages rich in Fe and Ni were also observed. All major mineral phases in Hoopoe display relatively flat REE patterns, except for varying Eu and Tm between phases (Fig. 2). There is a prominent negative Eu anomaly in perovskite and an average positive Eu anomaly in spinel, anorthite, and hibonite respectively (Fig. 2, 3). The mixed phases along the rim of the CAI also display a negative Eu anomaly, and all phases the CAI were depleted in Pb. Discussion: The CV3 CAIs analyzed in this study were classified based on their mineralogy and textures into Type A versus Type B CAIs [10]. Hibonite appears to be pseudomorphically replacing the spinel, (i.e., is hibonite in composition, but appears in the shape of spinel). Spinel palisades. The presence of spinel palisades present in Saguaro are consistent with the melting and recrystallization experienced by this CAI. Trace elemental analyses. Saguaro and Hoopoe display similar trace element patterns to each other, with both appearing generally flat, with anomalies in Eu, and Tm. Melilite and anorthite display positive Eu anomalies in both CAIs, in addition to the hibonite in Hoopoe (Fig. 2). The phases that are depleted in Eu are pyroxene and perovskite in both Saguaro and Hoopoe, respectively (Fig. 3). Given that Eu is volatile in reducing environments [11], this could possibly indicate reducing conditions at the time anorthite and melilite crystallized, with the gas they formed from containing Eu. As these CAIs continued to form, this gas as a result would become depleted in Eu. This also could be supported by the propensity of anorthite and melilite to take up Eu from its surroundings and incorporate it into their structure [12]. In addition, analyzing the assemblage of the phases in the Saguaro, melilite and anorthite (Eu enriched) often surround the pyroxene (Eu depleted) as they are crystallized. This intergrowth of phases and the proximity of the phases would support that the Eu is being incorporated into some phases, preventing it from incorporating into other. Trace elemental analyses of the CAI rims will be evaluated in more detail, as they are complicated by the transient signal being composed of a mixture of mineral phases. Broadly, however, the patterns in the rims of both CAIs are comparable to each other, and for Hoopoe, to the mixed phase patterns in the core (Fig. 3). Other studies have found that CAI rims can be depleted in Ce and Yb [13], however we did not observe these anomalies in the two CAIs discussed here. Given their similarity, the trace elemental analyses of the mixed interior (i.e. core) and rim phases could be interpreted as forming from similar, if not the same, reservoirs. The REE abundance between the rim and core of Hoopoe are also similar, indicating they may have formed from a gas of the same or similar composition. Acknowledgments: We thank the ASU Center for Meteorite Studies for loaning the samples used in this work and Tabb Prissel for his assistance with the analysis. Mouti Al-Hashimi thanks Sam Crossley and Cyrena Goodrich for their help with the LPI SEM training. This work was supported by the LPI Summer Intern Program in Planetary Science and the LPI Cooperative Agreement. References: [1] Connelly J.N. (2012) Science, 338, 651-655. [2] MacPherson G. J. (2014) Treatise on Geochem., 2, 139-179. [3] Grossman L. (1972) GCA, 36, 597-619. [4] Ebel, D.S. (2006) Meteorites and the Early Solar System II (D. S. Lauretta & H. Y. McSween, Eds.) 253-277. [5] MacPherson G. J. (2012) Earth Planet. Sci. Lett., 331-332, 43-54. [6] MacPherson G.J. (2017) GCA, 201, 65-82. [7] Krot A.N. (1995) Meteoritics & Planet. Sci., 30, 748-775. [8] Wark and Lovering (1982) GCA, 46, 2595-2607. [9] Palme H. and Jones A. (2003) Treatise on Geochemistry (H. D. Holland and K. K. Turekian Eds.), 1, 41-61. [10] Grossman L. (1980) Ann. Rev. Earth Planet. Sci., 8, 559-608. [11] Floss C. et al. (1996) GCA, 60, 1975-1997. [12] Mason B. and Martin P. M. (1974) Earth Planet. Sci. Lett., 22, 141-144. [13] Wark B. and Boynton W. V. (2001) Meteoritics & Planet. Sci., 36, 1135-1166.
Twenty five glasses were formulated. They were batched from HLW AZ-101 simulant or raw chemicals and melted and tested with a series of tests to elucidate the effect of spinel-forming components (Ni, Fe, Cr, Mn, and Zn), Al, and noble metals (Rh2O3 and RuO2) on the accumulation rate of spinel crystals in the glass discharge riser of the high-level waste (HLW) melter. In addition, the processing properties of glasses, such as the viscosity and TL, were measured as a function of temperature and composition. Furthermore, the settling of spinel crystals in transparent low-viscosity fluids was studied at room temperature to access the shape factor and hindered settling coefficient of spinel crystals in the Stokes equation. The experimental results suggest that Ni is the most troublesome component of all the studied spinel-forming components producing settling layers of up to 10.5 mm in just 20 days in Ni-rich glasses if noble metals or a higher concentration of Fe was not introduced in the glass. The layer of this thickness can potentially plug the bottom of the riser, preventing glass from being discharged from the melter. The noble metals, Fe, and Al were the components that significantly slowed down or stopped the accumulation of spinel at the bottom. Particles of Rh2O3 and RuO2, hematite and nepheline, acted as nucleation sites significantly increasing the number of crystals and therefore decreasing the average crystal size. The settling rate of ≤10-μm crystal size around the settling velocity of crystals was too low to produce thick layers. The experimental data for the thickness of settled layers in the glasses prepared from AZ-101 simulant were used to build a linear empirical model that can predict crystal accumulation in the riser of the melter as a function of concentration of spinel-forming components in glass. The developed model predicts the thicknesses of accumulated layers quite well, R2 = 0.985, and can be become an efficient tool for the formulation of the crystal-tolerant HLW glasses for higher waste loading. A physical modeling effort revealed that the Stokes and Richardson-Zaki equations can be used to adequately predict the accumulation rate of spinel crystals of different sizes and concentrations in the glass discharge riser of HLW melters. The determined shape factor for the glass beads was only 0.73% lower than the theoretical shape factor for a perfect sphere. The shape factor for the spinel crystals matched the theoretically predicted value to within 10% and was smaller than that of the beads, given the larger drag force caused by the larger surface area-to-volume ratio of the octahedral crystals. In the hindered settling experiments, both the glass bead and spinel suspensions were found to follow the predictions of the Richardson-Zaki equation with the exponent n = 3.6 and 2.9 for glass beads and spinel crystals, respectively.
Spinels and ilmenites are relatively sparse in the Luna 24 gabbro and basalts. Spinel compositions show some affinities to those of spinels in Apollo 12, Apollo 14 and Luna 16 basalts; a characteristic feature is high Al2O3, reaching a maximum of 19.8 wt%. A comparison of spinels in the Luna 24 gabbro with those in other deep-seated lunar intrusive rocks shows a characteristic trend for Fe/Mg. This trend is systematic from gabbro to anorthosite to troctolite and is interpreted to be P-T dependent. Compositions of spinels in the gabbro fall within the Cr/Al trend defined by the spinels of the basalts, but form a Fe/Mg trend parallel to that of the basalts; this relationship suggests that both the gabbro and the basalts are derived from a closely similar source region, with the basalts originating at a slightly greater depth than the gabbro. The spinels in both rock types are considered to have formed at high crustal levels, at low pressures. The Luna 24 data suggest that the compositional discontinuities which exist between chromian spinels and titanian spinels in a large proportion of mare basalts are the result of nucleation of chromian spinels at high crustal levels prior to eruption, and of titanian spinels during melt crystallization at the lunar surface.
Anomalous X-ray Diffraction (AXRD) has become a useful technique in characterizing bulk and nanomaterials as it provides specific information about the crystal structure of materials. In this project we present the results of AXRD applied to materials for photovoltaic applications: ZnO loaded with Ga and ZnCo{sub 2}O{sub 4} spinel. The X-ray diffraction data collected for various energies were plotted in Origin software. The peaks were fitted using different functions including Pseudo Voigt, Gaussian, and Lorentzian. This fitting provided the integrated intensity data (peaks area values), which when plotted as a function of X-ray energies determined the material structure. For the first analyzed sample, Ga was not incorporated into the ZnO crystal structure. For the ZnCo{sub 2}O{sub 4} spinel Co was found in one or both tetrahedral and octahedral sites. The use of anomalous X-ray diffraction (AXRD) provides element and site specific information for the crystal structure of a material. This technique lets us correlate the structure to the electronic properties of the materials as it allows us to probe precise locations of cations in the spinel structure. What makes it possible is that in AXRD the diffraction pattern is measured at a number of energies near an X-ray absorption edge of an element of interest. The atomic scattering strength of an element varies near its absorption edge and hence the total intensity of the diffraction peak changes by changing the X-ray energy. Thus AXRD provides element specific structural information. This method can be applied to both crystalline and liquid materials. One of the advantages of AXRD in crystallography experiments is its sensitivity to neighboring elements in the periodic tables. This method is also sensitive to specific crystallographic phases and to a specific site in a phase. The main use of AXRD in this study is for transparent conductors (TCs) analysis. TCs are considered to be important materials because of their efficiency and low risk of environmental pollution. These materials are important to solar cells as a result of their remarkable combination of optical and electrical properties, including high electrical conductivity and high optical transparency in the spectrum of visible light. TCs provide a transparent window, which allows sunlight to pass through while also allowing electricity to conduct out of the cell. Spinel materials have the chemical form AB{sub 2}O{sub 4}, and are made of a face-centered cubic (FCC) lattice of oxygen anions and cations in specific interstitial sites. A normal spinel has all A cations on tetrahedral sites and B cations on octahedral sites. In contrast; an inverse spinel has the A and half of the B cations on octahedral sites and the other half of the B cations on tetrahedral sites; a mixed spinel lies between. In the spinel structure, 8 of 64 possible tetrahedral sites and 16 of 32 possible octahedral sites are filled. Normal spinels have particularly high conduction as the linear octahedral chains of B cations likely serve as conduction paths. In this paper we present how the data obtained with AXRD is used to analyze TCs properties as they apply to photovoltaic applications. One of the materials used for this analysis is zinc oxide. It has been loaded with 5% and 10% of Ga, which has an absorption edge of 10367 eV. The peak (100) was measured for the zinc oxide loaded with 10% Ga. In the case of 5% Ga, we measured peaks (100) and (101). With the information provided by the AXRD we can identify if Ga is being incorporated in the ZnO crystal structure. The analysis of 311 plane in the ZnCo{sub 2}O{sub 4} spinel shows if Co is in tetrahedral or octahedral site.
Li(Mn1.5Ni0.5)O4 (MNO) is promising spinel cathode material for lithium ion batteries (LIB) due to its increased intercalation potential and improved capacity retention compared to LiMn2O4. Still, improvements to this materials performance must be achieved before MNO is a viable option for commercial LIB cells. In situ X-ray diffraction of Li(Mn1.5Ni0.5)O4 was performed using a novel electrochemical cell based on coin cell hardware. A diffractogram of the pristine material showed a spinel structure with a Ni2+ oxidation state. As the cell was charged through its 4.75V plateau, a transition between spinels with Ni2+, Ni3+, and Ni4+ oxidation was observed. As the oxidation stage on the nickel increased the lattice parameter of the corresponding spinel was reduced. As discharged ensued the spinel reversed its phases change until only the Ni2+ spinel was present. When discharge reached the 2.75V plateau a tetragonal spinel phase was formed, which upon subsequent cell charging was completely converted back to a cubic spinel phase. Lattice parameter changes of each phase were calculated and showed a characteristic strain release during phase changes. After 15 full cycles the transition between these phases was no longer complete and the formation of the tetragonal spinel phase was no longer detected. A discussion of how these cycle-induced changes to phase transition behavior relate to capacity fade and overall cell performance is presented.
We used focused ion beam thin section preparation and scanning transmission electron microscopy (FIB/STEM) to examine the interfacial region between spinel and host melilite for three spinel grains, two from the mantle and one from the core of an Allende type B1 inclusion, and a second pair of spinel grains from a type B1 inclusion from the Leoville carbonaceous chondrite. The compositions of boundary clinopyroxenes decorating spinel surfaces are generally consistent with those of coarser clinopyroxenes from the same region of the inclusion, suggesting little movement of spinels between mantle and core regions after the formation of boundary clinopyroxenes. The host melilite displays no anomalous compositions near the interface, and anorthite or other late-stage minerals are not observed, suggesting that crystallization of residual liquid was not responsible for the formation of boundary clinopyroxenes. Allende spinels display either direct spinel-melilite contact or an intervening boundary clinopyroxene between the two phases. In the core, boundary clinopyroxene is mantled by a thin (1-2 {micro}m thick) layer of normally zoned (X{sub Ak} increasing away from the melilite-clinopyroxene contact) melilite with X{sub Ak} matching that of the host melilite at the melilite-melilite contact. In the mantle, X{sub Ak} near boundary spinels is constant. Spinels in a Leoville type B1 inclusion are more complex with boundary clinopyroxene, as observed in Allende, but also variable amounts of glass ({approx}1 {micro}m width), secondary calcite, perovskite, and an unknown Mg-, Al-, OH-rich and Ca-, Si-poor crystalline phase that may be a layered double hydrate. Glass compositions are consistent to first order with a precursor consisting mostly of Mg-carpholite or sudoite with some aluminous diopside. One possible scenario of formation for the glass veins is that open system alteration of melilite produced a porous, hydrated aggregate of Mg-carpholite or sudoite + aluminous diopside that was shock melted and quenched to a glass. The unknown crystalline phase may be a shocked remnant of the precursor phase assemblage but is more likely to have formed later by alteration of the glass. Calcite appears to be an opportunistic fracture filling that postdated all major shock events. Boundary clinopyroxenes probably share a common origin with coarser-grained pyroxenes from the same region of the inclusion. In the mantle, these crystals may represent clinopyroxene crystallized in Ti-rich liquids caused by the direct dissolution of perovskite and an associated Sc-Zr-rich phase or as a reaction product between dissolving perovskite and liquid (i.e., indirect dissolution of perovskite). In the core, any perovskite and associated Ti-enriched liquids that may have originally been present disappeared before the growth of boundary clinopyroxene.
Layered LiNi 0.80 Co 0.15 Al 0.05 O 2 (NCA) holds great promise as a potential cathode material for high energy density lithium ion batteries. However, its high capacity is heavily dependent on the stability of its layered structure, which suffers from a severe structure degradation resulting from a not fully understood layered → spinel phase transformation. Using high-resolution transmission electron microscopy and electron diffraction, we probe the atomic structure evolution induced by the layered → spinel phase transformation in the NCA cathode. We show that the phase transformation results in the development of a particle structure with the formation of complete spinel, spinel domains, and intermediate spinel from the surface to the subsurface region. The lattice planes of the complete and intermediate spinel phases are highly interwoven in the subsurface region. The layered → spinel transformation occurs via the migration of transition metal (TM) atoms from the TM layer into the lithium layer. Incomplete migration leads to the formation of the intermediate spinel phase, which is featured by tetrahedral occupancy of TM cations in the lithium layer. Finally, the crystallographic structure of the intermediate spinel is discussed and verified by the simulation of electron diffraction patterns.
Introduction: Primitive meteorites contain Calcium-Aluminum-rich Inclusions (CAIs)that preserve the records of the earliest times in the Solar System. CAIs record O isotopic variations with time and/or location from solar (16O-rich) to planetary (16O-poor) compositions [e.g., 1, 2].However, CAIs were also affected by parent body processing to varying degrees. The goal of this work was to identify the processes that resulted in the fine-scale spatial variations in oxygen isotopic compositions within the most ancient Solar System solids. We report oxygen isotopic composition of CAIs from MIL 090019 CO3.1 carbonaceous chondrite. MIL 090019 contains a high abundance of CAIs showing mineralogical as well as textural variations [3]. Methods: We analyzed 10 CAIs with different mineralogical assemblages, classified as corundum-bearing, grossite-bearing, hibonite-bearing, melilite-bearing, anorthite-bearing inclusions and amoeboid olivine aggregates(AOA’s). The mineralogical and petrological characterization of CAIs was performed using the JOEL Hyperprobe 8530 electron microprobe at NASA JSC. Oxygen isotopic imaging of the CAIs was done using the Cameca NanoSIMS 50L ion microprobe at NASA JSC. We followed the analytical protocol described in [4]. O-isotopic maps of the CAI were acquired by rastering a ~3 pA primary Cs+beam at 16 keVover an area of 20 ×20μm2over a period of ~7 hours. Negative secondary ions of 16O−, 17O−, 18O−, 28Si−, 24Mg16O−, 27Al16O−, and 40Ca16O−were simultaneously acquired using electron multiplier detectors at a mass resolving power sufficient to resolve the 16OH−interference from the 17O−peak, where the contribution of 16OH−was <0.1%.An electron flood gun was used to mitigate sample charging during the analyses. We used San Carlos olivine and Madagascar hibonite as isotopic standards to correct for the instrumental mass fractionation. The O-isotopic ratios were corrected for the quasi simultaneous arrival (QSA) effect and the detector dead time. All reported errors are 1 sigma. Results: The MIL 090019 carbonaceous chondrite hosts refractory inclusions varying in their mineralogies and textures[2, 3]. We found the oxygen isotopic compositions of mineral phases in MIL 090019 CAIs show large variations with Δ17O values varying from -27 to 0‰. A corundum-bearing inclusion records isotopic variations with corundum, melilite, perovskite, and anorthite showing Δ17Ovalues of -20 ±2.5, -10.2 ± 6.5, -10.7 ± 1.3,and -1.2 ± 3.2‰ respectively. A grossite-hibonite-bearing inclusion also records O-isotopic heterogeneity, where grossite, hibonite, Mg-rich spinel, and melilite show -3.7 ± 2.7, -22.9 ± 2.5, -21.4 ± 2.6, and -17.3 ± 2.8‰ respectively, whereas perovskite grains record a heterogenous isotopic composition ranging from -22.6 to -13.9‰. A hibonite-bearing inclusion shows average Δ17Ο values of -17.6 ± 5.3 ‰ and -15.1 ± 4.8 ‰ for hibonite and spinel respectively. The two perovskite grains also show relatively 16O-poor composition (Δ17Ο = -11.8 ± 6.4 ‰ and -8.6 ± 5.2 ‰). Anorthite has ~0.1 wt% Na2O and ~0.52 wt% FeO and a Δ17Ο value of -7.2 ± 5.0 ‰, whereas diopside records a Δ17Ο value of -3.5 ± 5.0 ‰. A hibonite-spinel-rich inclusion contains spinel and hibonite that are16O-rich (Δ17Οvalues -21.3 ± 2.8‰ and -19.4 ± 3.0‰, respectively). Melilite shows heterogenous oxygen isotopic composition, with an inner 16O-rich region and an outer 16O-poor region separated by a sharp boundary, with a bulk Δ17Ο= -16.2 ± 2.1‰, whereas two perovskite grains are relatively 16O-poor (Δ17Ο= -13.2 ± 3.7‰ and -7.1 ± 3.4‰).A spinel-rich inclusion contains perovskite grains with Δ17Οranging from -27.0 to -22.8 ‰and spinel with average Δ17Οvalue of -21.4 ± 2.8 ‰. In a melilite and spinel-rich CAI, perovskite, spinel, diopside, melilite, and Al-Ti-rich pyroxene record Δ17Ο values of-26.9 ± 4.6‰, -22.4 ± 4.3‰,-23.4 ± 4.9, -19.3 ± 3.4, and -19.0 ± 4.3 ‰ respectively. Olivine and spinel components of 2 AOA’s record a 16O-rich composition with Δ17O~-23‰. Discussion: The coexistence of 16O-rich and 16O-poor minerals within CAIs has been attributed to differing degrees of O isotopic exchange, reflecting a wide range of O diffusion rates[5]. However, the O isotopic heterogeneity observed in these CAIs cannot be explained by oxygen diffusion in nebular or parent body settings alone. The isotopic imaging of CAIs from the MIL 090019 meteorite shows variations in the O isotopic composition recorded in their mineral components, suggesting that these CAIs record the oxygen isotopic heterogeneity in the nebular gas from which they condensed. The coexistence of 16O-rich and 16O-poor mineral components in the CAI-forming region suggests that the gas in this region was not well-mixed and consisted of distinct 16O-rich and 16O-poor gaseous reservoirs.
The buildup of corrosion product deposits (CRUD) on the fuel cladding of the boiling water reactor (BWR) before and after zinc injection has been investigated by applying local experimental analytical techniques. Under the BWR water chemistry conditions, Zn addition together with the presence of Ni and Mn induce the formation of (Zn,Ni,Mn)[Fe{sub 2}O{sub 4}] spinel solid solutions. X-ray absorption spectroscopy (XAS) revealed inversion ratios of cation distribution in spinels deposited from the solid solution. Based on this information, a two-site ferrite spinel solid solution model is proposed. Electron probe microanalysis (EPMA) and extended X-ray absorption fine structure (EXAFS) findings suggest the zinc-rich ferrite spinels formation on BWR fuel cladding mainly at lower pin. - Graphical Abstract: Analysis of spinels in corrosion product deposits on boiling water reactor fuel rod. Combining EPMA and XAFS results: schematic representation of the ferrite spinels in terms of the end members and their extent of inversion. Note that the ferrites are represented as a surface between the normal (upper plane, M[Fe{sub 2}]O{sub 4}) and the inverse (lower plane, Fe[MFe]O{sub 4}). Actual compositions red Black-Small-Square for the specimen at low elevation (810 mm), blue Black-Small-Square for the specimen at mid elevation (1800 mm). The results have an impact on the properties of the CRUD material. Highlights: Black-Right-Pointing-Pointer Buildup of corrosion product deposits on fuel claddings of a boiling water reactor (BWR) are investigated. Black-Right-Pointing-Pointer Under BWR water conditions, Zn addition with Ni and Mn induced formation of (Zn,Ni,Mn)[Fe{sub 2}O{sub 4}]. Black-Right-Pointing-Pointer X-Ray Adsorption Spectroscopy (XAS) revealed inversion of cations in spinel solid solutions. Black-Right-Pointing-Pointer Zinc-rich ferrite spinels are formed on BWR fuel cladding mainly at lower pin elevations.
The interface structure and magnetism of hybrid magnetic tunnel junction-spin filter devices have been investigated and correlated with their transport properties. Magnetic tunnel junctions made of a spinel NiMn2O4 tunnel barrier sandwiched by theoretically predicted half-metallic electrodes, perovskite La0.7Sr0.3MnO3 and spinel Fe3O4, exhibit very high crystalline quality as observed by transmission electron microscopy. Structurally abrupt interfaces allow for the distinct magnetic switching of the electrodes as well as large junction magnetoresistance. The change in the magnetic anisotropy observed at the spinel-spinel interface is indicative of a thin interdiffused magnetically soft interfacial layer. The strong exchange coupling at this interface allows for low background magnetoresistance, and a spin-filter effect with when the barrier is ferrimagnetic.
Technetium (Tc) remains a priority remediation concern due to persistent challenges, including rapid re-oxidation of immobilized Tc, and competing contaminants, e.g. Cr(VI), that inhibit targeted Tc reduction and incorporation into stable mineral phases. Here Fe(OH) 2 (s) is investigated as a comprehensive solution for overcoming these challenges, by serving as both the reductant, (Fe(II)), and immobilization agent to form Tc-incorporated magnetite (Fe 3 O 4 ). Trace metal analysis suggests removal of Tc(VII) and Cr(VI) from solution occurs simultaneously; however, complete removal and reduction of Cr(VI) is achieved earlier than the removal/reduction of co-mingled Tc(VII). Bulk oxidation state analysis of the magnetite solid phase by XANES confirms that the majority of Tc is Tc(IV), which is corroborated by XPS. Furthermore, EXAFS results show successful Tc(IV) incorporation into magnetite octahedral sites without additional substitution of Cr or Tc into neighboring Fe octahedral sites. XPS analysis of Cr confirms reduction to Cr(III) and the formation of a Cr-incorporated spinel, Cr2O 3 , and Cr(OH)3 phases. Spinel (modeled as Fe 3 O 4 ), goethite, and feroxyhyte are detected in all reacted solid phase samples analyzed by XRD, where Tc(IV) incorporation has little effect on the spinel lattice structure. In the presence of Cr(III) a spinel phase along the magnetite-chromite (Fe 3 O 4 -FeCr 2 O 4 ) solid-solution line is formed.
Capacity loss, and voltage fade upon electrochemical charge-discharge cycling observed in lithium-rich layered cathode oxides (Li[LixMnyTM1-x-y]O2 , TM = Ni, Co or Fe) have recently been identified to be correlated to the gradual phase transformation, featuring the formation of a surface reconstructed layer (SRL) that evolves from a thin (<2 nm), defect spinel layer upon the first charge, to a relatively thick (~5 nm), spinel or rock-salt layer upon continuous charge-discharge cycling. Here we report observations of a SRL and structural evolution of the SRL on the Li[Li0.2Ni0.2Mn0.6]O2 (LMR) particles, which are identical to those reported due to the charge-discharge cycle but are a result of electron-beam irradiation during scanning transmission electron microscopy (STEM) imaging. Sensitivity of the lithium-rich layered oxides to high-energy electrons leads to the formation of thin, defect spinel layer on surfaces of the particles when exposed to a 200 kV electron beam for as little as 30 seconds under normal high-resolution STEM imaging conditions. Further electron irradiation produces a thicker layer of the spinel phase, ultimately producing a rock-salt layer at a higher electron exposure. Atomic-scale chemical mapping by energy dispersive X-ray spectroscopy in STEM indicates the electron-beam-induced SRL formation on LMR is accomplished by migration of the transition metal ions to the Li sites without breaking down the lattice. This study provides an insight for understanding the mechanism of forming the SRL and also possibly a mean to study structural evolution in the Li-rich layered oxides without involving the electrochemistry.
Abstract During the vitrification of high‐level radioactive waste ( HLW ) in HLW melters in the Waste Treatment and Immobilization Plant located in Washington State, spinel crystals may precipitate from glass and accumulate in the melter riser, preventing the discharge of molten glass into canisters. Therefore, an effort is being made to develop an electrical conductivity method to monitor crystal buildup in the melter riser. A vertically configured electrical conductivity ( EC ) probe with an alumina shaft and Pt‐10%Rh‐electrodes was designed and tested in standard conductivity solutions and glass melts both with and without spinel crystals. The EC probe measured conductivity in conductivity solutions within 10% of their certified values and showed a linear relationship with increased spinel layer thicknesses. Testing in silicate glass containing spinel crystals allowed for the determination of spinel conductivity as a function of temperature. The conductivities of spinel crystals of 20‐24 S/m at 800°C were in excellent agreement with the conductivity of trevorite (NiFe 2 O 4 ) crystals at 800°C reported in the literature. The conductivities of spinel crystals and measured changes in the conductivity across the accumulated layer allowed for a successful measurement of spinel crystal accumulation in simulated HLW glass.
Here, we report on the mineralogy, petrology, oxygen, and aluminum–magnesium isotopic systematics of the secondary corundum-bearing assemblages in type B CAIs 3529Z and 3529G and fluffy type A (FTA) CAI ALH-2 from Allende (CV > 3.6). In 3529Z and 3529G, 2–5 μm-sized euhedral-to-subhedral corundum grains associate with secondary alumoåkermanite [(Ca,Na) 2 AlSi 2 O 7 ], grossular, spinel, grossite, celsian, kushiroite, and wadalite. In ALH-2, 2–5 μm-sized euhedral-to-subhedral corundum grains associate with secondary grossular, nepheline, spinel, and kushiroite. In 3529Z and 3529G, corundum and associated secondary grossite, spinel, alumoåkermanite, grossular, and kushiroite have similar 16 O-poor compositions (Δ 17 O = −2.2 ± 1.5‰); primary spinel is 16 O-rich (Δ 17 O ~ −23‰); Al,Ti-diopside shows a range of Δ 17 O (from ~ −24‰ to ~ −15‰); anorthite and melilite are 16 O-depleted to various degrees (−6.5‰ ≤ Δ 17 O ≤ −4.5‰ and Δ 17 O = −2.7 ± 0.8‰, respectively). In ALH-2, corundum shows a range of Δ 17 O, from ~ −9‰ to ~ −1‰; primary hibonite and spinel are 16 O-rich (Δ 17 O ~ −23‰); melilite and perovskite are 16 O-poor (Δ 17 O = −2.6 ± 1.5‰ and −3.1 ± 1.3‰, respectively). On the Al-Mg isotope diagram ( 26 Mg* versus 27 Al/ 24 Mg), primary Al,Ti-diopside, hibonite, melilite, and spinel in the Allende CAIs studied along the canonical isochron with inferred initial 26 Al/ 27 Al ratio [( 26 Al/ 27 Al) 0 ] of ~5 × 10 −5 . All secondary minerals have resolved excesses of 26 Mg*: alumoåkermanite, corundum, and grossite plot below the canonical isochron, whereas most spinel analyses plot above it. An internal isochron defined by the coexisting secondary corundum and alumoåkermanite in 3529Z has ( 26 Al/ 27 Al) 0 = (7.5 ± 2.6) × 10 −7 . We conclude that the corundum-bearing assemblages in Allende CAIs resulted from metasomatic alteration of primary melilite and anorthite, ~4–5 Ma after their crystallization. Metasomatic alteration of CAIs in the Allende parent asteroid by an aqueous fluid having Δ 17 O of ~ −3 ± 2‰ modified the O-isotope composition of their primary melilite, anorthite, and Ti-rich pyroxene; O-isotope compositions of primary hibonite, spinel, and low-Ti pyroxene escaped this modification.