Correlation of uniaxial yielding and substructure in aluminum-stainless steel composites
Uniaxial yielding correlation with substructure in Al-stainless steel metal matrix composites, using compressive loading test
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Uniaxial yielding correlation with substructure in Al-stainless steel metal matrix composites, using compressive loading test
Physisorption isotherms for nitrogen on stainless steel at various temperatures and very low pressures
Accelerated failure tests of ammonia-Al-stainless steel heat pipes for fluid loss or energy transport degradation
Thermal cycling effects on integrity of refractory stainless steel tubular coextruded joint
Surface roughness of 304 stainless steel by Brunauer-Emmett-Teller measurements, using ethylene as adsorbate
The elevated-temperature mechanical properties of several ferritic stainless steels were determined. The alloys evaluated included Armco 18SR, GE 1541, and NASA-18T-A. Tensile and creep strength properties at 1073 and 1273 K and residual room temperature tensile properties after creep testing were measured. In addition, 1273 K tensile and creep tests and residual property testing were conducted with Armco 18SR and GE 1541 which were exposed for 200 hours to a severe oxidizing environment in automotive thermal reactors. Aside from the residual tensile properties for Armco 18SR, prior exposure did not affect the mechanical properties of either alloy. The 1273 K creep strength parallel to the sheet-rolling direction was similar for all three alloys. At 1073 K, NASA-18T-A had better creep strength than either Armco 18SR or GE 1541. NASA-18T-A possesses better residual properties after creep testing than either Armco 18SR or Ge 1541.
The cumulative creep-fatigue damage behavior of 316 stainless steel at 1500 F was experimentally established for the two-level loading cases of fatigue followed by fatigue, creep fatigue followed by fatigue, and fatigue followed by creep fatigue. The two-level loadings were conducted such that the lower life (high strain) cycling was applied first for a controlled number of cycles and the higher life (low strain) cycling was conducted as the second level to failure. The target life levels in this study were 100 cycles to failure for both the fatigue and creep-fatigue lowlife loading, 5000 cycles to failure for the higher life fatigue loading and 10,000 cycles to failure for the higher life creep-fatigue loading. The failed specimens are being examined both fractographically and metallographically to ascertain the nature of the damaging mechanisms that produced failure. Models of creep-fatigue damage accumulation are being evaluated and knowledge of the various damaging mechanisms is necessary to ensure that predictive capability is instilled in the final failure model.
Presentation titled "Discussion of Techniques for UT of Austenitic Stainless Steel"
The adsorption behavior of molecular iodine is important for understanding the spread of radioiodine in a nuclear accident. Prior experiments indicate that, in addition to the interaction with Fe, molecular iodine [i.e., I 2(g) ] also interacts with the next most abundant components of austenitic stainless steel (i.e., Ni, and Cr) at room temperature. Here, we investigate iodine adsorption on Fe, Ni, and Cr while focusing on understanding the variables affecting adsorption as well as the iodine compounds that are formed during adsorption. Scanning electron microscopy and energy-dispersive X-ray spectroscopy were used to characterize the surfaces of exposed metal particles and aid in the understanding of the morphology and chemistry of iodine interactions with the substrates. Inductively coupled plasma optical emission spectroscopy was used to detect low levels of metal iodides and X-ray photoelectron spectroscopy was used to confirm the formation of the metal iodides. The role of environmental factors (e.g., humidity and oxygen content) for iodine adsorption on metal substrates is addressed. The individual metals demonstrated formation of metal iodides for Fe and Ni particles from interaction with I 2(g) . The formation of metal iodides may indicate the affinity of iodine for the respective metal. In this study, the iodine affinities ranked Fe > Ni > Cr as determined by the quantity of chemisorbed iodine. This trend is also supported by the distributions and proportions of metals in the corrosion product of the stainless steels. The exposures without oxygen and humidity indicate the potential of a multistep iodine adsorption process where iodine first attacks the oxide layer and then chemisorbs to the exposed metal.
The subject of the research that has been conducted in this paper was to analyze precipitation-hardened martensitic stainless steel 17-4 PH after flow forming with four different strains and subsequent standard heat treatment. Four cylinders were obtained with a 16, 30, 48 and 68% reduction in thickness, respectively. The samples were analyzed in terms of their mechanical properties and microstructural changes before and after the heat treatment. The results showed that a higher strain resulted in an overall higher strength (up to 1200 MPa UTS) and refinement of the structure, although at a cost of the elongation. High deformation influenced the precipitation process, and the ratio of the grain boundaries significantly increased. Nonetheless, comparing the obtained results with other similar research, it seems that the formation of nano-precipitates of Cu is the key-strengthening mechanism. Strain hardening contributes to an increase in the strength of the steel, although the effect decreases after heat treatment. The relatively small values of residual stress in the steel, especially after the heat treatment, confirmed these claims. Overall, flow forming allowed high deformations of the 17-4 PH steel to be obtained although it did not significantly change the mechanical properties of the material due to the dominant precipitation hardening mechanism.
The influence of sigma phase precipitation on the texture of austenite in a duplex stainless steel UNS S31803 was investigated. Sigma phase quantification was precisely performed by electron backscattered scanning diffraction (EBSD) for some conditions. It was found that the increase of the sigma phase precipitation enhances the amount of Brass texture in the austenite phase.
Data obtained at minus 320 degrees f from both aged and unaged cryogenically stretched spheres of stainless steel
This study examined how cold forging (CF) affects the corrosion of 316 stainless steel (SS) in molten FLiNaK salt at 700 °C for 48 h. CF samples had two corrosion areas: one near the top and another displaying intergranular corrosion (IGC). Samples with lower CF (5–30 %) showed more IGC, while the 50 % CF sample had less IGC but the shallowest corrosion depth. This was due to the increased number of grain boundaries, which raised the potential corrosion initiation sites, and certain grain boundaries promoting chromium dissolution, thus enhancing IGC.
Low-temperature salt bath nitriding of heat treated and tempered 13/4 Martensitic stainless steel (13/4HTT) was carried at 450 °C (N450) and 500 °C (N500) for 10 h each. The nitrided samples were characterized by using x-ray diffractometer, field emission scanning electron microscope and optical microscope. The nanohardness and elastic modulus of the cross section of nitrided specimen were measured by nanoindentation test using Hysitron TI950 triboindenter. The nitrided 13/4HTT (N450 and N500) and 13/4HTT specimens were subjected to slurry erosion test in a slurry pot tester. The test was conducted for 48 h, and weight loss was measured after every 6 h. The relative speed of slurry with respect to specimen was 4.55 m/s. It was found that the weight loss due to erosion of the N450 is 83% less than that of 13/4HTT and that of N500 was 92% more than that of 13/4HTT. The erosion mechanism is correlated to the phases present in the specimens. The improvement in the slurry erosion resistance of N450 is due to presence of expanded martensite (α{sub N}-Fe). Increasing the temperature of nitriding to 500 °C led to the decrease in the slurry erosion resistance of N500 due to the formation of brittle CrN phase.
Carbon nanotube (CNT) reinforced 316L stainless steel (SS) composites were fabricated by laser powder bed fusion (LPBF) additive manufacturing (AM). This study focuses on microstructure evolution, hardness, and wear behavior. The wear behavior for AM 316L SS and 1 wt% CNT/316L SS was studied by a dry sliding test under normal loads of 10, 15, and 25 N. The addition of CNT to 316L SS led to the change of solidification mode from cellular/columnar to dendritic growth, producing grain refinement. Nanoscale dendrites were observed. Although TEM characterization confirmed the existence of CNT in cell interior, most CNT were damaged, resulting in carbon material segregation along cellular/dendritic boundaries. The wear rate was found dramatically decreased due to the improved hardness. Compared to the adhesive and abrasive wear in AM 316L SS, the wear mechanism of CNT/316L composite was adhesion and oxidative wear. Furthermore, enhanced cellular/dendritic boundary strengthening by carbon segregation was the main strengthening mechanism of CNT/316L composite.
The Industry-Sponsored Metals Combustion Test Program 96-1 was coordinated through Wendell Hull & Associates, Inc. on behalf of several contributing companies, and all design and testing was performed at the NASA White Sands Test Facility. Phase I of this test program studied the threshold pressure for self-sustained burning of various types and sizes of stain less steel rods in nonflowing oxygen, as observed in Standard Test Method for Determining the Combustion Behavior of Metallic Materials in Oxygen-Enriched Atmospheres (ASTM G 124-95). Phase II studied the ignition and propagation of burning of 316L stainless steel rods and pipe in flowing gaseous oxygen. The test sample configurations were chosen to replicate previous promoted ignition and burning tests as well as to represent geometries and cross-sectional thicknesses common in industrial piping applications. The gas pressw'es and velocities for the test matrix were selected to generally compare with CGA G-4.4 guidelines for the use of stain less steel in oxygen service. This paper summarizes the results from the Phase I nonflowing oxygen tests and presents in detail the results of the Phase II flowing oxygen tests. The maximum sample burn-length is shown as a function of test pressure in Phase 1 and also as a function of gas velocity in Phase IT. These results indicate that flowing oxygen, under the given test conditions, significantly affects maximum sample burn length as compared to nonflowing oxygen. Supplementary flowing oxygen test data on stainless steel rods from a follow-up test program are consistent with these results and are presented herein.
316L stainless steel coated with sputter deposited HfO{sub 2}, Al{sub 2}O{sub 3}, and HfO{sub 2}-Al{sub 2}O{sub 3} nanolaminate films were subjected to direct current cyclic potentiodynamic polarization (DCP) in Hanks' balanced salt solution electrolyte. Postexposure morphology was characterized by scanning electron microscopy (SEM) with in situ energy dispersive spectroscopy (EDS). SEM/EDS data show that bare steel and steel coated with single-layer HfO{sub 2} develop pits with perforated covers. These pits become autocatalytic, consistent with an observed positive DCP hysteresis. On the other hand, SEM/EDS data show that steel coated with Al{sub 2}O{sub 3} and HfO{sub 2}-Al{sub 2}O{sub 3} nanolaminate films does not develop autocatalytic pits, consistent with an observed negative DCP hysteresis. However, Al{sub 2}O{sub 3} splinters upon polarization whereas the HfO{sub 2}-Al{sub 2}O{sub 3} nanolaminate remains intact. The areas of worst damage in the nanolaminate correspond to pit cover rupture before autocatalysis, allowing pit and bulk electrolyte to mix and the newly exposed steel surface to repassivate. The films' diverse behavior is discussed in terms of a model for perforated pit growth that requires occlusion until an autocatalytic geometry is established. The authors conclude that the key property a film must have to arrest autocatalytic geometry development is the ability to rupture locally at an early stage of pit growth.
Tensile properties of five low-alloy and stainless steels under high heating rate and constant temperature