Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CALORIMETRY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 739 records · Page 41

Structural evolution of an Al-Te mixture during ball milling

An Al-Te mixture was mechanically alloyed with a planetary ball mill, and the structural evolution of the Al-Te mixture during ball milling was characterized by X-ray diffractiometry (XRD), differential scanning calorimetry (DSC), scanning electron microscopy (SEM), and thermodynamic computation. Although crystalline {alpha}-Al{sub 2}Te{sub 3} was synthesized in the initial stage of milling, but the final product is a metastable Al{sub 2}Te{sub 3-{delta}} (Space group: Fm 3-bar m) with lattice parameter a = 5.925 A. The metastable Al{sub 2}Te{sub 3-{delta}} decomposes into Al and Te at about 140 deg. C.

36 MATERIALS SCIENCE↗

Cation distribution in the Bi{sub 4-x}RE{sub x}Ti{sub 3}O{sub 12} (RE = La, Nd) solid solution and Curie temperature dependence

Bi{sub 4-x}RE{sub x}Ti{sub 3}O{sub 12} (RE = La, Nd) ferroelectric powders were prepared by a co-precipitation route. Raman spectroscopy and X-ray diffraction were employed to determine the crystal site of La{sup 3+} and Nd{sup 3+} as well as the effect of their addition on the crystal structure. It was found that La atoms were not only placed preferentially in pseudo-perovskite A sites for concentrations x {<=} 1.2 but also substituted for Bi{sup 3+} in (Bi{sub 2}O{sub 2}){sup 2+} layers for greater concentrations. A similar behavior was observed with the limit value x = 0.8 in case of Nd{sup 3+}. In solid solution La or Nd{sup 3+} ions diminish the distortions in the octahedron formed by oxygen atoms, so there is a tendency to undergo a transition in crystal symmetry from orthorhombic to tetragonal. Finally differential scanning calorimetry (DSC) shows a linear dependence of the Curie temperature (T{sub c}) when the amount of La{sup 3+} or Nd{sup 3+} was increased.

36 MATERIALS SCIENCE↗

Effect of heat treatments on discontinuous precipitation kinetics in Al-30 wt.% Zn alloy

The discontinuous precipitation kinetics in Al-30% wt. Zn alloy have been investigated at temperatures ranging from 348 to 503 K (75 to 230 deg. C) by using an optical microscopy, X-ray diffraction, differential dilatometer, differential scanning calorimetry and microhardness measurement. We have found that at all temperatures less than 180 deg. C the supersaturated solid solution of quenched alloy was observed to decompose completely by a cellular precipitation reaction. Quantitative metallography methods have been applied to measure the corresponding transformed volume fractions at different temperatures and times of precipitation. The variation of the heating rate and the application of different methods have allowed us to calculate two kinetic parameters of precipitation: the activation energy of the process and the Avrami exponent.

36 MATERIALS SCIENCE↗

Use of time history speckle pattern and pulsed photoacoustic techniques to detect the self-accommodating transformation in a Cu-Al-Ni shape memory alloy

Continuous and pulsed electromagnetic radiation was used to detect the self-accommodation mechanism on a polycrystalline Cu-13.83 wt.%Al-2.34 wt.%Ni shape memory alloy. Rectangular samples of this alloy were mechanically polished to observe the austenite and martensite phases. The samples were cooled in liquid nitrogen prior to the experiments to obtain the martensite phase. Using a dynamic speckle technique with a continuous wave laser we obtained the time history of the speckle pattern image and monitored the surface changes caused by the self-accommodation mechanism during the inverse (martensitic to austenitic) transformation. Using a photoacoustic technique based on a pulsed laser source it was also possible to detect the self-accommodation phenomena in a bulk sample. For comparison purposes, we used differential scanning calorimetry (DSC) to detect the critical temperatures of transformation and use these as reference to evaluate the performance of the optical and photoacoustical techniques. In all cases, the same range of temperature was obtained during the inverse transformation. From these results, we conclude that time history speckle pattern (THSP) and pulsed photoacoustic are complementary techniques; they are non-destructive and useful to detect surface and bulk martensitic transformation induced by a temperature change.

36 MATERIALS SCIENCE↗

Effects of strain amplitude and temperature on the damping capacity of an Fe-19Mn alloy with different microstructures

The influences of strain amplitude (10{sup -5}-10{sup -4}) and temperature (25 deg. C-500 deg. C) on the internal friction of a cold-drawn and solution treated Fe-19Mn alloy were investigated. The internal friction was measured using reversal torsion pendulum and multifunction internal friction equipment. The microstructure was observed using scanning electron microscopy. The phase transformation temperatures were determined using differential scanning calorimetry. The results indicated that the internal friction of the solution treated alloy was related to strain amplitude, which could be explained using the movement of Shockley partial dislocations (bowing out and breaking away). But the internal friction of the cold-drawn alloy was independent of strain amplitude because of high density dislocations formed by cold forming. Moreover, when the temperature was changed between 25 deg. C and 500 deg. C, the internal friction of the cold-drawn alloy increased slowly from 25 deg. C to 375 deg. C, and then increased quickly from 375 deg. C to 500 deg. C. However, for the solution treated alloy, there was an internal friction peak at about 210 deg. C in the heating process (from 25 deg. C to 500 deg. C), and there was another internal friction peak at about 150 deg. C in the cooling process. These peaks could be explained using the heat-assisted movement of dislocations. - Research Highlights: {yields}Internal friction of solution treated Fe-19Mn alloy is related to strain amplitude. {yields}Internal friction of cold-drawn Fe-19Mn alloy is independent of strain amplitude. {yields}IF of cold-drawn alloy increases from RT to 500 deg. C. {yields}There is an IF peak of solution treated alloy in heating and cooling process separately. {yields}The results can be explained using the movement of dislocations.

36 MATERIALS SCIENCE↗

Effects of double aging heat treatment on the microstructure, Vickers hardness and elastic modulus of Ti-Nb alloys

Aging heat treatment can be a good way to optimize mechanical properties, changing the microstructure, and hence, the mechanical behavior of Ti alloys. The effects of aging heat treatments on {beta}-type Ti-30Nb alloy were investigated to evaluate the kinetics of {alpha}'' {yields} {alpha} + {beta} transformation. The results obtained from differential scanning calorimetry and high-temperature X-ray diffraction experiments indicated the complete decomposition of orthorhombic {alpha}'' phase at close to 300 deg. C, followed by {alpha} phase precipitation at 470 deg. C. The aging heat treatments also enabled us to observe a transformation sequence {alpha}'' {yields} {beta} + {omega} {yields} {beta} + {omega} + {alpha}, indicating martensite decomposition and {omega} phase precipitation at 260 deg. C after 2 h, followed by {alpha} phase nucleation after heating at 400 deg. C for 1 h. The elastic modulus and Vickers hardness of Ti-30Nb alloy were found to be very sensitive to the microstructural changes caused by heat treatment. - Highlights: {yields} DSC and XRD shed light on the {alpha}'' decomposition and nucleation of {omega} and {alpha} phases. {yields} Aging allows for {alpha}''{yields}{beta} transformation and nucleation of {omega} dispersed in the {beta} matrix. {yields} During aging, {alpha}'' interplanar distances are reduced to enable {beta} phase nucleation. {yields} Mechanical behavior is dependent on the microstructure and the phases in the alloy. {yields} It is not possible to obtain high strength and low elastic modulus by applying aging.

36 MATERIALS SCIENCE↗

Calorimetric study on mechanically milled aluminum and multiwall carbon nanotube composites

Pure aluminum reinforced with carbon nanotube (CNT) composites have been prepared by high energy attritor milling up to 48 hrs. Differential Scanning Calorimetry (DSC) has been carried out to investigate apparent activation energy and order of the reaction between carbon nanotubes and aluminum by Kissinger equation and Crane equation under non-isothermal conditions. The DSC results clearly reveal that an exothermic reaction occurs before the melting of aluminum. The effect of milling time on the initiation of this exothermic reaction has been studied. The peak temperature of the reaction of carbon nanotubes and aluminum is found to depend on the heating rate during the continuous heating. Apparent activation energy was found to get doubled after milling for 36 hrs compared to 24 hrs milled samples. The mechanism of the reaction kinetics which depends on reaction order is instantaneous nucleation and one dimensional growth for both samples. Formation of Al{sub 4}C{sub 3} was confirmed by X-ray diffraction (XRD) of as-milled powders and after performing DSC of the milled powders. Highlights: {yields} Attritor milling used for processing Al-CNT composites. {yields} Powder morphology as a function of time studied. {yields} Apparent activation energy and order of the reaction calculated for Al{sub 4}C{sub 3} formation. {yields} Apparent activation energy increases two fold with increase in milling time from 24 to 36 hours.

36 MATERIALS SCIENCE↗

Microstructures and microhardness evolutions of melt-spun Al-8Ni-5Nd-4Si alloy

Al-Ni-Nd-Si alloy with nominal composition of Al-8 wt.%Ni-5 wt.%Nd-4 wt.%Si was rapidly solidified by using melt-spinning technique to examine the influence of the cooling rate/conditions on microstructure and mechanical properties. The resulting conventional cast (ingot) and melt-spun ribbons were characterized by X-ray diffraction, optical microscopy, scanning electron microscopy together with energy dispersive spectroscopy, differential scanning calorimetry, differential thermal analysis and Vickers microhardness tester. The ingot alloys consists of four phases namely {alpha}-Al, intermetallic Al{sub 3}Ni, Al{sub 11}Nd{sub 3} and fcc Si. Melt-spun ribbons are completely composed of {alpha}-Al phase. The optical microscopy and scanning electron microscopy results show that the microstructures of rapidly solidified ribbons are clearly different from their ingot alloy. The change in microhardness is discussed based on the microstructural observations. - Highlights: Black-Right-Pointing-Pointer Rapid solidification allows a reduction in grain size, extended solid solution ranges. Black-Right-Pointing-Pointer We observed the matrix lattice parameter increases with increasing wheel speed. Black-Right-Pointing-Pointer Melt-spun ribbons consist of partly amorphous phases embedded in crystalline phases. Black-Right-Pointing-Pointer The solidification rate is high enough to retain most of alloying elements in the Al matrix. Black-Right-Pointing-Pointer The rapid solidification has effect on the phase constitution.

36 MATERIALS SCIENCE↗

Fabrication and photocatalytic properties of free-standing TiO{sub 2} nanotube membranes with through-hole morphology

Anodic growth of TiO{sub 2} nanotubes has recently attracted intensive interests. However, the insulating, closed barrier layer has restricted their feasibility for the applications such as flow-through photocatalytic reactions, biofiltration, and diffusion controlling. In the present work, we fabricated free-standing TiO{sub 2} membranes with through-hole morphology by elevating the anodizing voltage at the end of anodization process. Characterization of the samples was carried out by means of scanning electron microscope, X-ray diffraction and thermogravimetry-differential scanning calorimetry. The experimental results show that the TiO{sub 2} membranes start to transform from amorphous phase to anatase at 300 Degree-Sign C, and the phase transformation from anatase to rutile starts at 650 Degree-Sign C. In addition, photocatalytic degradation of rhodamine B by the TiO{sub 2} membranes with closed bottoms and opened bottoms has also been systematically investigated. As compared to TiO{sub 2} membranes with closed bottoms, TiO{sub 2} membranes with opened bottoms exhibited superior photocatalytic activity due to its better access for rhodamine B molecules as well as the enhanced light harvesting and electron collection efficiencies. Highlights: Black-Right-Pointing-Pointer The closed bottoms were opened by elevating the anodizing voltage. Black-Right-Pointing-Pointer Phase transformation from anatase to rutile starts at 650 Degree-Sign C. Black-Right-Pointing-Pointer TiO{sub 2} membranes in the anatase form have a better catalytic performance. Black-Right-Pointing-Pointer Opened-bottom TiO{sub 2} membranes with exhibited superior photocatalytic activity.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Lamellar {gamma}-AlOOH architectures: Synthesis and application for the removal of HCN

Using hexadecyl trimethyl ammonium bromide (CTAB) as a structure-directing agent and precipitator, the complete synthesis of lamellar {gamma}-AlOOH architectures was successfully accomplished via a hydrothermal route. Different product structures were obtained by varying the molar ratio of aluminum nitrate and CTAB. Several techniques, including X-ray powder diffraction, Fourier transform infrared spectroscopy, field-emission scanning electron microscopy, transmission electron microscopy, and differential scanning calorimetry thermal analysis, were used to characterize the products. The effects of CTAB concentration, reaction temperature and time, and the molar ratio of Al{sup 3+}/CTAB on the product morphologies were investigated. The nitrogen adsorption and desorption measurements indicated that the {gamma}-AlOOH architectures possess a Brunauer-Emmett-Teller surface area of approximately 75.02 m{sup 2}/g. It was also demonstrated that 10 mg {gamma}-AlOOH architectures can remove 45.3% of the HCN (1.68 {mu}g/mL) from model wastewater. When 0.03 mg/cig {gamma}-AlOOH architectures were combined with cigarette paper, 8.12% of the present HCN was adsorbed. These results indicate that lamellar {gamma}-AlOOH architectures may be a potential adsorbent for removing HCN from highly toxic pollutant solutions and harmful cigarette smoke. Highlights: Black-Right-Pointing-Pointer Hexadecyl trimethyl ammonium bromide (CTAB) was used as a structure-directing agent and precipitator. Black-Right-Pointing-Pointer Hydrothermal treatment enables growth of lamellar {gamma}-AlOOH architectures. Black-Right-Pointing-Pointer Lamellar {gamma}-AlOOH architectures were demonstrated to exhibit high BET surface area and excellent adsorptive capacity. Black-Right-Pointing-Pointer HCN in contaminated water and cigarette smoke can be effectively removed by the prepared lamellar {gamma}-AlOOH superstructures.

36 MATERIALS SCIENCE↗

Effects of high magnetic field on the evolutions of constituent phases in 7085 aluminum alloy during homogenization

The evolutions of coarse constituent phases in homogenized 7085 aluminum alloy at different conditions with or without the application of 12 T high magnetic field were examined by using differential scanning calorimetry, scanning electronic microscope, energy dispersive spectroscopy and X-ray diffraction. It is found that the main constituent phases including quaternary phase T(AlZnMgCu), Al{sub 7}Cu{sub 2}Fe, and AlTiCuFeSi are present in as-cast 7085 alloy. During homogenization, {alpha} + T eutectics become discontinuous and spheroidized, and Al{sub 2}CuMg phase nucleates and grows along {alpha} + T eutectics. High magnetic field significantly accelerates the melting of quaternary phase T and Al{sub 2}CuMg phase. When the alloy homogenized at 460 Degree-Sign C/10 h + 480 Degree-Sign C/8 h with 12 T magnetic field, the least amount of constituent phases is obtained. - Highlights: Black-Right-Pointing-Pointer Most of published reports of magnetic field are focused on ferrous alloys. Black-Right-Pointing-Pointer Effect of magnetic field on microstructure of 7085 during homogenization is studied. Black-Right-Pointing-Pointer Magnetic field accelerates the melting of AlZnMgCu and S phase.

36 MATERIALS SCIENCE↗

Investigation of thermal, mechanical and magnetic behaviors of the Cu-11%Al alloy with Ag and Mn additions

The investigation of thermal, mechanical and magnetic behaviors of the Cu-11%Al, Cu-11%Al-3%Ag, Cu-11%Al-10%Mn and Cu-11%Al-10%Mn-3%Ag alloys was made using microhardness measurements, differential scanning calorimetry, X-ray diffractometry, scanning electron microscopy, energy dispersion X-ray spectroscopy and magnetic moment change with applied field measurement. The results indicated that the Mn addition changes the phase stability range, the microhardness values and makes undetectable the eutectoid reaction in annealed Cu-11%Al and Cu-11%Al-3%Ag alloys while the presence of Ag does not modify the phase transformation sequence neither microhardness values of the annealed Cu-11%Al and Cu-11%Al-10%Mn alloys, but it increases the magnetic moment of this latter at about 2.7 times and decreases the rates of eutectoid and peritectoid reactions of the former. - Highlights: Black-Right-Pointing-Pointer The microstructure of Cu-Al alloy is modified in the Ag presence. Black-Right-Pointing-Pointer ({alpha} + {gamma}) phase is stabilized down to room temperature when Ag is added to Cu-Al alloy. Black-Right-Pointing-Pointer Ag-rich phase modifies the magnetic characteristics of Cu-Al-Mn alloy.

36 MATERIALS SCIENCE↗

Characterization of a Messer – The late-Medieval single-edged sword of Central Europe

Metallurgical characterization of a sword blade fragments dating from the second half of the 15th century found in central Slovenia was performed in order to determine its chemical composition, microstructure, microhardness, and to obtain insight into the methods of manufacture of a late-medieval Messer sword. As the artefact was broken, examinations were limited to six very small fragments that were allowed to be removed from the cutting edge, core and the back of the blade. Light optical microscopy, scanning electron microscopy, energy dispersive X-ray spectroscopy, energy dispersive X-ray fluorescence spectrometry, differential scanning calorimetry, thermodynamics approach and Vickers micro-hardness tests were employed to analyze the microstructure and mechanical properties. The results show that the sword was manufactured from a single wrought iron billet. The surface of the sword was carburized. No evidence of quenching was found. The ferritic microstructure is concentrated in the core, and the pearlitic in the outer layer of the blade. All metal fragments contained non-metallic inclusions that were derived mostly from slag and some from hammer scale. - Highlights: • A metallurgical characterization of a medieval sword blade has been performed. • The carbon content decreased from the surface to the core of the blade. • The dominant microstructure in the outer layer is pearlite and in the core is ferrite. • The presence of lump shaped and elongated non-metallic inclusions was observed. • The sword was manufactured from a single wrought iron billet.

36 MATERIALS SCIENCE↗

Properties, characterization, and decay of sticky rice–lime mortars from the Wugang Ming dynasty city wall (China)

Urgent restoration of the Wugang Ming dynasty city wall brings about the need for a study of the formulation and properties of mortars. In the present paper, mortar samples from the Wugang Ming dynasty city wall were characterized in a combination of sheet polarized light optical microscopy, scanning electron microscopy with X-ray energy dispersive spectrometer, thermogravimetric/differential scanning calorimetry, X-ray powder diffraction, Fourier transform infrared spectroscopy, and inductively coupled plasma emission spectroscopy. Results show that mortars are mainly built up from inorganic calcium carbonate based organic–inorganic hybrid material with a small amount of sticky rice, which plays a crucial role in forming dense and compact microstructure of mortars and effectively hindering penetration of water and air into mortars. Analysis of decayed products shows that the detrimental soluble salts originates from ambient environment. - Highlights: • Mortars used in the Wugang city wall are a calcium carbonate-sticky rice hybrid bonding material. • Carbonation processing is extremely slow due to dense and compact microstructure of mortars. • Decying of mortars results from the appearance of soluble salt from ambient environment.

36 MATERIALS SCIENCE↗

Dual-phase glassy/nanoscale icosahedral phase materials in Cu–Zr–Ti–Pd system alloys

The present work is devoted to an investigation of the formation kinetics, stability and homogeneity area of the nanoscale icosahedral phase formed on heating in the dual-phase glassy/quasicrystalline phase Cu–Zr–Ti–Pd alloys. The data obtained indicate that the Cu–Zr–Ti–Pd icosahedral phase is not a Cu-rich part of the compositional homogeneity area of the Zr–Cu–Pd one. Moreover, Ti, as well as Pd, is found to be an important element stabilizing quasicrystalline phase in the Cu–Zr–Ti–Pd alloys. The formation criteria for Cu- and Zr/Hf-based icosahedral phases are discussed based on the quasilattice constant to average atomic diameter ratio. Deviation from a certain ratio leads to destabilization of the icosahedral phase. By using the isothermal calorimetry traces transformation kinetics above and below the glass-transition region was analyzed. Some difference in the transformation kinetics above and below the glass-transition region allows us to suggest that possible structure changes occur upon glass-transition. - Highlights: • Formation kinetics, stability and homogeneity area of nanoscale icosahedral phase • Cu–Zr–Ti–Pd icosahedral phase is not a Cu-rich part of Zr–Cu–Pd one. • Ti, as well as Pd, is an important element stabilizing quasicrystalline phase. • Difference in transformation kinetics above and below glass-transition region.

36 MATERIALS SCIENCE↗

Development of nano-structured duplex and ferritic stainless steels by pulverisette planetary milling followed by pressureless sintering

Nano-structured duplex and ferritic stainless steel powders are prepared by planetary milling of elemental Fe, Cr and Ni powder for 40 h and then consolidated by conventional pressureless sintering. The progress of milling and the continuous refinement of stainless steel powders have been confirmed by means of X-ray diffraction and scanning electron microscopy. Activation energy for the formation of duplex and ferritic stainless steels is calculated by Kissinger method using differential scanning calorimetry and is found to be 159.24 and 90.17 KJ/mol respectively. Both duplex and ferritic stainless steel powders are consolidated at 1000, 1200 and 1400 °C in argon atmosphere to study microstructure, density and hardness. Maximum sintered density of 90% and Vickers microhardness of 550 HV are achieved for duplex stainless steel sintered at 1400 °C for 1 h. Similarly, 92% sintered density and 263 HV microhardness are achieved for ferritic stainless steel sintered at 1400 °C. - Highlights: • Synthesized duplex and ferritic stainless steels by pulverisette planetary milling • Calculated activation energy for the formation of duplex and ferritic stainless steels • Studied the effect of sintering temperature on density, hardness and microstructure • Duplex stainless steel exhibits 90% sintered density and microhardness of 550 HV. • Ferritic stainless steel shows 92% sintered density and 263 HV microhardness.

36 MATERIALS SCIENCE↗

TEM and XPS studies on the faceted nanocrystals of Ce{sub 0.8}Zr{sub 0.2}O{sub 2}

Faceted nanocrystals of Ce{sub 0.8}Zr{sub 0.2}O{sub 2} synthesised by co-precipitation method were characterised by X-ray diffraction, high-resolution transmission electron microscopy, thermogravimetry–differential scanning calorimetry and X-ray photoelectron spectroscopy techniques. The nanocrystals were highly faceted and exhibited a cubic phase. X-ray photoelectron spectroscopy analyses confirmed the presence of vacancy related defects and revealed the presence of ~ 22% of Ce{sup 3} {sup +} in the nanopowders. High-resolution transmission electron microscopy results confirmed that the nanocrystal sizes are around 31 ± 5 nm and the obtained hexagonal cross-section shape is bound by hexagonal (111) and square (100) facets. The shape-controlled nanocrystals were synthesised without using any surfactants or complexing agents and retained their morphology beyond 800 °C. This is a simple and easy method for producing shape-controlled Ce{sub 0.8}Zr{sub 0.2}O{sub 2} nanoparticles which can be used for catalytic conversion and other related advanced technological areas. - Graphical abstract: Display Omitted - Highlights: • Synthesis of Ce{sub 0.8}Zr{sub 0.2}O{sub 2} faceted nanocrystal of hexagonal morphology. • Nanopowders synthesised without any surfactant; retained morphology beyond 800 °C. • XPS analyses confirm the potential of these powders for catalytic applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Through-thickness recrystallization characteristics of a laminated AA3xxx–AA6xxx aluminum alloy system

The through-thickness annealing behavior of a laminated AA3xxx–AA6xxx alloy system at 300 °C has been studied by scanning electron microscopy, electron backscatter diffraction analysis, electron probe micro-analysis, differential scanning calorimetry, and hardness measurement. Results show that the recrystallization process starts at the interface region between the AA3xxx (clad) and AA6xxx (core) layers. Subsequently, the recrystallization process front progresses into the core layer, while the clad layer is the last region to recrystallize. It is also found that precipitation precedes recrystallization in the entire laminate at the investigated temperature. The preferential onset of recrystallization at the interface region is attributed to the net driving pressure being the highest in this region. The factors that lead to such enhanced net driving pressure are (a) deformation incompatibility between the two alloy layers, (b) lower solute content of the interface, which also leads to lower volume fraction of precipitates, and (c) an accelerated rate of precipitate coarsening due to the presence of a higher density of dislocations. The gradual progress of recrystallization from the interface towards the core layer is dictated by precipitate coarsening and the dependence of its rate on the density of deformation-induced dislocations. The lower driving pressure due to lower work hardening capacity, high solute drag pressure due to Mn, and additional Zener drag from precipitates that form due to solute redistribution during annealing explain the late initiation of recrystallization in the clad layer. - Highlights: • The through-thickness recrystallization of a laminated system is investigated. • The early onset of recrystallization at the interface is discussed. • The effects of precipitation and coarsening on recrystallization are analyzed.

36 MATERIALS SCIENCE↗