Advanced cast aluminum alloys for automotive engine application with superior high-temperature properties

A high fatigue strength aluminum alloy comprises in weight percent copper 3.0-3.5%, iron 0-1.3%, magnesium 0.24-0.35%, manganese 0-0.8%, silicon 6.5-12.0%, strontium 0-0.025%, titanium 0.05-0.2%, vanadium 0.20-0.35%, zinc 0-3.0%, zirconium 0.2-0.4%, a maximum of 0.5% other elements and balance aluminum plus impurities. The alloy defines a microstructure having an aluminum matrix with the Zr and the V in solid solution after solidification. The matrix has solid solution Zr of at least 0.16% after heat treatment and solid solution V of at least 0.20% after heat treatment, and both Cu and Mg are dissolved into the aluminum matrix during the heat treatment and subsequently precipitated during the heat treatment. A process for heat treating an Al—Si—Cu—Mg—Fe—Zn—Mn—Sr-TMs alloy comprises heat treating the alloy to produce a microstructure having a matrix with Zr and V in solid solution after solidification.

36 MATERIALS SCIENCE↗

Preparation, crystal structure and photoluminescence of garnet-type calcium tin titanium aluminates

Colorless and transparent single crystals of Ca{sub 3}Sn{sub 2.2}Ti{sub 0.8}Al{sub 2}O{sub 12}, which emit blue-white light under ultraviolet light, were prepared by heating a mixture of oxides and calcium carbonate with a calcium and aluminum-rich composition at 1500 {sup o}C. Single crystal X-ray diffraction revealed that the crystal structure is the garnet-type with a cubic cell parameter (a=12.5309(3) A) and the space group, Ia 3-bar d (R1=0.0277, wR2=0.0663, and S=1.367 for all data). The structural formula is presented as Ca{sub 3}[Sn{sub 0.96}Ti{sub 0.04}]{sub octa}[Al{sub 0.67}Ti{sub 0.24}Sn{sub 0.09}]{sub tetra}O{sub 12}. Polycrystalline solid solutions of Ca{sub 3}Sn{sub 3-x}Ti{sub x}Al{sub 2}O{sub 12} were prepared by solid state reaction in air at 1370 {sup o}C with nominal titanium contents from x=0.6 to 1.4. The refined unit cell parameter decreased with increasing x. A broad blue-white emission with a peak wavelength of 465 nm was observed for the solid solutions at room temperature. -- Graphical abstract: Garnet-type solid solutions of Ca{sub 3}Sn{sub 3-x}Ti{sub x}Al{sub 2}O{sub 12} (x=0.6-1.4) were prepared. Sn{sup 4+} and Ti{sup 4+} partially occupy both tetrahedral and octahedral sites. The solid solutions showed a broad emission band peaking at 465 nm under UV excitation. Display Omitted Research highlights: {yields} New garnet-type solid solutions were found in the CaO-Al{sub 2}O{sub 3}-TiO{sub 2}-SnO{sub 2} system. {yields} Single crystals of Ca{sub 3}Sn{sub 2.2}Ti{sub 0.8}Al{sub 2}O{sub 12} were obtained by the self-flux method. {yields} Solid solutions with nominal compositions Ca{sub 3}Sn{sub 3-x}Ti{sub x}Al{sub 2}O{sub 12} (x=0.6-1.4) were prepared by solid state reaction at 1370 {sup o}C. {yields} Sn{sup 4+} and Ti{sup 4+} partially occupy both tetrahedral and octahedral sites, respectively, in the garnet-type structure. {yields} Ca{sub 3}Sn{sub 3-x}Ti{sub x}Al{sub 2}O{sub 12} solid solutions emitted blue-white light with a peak wavelength at 465 nm under UV irradiation.

36 MATERIALS SCIENCE↗

Synthesis and properties of In{sub x}Al{sub y}Ga{sub 1–x–y}P{sub z}As{sub 1–z}/GaAs heterostructures

Phase equilibria in the In–Al–Ga–P–As system have been analyzed in terms of a simple solution model. We have calculated the stability limits of InAlGaPAs solid solutions on GaAs substrates in the temperature range 937–1223 K. The addition of indium to AlGaPAs solid solutions leads to a slight decrease in growth rate under diffusion control and a considerable increase under kinetic control. Moreover, the addition of indium to AlGaPAs solid solutions has been shown to reduce the full width at half maximum of their X-ray rocking curves and photoluminescence spectra and increase the photoluminescence intensity. Increasing the indium concentration in In{sub x}Al{sub y}Ga{sub 1–x–y}P{sub z}As{sub 1–z} solid solutions to x > 0.3 extends their stability region, increases their band gap, and reduces the composition region of lattice-matched In{sub x}Al{sub y}Ga{sub 1–x–y}P{sub z}As{sub 1–z}/GaAs heterostructures, but these become thermal expansion-matched. With increasing indium concentration in the solid solutions, the distribution coefficients of P and As decrease, whereas those of Al and In increase.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Organic-Mineral Interfacial Chemistry Drives Heterogeneous Nucleation of Sr-Rich (Bax, Sr1-x)SO4 from Undersaturated Solution

Sr-bearing marine barite [(Bax, Sr1-x)SO4] cycling has been widely used to reconstruct geochemical evolutions of paleoenvironments. However, an understanding of barite precipitation in the ocean, which is globally undersaturated with respect to barite, is missing. Moreover, the reason for the occurrence of higher Sr content in marine barites than expected for classical crystal growth processes remains unknown. Field data analyses suggested that organic molecules may regulate the formation and composition of marine barites; however, the specific organic–mineral interactions are unclear. Using in situ grazing incidence small-angle X-ray scattering (GISAXS), size and total volume evolutions of barite precipitates on organic films were characterized. The results show that barite forms on organic films from undersaturated solutions. Moreover, from a single supersaturated solution with respect to barite, Sr-rich barite nanoparticles formed on organics, while micrometer-size Sr-poor barites formed in bulk solutions. Ion adsorption experiments showed that organic films can enrich cation concentrations in the adjacent solution, thus increasing the local supersaturation and promoting barite nucleation on organic films, even when the bulk solution was undersaturated. The Sr enrichment in barites formed on organic films was found to be controlled by solid-solution nucleation rates; instead, the Sr-poor barite formation in bulk solution was found to be controlled by solid-solution growth rates. This study provides a mechanistic explanation for Sr-rich marine barite formation and offers insights for understanding and controlling the compositions of solid solutions by separately tuning their nucleation and growth rates via the unique chemistry of solution–organic interfaces.

Deng, Ning↗

In Situ XRD Studies of ZnO/GaN Mixtures at High Pressure and High Temperature: Synthesis of Zn-Rich (Ga1-xZnx)(N1-xOx) Photocatalysts

The high-pressure, high-temperature conditions for the synthesis of Zn-rich (Ga{sub 1-x}Zn{sub x})(N{sub 1-x}O{sub x}) solid solutions from mixtures of ZnO/GaN were explored using synchrotron-based in situ time-resolved X-ray diffraction (XRD). Following a new synthetic path, (Ga{sub 1-x}Zn{sub x})(N{sub 1-x}O{sub x}) solid solutions with a Zn content up to 75% were prepared for the first time. The structures of the (Ga{sub 1-x}Zn{sub x})(N{sub 1-x}O{sub x}) solid solutions were characterized by XRD and X-ray absorption fine structure (XAFS) analyses and were in excellent agreement with the predictions of density functional calculations. These materials adopt a wurtzite crystal structure with metal-N or metal-O bond distances in the range of 1.95-1.98 {angstrom}. Although the (Ga{sub 1-x}Zn{sub x})(N{sub 1-x}O{sub x}) solid solutions seem to be stable over the full range of compositions, no ideal solid solution formation was observed. In all cases, the lattice parameters were larger than those of ideal solid solutions. The variation of the lattice parameter c showed an upward double bowing curve, as was predicted by theoretical calculations. Also, no ideal behavior was observed in the electronic properties of the (Ga{sub 1-x}Zn{sub x})(N{sub 1-x}O{sub x}) solid solutions. X-ray absorption spectra at the Zn and Ga K-edges of the (Ga{sub 1-x}Zn{sub x})(N{sub 1-x}O{sub x}) systems showed significant electronic perturbations with respect to ZnO and GaN. The synthesized (Ga{sub 1-x}Zn{sub x})(N{sub 1-x}O{sub x}) solid solution with a Zn content of 50% displayed the ability to absorb visible light well above 500 nm. This material has a great potential for splitting water under visible light irradiation. The availability of (Ga{sub 1-x}Zn{sub x})(N{sub 1-x}O{sub x}) solid solutions with a high Zn content opens the door to fully explore the application of these materials in photocatalysis.

36 MATERIALS SCIENCE↗

In Situ XRD Studies of ZnO/GaN Mixtures at High Pressure and High Temperature: Synthesis of Zn-Rich (Ga1-xZnx)(N1-xOx) Photocatalysts

The high-pressure, high-temperature conditions for the synthesis of Zn-rich (Ga{sub 1-x}Zn{sub x})(N{sub 1-x}O{sub x}) solid solutions from mixtures of ZnO/GaN were explored using synchrotron-based in situ time-resolved X-ray diffraction (XRD). Following a new synthetic path, (Ga{sub 1-x}Zn{sub x})(N{sub 1-x}O{sub x}) solid solutions with a Zn content up to {approx}75% were prepared for the first time. The structures of the (Ga{sub 1-x}Zn{sub x})(N{sub 1-x}O{sub x}) solid solutions were characterized by XRD and X-ray absorption fine structure (XAFS) analyses and were in excellent agreement with the predictions of density functional calculations. These materials adopt a wurtzite crystal structure with metal-N or metal-O bond distances in the range of 1.95-1.98 {angstrom}. Although the (Ga{sub 1-x}Zn{sub x})(N{sub 1-x}O{sub x}) solid solutions seem to be stable over the full range of compositions, no ideal solid solution formation was observed. In all cases, the lattice parameters were larger than those of ideal solid solutions. The variation of the lattice parameter c showed an upward double bowing curve, as was predicted by theoretical calculations. Also, no ideal behavior was observed in the electronic properties of the (Ga{sub 1-x}Zn{sub x})(N{sub 1-x}O{sub x}) solid solutions. X-ray absorption spectra at the Zn and Ga K-edges of the (Ga{sub 1-x}Zn{sub x})(N{sub 1-x}O{sub x}) systems showed significant electronic perturbations with respect to ZnO and GaN. The synthesized (Ga{sub 1-x}Zn{sub x})(N{sub 1-x}O{sub x}) solid solution with a Zn content of 50% displayed the ability to absorb visible light well above 500 nm. This material has a great potential for splitting water under visible light irradiation. The availability of (Ga{sub 1-x}Zn{sub x})(N{sub 1-x}O{sub x}) solid solutions with a high Zn content opens the door to fully explore the application of these materials in photocatalysis.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A DFT+U study of cerium solubility in La2Zr2O7

Density functional theory plus Hubbard U correction is employed to study the solubility of cerium in La2Zr2O7. The results show that La2Zr2O7 and Ce2Zr2O7 form a solid solution over the whole range of cerium content. The solubility of Ce in La2Zr2O7 can be partially attributed to the similar ionic radii of La3+ and Ce3+. Electronic structures of the La2-yCeyZr2O7 solid solution have been analyzed. The Ce 4f states are found to be partially occupied, and Ce in the La2-yCeyZr2O7 solid solution exhibits a reduced charge state.

36 MATERIALS SCIENCE↗

Mixed conductivity, structural and microstructural characterization of titania-doped yttria tetragonal zirconia polycrystalline/titania-doped yttria stabilized zirconia composite anode matrices

Taking advantage of the fact that TiO{sub 2} additions to 8YSZ cause not only the formation of a titania-doped YSZ solid solution but also a titania-doped YTZP solid solution, composite materials based on both solutions were prepared by solid state reaction. In particular, additions of 15 mol% of TiO{sub 2} give rise to composite materials constituted by 0.51 mol fraction titania-doped yttria tetragonal zirconia polycrystalline and 0.49 mol fraction titania-doped yttria stabilized zirconia (0.51TiYTZP/0.49TiYSZ). Furthermore, Y{sub 2}(Ti{sub 1-y}Zr{sub y}){sub 2}O{sub 7} pyrochlore is present as an impurity phase with y close to 1, according to FT-Raman results. Lower and higher additions of titania than that of 15 mol%, i.e., x=0, 5, 10, 20, 25 and 30 mol% were considered to study the evolution of 8YSZ phase as a function of the TiO{sub 2} content. Furthermore, zirconium titanate phase (ZrTiO{sub 4}) is detected when the titania content is equal or higher than 20 mol% and this phase admits Y{sub 2}O{sub 3} in solid solution according to FE-SEM-EDX. The 0.51TiYTZP/0.49TiYSZ duplex material was selected in this study to establish the mechanism of its electronic conduction under low oxygen partial pressures. In the pO{sub 2} range from 0.21 to 10{sup -7.5} atm. the conductivity is predominantly ionic and constant over the range and its value is 0.01 S/cm. The ionic plus electronic conductivity is 0.02 S/cm at 1000 {sup o}C and 10{sup -12.3} atm. Furthermore, the onset of electronic conductivity under reducing conditions exhibits a -1/4 pO{sub 2} dependence. Therefore, it is concluded that the n-type electronic conduction in the duplex material can be due to a small polaron-hopping between Ti{sup 3+} and Ti{sup 4+}. -- Graphical abstract: FE-SEM micrograph of a polished and thermal etched surface of a Ti-doped YTZP/Ti-doped YSZ composite material. Display Omitted Research highlights: {yields} Ti-doped YTZP/Ti-doped YSZ composite materials are mixed conductors under low partial pressures. {yields} From 5 mol% of TiO{sub 2}, Y{sub 2}(Ti{sub 1-y},Zr{sub y}){sub 2}O{sub 7} pyrochlore is present as a minor phase, being y close to 1 according to FT-Raman studies. {yields} The onset of the electronic conductivity under reducing conditions exhibit a -1/4 pO{sub 2} dependence. The n-type electronic conduction is due to a small polaron-hopping between Ti{sup 3+} and Ti{sup 4+}.

36 MATERIALS SCIENCE↗

Investigation of the phase relations in the U-Al-Ge ternary system: Influence of the Al/Ge substitution on the properties of the intermediate phases

The phase relations within the U-Al-Ge ternary system were studied for two isothermal sections, at 673 K for the whole Gibbs triangle and at 1173 K for the concentration range 25–100 at% U. The identification of the phases, their composition ranges and stability were determined by x-ray powder diffraction, scanning electron microscopy coupled to energy dispersive spectroscopy and differential thermal analysis. The tie-lines and the solubility domains were determined for the U-Ge and U-Al binaries, the UAl{sub 3}-UGe{sub 3} solid-solution and for the unique ternary intermediate phase U{sub 3}Al{sub 2−x}Ge{sub 3+x}. The experimental isopleth section of the pseudo-binary UAl{sub 3}-UGe{sub 3} reveals an isomorphous solid solution based on the Cu{sub 3}Au-type below the solidus. The U{sub 3}Al{sub 2−x}Ge{sub 3+x} solid solution extends for −0.1≤x≤1.35 and −0.2≤x≤1.5 at 673 K and 1173 K respectively. It crystallizes in the I-centered tetragonal symmetry. The reciprocal lattice of several compositions of the U{sub 3}Al{sub 2−x}Ge{sub 3+x} solid solution was examined by electron diffraction at room temperature, revealing the presence of a c-glide plane. Their crystal structure was refined by single crystal x-ray diffraction suggesting an isomorphous solid solution best described with the non-centrosymmetric space group I4cm in the paramagnetic domain. The magnetic measurements confirm the ferromagnetic ordering of the solid solution U{sub 3}Al{sub 2−x}Ge{sub 3+x} with an increase of Tc with the Al content. The thermal variation of the specific heat bear out the magnetic transitions with some delocalized character of the uranium 5f electrons. - Graphical abstract: The phase relations within the U-Al-Ge ternary system were experimentally assessed for two isothermal sections, at 673 K for the whole Gibbs triangle and at 1173 K for the concentration range 25–100 at% U. A complete UAl{sub 3}-UGe{sub 3} solid-solution based on the Cu{sub 3}Au-type forms below the solidus. A unique ternary phase showing a large homogeneity domain, U{sub 3}Al{sub 2−x}Ge{sub 3+x} for −0.1≤x≤1.35 and −0.2≤x≤1.5 at 673 K and 1173 K respectively has been evidenced. It is best described with the non-centrosymmetric space group I4cm above room temperature. A linear increase of the ferromagnetic ordering is observed with the Al content. - Highlights: • Isothermal sections of the U-Al-Ge system were investigated for 673 K and 1173 K. • An isomorphous solid-solution UAl{sub 3}-UGe{sub 3} forms for the whole composition range. • U{sub 3}Al{sub 2−x}Ge{sub 3+x} the unique ternary phase to form exists for a large homogeneity domain. • U{sub 3}Al{sub 2−x}Ge{sub 3+x} is best described in I4cm space group above room temperature. • The ferromagnetic transition of U{sub 3}Al{sub 2−x}Ge{sub 3+x} linearly increases with the Al content.

36 MATERIALS SCIENCE↗

Magnetism and magnetocaloric effect in multicomponent Laves-phase compounds: Study and comparative analysis

This paper presents a review and results of comparative study of the influence of Gd on some physical properties of (R{sub 0.9}R′{sub 0.1}){sub 1−x}Gd{sub x}Co{sub 2} solid solutions with R=Dy, Ho and R′=Er, Ho and x varied from 0.05 to 0.15. Powder X-ray diffraction analysis performed at room temperature revealed that all studied solid solutions solidify with the formation of a Laves-phase MgCu{sub 2}-type structure (space group Fd−3m). The magnetization behavior and the magnetic transition are analyzed in terms of the Landau theory. The studies of magnetic properties and heat capacity showed that a relatively small Gd addition significantly increases T{sub C} of the compounds. The maximum percentage increase in T{sub C}, namely, ∼43% was observed for (Ho{sub 0.9}Er{sub 0.1}){sub 1−x}Gd{sub x}Co{sub 2}. However, the highest temperature was noted for the (Dy{sub 0.9}Ho{sub 0.1}){sub 0.85}Gd{sub 0.15}Co{sub 2} solid solution; it is T{sub C}=183.4 K. Below the ordering temperature, all samples are ferrimagnetically ordered; at high temperatures, they are Curie–Weiss paramagnets. Moreover, a small Gd addition eliminates the field-induced magnetic transition near T{sub C} and, as consequence, transforms the nature of magnetic transition from the first- to second-order. The magnetocaloric effect has been estimated in terms of both isothermal magnetic entropy and adiabatic temperature changes. The highest adiabatic temperature change ΔT{sub ad}=3 K and highest isothermal entropy change ΔS{sub mag}=12.1 J/kg K were observed for (Ho{sub 0.9}Er{sub 0.1}){sub 0.95}Gd{sub 0.05}Co{sub 2} at ∼90 K in magnetic fields of 2 T and 3 T, respectively. A decrease in the entropy change has been observed with increasing Gd content in all studied samples. The smallest values of ΔS{sub mag} were observed for the (Dy{sub 0.9}Ho{sub 0.1}){sub 1−x}Gd{sub x}Co{sub 2} solid solutions. Under an external field change of from 0 to 3 T, the maximum entropy change for (Dy{sub 0.9}Ho{sub 0.1}){sub 1−x}Gd{sub x}Co{sub 2} compounds decreases from 6.9 at x=0.05–4.3 J/kg K at x=0.15. The refrigerant capacity for all solid solutions (with 0.05≤x≤0.15) is reported. The effect of increasing Gd content in the solid solutions on their magnetic and magnetocaloric properties is discussed. - Graphical abstract: Temperature dependencies of ΔT{sub ad} induced by µ{sub 0}H=1 and 2 T in (a) (Ho{sub 0.9}Er{sub 0.1}){sub 1−x}Gd{sub x}Co{sub 2} and (b) (Dy{sub 0.9}Er{sub 0.1}){sub 1−x}Gd{sub x}Co{sub 2} solid solutions. Display Omitted.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Single- and Double-Site Substitutions in Mixed-Metal Oxides: Adjusting the Band Edges Toward the Water Redox Couples

New mixed-metal oxide solid solutions, i.e., the single-metal substituted Na 2 Ta 4–y Nb y O 11 (0 ≤ y ≤ 4) and the double-metal substituted Na 2–2x Sn x Ta 4–y Nb y O 11 (0 ≤ y ≤ 4; 0 ≤ x ≤ 0.35), were investigated and used to probe the impact of composition on their crystalline structures, optical band gaps, band energies, and photocatalytic properties. The Na 2 Ta 4 O 11 (y = 1) phase was prepared by flux-mediated synthesis, while the members of the Na 2 Ta 4–y Nb y O 11 solid solution (1 ≤ y ≤ 4) were prepared by traditional high-temperature reactions. The Sn(II)-containing Na 2–2x Sn x Ta 4–y Nb y O 11 (0 ≤ y ≤ 4) solid solutions were prepared by flux-mediated ion-exchange reactions of the Na 2 Ta 4–y Nb y O 11 solid solutions within a SnCl 2 flux. The crystalline structures of both solid solutions are based on the parent Na 2 B 4 O 11 (B = Nb, Ta) phases and consist of layers of edge-shared BO 7 pentagonal bipyramids that alternate with layers of isolated BO 6 octahedra surrounded by Na(I) cations. Rietveld refinements of the Na 2 Ta 4–y Nb y O 11 solid solution showed that Nb(V) cations were disordered equally over both the BO 7 and BO 6 atomic sites, with a symmetry-lowering distortion from R$\overline{3c}$ to C2/c occurring at ~67–75% Nb (y = ~2.7–3.0). A red-shift in the optical band gaps from ~4.3 to ~3.6 eV is observed owing to a new conduction band edge that arises from the introduction of the lower-energy Nb 4d-orbitals. Reactions of these phases within a SnCl 2 flux yielded the new Na 2–2x Sn x Ta 4–y Nb y O 11 solid solution with Sn-content varying from ~11% to ~21%. However, significant red-shifting of the band gap is found with increasing Nb-content, down to ~2.3 eV for Na 1.4 Sn 0.3 Nb 4 O 11 , because of the higher energy valence band edge upon incorporation of Sn(II) into the structure. Aqueous suspensions of the particles irradiated at ultraviolet–visible energies yielded the highest photocatalytic hydrogen production rates for Na 1.3 Sn 0.35 Ta 1.2 Nb 2.8 O 11 (~124 μmol H 2 ·g –1 ·h –1 ) and Na 1.4 Sn 0.3 Ta 3 NbO 11 (~105 μmol H 2 ·g –1 ·h –1 ), i.e., for the compositions with the highest Sn(II)-content. Further, polycrystalline films show n-type anodic photocurrents under ultraviolet–visible light irradiation. These results show that the valence and conduction band energies can be raised and lowered, respectively, using single-metal and double-metal substituted solid solutions. Furthermore, a novel approach is revealed for achieving smaller visible-light bandgap sizes and a closer bracketing of the water redox couples in order to drive total water splitting reactions that are critical for efficient solar energy conversion.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Study of phase relationships in the Sr{sub 3}(PO{sub 4}){sub 2}–CePO{sub 4} system. Phase diagram and thermal characteristics of phases

A diagram representing phase relationships in the Sr{sub 3}(PO{sub 4}){sub 2}–CePO{sub 4} phosphate system has been developed on the basis of results obtained by thermal analysis (DTA/DSC/TGA) and X-ray diffraction (XRD) methods. One intermediate compound with the formula Sr{sub 3}Ce(PO{sub 4}){sub 3} occurs in the Sr{sub 3}(PO{sub 4}){sub 2}–CePO{sub 4} system at temperatures exceeding 1045 °C. The compound has a eulytite structure with the following structural parameters: a=b=c=10.1655(8) Å, α=β=γ=90.00°, V=1050.46(6) Å{sup 3}. It's melting point exceeds 1950 °C. A limited solid solution exists in the system, which possesses the structure of a low-temperature form of Sr{sub 3}(PO{sub 4}){sub 2}. At 1000 °C the maximal concentration of CePO{sub 4} in the solid solution is below 20 mol%. The solid solution phase field narrows with increased temperature. There is a eutectic point in the (Sr{sub 3}(PO{sub 4}){sub 2}+Sr{sub 3}Ce(PO{sub 4}){sub 3}) phase field at 1765 °C and 15 mol% of CePO{sub 4}. The melting temperature of Sr{sub 3}(PO{sub 4}){sub 2} is 1882±15 °C. - Graphical abstract: The phase diagram of Sr{sub 3}(PO{sub 4}){sub 2}–CePO{sub 4} system showing the stability ranges of limited solid solution and Sr{sub 3}Ce(PO{sub 4}){sub 3} phases. - Highlights: • Sr{sub 3}(PO{sub 4}){sub 2} melts at 1882 °C. • Phase diagram of Sr{sub 3}(PO{sub 4}){sub 2}–CePO{sub 4} system has been proposed. • Limited solid solution of CePO{sub 4} in Sr{sub 3}(PO{sub 4}){sub 2} forms in the system. • The Sr{sub 3}Ce(PO{sub 4}){sub 2} phosphate is stable at temperatures above 1045 °C.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Molecularly Mixed Composite Membranes: Challenges and Opportunities

The fabrication of porous molecules, such as metal–organic polyhedra (MOPs), porous organic cages (POCs) and others, has given rise to the potential for creating “solid solutions” of molecular fillers and polymers. Such solid solutions circumvent longstanding interface issues associated with mixed matrix membranes (MMMs), and are referred to as molecularly mixed composite membranes (MMCMs) to distinguish them from traditional two-phase MMMs. Early investigations of MMCMs highlight the advantages of solid solutions over MMMs, including dispersion of the filler, anti-plasticization of the polymer network, and removal of deleterious interfacial issues. However, the exact microscopic structure as well as the transport modality in this new class of membrane are not well understood. Moreover, there are clear engineering challenges that need to be addressed for MMCMs to transition into the field. Finally in this Minireview, the authors outline several scientific and technological challenges associated with the aforementioned questions and their suggestions to tackle them.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Phase equilibria, crystal structure and oxygen content of intermediate phases in the Y–Ba–Co–O system

The phase equilibria in the Y–Ba–Co–O system were systematically studied at 1373 K in air. The intermediate phases formed in the Y–Ba–Co–O system at 1373 K in air were: YBaCo₂O 5+δ , YBaCo₄O₇ and BaCo 1–y Y y O 3–δ (0.09≤y≤0.42). It was shown that YBaCo₂O 5+δ possesses tetragonal structure with the 3aₚ×3aₚ×2aₚ superstructure (sp. gr. P4/mmm). High-temperature X-ray diffraction analysis of the YBaCo₂O 5+δ in the temperature range from 298 K up to 1073 K under Po₂=0.21 atm has not shown any phase transformations. The value of oxygen content for the YBaCo₂O 5+δ at room temperature was estimated as 5.40 and at 1323 K it was equal to 5.04. Thermal expansion of sample shows a linear characteristics and the average thermal expansion coefficient (TEC) is about 13.8×10⁻⁶, K⁻¹ in the temperature range 298–1273 K. The homogeneity range and crystal structure of the BaCo 1–y Y y O 3–δ (0.09≤y≤0.42) solid solutions were determined by X-ray diffraction of quenched samples. All BaCo 1–y Y y O 3–δ solid solutions were found to have cubic structure (sp. gr. Pm3m). The unit cell parameters were refined using Rietveld full-profile analysis. Oxygen nonstoichiometry of BaCo 1–y Y y O 3–δ solid solutions with 0.1≤y≤0.4 was measured by means of thermogravimetric technique within the temperature range 298–1373 K in air. Thermal expansion of BaCo 1–y Y y O 3–δ (y=0.0; 0.1; 0.2; 0.3) samples was studied within the temperature range 298–1200 K in air. The projection of isothermal–isobaric phase diagram for the Y–Ba–Co–O system to the compositional triangle of metallic components was presented. - Graphical abstract: A projection of isobaric isothermal phase diagram of the Y–Ba–Co–O system to the metallic components triangle (T=1373 K, Po₂=0.21 atm). Highlights: • High-temperature X-ray diffraction analyses of the YBaCo₂O 5+δ in the temperature range 298–1073 K. • The value of oxygen content for the YBaCo₂O 5+δ in the temperature range 298 –1323 K. • The homogeneity range and crystal structure of the BaCo 1–y Y y O 3–δ (0.09≤y≤0.42) solid solutions. • Oxygen nonstoichiometry of BaCo 1–y Y y O 3–δ solid solutions. • The projection of isothermal–isobaric phase diagram for the Y–Ba–Co–O system.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Potential-pH diagrams considering complex oxide solution phases for understanding aqueous corrosion of multi-principal element alloys

The potential-pH diagram, a graphical representation of the thermodynamically predominant reaction products in aqueous corrosion, is originally proposed for the corrosion of pure metals. The original approach only leads to stoichiometric oxides and hydroxides as the oxidation products. However, numerous experiments show that non-stoichiometric oxide scales are prevalent in the aqueous corrosion of alloys. In the present study, a room temperature potential-pH diagram considering oxide solid solutions, as a generalization of the traditional potential-pH diagram with stoichiometric oxides, is constructed for an FCC single-phase multi-principal element alloy (MPEA) based on the CALculation of PHAse Diagram method. The predominant reaction products, the ions in aqueous solution, and the cation distribution in oxides are predicted. The oxide solid solution is stabilized by the mixing free energy (or mixing entropy) and the stabilizing effect becomes more significant as the temperature increases. Consequently, solid solution oxides are stable in large regions of the potential-pH diagram and the mixing free energy mostly affects the equilibrium composition of the stable oxides, while the shape of stable regions for oxides is mostly determined by the structure of the stable oxides. Agreements are found for Ni 2+ , Fe 2+ , and Mn 2+ between the atomic emission spectroelectrochemistry measurements and thermodynamic calculations, while deviations exist for Cr 3+ and Co 2+ possibly due to surface complexation with species such as Cl - and the oxide dissolution. By incorporating the solution models of oxides, the current work presents a general and more accurate way to analyze the reaction products during aqueous corrosion of MPEAs.

Materials Science↗

Microstructural and mechanical characteristics of Ni–Cr thin films

Highlights: • Ni–Cr thin films of varied composition deposited by DC magnetron co-sputtering. • Thin film with Ni–Cr: 80–20 at% composition exhibits most distinct behavior. • The films were tensile tested and exhibited no cracking till the substrate yielding. - Abstract: Ni–Cr alloy thin films have been deposited using magnetron co-sputtering technique at room temperature. Crystal structure was evaluated using GIXRD. Ni–Cr solid solution upto 40 at% of Cr exhibited fcc solid solution of Cr in Ni and beyond that it exhibited bcc solid solution of Ni in Cr. X-ray diffraction analysis shows formation of (1 1 1) fiber texture in fcc and (2 2 0) fiber texture in bcc Ni–Cr thin films. Electron microscopy in both in-plane and transverse direction of the film surface revealed the presence of columnar microstructure for films having Cr upto 40 at%. Mechanical properties of the films are evaluated using nanoindentation. The modulus values increased with increase of Cr at% till the film is fcc. With further increase in Cr at% the modulus values decreased. Ni–Cr film with 20 at% Ni exhibits reduction in modulus and is correlated to the poor crystallization of the film as reflected in XRD analysis. The Ni–Cr thin film with 80 at% Ni and 20 at% Cr exhibited the most distinct columnar structure with highest electrical resistivity, indentation hardness and elastic modulus.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Low-Activation Fe-Cr-V Multicomponent Single-Phase Alloys

A ternary equiatomic and nearly equiatomic alloy composed of the low-activation elements Fe, Cr, and V was designed for potential application as low-activation structural materials for the first wall of fusion reactors. The optimal composition of the multicomponent alloy was determined by minimizing the Gibbs free energy for solid-solution formation. The microstructure, phase stability, and mechanical properties of the equiatomic and optimized Fe-Cr-V alloys were studied. The equiatomic alloy consisted of a body-centered-cubic (BCC) solid-solution phase with a small amount of a face-centered-cubic (FCC) solid-solution phase, whereas the optimized alloy consisted of a single BCC solid-solution phase in the as-cast state. The crystal grains of both alloys were equiaxial. No phase transition was observed in the optimized alloy after homogenization; however, for the equiatomic alloy, the FCC solid-solution phase disappeared and surface relief was observed. The Vickers microhardness and yield strength of the Fe-Cr-V alloys increased after homogenization compared with those of the as-cast alloys.

36 MATERIALS SCIENCE↗