Characteristics and Tribological Behaviors of TiAlN/Cr-Ni Composite Coatings at Elevated Temperatures
A TiAlN/Cr-Ni composite coating was fabricated on H13 hot work mold steel using a cathode ion arc plating and laser cladding. The surface and cross-sectional morphologies, chemical compositions, phases and surface roughness of obtained coating were analyzed using a scanning electron microscope, energy disperse spectroscopy, x-ray diffraction and atomic force microscope, respectively, and the bonding strength was measured using a scratch test. The friction-wear properties of TiAlN/Cr-Ni coating at 400, 500 and 600 °C were investigated using a ball-on-disc wear test. The results show that the TiAlN coating is primarily composed of c-TiN and c-AlN hard phases, and the bonding strength of TiAlN coating with the Cr-Ni coating is 22.15 N. The average coefficients of friction of TiAlN/Cr-Ni coating at 400, 500 and 600 °C are 0.458, 0.318 and 0.449, respectively, and the corresponding wear rates are 0.329 × 10{sup −3}, 0.384 × 10{sup −3} and 0.205 × 10{sup −3} mm{sup 3} N{sup −1} s{sup −1}, respectively, and the wear mechanism includes adhesive wear and oxidation wear.