At least 721 records · Page 40

Molecular relaxations, molecular orientation, and the friction characteristics of polyimide films

The friction characteristics of polyimide films bonded to metallic substrates were studied from 25 to 500 C. These results were interpreted in terms of molecular orientation and thermomechanical data obtained by torsional braid analysis (TBA). A large friction transition was found to occur at 40 + or - 10 C in a dry argon atmosphere (10 ppm H2O). It was postulated that the mechanical stresses of sliding transform or reorder the molecules on the surface into a configuration conducive to easy shear, such as an extended chain. The molecular relaxation which occurs in this temperature region appears to give the molecules the necessary freedom for this reordering process to occur. The effects of velocity, reversibility, and thermal prehistory on the friction properties of polyimide were also studied.

Fusaro, R. L.↗

Friction and wear behavior of graphite fiber reinforced polyimide composites

The friction and wear rate characteristics of 50/50 (weight per cent) graphite fiber-polyimide composites were studied by sliding metallic hemispherically tipped riders against disks made from the composites. Two different polyimides and two different graphite fibers were evaluated. Also studied were such variables as the effect of adding 10 per cent weight additions of powdered (CF-1.1)n, CdI2, or CdO, the effect of moisture in an air atmosphere, the effect of temperature, and the effect of different sliding speeds. In general, wear to the metallic riders was negligible and composite wear increased at a constant rate as a function of number of sliding cycles.

Fusaro, R. L.↗

Combination Thermal Barrier And Wear Coatings For Engines

Thermal-barrier layers covered with self-lubricating surface layers. Zirconia thermal-barrier coat applied to surface of combustion chamber in engine by plasma-arc spraying. Then PS-200 plasma-arc sprayed onto zirconia. Self-lubricating coat prevents sliding contact between thermal barrier and piston ring, effectively preventing both wear and production of additional heat via friction. Other combinations of thermal-barrier and self-lubricating, wear-resistant coating materials used as long as two materials adhere to each other, applied by use of similar or compatible processes, have similar coefficients of thermal expansion, sufficiently strong at high temperatures, and affordable.

Weingart, Mike↗

Multivalent counterions diminish the lubricity of polyelectrolyte brushes

Polyelectrolyte brushes provide wear protection and lubrication in many technical, medical, physiological, and biological applications. Wear resistance and low friction are attributed to counterion osmotic pressure and the hydration layer surrounding the charged polymer segments. However, the presence of multivalent counterions in solution can strongly affect the interchain interactions and structural properties of brush layers. We evaluated the lubrication properties of polystyrene sulfonate brush layers sliding against each other in aqueous solutions containing increasing concentrations of counterions. The presence of multivalent ions (Y 3+ , Ca 2+ , Ba 2+ ), even at minute concentrations, markedly increases the friction forces between brush layers owing to electrostatic bridging and brush collapse. Furthermore, our results suggest that the lubricating properties of polyelectrolyte brushes in multivalent solution are hindered relative to those in monovalent solution.

47 OTHER INSTRUMENTATION↗

Roller Sliding in Wind Turbine Gearbox High-Speed-Shaft Bearings

Failures in gearbox bearings have been a primary source of reliability issues for wind turbine drivetrains, leading to costly downtime and unplanned maintenance. The most common failure mode is attributed to so-called white-etching cracks (WECs). This mode of failure can occur at 5%-20% of the predicted design life and has been observed in many other industries, bearing locations, bearing types, bearing parts, and steel types. The main drivers for the creation of WECs in steel specimens have been identified and verified by material testing. In a full-scale wind turbine gearbox, however, the conditions leading to WECs, the process by which this failure culminates, and the reasons for their apparent prevalence are all still highly debated. In a collaborative project, Flender Corporation, SKF and the National Renewable Energy Laboratory have instrumented a commercial drivetrain, installed it in a wind turbine, and operated the turbine for over a year. In this report, these measurements are used to validate two different modelling approaches for bearing sliding, one analytical dynamic model and one multi-body model. Once validated, these models can then be used to evaluate the roller slip losses or cumulative frictional energy that are each considered as potential driving factors for wind turbine gearbox bearing failures by WEC.

17 WIND ENERGY↗

Electrodeposition and Characterization of Ni-Al{sub 2}O{sub 3} Nanocomposite Coatings on Steel

Monodispersed alumina particles were synthesized by the homogeneous precipitation under reflux boiling. The particles were employed as reinforcement additives in the electrodeposited Ni-Al{sub 2}O{sub 3} composite coatings on steel. The deposited pure Ni and Ni-Al{sub 2}O{sub 3} composite coatings were analyzed by SEM, XRD, and microhardness tester. The wear resistance and friction coefficient of the coated samples were determined by using a ball-on-disk tribometer. Furthermore, XRD analysis showed that coating temperature and the presence of particles in the deposited coatings had a noticeable effect on the preferred orientation of the crystalline faces of the nickel grains. Significant differences were noted in the texture coefficient of the pure Ni and Ni-Al{sub 2}O{sub 3} composite coatings produced at different temperatures. These differences were attributed to the changes in the microstructure of the matrix caused by the embedded Al{sub 2}O{sub 3} particles. Results revealed that wear resistance and the friction coefficient were turned out to be higher and smaller, respectively, for the composite coatings as compared to pure Ni coating at a given sliding distance. It was noted that the corrosion resistance of these specimens increased in the following order: bare substrate < pure Ni coating < Ni-Al{sub 2}O{sub 3} nanocomposite coatings.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Slide Conveying of Granular Materials-Thinking Out of the Glovebox

The vibratory conveyor, routinely employed for normal-gravity transport of granular materials, usually consists of a continuous open trough vibrated sinusoidally to induce axial movement of a granular material. Motivated in part by a hypothetical application in zero gravity, we propose a novel modification of the vibratory conveyor based on a closed 2d trough operating in a "slide-conveying" mode, with the granular mass remaining permanently in contact with the trough walls. We present a detailed analysis of the mechanics of transport, based on a rigid-slab model for the granular mass with frictional (Coulomb) slip at the upper and lower walls. The form of the vibration cycle plays a crucial role, and the optimal conveying cycle is not the commonly assumed rectilinear sinusoidal motion. The conveying efficiency for the novel slide conveyor will be presented for several simple vibration cycles, including one believed to represent the theoretical optimum.

Goddard, J. D.↗

Molecular relaxations, molecular orientation and the friction characteristics of polyimide films

The friction characteristics of polyimide films bonded to metallic substrates were studied from 25 to 500 C. These results were interpreted in terms of molecular orientation and thermomechanical data obtained by torsional braid analysis (TBA). A large friction transition was found to occur at 40 plus or minus 10 C in a dry argon atmosphere (10 ppm H2O). It was postulated that the mechanical stresses of sliding transform or reorder the molecules on the surface into a configuration conducive to easy shear, such as an extended chain. The molecular relaxation which occurs in this temperature region appears to give the molecules the necessary freedom for this reordering process to occur. The effects of velocity, reversibility, and thermal prehistory on the friction properties of polyimide were also studied.

Fusaro, R. L.↗

Faulting parameters derived from computer simulation of earthquakes

Seismic source parameters, average displacement, rupture length, and strain energy release are investigated by computer simulation using a coupled massive block model of the sliding along an active fault. Average displacements and energy release vary considerably with the degree of heterogeneity in the friction and elastic parameters used in the model. Strain energy release is determined primarily by the product of dynamic friction, rupture length, and average displacement. Interrelationships among the faulting parameters are consistent with theoretical arguments and experimental data. The variation in the frequency of occurrence of simulation events with strain energy release is different from the variation in the frequency of naturally occurring events with seismic energy.

Cohen, S. C.↗

Sputtered silver films to improve chromium carbide based solid lubricant coatings for use to 900 C

Thin silver films, 250 to 3500 A thick, were sputtered onto PS200, a plasma sprayed, chromium carbide based solid lubricant coating, to reduce run-in wear and improve tribological properties. The coating contains bonded chromium carbide as the wear resistant base stock with silver and barium fluoride/calcium fluoride eutectic added as low and high temperature lubricants respectively. Potential applications for the PS200 coating are cylinder wall/piston ring lubrication for Stirling engines and foil bearing journal lubrication. In this preliminary program, the silver film overlay thickness was optimized based on tests using a pin-on-disk tribometer. The friction and wear studies were performed in a helium atmosphere at temperatures from 25 to 760 C with a sliding velocity of 2.7 m/s under a 4.9 N load. Films between 1000 and 1500 A provide the best lubrication of the counterface material. The films enrich the sliding surface with lubricant and reduce the initial abrasiveness of the as ground, plasma-sprayed coating surface, thus reducing wear.

Dellacorte, Christopher↗

Sputtered silver films to improve chromium carbide based solid lubricant coatings for use to 900 C

Thin silver films, 250 to 3500 A thick, were sputtered onto PS200, a plasma sprayed, chromium carbide based solid lubricant coating, to reduce run-in wear and improve tribological properties. The coating contains bonded chromium carbide as the wear resistant base stock with silver and barium fluoride/calcium fluoride eutectic added as low and high temperature lubricants, respectively. Potential applications for the PS200 coating are cylinder wall/piston ring lubrication for Stirling engines and foil bearing journal lubrication. In this preliminary program, the silver film overlay thickness was optimized based on tests using a pin-on-disk tribometer. The friction and wear studies were performed in a helium atmosphere at temperatures from 25 to 760 C with a sliding velocity of 2.7 m/s under a 4.9 N load. Films between 1000 and 1500 A provide the best lubrication of the counterface material. The films enrich the sliding surface with lubricant and reduce the initial abrasiveness of the as ground, plasma-sprayed coating surface, thus reducing wear.

Dellacorte, Christopher↗

Utah FORGE: Slide-Hold-Slide Experiments on Westerly Granite at Temperatures up to 250 Degrees C

Laboratory slide-hold-slide tests were conducted in a conventional triaxial deformation configuration on 1-inch diameter cylindrical cores of Westerly granite bisected by a sawcut oriented at 30 degrees from vertical. Tests were conducted at a constant confining pressure of 30 MPa with a 10 MPa pore fluid pressure. The pore fluid was deionized water. Experiments were conducted at temperatures of 22, 100, 200, and 250 C. This data was collected to examine fault strength recovery in hydrothermal conditions.

15 GEOTHERMAL ENERGY↗

Abrasion behavior of aluminum and composite skin coupons, stiffened skins and stiffened panels representative of transport airplane structures

A three-phase investigation was conducted to compare the friction and wear response of aluminum and graphite-epoxy composite materials when subjected to loading conditions similar to those experienced by the skin panels on the underside of a transport airplane during an emergency belly landing on a runway surface. The first phase involved a laboratory test which used a standard belt sander to provide the sliding abrasive surface. Small skin-coupon test specimens were abraded over a range of pressures and velocities to determine the effects of these variables on the coefficient of friction and wear rate. The second phase involved abrading I-beam stiffened skins on actual runway surface over the same range of pressures and velocities used in the first phase. In the third phase, large stiffened panels which most closely resembled transport fuelage skin construction were abraded on a runway surface. This report presents results from each phase of the investigation and shows comparisons between the friction and wear behavior of the aluminum and graphite-epoxy composite materials.

Jackson, K. E.↗

Frictional and morphological properties of Au-MoS2 films sputtered from a compact target

AuMoS2 films 0.02 to 1.2 microns thick were sputtered from target compacted from 5 wt % Au + 95 wt % MoS2, to investigate the frictional and morphological film growth characteristics. The gold dispersion effects in MoS2 films are of interest to increase the densitification and strengthening of the film structure. Three microstructural growth stages were identified on the nano-micro-macrostructural level. During sliding both sputtered Au-MoS2 and MoS2 films have a tendency to break within the columner region. The remaining or effective film, about 0.2 microns thick, performs the lubrication. The Au-MoS2 films displayed a lower friction coefficient with a high degree of frictional stability and less wear debris generation as compared to pure MoS2 films. The more favorable frictional characteristics of the Au-MoS2 films are attributed to the effective film thickness and the high density packed columner zone which has a reduced effect on the fragmentation of the tapered crystallites during fracture.

Spalvins, T.↗

Frictional and morphological properties of Au-MoS2 films sputtered from a compact target

AuMoS2 films 0.02 to 1.2 microns thick were sputtered from target compacted from 5 wt percent Au + 95 wt percent MoS2, to investigate the frictional and morphological film growth characteristics. The gold dispersion effects in MoS2 films are of interest to increase the densification and strengthening of the film structure. Three microstructural growth stages were identified on the nano-micro-macrostructural level. During sliding both sputtered Au-MoS2 and MoS2 films have a tendency to break within the columner region. The remaining or effective film, about 0.2 microns thick, performs the lubrication. The Au-MoS2 films displayed a lower friction coefficient with a high degree of frictional stability and less wear debris generation as compared to pure MoS2 films. The more favorable frictional characteristics of the Au-MoS2 films are attributed to the effective film thickness and the high density packed columner zone which has a reduced effect on the fragmentation of the tapered crystallites during fracture.

Spalvins, T.↗

Frictional and morphological properties of Au-MoS2 films sputtered from a compact target

AuMoS2 films 0.02 to 1.2 microns thick were sputtered from target compacted from 5 wt pct. Au + 95 wt pct. MoS2, to investigate the frictional and morphological film growth characteristics. The gold dispersion effects in MoS2 films are of interest to increase the densitification and strengthening of the film structure. Three microstructural growth stages were identified on the nano-micro-macrostructural level. During sliding both sputtered Au-MoS2 and MoS2 films have a tendency to break within the columner region. The remaining or effective film, about 0.2 microns thick, performs the lubrication. The Au-MoS2 films displayed a lower friction coefficient with a high degree of frictional stability and less wear debris generation as compared to pure MoS2 films. The more favorable frictional characteristics of the Au-MoS2 films are attributed to the effective film thickness and the high density packed columner zone which has a reduced effect on the fragmentation of the tapered crystallites during fracture.

Spalvins, T.↗

Tribological Performance of M50-Ag-TiC Self-Lubricating Composites at Elevated Temperature

M50 steel is widely used in aero-engine bearings and other high-temperature bearings. However, the poor wear of M50 steel resistance restrains its further applications. In this paper, the sliding tribological behaviors of M50 steel, M50-Ag composites (MAC) and M50-Ag-TiC composites (MATC) against Si{sub 3}N{sub 4} ball were investigated from 150 to 600 °C at 15 N-0.2 m/s. MATC showed better tribological properties in comparison with M50 and MAC. Especially at 450 °C, MATC obtained the lowest friction coefficient of 0.15 and smallest wear rate of 1.3 × 10{sup −5} mm{sup 3} N{sup −1} m{sup −1}. The excellent tribological performance of MATC during the friction test was attributed to the continuous lubricating film containing lubricant Ag and reinforcement TiC, as well as the subsurface compacted layer that could well support the lubricating film to prevent it from being destroyed. At 600 °C, because of the tribo-chemical reaction between Ag and Mo oxide during sliding process, the newly formed Ag{sub 2}MoO{sub 4} lubricating film was well spread out on the friction surface, which could continuously improve the tribological behavior of MATC. This investigation was meaningful to improve the anti-friction and wear resistance of M50 matrix bearing over a wide temperature range.