Morphology-controlled synthesis of grass-like GO-CdSe nanocomposites with excellent optical properties and field emission properties

Four different morphologies of the CdSe semiconductor nanograss have been successfully grown on graphene oxide (GO) sheets via hydrothermal method at 220 °C for 12 h. The morphologies, structures, chemical compositions and optical properties of the as-obtained GO-CdSe nanocomposites were characterized by XRD, SEM, TEM, EDS, XPS and Raman spectra. It was found that the EDTA/Cd{sup 2+} molar ratio is important for the formation of morphology of GO-CdSe nanocomposites. The results of XRD revealed that all the as-obtained GO-CdSe nanocomposites have zinc blend structure. Room temperature photoluminescence (PL) showed that the sample emits red light under different excitation wavelengths. The results of Raman spectra, EDS and XPS showed that the CdSe nanograss is grown on GO sheets. The results showed that GO-CdSe nanocomposites composed of nanorods have best field emission (FE) properties with a low turn-on electric field of 4.14 V μm{sup −1} and a high field enhancement factor of 3315 among all the samples. - Graphical abstract: SEM images of as-synthesized CdSe nanograss grown on GO sheets. Room temperature PL emission spectra of the as-synthesized CdSe nanograss grown on GO sheets. Field emission J–E curve of the as-synthesized CdSe nanograss grown on GO sheets. - Highlights: • Novel CdSe nanograsses are grown on graphene oxide sheets by hydrothermal method. • The morphology of CdSe nanograsses is controlled by adjusting EDTA/Cd{sup 2+} molar ratio. • The FE performance of sample is investigated. • Optimum morphology for FE performance is CdSe nanograsses composed of nanorods on GO.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Complete doping in solid-state by silica-supported perchloric acid as dopant solid acid: Synthesis and characterization of the novel chiral composite of poly [(±)-2-(sec-butyl) aniline]

Poly [(±)-2-(sec-butyl) aniline]/silica-supported perchloric acid composites were synthesized by combination of poly[(±)-2-sec-butylaniline] base (PSBA) and the silica-supported perchloric acid (SSPA) as dopant solid acid in solid-state. The X-ray photoelectron spectroscopy (XPS) and CHNS results confirm nigraniline oxidation state and complete doping for composites (about 75%) and non-complete for the PSBA·HCl salt (about 49%). The conductivity of samples was (≈0.07 S/cm) in agreement with the percent of doping obtained of the XPS analysis. Also, contact resistance was determined by circular-TLM measurement. The morphology of samples by the scanning electron microscopy (SEM) and their coating were investigated by XPS, SEM-map and energy-dispersive X-ray spectroscopy (EDX). The key benefits of this work are the preparation of conductive chiral composite with the delocalized polaron structure under green chemistry and solid-state condition, the improvement of the processability by inclusion of the 2-sec-butyl group and the use of dopant solid acid (SSPA) as dopant. - Highlights: • The solid-state synthesis of the novel chiral composites of poly[(±)-2-(sec-butyl)aniline] (PSBA) and silica-supported perchloric acid (SSPA). • It takes 120 h for complete deprotonation of PSBA.HCl salt. • Use of SSPA as dopant solid acid for the first time to attain the complete doping of PSBA. • The coating of silica surface with PSBA.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Understanding the formation and growth of Ag nanoparticles on silver chromate induced by electron irradiation in electron microscope: A combined experimental and theoretical study

Ag{sub 2}CrO{sub 4} microcrystals were synthesized using the co-precipitation method. These microcrystals were characterized through X-ray diffraction (XRD) with Rietveld analysis, field-emission scanning electron microscopy (FE-SEM), transmission electron microscopy (TEM) with energy-dispersive spectroscopy (EDS), micro-Raman (MR). XRD patterns and Rietveld refinement data showed that the material exhibits an orthorhombic structure without any deleterious phases. FE-SEM and TEM micrographs revealed the morphology and the growth of Ag nanoparticles on Ag{sub 2}CrO{sub 4} microcrystals during electron beam irradiation. These events were directly monitored in real-time. Their optical properties were investigated using ultraviolet-visible (UV–vis) diffuse reflectance spectroscopy that allowed the calculation of the optical band gap energy. Theoretical analyses based on the density functional theory level indicate that the incorporation of electrons is responsible for structural modifications and formation of defects on the [AgO{sub 6}] and [AgO{sub 4}] clusters, generating ideal conditions for the growth of Ag nanoparticles. - Graphical abstract: Theoretical representation of the Ag{sub 2}CrO{sub 4} orthorhombic structure. Display Omitted - Highlights: • The Ag{sub 2}CrO{sub 4} microcrystals indicate an orthorhombic structure. • The formation of Ag{sup 0} promotes Ag-nanoparticle growth on the surface of the Ag{sub 2}CrO{sub 4}. • Electron irradiation of the material induces the formation of Ag vacancies.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Fabrication of MCM-41 fibers with well-ordered hexagonal mesostructure controlled in acidic and alkaline media

In this paper, synthesis and characterization of two type morphologies of the MCM-41mesoporous material, nano and microfibers, were investigated by electrospinning technique. The synthesis was performed in acidic and alkaline media, separately. The MCM-41 morphologies were characterized by scanning electron microscopy (SEM), transmission electron microscopy (TEM), x-ray powder diffraction (XRD), and nitrogen adsorption–desorption measurement. Tetraethylorthosilicate (TEOS) and cetyltrimethylammonium bromide (CTAB) were used as silica and template sources for the synthesis of MCM-41 morphologies, respectively. The SEM results showed that MCM-41 nanofibers were spun in acidic media and microfibers of MCM-41 were produced in alkaline media. The XRD study revealed a long range structural ordering of mesoporous materials. The TEM results indicated rough surfaces with uniform average diameter 200 nm for nanofibers and 2 µm for microfibers. The pore diameter and surface area of calcined MCM-41 nanofibers were 2.2 nm and 970 m{sup 2}/g, respectively. For the MCM-41 microfibers, pore sizes of 2.7 nm and surface areas 420 m{sup 2}/g was measured. - Graphical abstract: Electrospinning method was used for fabricating of MCM-41 microfibers from TEOS in alkaline media (top) and MCM-41 nanofibers in acidic media (bottom). - Highlights: • Synthesis of MCM-41 nanofibers and microfibers by electrospinning technique. • MCM-41 nanofibers were synthesized in acidic media. • MCM-41 manofibers spun in alkaline media. • Electrospinning was a simple method for preparing of fibers with respect to chemical method.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Structural, electronic and optical properties of monoclinic Na{sub 2}Ti{sub 3}O{sub 7} from density functional theory calculations: A comparison with XRD and optical absorption measurements

Powder samples of bulk monoclinic sodium trititanate Na{sub 2}Ti{sub 3}O{sub 7} were prepared carefully by solid state reaction, and its monoclinic P2{sub 1}/m crystal structure and morphology were characterized by X-ray powder diffraction (XRD) and scanning electron microscopy (SEM), respectively. Moreover, the sodium trititanate main energy band gap was estimated as E{sub g}=3.51±0.01 eV employing UV–Vis spectroscopy, which is smaller than the measured 3.70 eV energy gap published previously by other authors. Aiming to achieve a better understanding of the experimental data, density functional theory (DFT) computations were performed within the local density and generalized gradient approximations (LDA and GGA, respectively) taking into account dispersion effects through the scheme of Tkatchenko and Scheffler (GGA+TS). Optimal lattice parameters, with deviations relative to measurements Δa=−0.06 Å, Δb=0.02 Å, and Δc=−0.09 Å, were obtained at the GGA level, which was then used to simulate the sodium trititanate electronic and optical properties. Indirect band transitions have led to a theoretical gap energy value of about 3.25 eV. Our results, however, differ from pioneer DFT results with respect to the specific Brillouin zone vectors for which the indirect transition with smallest energy value occurs. Effective masses for electrons and holes were also estimated along a set of directions in reciprocal space. Lastly, our calculations revealed a relatively large degree of optical isotropy for the Na{sub 2}Ti{sub 3}O{sub 7} optical absorption and complex dielectric function. - Graphical abstract: Monoclinic sodium trititanate Na2Ti3O7 was characterized by experiment and dispersion-corrected DFT calculations. An indirect gap of 3.5 eV is predicted, with heavy electrons and anisotropic holes ruling its conductivity. - Highlights: • Monoclinic Na2Ti3O7 was characterized by experiment (XRD, SEM, UV–Vis spectroscopy). • DFT GGA+TS optimized geometry and optoelectronic properties were obtained. • An experimental (theoretical) indirect gap of 3.5 (3.25) eV is predicted. • Heavy electrons and anisotropic holes rule the conductivity. • Ti-O bond lengths and charge states probably cause oxygen reactivity variations.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Synthesis of zeolitic imidazolate framework-69 for adsorption separation of ethane and ethylene

The zeolitic imidazolate framework ZIF-69 with topology of GME has been synthesized successfully via a facile hydrothermal synthetic method, and characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), nitrogen adsorption-desorption measurements, thermal gravimetric analysis (TGA) and X-ray photoelectron spectroscopy (XPS). The ethane/ethylene separation potential was measured by single-component adsorption isotherms, and the selectivity was calculated based on the ideal adsorbed solution theory (IAST). SEM and TEM images confirmed that the as-synthesized seeds possessed a well-crystallized and uniform morphology, appearing as a flat hexagonal prism with double hexagonal pyramid heads. The obtained ZIF-69 exhibited a higher adsorption capacity of C{sub 2}H{sub 6} over C{sub 2}H{sub 4} at 100 kPa, and the C{sub 2}H{sub 6}/C{sub 2}H{sub 4} adsorption selectivity was about 1.7 at below 100 kPa. The outcome would provide a new insight into the study on the effective separation of ethane/ethylene using different topological structures of ZIFs. - Highlights: • The well-crystallized and uniform ZIF-69 seeds were successfully synthesized. • ZIF-69 exhibited great preferential adsorption of C{sub 2}H{sub 6} over C{sub 2}H{sub 4}, with the C{sub 2}H{sub 6} adsorption capacity of 2.2 mmol/g. • C{sub 2}H{sub 6}/C{sub 2}H{sub 4} adsorptive selectivity was about 1.7 at pressure below 100 kPa. • The isosteric heat of C{sub 2}H{sub 6} was around 26 kJ/mol, much lower compared to those π -complexation sorbents.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Immobilizing of ZIF-8 derived ZnO with controllable morphologies on zeolite A for efficient photocatalysis

ZIF-8@Zeolite A (ZIF-8@Z) catalysts were successfully prepared by sonochemical synthesizing method using metal organic frameworks as precursors and zeolite A as support. Then, ZIF-8@Z catalysts were transformed into ZnO@Zeolite A (ZnO@Z) photocatalysts by calcining at different temperatures to remove the organic functional groups of ZIF-8. All samples were characterized by XRD, SEM, BET and UV–vis diffuse reflectance spectra respectively. SEM images show that ZIF-8 nanoparticles were tightly loaded on the surface of zeolite A. The XRD patterns exhibit that ZIF-8 was transformed into ZnO. The photocatalysis of ZnO@Z was investigated by degradation of rhodamine B (RhB) aqueous solution under UV light and ZnO@Z exhibited rapider photodegradation of RhB than porous ZnO derived from ZIF-8. The degradation of RhB reveals that ZnO@Z, calcined at 550 °C for 5 h, (ZnO@Z550) shows the highest photocatalytic efficiency (99.4%). - Graphical abstract: Schematic Illustration of the Preparation of the ZnO@Z via Sonochemical Synthesis. Display Omitted - Highlights: • Hybrid structure of ZIF-8 derived ZnO loaded on Zeolite A is first obtained. • ZnO@Z hybrid show higher photocatalytic activity on RhB than ZnO. • The preparation is facile, cheap and easily to scale-up.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Boron doped diamond synthesized from detonation nanodiamond in a C-O-H fluid at high pressure and high temperature

Boron doped diamond (BDD) was synthesized under high pressure and high temperature (HPHT) of 7 GPa, 1230 °C in a short time of 10 s from a powder mixtures of detonation nanodiamond (DND), pentaerythritol C{sub 5}H{sub 8}(OH){sub 4} and amorphous boron. SEM, TEM, XRD, XPS, FTIR and Raman spectroscopy indicated that BDD nano- and micro-crystals have formed by consolidation of DND particles (4 nm in size). XRD showed the enlargement of crystallites size to 6–80 nm and the increase in diamond lattice parameter by 0.02–0.07% without appearance of any microstrains. Raman spectroscopy was used to estimate the content of boron atoms embedded in the diamond lattice. It was found that the Raman diamond peak shifts significantly from 1332 cm{sup −1} to 1290 cm{sup −1} without appearance of any non-diamond carbon. The correlation between Raman peak position, its width, and boron content in diamond is proposed. Hydrogenated diamond carbon in significant amount was detected by IR spectroscopy and XPS. Due to the doping with boron content of about 0.1 at%, the electrical conductivity of the diamond achieved approximately 0.2 Ω{sup −1} cm{sup −1}. Reaction mechanism of diamond growth (models of recrystallization and oriented attachment) is discussed, including the initial stages of pentaerythritol pyrolysis and thermal desorption of functional groups from the surface of DND particles with the generation of supercritical fluid of low-molecular substances (H{sub 2}O, CH{sub 4}, CO, CO{sub 2}, etc.), as well as byproducts formation (B{sub 2}O{sub 3}, B{sub 4}C). - Highlights: • Boron doped diamond BDD synthesized from detonation nanodiamond, C{sub 5}H{sub 8}(OH){sub 4} and boron. • BDD nano/microcrystals are studied by XRD, SEM, TEM, XPS, FTIR, Raman spectroscopy. • Diamond growth and transition to electro-conductive state (0.2 Ω{sup −1} cm{sup −1}) is observed. • Correlations of Raman bands position and width versus boron content are considered. • High-pressure/temperature reaction mechanism (stages, routes, products) is described.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Factors controlling pore network development of thermally mature Early Palaeozoic mudstones from the Baltic Basin (N Poland)

Understanding the formation of pore space, especially in low porosity shales (as source rocks and as unconventional resources), is critical to the oil and gas industry, since pores control the space available for hydrocarbon and participate in hydrocarbon transport. We examined 87 Ordovician and Silurian mudstone samples collected from four wells located in the Pomeranian part of the Baltic Basin (northern Poland), one of the primary Polish targets for hydrocarbon exploration. These samples represent the Pelplin, the Paslek, the Jantar, the Prabuty, and the Sasino Formations, which still requires more detailed porosity studies. Our study aimed to identify factors controlling porosity development, by applying bulk techniques (organic petrology and TOC analyses, quantitative mineralogy, and porosimetry) as well as nano- to microscale techniques (thin section petrography, electron microscopy). The studied samples are mainly argillaceous mudstones. The results of porosimetry measurements, combined with image analysis, indicate that the pores of all studied rocks are dominated by micropores (pores < 2 nm in diameter), mesopores (2-50 nm in diameter) and small macropores. The SEM images showed three main pore types: a) voids related to clay mineral aggregates, b) pores inside organic matter particles, and c) pores between other mineral grains. In the Jantar and Sasino mudstones, the organic matter content and its thermal maturity control porosity. The occurrence of solid bitumen in the rocks from these formations reduces samples’ mesoporosity because of the pore-clogging effect. In contrast, in the Paslek and Prabuty Formations, there is low organic matter content and specific surface area and the volume of mesopores increase with clay minerals content. In the Pelplin mudstones, there are no prevailing factors controlling porosity. As a result, we suggest that a combination of SEM image analysis and dual liquid porosity (DLP) measurements is a powerful method to assess porosity available for petroleum flow in mudstones.

03 NATURAL GAS↗

A study of the composition and microstructure of nanodispersed Cu-Ni alloys obtained by different routes from copper and nickel oxides

Mixtures of CuO and NiO were prepared by two different techniques, and then the oxides were reduced with H{sub 2}. Method A involved the preparation of mechanical mixtures of CuO and NiO using different milling and pelletizing processes. Method B involved the chemical synthesis of the mixture of CuO and NiO. The route used to prepare the copper and nickel oxide mixture was found to have great influence on the characteristics of bimetallic Cu-Ni particles obtained. Observations performed using the X-ray diffraction (XRD) technique showed that although both methods led to the Cu-Ni solid solution, the diffractogram of the alloy obtained with method A revealed the presence of NiO together with the alloy. The temperature-programmed reduction (TPR) experiments indicated that the alloy is formed at lower temperatures when using method B. The scanning electron microscopy (SEM) studies revealed notable differences in the morphology and size distribution of the bimetallic particles synthesized by different routes. The results of the electron probe microanalysis (EPMA) studies evidenced the existence of a small amount of oxygen in both cases and demonstrated that the alloy synthesized using method B presented a homogeneous composition with a Cu-Ni ratio close to 1:1. On the contrary, the alloy obtained using method A was not homogeneous in all the volume of the solid. The homogeneity depended on the mechanical treatment undergone by the mixture of the oxides. - Research Highlights: {yields}Study of the properties of Cu-Ni alloys synthesized by two different routes. {yields}Mixtures of Cu and Ni oxides prepared by two techniques were reduced with H{sub 2}. {yields}Mixtures of oxides were obtained by a mechanical process and the citrate-gel route. {yields}The characterizations were carried out by TPR, XRD, SEM and EPMA. {yields}The route used to prepare oxide mixtures influences on the Cu-Ni alloy obtained.

36 MATERIALS SCIENCE↗

Microstructural characterization of as-cast biocompatible Co-Cr-Mo alloys

The microstructure of a cobalt-base alloy (Co-Cr-Mo) obtained by the investment casting process was studied. This alloy complies with the ASTM F75 standard and is widely used in the manufacturing of orthopedic implants because of its high strength, good corrosion resistance and excellent biocompatibility properties. This work focuses on the resulting microstructures arising from samples poured under industrial environment conditions, of three different Co-Cr-Mo alloys. For this purpose, we used: 1) an alloy built up from commercial purity constituents, 2) a remelted alloy and 3) a certified alloy for comparison. The characterization of the samples was achieved by using optical microscopy (OM) with a colorant etchant to identify the present phases and scanning electron microscopy (SE-SEM) and energy dispersion spectrometry (EDS) techniques for a better identification. In general the as-cast microstructure is a Co-fcc dendritic matrix with the presence of a secondary phase, such as the M{sub 23}C{sub 6} carbides precipitated at grain boundaries and interdendritic zones. These precipitates are the main strengthening mechanism in this type of alloys. Other minority phases were also reported and their presence could be linked to the cooling rate and the manufacturing process variables and environment. - Research Highlights: {yields}The solidification microstructure of an ASTM-F75 type alloy were studied. {yields}The alloys were poured under an industrial environment. {yields}Carbides and sigma phase identified by color metallography and scanning microscopy (SEM and EDS). {yields}Two carbide morphologies were detected 'blocky type' and 'pearlite type'. {yields}Minority phases were also detected.

36 MATERIALS SCIENCE↗

On the role of processing parameters in producing Cu/SiC metal matrix composites via friction stir processing: Investigating microstructure, microhardness, wear and tensile behavior

The main aim of this study is to produce copper reinforced metal matrix composite (MMC) layers using micron sized SiC particles via friction stir processing (FSP) in order to enhance surface mechanical properties. Microstructural evaluation using optical microscopy (OM) and scanning electron microscopy (SEM) indicated that an increase in traverse speed and a decrease in rotational speed cause a reduction in the grain size of stir zone (SZ) for the specimens friction stir processed (FSPed) without SiC particles. With the aim of determining the optimum processing parameters, the effect of traverse speed as the main processing variable on microstructure and microhardness of MMC layers was investigated. Higher traverse speeds resulted in poor dispersion of SiC particles and consequently reduced the microhardness values of MMC layers. It was found that upon addition of SiC particles, wear properties were improved. This behavior was further supported by SEM images of wear surfaces. Results demonstrated that the microcomposite produced by FSP exhibited enhanced wear resistance and higher average friction coefficient in comparison with pure copper. Tensile properties and fracture characteristics of the specimens FSPed with and without SiC particles and pure copper were also evaluated. According to the results, the MMC layer produced by FSP showed lower strength and elongation than pure copper while a remarkable elongation was observed for FSPed specimen without SiC particles. Research Highlights: {yields} Decrease in traverse speed leads to good dispersion of SiC particles in composites. {yields} No distinct TMAZ in side regions of SZ of FSPed specimens with SiC particles. {yields} Microhardness of FSPed specimens with SiC particles shows a remarkable increase. {yields} Reinforcement of Cu with SiC particles improves wear and friction behavior of surface. {yields} A weak bonding in tensile due to probable agglomeration for SiC containing samples.

36 MATERIALS SCIENCE↗

Study of dithiol monolayer as the interface for controlled deposition of gold nanoparticles

Self-assembled monolayer of dithiol molecules, deposited on polycrystalline Au (111), prepared at room atmosphere, was studied using scanning tunneling microscopy (STM) and X-ray photoelectron spectroscopy (XPS). Dithiols were used as interface, which chemically bonds to the deposited gold nanoparticles through strong covalent bonds. The size and size distribution of the deposited nanoparticles were measured using dynamic light scattering (DLS), scanning electron microscopy (SEM) and atomic force microscopy (AFM). The AFM results showed that nanoparticles are immobilized and stable during scanning procedure and do not contaminate the AFM tip. The size of monodisperse nanoparticles obtained from the DLS measurements is slightly higher than that obtained from the AFM and SEM measurements. This is due to the fact that the DLS measures the hydrodynamic radius, dependent on the protective chemical layer on nanoparticles. - Research Highlights: {yields} Dithiols molecules create chemically bounded layers on a Au (111) surface. {yields} Gold nanoparticles can be chemically bounded to a self-assembled monolayer. {yields} Nanoparticles are stable during AFM probe interactions.

36 MATERIALS SCIENCE↗

Evaluation of microstructural development in electron beam melted Ti-6Al-4V

In the current work an investigation of the microstructures of EBM built Ti-6Al-4V test bars has been performed using OM, SEM, TEM and XRD. It has been found that the prior {beta} phase, that formed during the initial solidification, possesses a column shaped morphology with growing direction parallel to built direction. Typical ({alpha} + {beta}) structures namely Widmanstaetten {alpha} platelets with rod-like {beta} phase formed on the interfaces of the fine {alpha} grains, have been observed in the columnar prior {beta} grains. Grain boundary {alpha} phase was found to be formed around the boundaries of the columnar prior {beta} grains. Different phases present in the parts, especially the BCC {beta} phases have been characterized. The TEM/EDX results indicate very high V composition in the {beta} phase. Results of TEM/SAED and XRD also revealed that a superlattice structure could be present in the {beta} phase. Phase transformation sequence is discussed according to the processing history and the microstructures observed. - Highlights: Black-Right-Pointing-Pointer {alpha} + {beta} and individual {beta} phase is observed and characterized by SEM, TEM and XRD. Black-Right-Pointing-Pointer {beta}-phase is identified as rod-like structure embedded in {alpha} matrix and platelets. Black-Right-Pointing-Pointer Phase transformation sequence is discussed as per thermal history and microstructures.

36 MATERIALS SCIENCE↗

Microstructural evolution during solution treatment of Co-Cr-Mo-C biocompatible alloys

Three different Co-Cr-Mo-C alloys conforming to ASTM F75 standard were poured in an industrial environment and subjected to a conventional solution treatment at 1225 Degree-Sign C for several time intervals. The microstructural changes and transformations were studied in each case in order to evaluate the way in which treatment time influences the secondary phase fraction and clarify the microstructural changes that could occur. To assess how treatment time affects microstructure, optical microscopy and image analyzer software, scanning electron microscopy and energy dispersion spectrometry analysis were employed. The main phases detected in the as-cast state were: {sigma}-phase, M{sub 6}C, and M{sub 23}C{sub 6} carbides. The latter presented two different morphologies, blocky type and lamellar type. Despite being considered the most detrimental feature to mechanical properties, {sigma}-phase and lamellar carbides dissolution took place in the early stages of solution treatment. M{sub 23}C{sub 6} carbides featured two different behaviors. In the alloy obtained by melting an appropriate quantity of alloyed commercial materials, a decrease in size, spheroidization and transformation into M{sub 6}C carbides were simultaneously observed. In the commercial ASTM F75 alloy, in turn, despite being the same phase, only a marked decrease in precipitates size was noticed. These different behaviors could be ascribed to the initial presence of other phases in the alloy obtained from alloyed materials, such as {sigma}-phase and 'pearlitic' carbides, or to the initial precipitate size which was much larger in the first than in the commercial ASTM F75 alloy studied. M{sub 6}C carbides dissolved directly in the matrix as they could not be detected in samples solution-treated for 15 min. - Highlights: Black-Right-Pointing-Pointer Three different Co-Cr-Mo alloys were poured under an industrial environment. Black-Right-Pointing-Pointer Transformation of existing phases followed during conventional solution treatment. Black-Right-Pointing-Pointer In as-cast/treated samples, phases were identified by color metallography, SEM and EDS. Black-Right-Pointing-Pointer M{sub 23}C{sub 6} {yields} M{sub 6}C transformation was corroborated by SEM and EDS analysis. Black-Right-Pointing-Pointer Carbide spheroidization was also detected prior a noticeably carbide size decreasing.

36 MATERIALS SCIENCE↗

Electrochemical study of Aluminum-Fly Ash composites obtained by powder metallurgy

In this paper, two different ASTM C 618 Class C fly ashes (FA) were used for the production of aluminum metal matrix composites (MMCs) using powder metallurgy (PM) technology. Calcareous FAs were sampled from the electrostatic precipitators of two different lignite-fired power stations: from Megalopolis, Southern Greece (MFA) and from Kardia, Northen Greece (KFA), under maximum electricity load. FAs were milled in order to reduce the mean particle diameter and Aluminum-FA composites containing 10% and 20% of FA were then prepared and compacted. The green products were sintered for 2 h at 600 Degree-Sign C. Sintered Al-FA MMCs showed increased hardness and wear resistance suggesting their possible use in industrial applications for example in covers, casings, brake rotors or engine blocks. As most possible industrial applications of MMCs not only require wear resistance, but also corrosion resistance in different mild aggressive medias, this paper aims to study the electrochemical behavior of FA MMCs in order to evaluate their corrosion resistance. The morphology and chemical composition of the phases in the Aluminum-FA composite samples were investigated using Scanning Electron Microscopy (SEM) and Energy Dispersive X-ray Spectroscopy (EDXS). Moreover, topographic and Volta potential maps were acquired by Scanning Kelvin Probe Force Microscopy (SKP-FM). Volta potential maps provide information about the electrochemical behavior of the different phases in absence of electrolyte. The electrochemical behavior was investigated by Open Circuit Potential measurements and potentiodynamic polarization, while the corrosion mechanisms were studied by SEM observations after different times of immersion in a mild corrosive medium. In all cases it could be stated that the addition of the FA particles into the Al matrix might cause an increase of the hardness and mechanical properties of the pure aluminum but deteriorates the corrosion resistance. The degradation phenomena occurring on the FA containing samples might be related to the following mechanisms: 1) Partial detachment or dissolution of the FA soluble phases, in particular based on Si, Fe and Ca; 2) dissolution of the Al matrix surrounding the FA particles due to crevice corrosion; 3) Al localized dissolution due to galvanic coupling between the Fe-rich intermetallics and the matrix. - Highlights: Black-Right-Pointing-Pointer Aluminum metal matrix composites containing two types of fly ashes have been characterized. Black-Right-Pointing-Pointer The microstructure and the electrochemical behavior have been studied using different techniques. Black-Right-Pointing-Pointer The addition of FA deteriorates the corrosion resistance of the aluminum. Black-Right-Pointing-Pointer Degradation mechanisms: galvanic coupling, crevice corrosion, detachment of FA particles.

36 MATERIALS SCIENCE↗

Modified Pechini synthesis of tricalcium aluminate powder

Tricalcium aluminate (Ca{sub 3}Al{sub 2}O{sub 6}-C{sub 3}A) was obtained by a modified Pechini synthesis in order to eliminate successive thermal treatments and intermediate grinding usually performed between the two sintering steps and in order to reduce the sintering temperature. Our results indicated that pure C{sub 3}A was obtained, by a single step thermal treatment at 1300 Degree-Sign C for 4 h and 1350 Degree-Sign C for 1 h. The synthesis was confirmed by XRD, FT-IR and free lime analyses. The morphology of synthesised C{sub 3}A was assessed by electron microscopy (SEM and TEM, HRTEM) and it was observed a high tendency of the particles to form aggregates and the individual particles seem to be single crystals. The bioactivity was assessed by specimen soaking in simulated body fluid (SBF) for 7 days; the hydrate (i.e. 3CaO Bullet-Operator Al{sub 2}O{sub 3} Bullet-Operator 6H{sub 2}O formed at the C{sub 3}A surface), can act as nucleation centers for the resulted phosphate phases. - Highlights: Black-Right-Pointing-Pointer A modified Pechini synthesis was used for obtained of tricalcium aluminate. Black-Right-Pointing-Pointer C{sub 3}A was obtained at 1300 Degree-Sign C/4 h and 1350 Degree-Sign C/1 h. Black-Right-Pointing-Pointer Were eliminated successive thermal treatments and intermediate grinding. Black-Right-Pointing-Pointer The morphology of synthesised C{sub 3}A was assessed by electron microscopy (SEM, TEM). Black-Right-Pointing-Pointer Was observed a high tendency of the particles to form aggregates.

36 MATERIALS SCIENCE↗

Solution heat-treatment of Nb-modified MAR-M247 superalloy

MAR-M247 superalloy has excellent mechanical properties and good oxidation resistance at elevated temperatures. Niobium is an element known as {gamma} Prime phase hardener in nickel-based superalloys, besides promoting homogeneous distribution of MC carbides. This work is inserted in a project that aims to evaluate the total replacement of tantalum by niobium atoms in MAR-M247 superalloy (10.2 Co, 10.2 W, 8.5Cr, 5.6 Al, 1.6 Nb, 1.4 Hf, 1.1 Ti, 0.7 Mo, 0.15 C, 0.06 Zr, 0.015 B, Ni balance-wt.%). Based on microstructural characterizations (SEM and FEG-SEM, both with EDS) of the as-cast material and heat-treated materials as well as utilizing Thermocalc simulations and experiments of differential thermal analysis (DTA), heat-treatment at 1260 Degree-Sign C for 8 h was chosen as an ideal condition for the solution of Nb-modified MAR-M247 superalloy. The hardness of as-cast and ideally solution treated materials was 390 {+-} 14 HV and 415 {+-} 6 HV, respectively. - Highlights: Black-Right-Pointing-Pointer DTA and microstructure of MAR-M247(Nb) showed a good agreement with Thermocalc. Black-Right-Pointing-Pointer An ideal condition for solution heat-treatment of MAR-M247(Nb) is 1260 Degree-Sign C for 8 h. Black-Right-Pointing-Pointer It was an observed evidence of incipient melting in samples heat-treated at 1280 Degree-Sign C.

36 MATERIALS SCIENCE↗