Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ROLL”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 721 records · Page 40

Microstructure and partitioning behavior characteristics in low carbon steels treated by hot-rolling direct quenching and dynamical partitioning processes

In this work, a new process and composition design are proposed for “quenching and partitioning” or Q&P treatment. Three low carbon steels were treated by hot-rolling direct quenching and dynamical partitioning processes (DQ&P). The effects of proeutectoid ferrite and carbon concentration on microstructure evolution and mechanical properties were investigated. The present work obtained DQ&P prototype steels with good mechanical properties and established a new notion on compositions for Q&P processing. Microstructures were characterized by means of electro probe microanalyzer (EPMA), scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), transmission electron microscopy (TEM) and X-ray diffraction (XRD), especially the morphology and size of retained austenite. Mechanical properties were measured by uniaxial tensile tests. The results indicated that introducing proeutectoid ferrite can increase the volume fraction of retained austenite and thus improve mechanical properties. TEM observation showed that retained austenite included the film-like inter-lath austenite and blocky austenite located in martensite/ferrite interfaces or surrounded by ferrites. It was interesting that when the carbon concentration is as low as ~ 0.078%, the film-like inter-lath untransformed austenite cannot be stabilized to room temperature and almost all of them transformed into twin martensite. The blocky retained austenite strengthened the interfaces and transformed into twin martensite during the tensile deformation process. The PSEs of specimens all exceeded 20 GPa.%. - Highlights: •This study focused on a new process: Q&P process applying dynamical partitioning. •Ferrite can increase the volume fraction of retained austenite. •The film-like austenite and the blocky austenite were observed. •The low carbon steels treated by new process reached PSEs higher than 20 GPa.%.

36 MATERIALS SCIENCE↗

Characterization of the microstructures and the shape memory properties of the Fe-Mn-Si-Cr-Ni-C shape memory alloy after severe plastic deformation by differential speed rolling and subsequent annealing

Highlights: • The Fe-SMA was subjected to severe plastic deformation and then annealed. • Recovery strain increased with increasing grain size. • An optimum grain size existed for the largest recovery stress. • Grain reduction is useful for having a high recovery stress. - Abstract: The Fe-13.51Mn-4.82Si-8.32Cr-3.49Ni-0.15C shape memory alloy was subjected to severe plastic deformation by high-ratio differential speed rolling and subsequent annealing (between 873 and 1373 K) to find the factors that affect recovery stress and recovery strain. As the annealing temperature increased (i. e., as grain size increased), the recovery strain increased. This was attributed to decrease in the density of grain boundaries and the density of twins with increasing grain size. The recovery stress, however, showed a different behavior. It increased with annealing temperature up to 973 K, at which an ultrafine grain size near 1.6 μm was obtained, and then decreased with further increase in the temperature. The difference between the recovery strain and the plastic strain induced by recovery stress under constrained displacement during cooling was proposed to determine the amount of recovery stress. There was an optimum grain size for the largest difference between the recovery strain and the plastic strain. The current study shows that grain-size reduction is not good for having a high recovery strain but it is beneficial for having a high recovery stress in the Fe-Mn-Si shape memory alloys.

36 MATERIALS SCIENCE↗

Effect of isochronal annealing on the microstructure, texture and mechanical properties of a cold-rolled high manganese steel

Highlights: • Recrystallised γ grains have similar orientations to reverted/recovered γ grains. • After reversion, γ orientations are correlated to ε and α′-martensite orientations. • γ nucleation at the boundary of reverted/recovered γ grains - Abstract: A Fe-17Mn-3Al-2Si-1Ni-0.06C wt.% steel was subjected to cold-rolling to 42% thickness reduction and isochronally annealed for 300 s between 500 and 850 °C. The high Mn steel was characterised via electron back-scattering diffraction, transmission electron microscopy and uniaxial tensile testing. The reversion of deformation-induced ε and α′-martensite to austenite (γ) was witnessed with the formation of fine twins in reverted/recovered γ grains after annealing to 650 °C. The nucleation of new γ grains at the boundary of reverted/recovered γ grains was also noted. Upon reversion, the γ orientations originated from the ε and α′-martensite orientations by phase transformation via the Shoji-Nishiyama and Kurdjumov-Sachs orientation relationships, respectively. Upon segmenting the γ grains, the recrystallised γ grains were observed to nucleate with orientations similar to those of the reverted/recovered γ grains. Uniaxial tension on a fully recrystallised γ microstructure showed that the initial γ grain size has a more significant effect on the yield strength than the ε and α′-martensite fractions. On the other hand, the initial ε and α′-martensite fractions affect the total elongation.

36 MATERIALS SCIENCE↗

Interface characteristics of Ti6Al4V-TiAl metal-intermetallic laminate (MIL) composites prepared by a novel hot-pack rolling

Highlights: • The Ti6Al4V/high Nb-TiAl metal-intermetallic (MIL) composite was fabricated. • The formation of γ and α{sub 2} phase at interface is diffusion controlled. • The formation of O phase at interface is due to the segregation of Nb atoms. • The Vickers hardness from Ti6Al4V to TiAl alloy shows a trend of a decrease then an increase and finally a decrease. - Abstract: Ti6Al4V (wt%)/Ti-44Al-8Nb-0.2W-0.2B-0.03Y (at.%) (high Nb-TiAl) metal–intermetallic laminate (MIL) composite with a defect-free interface was successfully prepared by hot-pack rolling and the interface microstructure was characterized by XRD, SEM, EBSD, and TEM techniques. The results showed that the interface was about 260 μm thick and consisted of four different microstructure regions. The thickness of each region was about 60–80 μm and the microstructure of the four regions consisted of acicular O, α{sub 2}, and β/B2 phases; acicular α{sub 2} phase; acicular α{sub 2} and β/B2 phases; and acicular γ, α{sub 2}, and β/B2 phases respectively. The resulting microstructure of the interface region was attributed to the interdiffusion of Ti atoms from the starting Ti6Al4V alloy layer to the high Nb-TiAl alloy layer and Al and Nb atoms from the high Nb-TiAl alloy layer to the Ti6Al4V alloy layer. The formation of acicular α{sub 2} and γ phases was diffusion-controlled and the Nb segregation at the interface caused the formation of O phase which had specific relationships with α{sub 2} and β/B2 phases. The detailed interface microstructural evolution of the Ti6Al4V/high Nb-TiAl MIL composite and the Vickers hardness of the composite are also discussed in this paper.

36 MATERIALS SCIENCE↗

Shape memory and superelasticity of nanograined Ti-51.2 at.% Ni alloy processed by severe plastic deformation via high-ratio differential speed rolling

A novel method of producing nanograined Ni-rich superelastic NiTi alloys in sheet form was proposed using a combination of severe plastic deformation via high-ratio differential speed rolling (HRDSR) and post-deformation annealing. The HRDSR-processed microstructure was composed of heavily deformed austenite and martensite grains, and amorphous phases. After annealing at 673 K, the severely deformed microstructure with no functional properties evolved to the nanograined structure (20–70 nm) composed of austenite and martensite nanograins and sub-nanograins through static recovery or continuous static recrystallization process. The nanograined microstructure had a high resistance to martensitic transformation upon cooling and slip deformation during straining. As a result, the HRDSR-processed alloy annealed at 673K exhibited superior superelasticity compared to the alloys with coarse grains. At the higher annealing temperature of 873 K, the micron-sized recrystallized grains with low dislocations developed through discontinuous static recrystallization process. In this case, deformation during straining was governed by the detwinning of twinned martensite, and as a result, shape memory effect was more significantly pronounced than superelasticity.

36 MATERIALS SCIENCE↗

Annealing-induced microstructural evolution and mechanical anisotropy improvement of the Mg-Gd-Y-Zr alloy processed by hot ring rolling

Highlights: • Growth of SRX grains in GBR is random, while that of TBR is anisotropic. • The new texture component in annealed MR weakens the anisotropy obviously. • T6 treatment leads to an excellent comprehensive mechanical property. - Abstract: Hot ring rolling (HRR) is widely used to fabricate large-size seamless ring-shape components. However, this process produces a severe mechanical anisotropy, which is not acceptable in practical industrial application and should be avoided. This paper reports the annealing-induced microstructural evolution and mechanical anisotropy improvement of HRRed Mg-8.12Gd-1.82Y-0.35Zr alloy ring. Results show that annealing treatment could improve the microstructural homogeneity of the ring owing to the occurrence of static recrystallization (SRX). SRX grains are preferentially formed at twin boundaries and initial grain boundaries due to high dislocation density, high level of stored energy, and stress concentration. Twin boundaries, to some extent, can suppress the migration of SRX grain boundaries. In addition, occurrence of SRX weakens the texture intensity and basal pole inclination, leading to a decrease in the mechanical anisotropy of the ring. Considering the weakened anisotropy, comparable strength, and improved ductility, annealing + aging (T6), compared with direct aging (T5), is a more suitable heat treatment schedule for the HRRed Mg-8.12Gd-1.82Y-0.35Zr alloy ring.

36 MATERIALS SCIENCE↗

Face-centered titanium induced by ultrasonic surface rolling process in Ti-6Al-4V alloy and its tensile behavior

Highlights: • A gradient nanostructure of fcc-Ti is formed from a depth of 440 μm to top surface. • The influence factor of hcp to fcc phase transformation is demonstrated. • The fcc phase induced by USRP decreases the yield strength of Ti-6Al-4V alloy. • The fcc phase improves combining good strength and ductility. - Abstract: The phase transformation of face-centered cubic (fcc) titanium (Ti), transformed from hexagonal close-packed (hcp) Ti, in Ti-6Al-4V alloy subjected to ultrasonic surface rolling process (USRP) and the tensile behavior were investigated. A gradient nanostructure of fcc-Ti was formed from the depth of 440 μm to the top surface. The stress concentration at the phase interface of α phase and β phase promoted hcp to fcc phase transformation in low strain and strain rate region (adjacent to the substrate) while the extremely high strain and strain rate induced this phase transformation in the surface to sub-surface regions. USRP increased the tensile strength of Ti-6Al-4V alloy slightly but decreased the yield strength dramatically, and kept a good combination strength and ductility of Ti-6Al-4V alloy mainly due to the formation of the gradient nanostructure surface layer and hcp to fcc phase transformation.

36 MATERIALS SCIENCE↗

Mechanical rolling and annealing of wire-arc additively manufactured stainless steel plates

Thin walls of 304L stainless steel were fabricated by wire-arc additive manufacturing (WAAM) followed by post build thermomechanical processing to modify the as built microstructure and properties. The walls were made using a high-deposition-rate robotically controlled gas-metal arc welding system and were characterized using optical microscopy and tensile tested for mechanical properties. Post processing consisted of mechanical rolling the walls to 25% and 40% strains, followed by annealing at 1050°C to demonstrate a wide range of properties. Results show that WAAM can be used to build custom sized semi-finished parts or blanks that can later be thermomechanically processed to increase strength and ductility through recrystallization of the as built microstructure, and/or processed into desired shapes with improved mechanical properties.

304L stainless steel↗

Effect of Oil Viscosity and Impact of Ionic Liquid Additive on Electrically Induced Pitting in Rolling Contact

Electrically induced bearing damage (EIBD) is a growing concern in electric drivetrains, where electrical discharge currents generate localized pitting that accelerates wear and premature failure. While ionic liquids (ILs) have shown promise as lubricant additives due to their natural physical adsorption, strong capabilities of tribofilm formation, and high molecular tunability, their role in mitigating EIBD is little known. This gap is especially evident because lubricant viscosity and film thickness affect discharge behavior, and additive performance in these regimes has not been well explored. In this study, tribological tests were performed using a ball-on-disk pure rolling-contact system under an applied voltage on polyalphaolefin oils of three viscosities (4, 10, and 150 cSt measured at 100 °C), with and without the addition of a phosphonium-phosphate IL. Surface damage was analyzed using scanning electron microscopy (SEM) and stylus profilometry. Damage quantification was based on pit morphology analysis of SEM images. The results provide new insights into how oil viscosity governs the discharge behavior and how an IL additive could influence the pit formation. While viscosity seems to play a significant role, an IL additive shows potential to reduce EIBD and deserves further study.

electrically induced bearing damage (EIBD)↗

Correction of Rolling Mill Mechatronic System to Limit Dynamic Loads

Regulation in the mechatronic system of a DUO-300 rolling mill is investigated. The dynamics of an electric drive with a predictive PI controller in the current loop is analyzed. Methods are proposed for damping of self-oscillation and decrease in dynamic loads within the mechatronic system.

42 ENGINEERING↗