Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “PARTIAL PRESSURE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 721 records · Page 40

Formation of Nitrogen Bubbles During Solidification of Duplex Stainless Steels

The nucleation and growth of nitrogen bubbles for duplex stainless steels are of great significance for the formation mechanism of bubbles during solidification. In the current study, numerical method and theoretical analysis of formula derivation were used to study the formation of nitrogen bubbles during solidification. The critical sizes of the bubble for homogeneous nucleation and heterogeneous nucleation at the solid–liquid interface during solidification were derived theoretically by the classical nucleation theory. The results show that the calculated values for the solubility of nitrogen in duplex stainless steel are in good agreement with the experimental values which are quoted by references: for example, when the temperature T = 1823 K and the nitrogen partial pressure P{sub N 2 =40P Θ , the calculated value (0.8042 wt pct) for the solubility of Fe-12Cr alloy nitrogen in molten steel is close to the experimental value (0.780 wt pct). Moreover, the critical radii for homogeneous nucleation and heterogeneous nucleation are identical during solidification. On the one hand, with the increasing temperature or the melt depth, the critical nucleation radius of bubbles at the solid–liquid interface increases, but the bubble growth rate decreases. On the other hand, with the decreasing initial content of nitrogen or the cooling rate, the critical nucleation radius of bubbles at the solid–liquid interface increases, but the bubble growth rate decreases. Furthermore, when the melt depth is greater than the critical depth, which is determined by the technological conditions, the change in the Gibbs free energy for the nucleation is not conducive enough to form new bubbles.

36 MATERIALS SCIENCE↗

Photoluminescence of as-grown and thermal annealed SiO{sub x}/Si-nanocrystals heterolayers grown by reactive rf sputtering

SiO{sub x}/Si-nanocrystals (Si NCs) heterolayers were fabricated employing a rf magnetron sputtering system. The synthesis process, through modification of the oxygen partial pressure of the plasma, promotes the synthesis of stoichiometric SiO{sub 2} layers and affect the Si NCs layer giving place to SiO{sub x}/Si NCs (1.64<x<2) interfaces. All as-grown samples showed strong photoluminescence (PL) bands in the visible and near-infrared regions; transmission electron microscopy measurements confirmed the presence of Si NCs. Thermal annealing at 1100 deg. C promoted the SiO{sub 2} stoichiometry in the interface and the crystallization of more Si NCs. The results allow us to clearly identify the origin of the PL bands; indicating that the near-infrared emission is related to the nonstoichiometric oxide while the red and green bands are originated in Si NCs.

36 MATERIALS SCIENCE↗

Thermal conductivity control by oxygen defect concentration modification in reducible oxides: The case of Pr{sub 0.1}Ce{sub 0.9}O{sub 2−δ} thin films

We demonstrate the impact on thermal conductivity of varying the concentration of oxygen vacancies and reduced cations in Pr{sub 0.1}Ce{sub 0.9}O{sub 2−δ} thin films prepared by pulsed laser deposition. The oxygen vacancy concentration is controlled by varying the oxygen partial pressure between 1 × 10{sup −4} and 1 atm at 650 °C. Corresponding changes in the oxygen non-stoichiometry (δ) are monitored by detecting the lattice parameters of the films with high-resolution X-ray diffraction, while the thermal properties are characterized by time-domain thermoreflectance measurements. The films are shown to exhibit a variation in oxygen vacancy content, and in the Pr{sup 3+}/Pr{sup 4+} ratio, corresponding to changes in δ from 0.0027 to 0.0364, leading to a reduction in the thermal conductivity from k = 6.62 ± 0.61 to 3.82 ± 0.51 W/m-K, respectively. These values agree well with those predicted by the Callaway and von Baeyer model for thermal conductivity in the presence of point imperfections. These results demonstrate the capability of controlling thermal conductivity via control of anion and cation defect concentrations in a given reducible oxide.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Cation Off-Stoichiometry Leads to High p-Type Conductivity and Enhanced Transparency in Co2ZnO4 and Co2NiO4 Thin Films

We explore the effects of cation off-stoichiometry on structural, electrical, optical, and electronic properties of Co{sub 2}ZnO{sub 4} normal spinel and Co{sub 2}NiO{sub 4} inverse spinel using theoretic and experimental (combinatorial and conventional) techniques, both at thermodynamic equilibrium and in the metastable regime. Theory predicts that nonequilibrium substitution of divalent Zn on nominally trivalent octahedral sites increases net hole density in Co{sub 2}ZnO{sub 4}. Experiment confirms high conductivity and high work function in Co{sub 2}NiO{sub 4} and Zn-rich Co{sub 2}ZnO{sub 4} thin films grown by nonequilibrium physical vapor deposition techniques. High p-type conductivities of Co{sub 2}ZnO{sub 4} (up to 5 S/cm) and Co{sub 2}NiO{sub 4} (up to 204 S/cm) are found over a broad compositional range, they are only weakly sensitive to oxygen partial pressure and quite tolerant to a wide range of processing temperatures. In addition, off-stoichiometry caused by nonequilibrium growth decreases the optical absorption of Co{sub 2}ZnO{sub 4} and Co{sub 2}NiO{sub 4} thin films, although the 500-nm thin films still have rather limited transparency. All these properties as well as high work functions make Co{sub 2}ZnO{sub 4} and Co{sub 2}NiO{sub 4} thin films attractive for technological applications, such as hole transport layers in organic photovoltaic devices or p-type buffer layers in inorganic solar cells.

14 SOLAR ENERGY↗

Chemisorption-induced n-doping of MoS{sub 2} by oxygen

Both chemisorption and physisorption affect the electronic properties of two-dimensional materials, such as MoS{sub 2}, but it remains a challenge to probe their respective roles experimentally. Through repeated in-situ electrical measurements of few-layer MoS{sub 2} field-effect transistors in an ultrahigh vacuum system with well-controlled oxygen partial pressure (6 × 10{sup −8} mbar–3 × 10{sup −7} mbar), we were able to study the effect of chemisorption on surface defects separately from physically adsorbed oxygen molecules. It is found that chemisorption of oxygen results in n-doping in the channel but negligible effect on mobility and on/off ratio of the MoS{sub 2} transistors. These results are in disagreement with the previous reports on p-doping and degradation of the device's performance when both chemisorption and physisorption are present. Through the analysis of adsorption-desorption kinetics and the first-principles calculations of electronic properties, we show that the experimentally observed n-doping effect originates from dissociative adsorption of oxygen at the surface defects of MoS{sub 2}, which lowers the conduction band edge locally and makes the MoS{sub 2} channel more n-type-like as compared to the as-fabricated devices.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Optical characteristics and parameters of gas-discharge plasma in a mixture of mercury dibromide vapor with argon

Results are presented from studies of the optical characteristics and parameters of the plasma of a dielectric barrier discharge in a mixture of mercury dibromide vapor with argon—the working medium of an exciplex gas-discharge emitter. It is established that the partial pressures of mercury dibromide vapor and argon at which the average and pulsed emission intensities in the blue—green spectral region (λ{sub max} = 502 nm) reach their maximum values are 0.6 and 114.4 kPa, respectively. The electron energy distribution function, the transport characteristics, the specific power spent on the processes involving electrons, the electron density and temperature, and the rate constants for the processes of elastic and inelastic electron scattering from the molecules and atoms of the working mixture are determined by numerical simulation, and their dependences on the reduced electric field strength are analyzed. The rate constant of the process leading to the formation of exciplex mercury monobromide molecules for a reduced electric field of E/N = 20 Td, at which the maximum emission intensity in the blue—green spectral region was observed in this experiment, is found to be 8.1 × 10{sup −15} m{sup 3}/s.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Some Fundamental Experiments on Apparent Dissolution Rate of Gas Phase in the Groundwater Recovery Processes of the Geological Disposal System - 12146

The apparent dissolution rates of gas phase in the co-presence of solid phase were examined by in-room experiments in this study. The apparent dissolution rate of gas phase q (mol/m{sup 3}.s) was generally defined by q=aK{sub L}(γP{sub g}-c), where a (1/m) is specific surface area of the interface between gas and liquid phases, K{sub L} (m/s) is overall mass transfer coefficient, γ (mol/(Pa.m{sup 3})) is reciprocal number of Henry constant, P{sub g} (Pa) is partial pressure of gas phase, and c (mol/m{sup 3}) is the concentration of gas component in liquid phase. As a model gas, CO{sub 2} gas was used. For evaluating the values of K{sub L}, this study monitored pH or the migration rate of the interface between water/gas phases, using some experiments such as the packed beds and the micro channel consisting of granite chip and rubber sheet including a slit. In the results, the values of K{sub L} were distributed in the range from 5.0x10{sup -6} m/s to 5.0x10{sup -7} m/s. These values were small, in comparison with that (7.8x10{sup -4} m/s) obtained from the bubbling test where gas phase was continually injected into deionized water without solid phase. This means that the solid phase limits the local mixing of water phase near gas-liquid interfaces. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Influence of annealing temperature on electronic and dielectric properties of ZrO{sub 2} thin films on Si

Zirconium oxide (ZrO{sub 2}) films were deposited on (100) silicon substrates by DC reactive magnetron sputtering of zirconium target at an oxygen partial pressure of 6 Multiplication-Sign 10{sup -2} Pa. The as-deposited films were annealed in air for 1 hour at different temperatures in the range 773 - 1173 K. The influence of annealing temperature on the structural properties of ZrO{sub 2} films and the electrical properties like Capacitance-Voltage and Current-Voltage of the capacitors of the type Al/ZrO{sub 2}/p-Si were studied. The capacitance and dielectric constant of the capacitors were found to increase with increase in annealing temperature from 773 to 973 K, however, with further increase in annealing temperature to 1173 K they were found to decrease. In addition, the leakage current density was decreased from 1 Multiplication-Sign 10{sup -6} to 4 Multiplication-Sign 10{sup -7} A/cm{sup 2} at 1V gate bias voltage and the electrical conduction mechanism was dominated by Schottky emission for all the films in lower electric fields.

36 MATERIALS SCIENCE↗

Synthesis, structural and magnetic characterisation of the fully fluorinated compound 6H-BaFeO{sub 2}F

The compound 6H-BaFeO{sub 2}F (P6{sub 3}/mmc) was synthesised by the low temperature fluorination of 6H-BaFeO{sub 3-d} using polyvinylidenedifluoride (PVDF) as a fluorination agent. Structural characterisation by XRD and NPD suggests that the local positions of the oxygen and fluorine atoms vary with no evidence for ordering on the anion sites. This compound shows antiferromagnetic ordering at room temperature with antiparallel alignment of the magnetic moments along the c-axis. The use of PVDF also allows the possibility of tuning the fluorine content in materials of composition 6H-BaFeO{sub 3-d}F{sub y} to any value of 0<y{<=}1. In addition, the oxygen content, and therefore the iron oxidation state, can be tuned by applying different partial pressures of oxygen during the reaction. - Graphical abstract: The crystal structure of the hexagonal perovskite phase 6H-BaFeO{sub 2}F. Highlights: Black-Right-Pointing-Pointer The crystal structure of the hexagonal perovskite phase 6H-BaFeO{sub 2}F. Black-Right-Pointing-Pointer H-BaFeO{sub 2}F and 6H-BaFeO{sub 3-d}F{sub y} were prepared via low temperature fluorination using PVDF. Black-Right-Pointing-Pointer A structural investigation of the compounds BaFeO{sub 2}F is presented in detail. Black-Right-Pointing-Pointer This analysis suggests differences for the local coordination of O{sup 2-} and F{sup -} anions. Black-Right-Pointing-Pointer H-BaFeO{sub 2}F shows antiferromagnetic ordering at 300 K. Black-Right-Pointing-Pointer The magnetic moments align parallel to the a-axis.

36 MATERIALS SCIENCE↗

Crystal Phases Formed in a CaO-Fe 2 O 3 System Under a High Cooling Rate in Air

A CaO-Fe 2 O 3 system is a fundamental binary system for the iron ore sintering process. Although the basic reactions have been investigated since the 1960s, melting and solidification caused by the combustion of coke results in an unstable state owing to extreme temperature variations. In this study, using a hot thermocouple method, samples of 10 pct CaO-90 pct Fe 2 O 3 and 20 pct CaO-80 pct Fe 2 O 3 were melted on a thermocouple and quenched with several techniques. The obtained samples were precisely examined by XRD. It was found that the sample containing 10 pct CaO-90 pct Fe 2 O 3 changed to 10 pct CaO-13 pct FeO-77 pct Fe 2 O 3 under an oxygen partial pressure (P O 2 ) of 0.21 during melting. For the 10 pct CaO sample, the crystal phases found at a low cooling rate (509 K/s) were WF ss , C 4 WF 8 (C: CaO, W: FeO, F: Fe 2 O 3 ), and C 2 W 4 F 9 . When the sample composition was 20 pct CaO, the precipitated crystal phases were C 4 WF 4 , C 4 F 7 , and C 4 WF 8 . On the other hand, the crystal phases for high cooling rates (1590 and 7900 K/s) with 10 pct CaO were WF ss (solid solution of WF and F), F, and C 2 W 4 F 9 . The formation of the equilibrium phases WF ss , F, C 4 WF 4 , and C 4 WF 8 can be understood by examining the isothermal section of the phase diagrams, while the unstable phases C 2 W 4 F 9 and C 4 F 7 are discussed on the basis of the reactions under an equilibrium state.

36 MATERIALS SCIENCE↗

Phase Equilibria in the ZnO-“FeO”-SiO{sub 2} System in Reducing Atmosphere and in the ZnO-“FeO”-SiO{sub 2}-“Cu{sub 2}O” System in Equilibrium with Liquid Copper Metal at 1250 °C (1523 K)

Recent experimental studies in the ZnO-“FeO”-SiO{sub 2} system in reducing atmosphere demonstrated significant discrepancies with the current FactSage thermodynamic model developed using previous experimental data in this system in equilibrium with metallic iron and air. The present experimental study on phase equilibria in the ZnO-“FeO”-SiO{sub 2}-“Cu{sub 2}O” system in equilibrium with liquid copper at 1250 °C (1523 K) at low copper oxide concentrations in slag was initiated and undertaken to resolve these discrepancies. A high-temperature equilibration–rapid quenching–electron-probe X-ray microanalysis (EPMA) technique using a primary phase substrate support and closed system approach with Cu metal introduced to determine effective equilibrium oxygen partial pressure from the Cu{sub metal}/Cu{sub 2}O{sub slag} equilibria was applied to provide accurate information on the liquidus and corresponding solid compositions in the spinel, willemite, and tridymite primary phase fields. The present results confirmed the accuracy of the FactSage model, resolved discrepancies, and demonstrated significant uncertainties in the recent studies by other authors on the system in the open reducing atmosphere. The present study shows how this closed system approach can be used to obtain key thermodynamic data on phase equilibria in systems containing volatile metal species, overcoming the limitations and uncertainties encountered in conventional open gas/condensed phase equilibration with these systems. The study highlights the importance of the focus on obtaining accurate experimental data and the risks of misleading information from inadequate experimental control and analysis. The study also demonstrates that continuing in-depth critical review and analysis of the elemental reactions taking place in complex systems is an essential step in phase equilibrium research.

36 MATERIALS SCIENCE↗

Reduction of Crosshatch Roughness and Threading Dislocation Density in Metamorphic GaInP Buffers and GaInAs Solar Cells

Surface crosshatch roughness typically develops during the growth of lattice-mismatched compositionally graded buffers and can limit misfit dislocation glide. In this study, the crosshatch roughness during growth of a compressive GaInP/GaAs graded buffer is reduced by increasing the phosphine partial pressure throughout the metamorphic growth. Changes in the average misfit dislocation length are qualitatively determined by characterizing the threading defect density and residual strain. The decrease of crosshatch roughness leads to an increase in the average misfit dislocation glide length, indicating that the surface roughness is limiting dislocation glide. Growth rate is also analyzed as a method to reduce surface crosshatch roughness and increase glide length, but has a more complicated relationship with glide kinetics. Using knowledge gained from these experiments, high quality inverted GaInAs 1 eV solar cells are grown on a GaInP compositionally graded buffer with reduced roughness and threading dislocation density. The open circuit voltage is only 0.38 V lower than the bandgap potential at a short circuit current density of 15 mA/cm{sup 2}, suggesting that there is very little loss due to the lattice mismatch.

14 SOLAR ENERGY↗

Genesis of a Cerium Oxide-Supported Gold Catalyst for CO Oxidation: Transformation of Mononuclear Gold Complexes into Clusters as Characterized by X-Ray Absorption Spectroscopy

CeO{sub 2}-supported mononuclear gold species synthesized from Au(CH{sub 3}){sub 2}(acac) catalyzed CO oxidation at 353 K, with a turnover frequency of 6.5 x 10{sup -3} molecules of CO (Au atom s){sup -1} at CO and O{sub 2} partial pressures of 1.0 and 0.5 kPa, respectively. As the catalyst functioned in a flow reactor, the activity increased markedly so that within about 10 h the conversion of CO had increased from about 1% to almost 100%. Activated catalyst samples were characterized by X-ray absorption spectroscopy and found to incorporate clusters of gold, which increased in size, undergoing reduction, with increasing time of operation. The X-ray absorption near-edge structure spectrum of the catalyst used for the longest period was indistinguishable from that characterizing gold foil. Extended X-ray absorption fine structure data characterizing the catalyst after the longest period of operation indicated the presence of clusters of approximately 30 Au atoms each, on average. The evidence that the catalytic activity increased as the clusters grew is contrasted with earlier reports pointing to increasing activity of supported gold clusters as they were made smallerin a cluster size range largely exceeding ours.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

On the influence of the char gasification reactions on NO formation in flameless coal combustion

Flameless combustion is a well known measure to reduce NO{sub x} emissions in gas combustion but has not yet been fully adapted to pulverised coal combustion. Numerical predictions can provide detailed information on the combustion process thus playing a significant role in understanding the basic mechanisms for pollutant formation. In simulations of conventional pulverised coal combustion the gasification by CO{sub 2} or H{sub 2} O is usually omitted since its overall contribution to char oxidation is negligible compared to the oxidation with O{sub 2}. In flameless combustion, however, due to the strong recirculation of hot combustion products, primarily CO{sub 2} and H{sub 2} O, and the thereby reduced concentration of O{sub 2} in the reaction zone the local partial pressures of CO{sub 2} and H{sub 2} O become significantly higher than that for O{sub 2}. Therefore, the char reaction with CO{sub 2} and H{sub 2} O is being reconsidered. This paper presents a numerical study on the importance of these reactions on pollutant formation in flameless combustion. The numerical models used have been validated against experimental data. By varying the wall temperature and the burner excess air ratio, different cases have been investigated and the impact of considering gasification on the prediction of NO formation has been assessed. It was found that within the investigated ranges of these parameters the fraction of char being gasified increases up to 35%. This leads to changes in the local gas composition, primarily CO distribution, which in turn influences NO formation predictions. Considering gasification the prediction of NO emission is up to 40% lower than the predicted emissions without gasification reactions being taken into account. (author)

01 COAL, LIGNITE, AND PEAT↗

Treatment of municipal landfill leachate by catalytic wet air oxidation: Assessment of the role of operating parameters by factorial design

Highlights: > Landfill leachates can be treated effectively by catalytic wet oxidation. > Addition of H{sub 2}O{sub 2} in the presence of transition metals promotes degradation. > Factorial design evaluates the statistically significant operating conditions. > H{sub 2}O{sub 2}, reaction time and temperature are critical in determining performance. - Abstract: The wet air oxidation (WAO) of municipal landfill leachate catalyzed by cupric ions and promoted by hydrogen peroxide was investigated. The effect of operating conditions such as WAO treatment time (15-30 min), temperature (160-200 deg. C), Cu{sup 2+} concentration (250-750 mg L{sup -1}) and H{sub 2}O{sub 2} concentration (0-1500 mg L{sup -1}) on chemical oxygen demand (COD) removal was investigated by factorial design considering a two-stage, sequential process comprising the heating-up of the reactor and the actual WAO. The leachate, at an initial COD of 4920 mg L{sup -1}, was acidified to pH 3 leading to 31% COD decrease presumably due to the coagulation/precipitation of colloidal and other organic matter. During the 45 min long heating-up period of the WAO reactor under an inert atmosphere, COD removal values up to 35% (based on the initial COD value) were recorded as a result of the catalytic decomposition of H{sub 2}O{sub 2} to reactive hydroxyl radicals. WAO at 2.5 MPa oxygen partial pressure advanced treatment further; for example, 22 min of oxidation at 200 deg. C, 250 mg L{sup -1} Cu{sup 2+} and 0-1500 mg L{sup -1} H{sub 2}O{sub 2} resulted in an overall (i.e. including acidification and heating-up) COD reduction of 78%. Amongst the operating variables in question, temperature had the strongest influence on both the heating-up and WAO stages, while H{sub 2}O{sub 2} concentration strongly affected the former and reaction time the latter. Nonetheless, the effects of temperature and H{sub 2}O{sub 2} concentration were found to depend on the concentration levels of catalyst as suggested by the significance of their 3rd order interaction term.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Influence of plasma-generated negative oxygen ion impingement on magnetron sputtered amorphous SiO{sub 2} thin films during growth at low temperatures

Growth of amorphous SiO{sub 2} thin films deposited by reactive magnetron sputtering at low temperatures has been studied under different oxygen partial pressure conditions. Film microstructures varied from coalescent vertical column-like to homogeneous compact microstructures, possessing all similar refractive indexes. A discussion on the process responsible for the different microstructures is carried out focusing on the influence of (i) the surface shadowing mechanism, (ii) the positive ion impingement on the film, and (iii) the negative ion impingement. We conclude that only the trend followed by the latter and, in particular, the impingement of O{sup -} ions with kinetic energies between 20 and 200 eV, agrees with the resulting microstructural changes. Overall, it is also demonstrated that there are two main microstructuring regimes in the growth of amorphous SiO{sub 2} thin films by magnetron sputtering at low temperatures, controlled by the amount of O{sub 2} in the deposition reactor, which stem from the competition between surface shadowing and ion-induced adatom surface mobility.

36 MATERIALS SCIENCE↗

SU-E-T-770: Tumor Control in Ion Beam Radiotherapy with Different Ions in Presence of Hypoxia

Purpose: The reduced concentration of oxygen in cells (hypoxia) results in a lower cell death rate after irradiation that can lead to treatment failure. The effect can be expressed by the oxygen enhancement ratio (OER). So far, only few attempts to include OER in treatment planning for ion beam therapy were made, which are based on the dose averaged LET estimates and do not distinguish among ion species and fractionation schemes. To overcome these limitations, we implemented a new OER model and used it to estimate tumor control in clinical cases. Methods: The model, based on the microdosimetric kinetic model, was benchmarked with in-vitro data from different ions irradiation. It was included in the simulation of treatments of a set of clinical cases (glioblastoma) using p, Li, He, C and O ion beams. Tumor Control Probability (TCP) was estimated as a function of oxygen partial pressure, dose per fraction and primary ion type. Results: The modelized OER was found to be strongly dependent on both LET and ion type, and showed a decreasing OER for increasing dose per fraction with a slope that depends on the LET and ion type, in good agreement with the experimental data. In the clinical cases studied, an increase in TCP by increasing ion charge and dose per fraction (more than 30% variation from p to O for moderate hypoxia) was found. Higher OER decrease rates as function of dose per fraction were found for lighter ions (up to 20% varying from 2 to 8 Gy(RBE)). Conclusions: A novel modeling of the OER that explicitly includes the dependence on ion type and dose per fraction was implemented. The model was exploited to evaluate the impact of hypoxia in ion beam radiotherapy, facilitating the identification of the treatment condition optimality, including fractionation scheme and ion type.

60 APPLIED LIFE SCIENCES↗