Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “JOINING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 721 records · Page 40

Grain structure, texture and mechanical property evolution of automotive aluminium sheet during high power ultrasonic welding

High power ultrasonic spot welding (HPUSW) is a joining technique which is performed within less than a second and provides a more energy-efficient alternative to friction stir spot welding (FSSW), which is considered a longer cycle manufacturing process for joining automotive alloys. To date, only a few reports exist on the deformation mechanisms that take place during high power ultrasonic spot welding. In this work, dynamic recrystallization and grain growth were examined using electron backscatter diffraction (EBSD). HPUSW causes extensive deformation within the weld zone where the temperature increases to 440 °C. An ultra-fine grain structure was observed in a thin band of flat weld interface within a short welding time of 0.10 s. With increasing welding time the interface was displaced and ‘folds’ or ‘crests’ appeared together with shear bands. The weld interface progressively changed from flat to sinusoidal and eventually to a convoluted wave-like pattern when the tool fully penetrated the workpiece, having a wavelength of ~ 1 mm after 0.40 s. Finally, the microstructure and texture varied significantly depending on the location within the weld. Although the texture near the weld interface was relatively weak, a shift was observed with increasing welding time from an initially Cube-dominated texture to one where the typical β-fibre Brass component prevailed. - Highlights: •Lap shear strength of ~2.9 kN was achieved in 0.30 sec welding time. •Temperature approached 440 °C along the weld centreline for the highest welding time. •The texture near the teeth was dominated by Brass, P and S components at optimum condition. •The weld interface showed typical β-fibre deformation texture at optimum condition.

36 MATERIALS SCIENCE↗

Microstructure, mechanical properties and microtexture of friction stir welded S690QL high yield steel

Two try-out campaigns of friction stir welding (FSW) were performed with different friction parameters to join S690QL high yield strength steel. The welds were investigated at macroscopic and microscopic scales using optical and electronic microscopy and microhardness mapping. Welds of the second campaign exhibit microstructures and mechanical properties in accordance with requirements for service use. Microtexture measurements were carried out in different zones of welds by electron backscattered diffraction (EBSD). It is shown that that texture of the bottom of the weld is similar to that of the base metal, suggesting a diffusion bonding mechanism. Finally, the mechanical properties (tensile strength, resilience, bending) were established on the most promising welds. It is shown that it is possible to weld this high yield strength steel using FSW process with satisfactory geometric, microstructural and mechanical properties. - Highlights: •1000 mm ∗ 400 mm ∗ 8 mm S690QL steel plates are joined by friction stir welding (FSW). •Maximum hardness is reduced by optimization of process parameters. •Various microstructures are formed but no martensite after process optimization. •Texture is modified in mechanically affected zones of the weld. •Texture in the bottom of the weld is preserved, suggesting diffusion bonding.

36 MATERIALS SCIENCE↗

Microstructure evolution and mechanical characterization of Nd:YAG laser beam welded titanium tubes

Highlights: • Joining of thin titanium tubes using laser beam welding. • Fusion zone exhibited coarse granular like grains with serrated and irregular boundaries. • Large spherical and irregular shape pores were observed at lower welding speeds. • Misorientation angle distribution indicated substructure boundaries along with single β grain formation from double α grains. • Fusion zone strengthened by substructure boundaries, solid solution strengthening and dislocation density. - Abstract: Grade 2 titanium tubes of outer diameter 60 mm and wall thickness 3.9 mm were effectively joined by Nd:YAG laser. The welding speed was varied in five levels (2.50, 2.75, 3.00, 3.25 and 3.50 m/min). The microstructure evolution was studied using optical microscopy and advanced characterization techniques. The bead geometry changed from parallel shape to wedge shape with increased welding speed due to changes in surface tension. The macrographs showed three zones namely fusion zone, heat affected zone (HAZ) and base metal. Coarse granular structure with irregular and serrated contours was observed in the fusion zone. Acicular α grains were observed at the extreme outer edge of the fusion zone due to rapid cooling. Spherical and irregular shaped pores were observed near the centerline of the fusion zone at lower welding speeds due to large amount of entrapped gases and downward sweeping solidification front. The grain size decreased with increased welding speed due to higher cooling rate. The misorientation angle distribution map showed three distinct regions. The increase in welding speed caused an increase in low angle boundaries and a reduction in very high angle boundaries. High density of dislocations was observed in the fusion zone due to thermal stresses caused by solidification. The microhardness of the fusion zone was recorded to be higher than base metal due to substructure boundaries, solute elements and dislocations. The increase in welding speed shifted the fracture location from fusion zone to base metal and fracture mode from brittle to ductile.

36 MATERIALS SCIENCE↗

Micro-structural evolution during diffusion bonding of C-SiC/C-SiC composite using Ti interlayer

Highlights: • Formation of Ti{sub 3}SiC{sub 2} MAX phase in the joint of C-SiC composite • EBSD revealed three zone microstructure of the joint • Formation of a thin continuous layer of TiSi{sub 2} • The apparent shear strength of 19 MPa - Abstract: Diffusion bonding of C-SiC composite was achieved with Ti interlayer at 1500 °C for 3 h with the applied pressure of 20 MPa. The joined C-SiC composite showed the apparent shear strength of 19 MPa and the sample fractured away from the joint. The microstructure of joint consists of Ti{sub 3}SiC{sub 2} MAX phase, TiSi{sub 2} and TiC in which Ti{sub 3}SiC{sub 2} was the major phase. The distribution of phases in the microstructure of joint was categorized into three different zones based on electron backscattered diffraction (EBSD) results. The first zone consists of a thin continuous TiSi{sub 2} phase, which was followed by a thick zone of Ti{sub 3}SiC{sub 2} MAX phase. In the middle of the sample, a mix phase zone was found. The reaction mechanism was established for the evolution above microstructure of joined C-SiC composite.

36 MATERIALS SCIENCE↗

Microstructures and mechanical properties of the welded AA5182/HC340LA joint by magnetic pulse welding

Highlights: • The magnetic pulse welding of 5× aluminum alloy with high strength steel is performed. • The microstructure evolution of welding interface under different parameters is investigated. • The intermediate layer is characterized by high-resolution transmission electron microscope and electron diffraction pattern. - Abstract: Magnetic pulse welding (MPW) is an innovative joining technology for dissimilar materials. The MPW with high joining qualities could be realized between high strength steel and 5× aluminum alloys. In this work, the MPW joints between aluminum alloy (AA 5182) sheet and high-strength low alloy steel (HC340LA) sheet were prepared under various discharge energies. The mechanical properties and microstructure observations were employed to evaluate the joint performance. Results showed that a lower discharge voltage tended to cause joints with poor quality. When the discharge energy increased, the failure position gradually changed from the weld zone to the weaker base metal (Al) during quasi-static tensile tests. In addition, the effect of discharge energies on microstructure evolution in the intermediate layer was revealed by high-resolution transmission electron microscopy (HRTEM) and scanning electron microscope (SEM). Atomic-scale diffusion was found to be the mainly welding mechanism of the Al/Fe joint. The intermetallic compound (IMC) FeAl{sub 2} and ultra-fine grains (UFG) were found in the intermediate layer under high discharge energy.

36 MATERIALS SCIENCE↗

Interfacial bonding mechanism and mechanical properties of micro friction stir blind riveting for multiple Cu/Al ultra-thin layers

Highlights: • Micro Friction Stir Blind Riveting is developed for joining multilayer ultra-thin dissimilar materials. • Interfacial bonding mechanism for different interfaces is identified. • Proposed technique offers better mechanical performance than conventional micro riveting process. • The relationship between each interfacial bonding mechanism and improved mechanical property is elucidated. - Abstract: In this research, bonding mechanisms and mechanical properties were investigated for a newly developed multilayer dissimilar material joining technique, micro friction stir blind riveting (viz. μFSBR), where the multilayer micro joint was made consisting of one Cu layer and three Al layers (each layer having 0.203 mm thickness) connected through Al rivet. Different microscopy techniques were employed (i.e. scanning electron microscopy and transmission electron microscopy) to unearth the bonding mechanisms of the three interfaces (i.e. Al rivet and Cu sheet interface, Cu sheet and Al sheet interface, and Al rivet and Al sheet interface) which revealed intricate yet distinct bonding phenomenon for each interface. A nano-scale diffusion layer in addition to two-way material flow consequential heterogeneous lamellar structures and mechanical interlocking was formed at the Al rivet and Cu sheet interface; Cu particles diffused into a non-uniform thickness thin oxide layer at the Cu sheet and Al sheet interface; and Al sheet experienced grain refinement near the interface close to Al rivet with a nano-scale gap. These observations revealed that both mechanical and metallurgical bonding occurred simultaneously in μFSBR. The formation of different bonding mechanisms resulted in superior bonding strength and absorbed energy compared to conventional micro blind riveting joints, which was further confirmed through layer by layer tensile tests.

36 MATERIALS SCIENCE↗

Cascading microstructures in aluminum-steel interfaces created by impact welding

With the rising need to develop light weight structures joining dissimilar metals is inevitable. Thus a fundamental understanding of the microstructure evolution and bond formation mechanism is necessary. In this work we probe the welded interface in aluminum and steel joined using vaporizing foil actuator welding (VFAW) a novel impact welding process. The goal of such a detailed characterization campaign is to understand the bond formation mechanism. The study demonstrates that the interfacial microstructure has a pronounced hierarchical nature. At the macro scale, the interface is characterized by a wavy interface which is a result of extensive plastic deformation that accompanies the process. Detailed transmission electron microscopy shows evidence for the formation of a liquid film at the interface resulting in significant inter diffusion of Fe. The solidified structure at the interface consisted of crystalline α-Al and an amorphous metastable Al-Fe intermetallic compound similar to the observations in rapid solidification of Al-Fe alloys. The sub-nm scale characterization of the interface using atom probe tomography showed two distinct zones 1. A magnesium (5 at.%) and oxygen (15 at.%) rich (not detectable using energy dispersive spectroscopy) which was probably from the decomposition of the surface oxide film 2. The rapidly solidified reaction zone consisting of primary crystalline α-Al and an amorphous Al-Fe (15 at.%)-O (0.5 at.%)-Si (1.5 at.%).Based on these observations a mechanism for the bond formation is presented.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of friction stir welded Haynes 282

Advanced ultrasupercritical (A-USC) steam plants are designed to operate at high temperatures and pressures due to the necessity for higher operational efficiency. The extreme operating conditions of A-USC requires the deployment of precipitation strengthened Ni-base alloys that exhibit elevated temperature strength and good fabricability. Fusion welding of precipitation strengthened nickel alloys lead to solidification cracking in fusion zone and/or liquation cracking in heat affected zone. Therefore, an alternative non-melting welding technique is a necessity to efficiently join nickel alloys. In the current study, friction stir welding, a solid state joining technique was implemented on a precipitation strengthened nickel-based superalloy, Haynes 282. Detailed microstructural and mechanical properties characterization was carried out. The processed region exhibited wrought, fine-grained microstructure, absence of weld defects such as voids and cracks and absence of elemental segregation. Both hardness and cross-weld tensile tests demonstrated that the weld region was stronger than the base material. And the cross-weld tensile samples failed in the base material. Based on joint efficiency analysis, friction stir welded Haynes 282 outperformed fusion welds.

36 MATERIALS SCIENCE↗

Direct diffusion bonding of Ti{sub 3}SiC{sub 2} and Ti{sub 3}AlC{sub 2}

Two typical layered ternary compounds, Ti{sub 3}SiC{sub 2} and Ti{sub 3}AlC{sub 2}, were joined directly by solid-state diffusion bonding method. By various bonding tests at 1100-1300 deg. C for 30-120 min under 10-30 MPa, and characterizing the microstructure and diffusion reactive phases of the joints by scanning electron microscopy (SEM), energy dispersive X-ray spectrometer (EDS), transmission electron microscopy (TEM) and X-ray diffraction (XRD), the optimal condition for direct joining of Ti{sub 3}SiC{sub 2} and Ti{sub 3}AlC{sub 2} was obtained. Strong joints of Ti{sub 3}SiC{sub 2}/Ti{sub 3}AlC{sub 2} can be achieved via diffusion bonding, which is attributed to remarkable interdiffusion of Si and Al at the joint interface. The shear strength of the Ti{sub 3}SiC{sub 2}/Ti{sub 3}AlC{sub 2} joints was determined.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of joints in sintered SiC fiber-bonded ceramics brazed with Ag Cu Ti alloy

Active metal brazing of a new high thermal conductivity sintered SiC-polycrystalline fiber-bonded ceramic (SA-Tyrannohexs) has been carried out using a Ti-containing Ag Cu active braze alloy (Cusil-ABAs). The brazed composite joints were characterized using scanning electron microscopy coupled with energy-dispersive X-ray spectrometry (SEM EDS). The results show that this material can be successfully joined using judiciously selected off-the shelf active braze alloys to yield metallurgically sound joints possessing high integrity. Uniform and continuous joints were obtained irrespective of differences in the fiber orientation in the substrate material. Detailed interfacial microanalysis showed that the titanium reacts with C and Si to form TiC layer and a Ti Si compound, respectively. Furthermore, the evaluation of shear strength of the joints was also conducted at ambient and elevated temperatures in air using the single-lap offset (SLO) shear test. The perpendicular-type SA-Tyrannohex joints exhibited apparent shear strengths of about 42 MPa and 25 MPa at 650 1C and 750 1C, respectively. The fracture at the higher temperature occurred at the interface between the reactionformed TiC layer and braze. This might be caused by generation of stress intensity when a shear stress was applied, according to m-FEA simulation results.

Singh, Mrityunjay↗

Investigations on the multiple-sector hard-copper X-band accelerating structures

The development of advanced, high gradient accelerating structures is one of the leading activity of the particle accelerator community. In the technological research of new construction methods for these devices, high-power testing is a critical step for the verification of their viability. Recent experiments showed that accelerating cavities made out of hard copper, fabricated without high-temperature processes, can achieve better performance as compared with soft copper ones. Recently, we have built cavities using Tungsten Inert Gas welding and the high-power experiments confirmed that this joining process is a robust and low-cost alternative to brazing or diffusion bonding. This is a good solution for high-gradient operation, with a gradient of about 150 MV/m in X-band, at a breakdown rate of 10 -3 /pulse/meter using a shaped RF pulse with a 150 ns flat part. We continue the design, construction and high power tests of three-cells standing-wave X-band accelerating cavities fabricated with a split-open geometry, made of hard copper and vacuum-sealed by welding. Our aim is the fabrication of accelerating structures made out of hard copper alloys by using innovative cost-effective technologies. Moreover, our method of multiple-sector structures opens the way to new technological approaches and design methods, for example providing the possibility of placing dampers of the parasitic higher-order modes. Such structures with dampers allow for acceleration of multi-bunch beams, both in standing and in travelling-wave accelerating modality. Here, this paper describes the design of two cavities made of multiple sectors that were fabricated at the Italian Institute for Nuclear Physics in Frascati, Italy (INFN-LNF), assembled by means of clamping and then joined with the Tungsten Inert Gas welding in order to preserve the hardness of the metal. These are three-cell standing-wave X-band accelerating cavities, to be operated in the π-mode. We report the low-power RF tests of the first one, made of two halves, and the RF design of the second one, made of four quadrants. Both structures were built for high-gradient tests at SLAC National Accelerator Laboratory.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Ultra-pure nickel for structural components of low-radioactivity instruments

The next generation of nuclear and particle physics rare-event search experiments demand structural materials combining ultra-low levels of radioactive contamination with exceptional mechanical strength. Here, this study evaluates chemical vapor deposition (CVD) nickel as a low radioactive background candidate structural material for such applications. Manufacturer-supplied CVD Ni grown on aluminum substrates was assayed via inductively coupled plasma mass spectrometry (ICP-MS) employing isotope-dilution. These material assays produced measured bulk concentration of 232 Th, 238 U, and nat K at the levels of ~70 ppq, ≲100 ppq, and ~900 ppt, respectively, which is the lowest reported in nickel. Surface-etch profiling uncovered higher concentrations of these contaminants extending ~10 μ m beneath the surface, likely associated with the aluminum growth substrate. Additionally, the CVD Ni underwent tensile testing alongside standard Ni samples. CVD Ni exhibited a planar tensile strength of ~600 MPa, significantly surpassing standard nickel. However, heat treatment was found to reduce the tensile strength to levels comparable to standard Ni, with implications for high-temperature weld joining methods. The results reported are compared to the one other well documented usage of CVD Ni in a low radioactive background physics research experiment and a discussion is provided on how the currently reported results may arise from changes in CVD fabrication or testing process. These results establish CVD Ni as a promising low-radioactivity structural material, while outlining the need for further development in surface cleaning and weld-joining techniques to fully realize its potential in large-scale, low radioactive background rare-event search experiments.

47 OTHER INSTRUMENTATION↗

Friction stir spot welding of hot-stamped boron steel

Hot-stamped, boron steel was successfully joined via friction stir spot welding using polycrystalline cubic boron nitride tooling. The resulting microstructure, microhardness and mechanical properties are reported, including a brief look into failure mechanisms. Relationships between the unique mechanical mixing, phase transformations and failure initiation sites associated with joining martensitic steels are characterized.

boron steel↗

Development of nanosized lanthanum strontium aluminum manganite as electrodes for potentiometric oxygen sensor

Nanocrystalline La 0.8 Sr 0.2 Al 0.9 Mn 0.1 O 3 (LSAM) was synthesized by a microwave-assisted citrate method, and characterized by electron microscopy and X-ray diffraction. Electrical behavior of LSAM was investigated by impedance spectroscopy and activation energy of conduction was obtained. Joining of sintered bodies of LSAM and yttria-stabilized tetragonal zirconia polycrystals (YTZP), an extensively studied oxygen ion conducting electrolyte, was examined by isostatic hot pressing methods. Characteristics of the joining region were evaluated with microprobe Raman spectroscopy, and products formed at the interface, primarily strontium zirconate, was confirmed by examination of high temperature chemical reaction between LSAM and YTZP powders. Finally, the electrical properties of the LSAM were exploited for development of a high temperature oxygen sensor in which LSAM functioned as the electrode and YTZP as electrolyte.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Obama quickly signals He means business on Green issues

President Obama has indicated that the U.S. will join the international community to find a resolution to the critical issue of climate change, but has made it clear that all major emitters must join the effort for it to be effective. The US is likely to agree to cut its emissions by 80 percent by 2050. The toughest task will be to convince a reluctant U.S. Congress to agree to comprehensive carbon legislation and to abide by any agreements reached in Copenhagen. Companies investing in such goods and services as coal-fired power plants and gas guzzling cars could start to incur heavy economic penalties in the near future for their greenhouse gas output.

29 ENERGY PLANNING, POLICY, AND ECONOMY↗

Native Chemical Ligation of Peptoid Oligomers

Bioorganic chemists are inspired by natural biopolymers to design peptidomimetic oligomers that can exhibit sequence-structure-function relationships. Biomimetic polymers can be synthesized to incorporate a specific sequence of nonbiological monomer units using a variety of iterative solution-phase or solid-phase reaction schemes. These protocols generally provide access to a vast diversity of oligomeric compounds but are limited with respect to their ability to attain protein-like chain lengths. This constraint can preclude access to sequence-defined synthetic macromolecules with sufficient sizes required to exhibit tertiary structure and other protein-mimetic attributes. In contrast, peptide chemists have overcome this limitation by developing convergent synthetic methods, such as native chemical ligation, to join individual, smaller peptide chains together to make larger peptides or full proteins. A similar convergent approach is needed to establish efficient synthetic routes to non-natural sequence-defined macromolecules. Herein, we adapt the peptide native chemical ligation method to peptoid oligomers, demonstrating how short chains can be conjoined to create sequence-defined peptoid macromolecules. Nanosheet-forming peptoid polymers with distinct surface loop display domains were generated by sequential ligation of several discrete fragments. This method provides a reliable convergent ligation route for sequence-defined polypeptoids that results in a native amide bond joining the fragments. We envision that this strategy will be useful in synthesizing peptoid-based proteomimetics that incorporate diverse chemical features.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A pathway for the growth of core-shell Pt-Pd nanoparticles

In this study, the aging of both Pt-Pd nanoparticles and core-shell Pt-Pd nanoparticles has been reported to result in alloying of Pt with Pd. In comparison to monometallic Pt catalysts, the growth of Pd-Pt bimetallics is slower; however, the mechanism of growth of particles and the mechanism by which Pd improves the hydrothermal durability of bimetallic Pd-Pt particles remains uncertain. In our work on hydrothermal aging of core-shell Pt-Pd nanoparticles, synthesized by solution methods, with varying Pd:Pt ratio of 1:4, 1:1, and 4:1, we compare the growth of core-shell Pt-Pd nanoparticles and find that particles grow by migrating and joining together. The unique feature of the observed growth is that Pd shells from both particles open up and join, allowing the cores to merge. At high temperatures, alloying occurs in good agreement with reports by other workers.

77 NANOSCIENCE AND NANOTECHNOLOGY↗