Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CHROMIUM ALLOY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 721 records · Page 40

Effects of composition and testing conditions on oxidation behavior of four cast commercial nickel-base superalloys

Four cast nickel-base superalloys were oxidized at 1000 and 1100 C for times up to 100 hr in static air and a Mach 1 gas stream. The oxidation resistance was judged by weight change, metal thickness loss, depletion-zone formation, and oxide formation and morphology. The alloys which formed mostly nickel aluminate (NiAl2O4) and aluminum oxide (Al2O3) (B-1900, VIA, and to a lesser extent 713C) were more oxidation resistant. Poorer oxidation resistance was associated with the appearance of chromium sesquioxide (Cr2O3) and chromite spinel (738X). Refractory metal content had little effect on oxidation resistance. Refractory metals appeared in the scale as tapiolite (NiM2O6, where M represents the refractory metal). Thermal cycling in static air appeared to supply sufficient data for the evaluation of oxidation resistance, especially for alloys which form oxides of low volatility. For alloys of higher chromium levels with high propensities toward forming a chromium-bearing scale of higher volatility, testing under conditions of high gas velocity is necessary to assess fully the behavior of the alloy.

Lowell, C. E.↗

First-principles insights into chromium-induced oxide phases in NiO

The high-temperature oxidation of Ni–Cr alloys leads to complex oxide scales comprising Ni(Cr)O solid solutions, NiCr 2 O 4 spinel, and Cr 2 O 3 corundum within the NiO matrix. Understanding the atomic-scale mechanisms of Cr segregation and precipitate formation is crucial for enhancing oxidation resistance. Here, we employ density functional theory calculations to investigate Cr behavior on NiO(100), (110), and (111) surfaces and in the bulk. Our results reveal that isolated Cr atoms preferentially segregate to the surfaces, stabilizing Ni(Cr)O solid solutions via strong Cr–O bonding, whereas Cr pairs and clusters favor subsurface migration and bulk aggregation, promoting nucleation of NiCr 2 O 4 and Cr 2 O 3 phases. These findings elucidate a size-dependent segregation mechanism linking Cr coordination environments to oxide phase evolution. This atomic-scale insight informs strategies to tailor oxide microstructures and enhance the high-temperature oxidation resistance of Ni–Cr alloys.

Chromium Segregation↗

Hydrogen and water interactions with CrMnFeCoNi alloy from density functional theory calculations

High entropy alloys (HEAs) are a promising class of materials with remarkable mechanical and catalytic properties. Among these, the quinary CrMnFeCoNi alloy (also called “Cantor alloy”) has attracted considerable attention given its thermodynamic stability and remarkable mechanical properties under different temperatures. Given that various degradation mechanisms involve multiple contaminants, such as hydrogen and water in hydrogen embrittlement and surface poisoning, respectively, understanding their interactions with the Cantor alloy is critical for its practical applications as structural, nuclear, or hydrogen storage material. In this work, we perform first-principles calculations based on Density Functional Theory (DFT) to investigate such interactions when considering various microstructures, including bulk materials and those containing certain defects, such as grain boundaries, stacking faults, and vacancies. We also employ Global Sensitivity Analysis to identify the importance of different factors in the stability of the impurities. We find that the accuracy of the H formation energy is significantly affected by spin polarization and chemical short-range order. The study also identifies a strong tendency for hydrogen interstitials to segregate to Σ5(210)/[001] symmetric tilt grain boundary, even when H concentrations are high, suggesting that a certain type of grain boundaries acts as H sinks within the alloy. Further, this result is reinforced by the low formation energy of vacancy-hydrogen complexes, which can contain multiple hydrogen atoms. Finally, the surface reactivity analysis reveals that the adsorption energy of oxygen and hydroxyl groups is highly sensitive to the specific metal atom involved in the binding, with a clear preference for chromium atoms, which could have implications for the alloy’s oxidation and corrosion behavior.

36 MATERIALS SCIENCE↗

Ab-initio investigation of the effect of adsorbed salts on segregation of Cr at the Ni (100) surface

The dissolution and depletion of chromium (Cr) in salt facing nickel (Ni) alloy surfaces is one of the predominant degradation mechanisms of structural components in molten salt technology. Here, we use density functional theory to investigate the role of electronic level interactions that may underlie the depletion phenomenon of Cr in a Ni (100) surface exposed to various adsorbed salt species. Our results show that, under vacuum, Ni preferentially segregates to the surface layer. Conversely, in the presence of adsorbed anionic salt species (e.g., chlorine (Cl), fluorine (F) or the impurity oxygen (O)) Cr segregation becomes more favorable. In these cases, Cl has the weakest effect on segregation, while O has the strongest effect. Our analysis reveals the strong correlation between Cr segregation and the amount of valence charge transferred between the Cr atom and surface adsorbate: the greater the charge transfer, the lower the segregation energy. We also show that, when considered, secondary cations screen Cr-anion interactions, which in turn reduce the magnitude of the anions effect on segregation. These results shed light on the role of salt impurities likely play in the overall corrosion phenomena in molten salt environments. This work provides insights into the atomic level interactions fundamental to molten salt corrosion and on the importance of maintaining salt purity.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Coolant Compatibility Studies for Fusion and Fusion-Fission Hybrid Reactor Concepts: Corrosion of Oxide Dispersion Strengthened Iron-Chromium Steels and Tantalum in High Temperature Molten Fluoride Salts

Alloys such as 12YWT & 14YWT have exceptional high-temperature strength at temperatures greater than 550 C. This class of materials has also demonstrated relatively little radiation induced swelling at damage levels of at least 75 dpa in sodium-cooled fast reactors. However, corrosion of oxide dispersion strengthened (ODS) steels in high temperature molten fluoride salts may limit the life of advanced reactor systems, including some fusion and fusionfission hybrid systems that are now under consideration. This paper reports corrosion studies of ODS steel in molten fluoride salts at temperatures ranging from 600 to 900 C. Electrochemical impedance spectroscopy (EIS) was used to measure the temperature dependence of charge transfer kinetics in situ, while an environmental electron microscope (ESEM) equipped with energy dispersive spectroscopy (EDS) was used for postexposure examination of test samples. ODS steel experienced corrosion in the molten fluoride salts at 550 to 900 C, even in carefully controlled glove-box environments with very low levels of oxygen and moisture. The observed rate of attack was found to accelerate dramatically at temperatures above 800 C. Tantalum and tantalum-based alloys such as Ta-1W and Ta-10W have exceptional high temperature strength, far better than ODS steels. Unlike ODS steels, tantalum has been found to exhibit some immunity to corrosive attack by molten fluoride salts at temperatures as high as 900 C, though there is some indication that grain boundary attack may have occurred. Unfortunately, tantalum alloys are known to become brittle during irradiation and exposure to hydrogen, both of which are important in fusion applications.

36 MATERIALS SCIENCE↗

Corrosivity Screening of Pyrolysis Bio-Oils by Short-Term Alloy Exposures. Laboratory Analytical Procedure (LAP), Issue Date: May 12, 2022

Bio-oils contain organic acids and oxygenated compounds that can lead to corrosion issues during bio-oil processing and storage. This Laboratory Analytical Procedure (LAP) allows for rapid screening of a bio-oil's corrosivity without the need for complex equipment and long-term exposures. A robust and repeatable method for assessing the corrosivity of bio-oils is necessary in order to remove materials degradation as an obstacle to research, upgrading, use and storage of bio-oils. This LAP involves the incubation of a representative alloy, 410 stainless steel (410 SS), specimen in bio-oil over a period of 48 hours at 50 degrees C in a sealed container. The corrosive species in the bio-oil react with and deplete alloy elements such as iron (Fe) and/or chromium (Cr) from the specimen into the bio-oil solution. The depletion of Fe and Cr from the specimen results in a significant mass loss that can be recorded. The mass loss is directly correlated to the corrosivity of a bio-oil. Examples of bio-oils in scope include the ones produced by fast pyrolysis and catalytic fast pyrolysis, as well as liquids produced from hydrothermal liquefaction.

09 BIOMASS FUELS↗

AFC FY 2023 HFIR Irradiation Test Matrix – Supported by the Design of a Ring Specimen Irradiation Vehicle

The development and deployment of accident-tolerant cladding materials in light water nuclear reactors requires the collection of neutron-irradiated properties of these materials with specific consideration to the material properties orientation (i.e., tube geometry). To that end, a test plan to irradiate several cladding tube and ring specimens in the High Flux Isotope Reactor (HFIR) at Oak Ridge National Laboratory (ORNL) was proposed, along with the development of a new capsule design that features ring specimens with a preexisting gauge section. This ring specimen geometry removes the need to machine a gauge section on the irradiated specimen and thus allows for direct application of a ring-pull test post-irradiation. The test matrix includes uncoated and chromium-coated Zircaloy-4 and advanced zirconium alloy cladding specimens, pre-characterized at ORNL. Plans are to irradiate the specimens at about 4 and 10 dpa—corresponding to two and five cycles at the HFIR centerline—with a target specimen gauge section temperature of 330°C.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effects of yttrium, aluminum, and chromium concentrations in bond coatings on the performance of zirconia-yttria thermal barriers

A cyclic furnace study was conducted between 990 - 280 C and 1095 - 280 C to evaluate the effects of yttrium, chromium, and aluminum concentrations in nickel base alloy bond coatings and also the effect of the bond coating thickness on the performance of yttria-stabilized zirconia thermal barrier coatings. The presence and the concentration of yttrium is very critical. Without yttrium, rapid oxidation of Ni-Al, Ni-Cr, and Ni-Cr-Al bond coatings causes zirconia thermal barrier coatings to fail very rapidly. Concentrations of chrominum and aluminum in Ni-Cr-Al-Y bond coating have a very significant effect on the thermal barrier coating life. This effect, however, is not as great as that due to yttrium. Furthermore, the thickness and the thickness uniformity also have a very significant effect on the life of the thermal barrier system.

Stecura, S.↗

Development of graphite/copper composites utilizing engineered interfaces

In situ measurements of graphite/copper alloy contact angles were made using the sessile drop method. The interfacial energy values obtained from these measurements were then applied to a model for the fiber matrix interfacial debonding phenomenon found in graphite/copper composites. The formation obtained from the sessile drop tests led to the development of a copper alloy that suitably wets graphite. Characterization of graphite/copper alloy interfaces subjected to elevated temperatures was conducted using Scanning Electron Microscopy, Energy Dispersive Spectroscopy, Auger Electron Spectroscopy, and X Ray Diffraction analyses. These analyses indicated that during sessile drop tests conducted at 1130 C for 1 hour, copper alloys containing greater than 0.98 at pct chromium form continuous reaction layers of approx. 10 microns in thickness. The reaction layers are adherent to the graphite surface. The copper wets the reaction layer to form a contact angle of 60 deg or less. X ray diffraction results indicate that the reaction layer is Cr3C2.

Devincent, Sandra M.↗

INCONEL 690 CORROSION IN WTP (WASTE TREATMENT PLANT) HLW (HIGH LEVEL WASTE) GLASS MELTS RICH IN ALUMINUM & BISMUTH & CHROMIUM OR ALUMINUM/SODIUM

Metal corrosion tests were conducted with four high waste loading non-Fe-limited HLW glass compositions. The results at 1150 C (the WTP nominal melter operating temperature) show corrosion performance for all four glasses that is comparable to that of other typical borosilicate waste glasses, including HLW glass compositions that have been developed for iron-limited WTP streams. Of the four glasses tested, the Bi-limited composition shows the greatest extent of corrosion, which may be related to its higher phosphorus content. Tests at higher suggest that a moderate elevation of the melter operating temperature (up to 1200 C) should not result in any significant increase in Inconel corrosion. However, corrosion rates did increase significantly at yet higher temperatures (1230 C). Very little difference was observed with and without the presence of an electric current density of 6 A/inch{sup 2}, which is the typical upper design limit for Inconel electrodes. The data show a roughly linear relationship between the thickness of the oxide scale on the coupon and the Cr-depletion depth, which is consistent with the chromium depletion providing the material source for scale growth. Analysis of the time dependence of the Cr depletion profiles measured at 1200 C suggests that diffusion of Cr in the Ni-based Inconel alloy controls the depletion depth of Cr inside the alloy. The diffusion coefficient derived from the experimental data agrees within one order of magnitude with the published diffusion coefficient data for Cr in Ni matrices; the difference is likely due to the contribution from faster grain boundary diffusion in the tested Inconel alloy. A simple diffusion model based on these data predicts that Inconel 690 alloy will suffer Cr depletion damage to a depth of about 1 cm over a five year service life at 1200 C in these glasses.

36 MATERIALS SCIENCE↗

Transition metal-based materials for use in high temperature and corrosive environments

A material (e.g., an alloy) comprises molybdenum, rhenium, and at least one element selected from the group consisting of tellurium, iodine, selenium, chromium, nickel, copper, titanium, zirconium, tungsten, vanadium, and niobium. Methods of forming the material (e.g., the alloy) comprise mixing molybdenum powder, rhenium powder, and a powder comprising at least one element selected from the group consisting of tellurium, iodine, selenium, chromium, nickel, copper, titanium, zirconium, tungsten, vanadium, and niobium. The mixed powders may be coalesced to form the material (e.g., the alloy).

Tripathy, Prabhat K.↗

Chemical and Microstructural Changes in Metallic and Ceramic Materials Exposed to Venusian Surface Conditions

The chemical and microstructural behavior of steels (304, 310, 316, and 1018), nickel-based alloys (beta-NiAl, G30, and 625), gold, coatings (4YSZ, SilcoNert(TradeMark) 1040 (SilcoTek Co.), Dursan(TradeMark) (SilcoTek Co.), and porcelain), and bulk ceramics (alpha-Al2O3, fused quartz, beta-SiC, and alpha-Si3N4) were probed after exposure to supercritical fluid with temperature, pressure, and composition mimicking the Venus lower atmosphere. Exposures were carried out in the Glenn Extreme Environments Rig (GEER) chamber with the Venusian gas mixture (96.5% CO2, 3.5% N2, 30 ppm H2O, 150 ppm SO2, 28 ppm CO, 15 ppm OCS, 3 ppm H2S, 0.5 ppm HCl, and 5 ppb HF) at 92 bar (1330 psi) and 467 C (873 F) for durations of 10 and 42 days. An additional 21-day exposure was done to stainless steel uncoated and coated with SilcoNert(TradeMark) and Dursan(TradeMark). Samples were characterized before and after the experiment by gravimetric analysis, X-ray diffraction, X-ray photoelectron and Auger electron spectroscopies, and cross section electron microscopy analysis. All steels exposed for 10 and 42 days formed double-layered scales consisting mainly of metal (Cr, Fe, Ni) oxides and sulfides showing different chemistry, microstructure, and crystalline phases. The alloys G30 and 625 formed double-layered scales consisting mainly of nickel sulfides. After 10 days, the beta-NiAl exhibited no detectable scale, suggesting only a very thin film was formed. The 304 and 316 stainless steels coated with 4YSZ that were exposed for 10 and 42 days exhibited no significant oxidation. Steel 1018 coated with 4YSZ exhibited a corrosion scale of iron and/or chromium oxide formed at the base of the alloy. The 304 steel coated with porcelain did not exhibit corrosion, although the coating exhibited recession. SilcoNert(TradeMark) exposed for 10 and 42 days exhibited recession, although no oxidation was found to occur at the base of the alloy. Stainless steel 316 coated with Dursan(TradeMark)  exhibited corrosion at the base of the alloy. All ceramics tested showed no clear evidence of reaction. The weight-gain-per-area performance of the materials exposed in the GEER for 10 and 42 days are reported from the lowest to the highest weight gain per area as follows: gold did not exhibit any weight change; nickel-based alloys: beta- NiAl < G30 < 625; steels: 304 < 310 < 316 < 1018; ceramics: considering the experimental uncertainties, no weight change was observed for all ceramics of this work (alpha-Al2O3, Si3N4, SiC, and amorphous SiO2).

Costa, Gustavo C. C.↗

Irradiation-induced swelling of pure chromium with 5 MeV Fe ions in the temperature range 450–650 °C

A surface coating using pure chromium has been proposed to increase the accident tolerance of Zircaloy cladding in pressurized water reactors. However, there is not much irradiation experience with Cr alloys and especially pure Cr. In the present study, pure chromium was irradiated with 5 MeV Fe ions to 50 peak dpa (displacements per atom) at temperatures of 450, 500, 550, 600 and 650 °C. Then irradiation at the peak swelling temperature of 550 °C was conducted to 50, 100, 150 peak dpa. Swelling at 50 dpa was observed over the entire temperature range studied, 450–650 °C, but appeared to be decreasing strongly at the temperature boundaries of the experiment. After an initial transient of rapid swelling, chromium was observed to swell at a rate of ~0.03–0.04%/dpa (up to 120 local dpa), which is much lower than pure Fe at 0.2%/dpa. This low swelling rate was found to be relatively insensitive to dpa rate, which varied by a factor of ~2 over the depth of data collection. Here, swelling was observed to begin quickly with an incubation period less than 10 dpa. Self-organization in the form of void ordering was observed to be developing at 50 dpa, becoming better defined with increasing dose. The void alignment direction is determined to be the $\langle$111$\rangle$ axial direction.

36 MATERIALS SCIENCE↗

Achieving perpendicular anisotropy in half-metallic Heusler alloys for spin device applications

Various full Heusler alloys are interfaced with MgO and the magnetic properties of the Heusler-MgO junctions are studied. Next to MgO, the cubic Heusler system distorts to a tetragonal one, thereby inducing an anisotropy. The half-metallicity and nature of anisotropy (in-plane or perpendicular) in the Heusler-MgO system is governed mostly by the interface Heusler layers. There is a trend that Mn-O bonding near the MgO-Heusler junction results in perpendicular anisotropy. The ability to remain half-metallic and have perpendicular anisotropy makes some of these alloys potential candidates as free-layers in Spin Transfer Torque Random Access Memory (STT-RAM) devices, particularly, Cr{sub 2}MnAs-MgO system with MnAs interface layers and Co{sub 2}MnSi-MgO system with Mn{sub 2} interface layers.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structure and elevated temperature properties of carbon-free ferritic alloys strengthened by a Laves phase

A Laves phase, Fe2Ta, was utilized to obtain good elevated temperature properties in a carbon-free iron alloy containing 1 at. pct Ta and 7 at. pct Cr. Room temperature embrittlement resulting from the precipitation of the Laves phase at grain boundaries was overcome by spheroidizing the precipitate. This was accomplished by thermally cycling the alloys through the alpha to gamma transformation. The short-time yield strength of the alloys decreased very slowly with increase in test temperature up to 600 C, but above this temperature, the strength decreased rapidly. Results of constant load creep and stress rupture tests conducted at several temperatures and stresses indicated that the rupture and creep strengths of spheroidized 1 Ta-7 Cr alloy were higher than those of several commercial steels containing chromium and/or molybdenum carbides but lower than those of steels containing substantial amounts of tungsten and vanadium. When molybdenum was added to the base Fe-Ta-Cr alloy, the rupture and creep strengths were considerably increased.

Bhandarkar, M. D.↗

Fundamental Corrosion Studies in High-Temperature Molten Salt Systems for Next Generation Concentrated Solar Power Systems

The objective of this project is to increase Concentrated Solar Power (CSP) system lifetime through characterization of corrosion mechanisms in heat transfer systems and identification of materials and corrosion resistance methods applicable at temperatures above 850°C. Coupling of experimental methods with thermodynamic and kinetic modeling has given greater insight into the corrosion phenomena and enabled modeling of the corrosion in molten chloride heat transfer systems. The project has been identified the selective oxidation of Cr along the grain boundaries of high Cr content alloys as the principle corrosion mechanisms occurring in CSP systems. The corrosion rate was also found to be mass transfer limited by diffusion of chromium chlorides along the grain boundaries. It was shown that the corrosion could be increased by adding naturally convective flow to mechanism using a thermosiphon. A reaction mechanism has been proposed for selective oxidation of Cr that is driven by the electrochemical potential difference between the Ni crucible for immersion testing and the alloy coupon. This driving force will be similar to the differences caused by having varying Ni content or Cr content throughout a heat transfer system. It could also mimic the differences in electrochemical potential between various parts of the system that are at different temperatures. The reaction mechanism consists of an initiation step due to system impurities and a set of propagation steps that results in formation of a NiCr alloy at the crucible that drives corrosion and selective oxidation of Cr from the alloy. The presences of chromium chlorides in the salt are also essential to the corrosion mechanism to transport the Cr. The formation of a NiCr alloy on the crucible surface with no contact between the alloy coupons and the crucible provides support to this mechanism of having corrosion reactions occurring at both the alloy and the crucible. The thermodynamics of this reaction mechanism have been modeled and were shown to be galvanic. A corrosion model has been developed based on this mechanism and has been implemented in CFD so that it can be used to predict corrosion in a wide variety of system geometries. The model was validated using the thermosiphon data and dimensionless analysis. The corrosion rates of the samples were modeled to within 10% percent of the experimental values. The model has been extended to include the effect of Mg corrosion inhibitor on the corrosion rate in the system. The use of Mg as a metallic corrosion inhibitor has been demonstrated as a method to reduce the corrosion rate of alloys in molten chlorides to below 15 microns per year. Mg is an effective corrosion inhibitor at concentrations as low as 0.3 mol%. Corrosion potential monitoring experiments have shown that the Mg lowers the corrosion potential for the alloy below the equilibrium potential for Cr oxidation and thus prevents corrosion. Experiments have been performed on the ability of Mg to inhibit corrosion in realistic environments that include lower purity salts and welded and stressed alloys. The results have shown that for all these scenarios the corrosion can be reduced to meet the DOE targets. The electrochemical monitoring of Mg for process control has also been demonstrated.

14 SOLAR ENERGY↗

Superalloy resources: Supply and availability

Over the past several decades there have been shortages of strategic materials because of our near total import dependence on such metals as chromium, cobalt, and tantalum. In response to the continued vulnerability of U.S. superalloy producers to disruptions in resource supplies, NASA has undertaken a program to address alternatives to the super-alloys containing significant quantities of the strategic materials such as chromium, cobalt, niobium, and tantalum. The research program called Conservation of Strategic Aerospace Materials (COSAM) focuses on substitution, processing, and alternate materials to achieve its goals. In addition to NASA Lewis Research Center, universities and industry play an important role in the COSAM Program. This paper defines what is meant by strategic materials in the aerospace community, presents a strategic materials index, and reviews the resource supply and availability picture from the U.S. point of view. In addition, research results from the COSAM Program are highlighted and future directions for the use of low strategic material alloys or alternate materials are discussed.

Stephens, Joseph R.↗