Effects of composition and testing conditions on oxidation behavior of four cast commercial nickel-base superalloys

Four cast nickel-base superalloys were oxidized at 1000 and 1100 C for times up to 100 hr in static air and a Mach 1 gas stream. The oxidation resistance was judged by weight change, metal thickness loss, depletion-zone formation, and oxide formation and morphology. The alloys which formed mostly nickel aluminate (NiAl2O4) and aluminum oxide (Al2O3) (B-1900, VIA, and to a lesser extent 713C) were more oxidation resistant. Poorer oxidation resistance was associated with the appearance of chromium sesquioxide (Cr2O3) and chromite spinel (738X). Refractory metal content had little effect on oxidation resistance. Refractory metals appeared in the scale as tapiolite (NiM2O6, where M represents the refractory metal). Thermal cycling in static air appeared to supply sufficient data for the evaluation of oxidation resistance, especially for alloys which form oxides of low volatility. For alloys of higher chromium levels with high propensities toward forming a chromium-bearing scale of higher volatility, testing under conditions of high gas velocity is necessary to assess fully the behavior of the alloy.

Lowell, C. E.↗

The preparation of new perfluoroether fluids exhibiting excellent thermal-oxidative stabilities

A series of low molecular weight perfluoroalkylethers (PFAE) were synthesized by direct fluorination. Viscosity-temperature properties and oxidation stabilities were determined. Viscosity-temperature correlations indicated that increases in branching and increases in the size of the branching substituent caused a deterioration in viscometric properties (i.e., an increase in ASTM slope). In addition, increasing the ratio of carbon to oxygen in these compounds also increased the ASTM slope. Preliminary oxidation stability tests indicated that highly branched PFAE fluids. (i.e., those containing quaternary carbons) may be less stable than either those containing a single trifluoromethyl pendant group or those containing no branching at all.

Jones, W. R., Jr.↗

The preparation of new perfluoro ether fluids exhibiting excellent thermal-oxidative stabilities

A series of low molecular weight perfluoroalkyl ethers (PFAEs) were synthesized by direct fluorination. Viscosity-temperature properties and oxidation stabilities were determined. Viscosity-temperature correlations indicated that increases in branching and increases in the size of the branching substituent caused a deterioration in viscometric properties (i.e., an increase in ASTM slope). In addition, increasing the ratio of carbon to oxygen in these compounds also increased the ASTM slope. Preliminary oxidation stability measurements indicated that highly branched PFAE fluids (i.e., those containing quaternary carbons) may be less stable than either those containing a single trifluoromethyl pendant group or those containing no branching at all.

Jones, William R., Jr.↗

Fibrous refractory composite insulation

A refractory composite insulating material was prepared from silica fibers and aluminosilicate fibers in a weight ratio ranging from 1:19 to 19:1, and about 0.5 to 30% boron oxide, based on the total fiber weight. The aluminosilicate fiber and boron oxide requirements may be satisfied by using aluminoborosilicate fibers and, in such instances, additional free boron oxide may be incorporated in the mix up to the 30% limit. Small quantities of refractory opacifiers, such as silicon carbide, may be also added. The composites just described are characterized by the absence of a nonfibrous matrix.

Leiser, D. B.↗

Oxidation of ZrB2-and HfB2-Based Ultra-High Temperature Ceramics: Effects of Ta Additions

Several compositions of ZrB2- and HfB2-based Ultra-High Temperature Ceramics (UHTC) were oxidized in stagnant air at 1627 C in ten minute cycles for times up to 100 minutes. These compositions include: ZrB2 - 20v% SiC, HfB2 - 20v% SiC, ZrB2 - 20v% SiC - 20v% TaSi2, ZrB2 - 33v% SiC, HfB2 - 20v% SiC - 20v% TaSi2, and ZrB2 - 20v% SiC - 20v% TaC. The weight change due to oxidation was recorded. The ZrB2 - 20v% SiC - 20v% TaSi2 composition was also oxidized in stagnant air at 1927 C and in an arc jet atmosphere. Samples were analyzed after oxidation by x-ray diffraction, field emission scanning electron microscopy, and energy dispersive spectroscopy to determine the reaction products and to observe the microstructure. The ZrB2 - 20v% SiC - 20v% TaSi2 showed the lowest oxidation rate at 1627 C, but performed poorly under the more extreme tests due to liquid phase formation. Effects of Ta-additions on the oxidation of the diboride-based UHTC are discussed.

Opila, Elizabeth↗

Supporting technology for the development of Controlled Ecological Life Support Systems (CELSS)

To support the development of Controlled Ecological Life Support Systems (CELSS) in the space program, a metabolic simulator has been selected for use in a closed chamber to test functions of the CELSS. This metabolic simulator is a catalytic reactor which oxidizes the methyl acetate to produce carbon dioxide and water vapor. In this project, kinetic studies of catalytic oxidation of methyl acetate were conducted using monolithic and pellet catalysts with 0.5% (by weight) platinum (Pt) on aluminum oxide (Al2O3). The reaction was studied at a pressure of one atmosphere and at temperatures varying from 160 C to 420 C. By-products were identified at the exit of the preheater and reactor. For the kinetic study with the monolithic catalyst, a linear regression method was used to correlate the kinetic data with zero-order, first-order and Langmuir-Hinshelwood models. Results indicate that the first-order model represents the data adequately at low concentrations of methyl acetate. For higher concentrations of methyl acetate, the Langmuir-Hinshelwood model best represents the kinetic data. Both rate constant and adsorption equilibrium constants were estimated from the regression. A Taguchi orthogonal array (L(sub 9)) was used to investigate the effects of temperature, flow rate, and concentration on the catalytic oxidation of methyl acetate. For the monolithic catalyst, temperature exerts the most significant effect, followed by concentration of methyl acetate. For the pellet catalyst, reaction temperature is the most significant factor, followed by gas flow rate and methyl acetate concentration. Concentrations of either carbon dioxide or oxygen were seen to have insignificant effect on the methyl acetate conversion process. Experimental results indicate that the preheater with glass beads can accomplish thermal cracking and catalytic reaction of methyl acetate to produce acetic acid, methanol, methyl formate, and 1-propanol. The concentration of all by-products was measured in ppmv (parts per million by volume). At higher temperatures, greater amounts of these products are produced, as expected. In all cases, methanol was the predominant concentration detected, followed by methyl formate. At temperatures lower than 320 C for the P-type monolithic catalyst, methanol, acetic acid, and acetone were detected, whereas, for the E-type monolithic catalyst, only methanol was detected at 160 C. Both P and E types of the monolithic catalyst were specified with the same substrates (ceramic), washcoat (Al2O3), and promoter (Pt). However, the manufacturing and treatment procedures were quite different. It was therefore concluded that the performance of the E-type monolithic catalyst is superior to that of the P-type for oxidation of methyl acetate. At higher reaction temperatures, e.g., above 420 C, all reactants and byproducts were completely oxidized using these two types of monolithic catalyst to produce carbon dioxide and water vapor. A complex heterogenous catalytic reaction mechanism was proposed to explain the formation of the byproducts (methanol, acetic acid, and methyl formate) as the methyl acetate traveled through the preheater packed with glass beads. The by-product, 1-propanol, may be formed only through a homogeneous reaction, since it is difficult to develop a reasonable sequence of heterogeneous reaction steps to explain its formation. The homogeneous thermal decomposition of methyl acetate to form free radicals was proposed to explain the formation of 1-propanol, and also methanol, in the preheater. A dual-site catalytic reaction mechanism was proposed for the oxidation of methyl acetate over Pt/Al2O3 monolithic catalyst. The dual-site mechanism describes the chemisorption of oxygen molecules as well as a physical adsorption of methyl acetate on the active sites. On the active sites, methyl acetate is oxidized rapidly to form carbon dioxide and water vapor. A rate equation derived from this mechanism gives the Langmuir-Hinshelwood rate formula which has been observed from the experimental data obtained in this project for high methyl acetate concentration (greater than 1000 ppmv) over a monolithic catalyst. If the oxygen concentration is very high and methyl acetate concentration is very low, the reaction rate equation is then reduced to a first-order with respect to methyl acetate concentration. The first-order model has also been observed from the experimental data obtained in this project for low methyl acetate concentration (less than 1000 ppmv).

Li, Ku-Yen↗

Effect of alloy chemistry and exposure conditions on the oxidation of titanium

Multiwall is a new thermal protection system concept for advanced space transportation vehicles. The system consists of discrete panels made up of multiple layers of foil gage metal. Titanium is the proposed candidate metal for multiwall panels in the reentry temperature range up to 675 C. Oxidation and embrittlement are the principal concerns related to the use of Ti in heat shield applications. The results of a broad study on the oxidation kinetics of several titanium alloys subjected to different exposure conditions are described. The alloys include commercially pure titanium, Ti-6Al-4V, and Ti-6Al-2Sn-4Zr-2Mo. Oxidation studies were performed on these alloys exposed at 704 C in 5-760 torr air pressure and 0 to 50% relative humidity. The resulting weight gains were correlated with oxide thickness and substrate contamination. The contamination depth and weight gains due to solid solutioning were obtained from microhardness depth profiles and hardness versus weight percent oxygen calibration data.

Unnam, J.↗

Microstructure, strength, and oxidation of a 10 wt pct zyttrite-Si3N4 ceramic

Hot pressed Si3N4 doped with 10 wt pct zyttrite as a sintering aid was studied. An equiaxed, fine grained microstructure was predominant, with no apparent porosity. Bend strengths were determined at room temperature and high temperatures (up to 1370 C). Oxidation was measured by weight gain at 1370 C in air. The resulting material exhibited very good room temperature strength (755 MPa). The work showed that room temperature strength can be improved significantly by using controlled Si3N4 powder with 10 wt pct zyttrite. High temperature strength (514 MPa) at 1370 C was nearly double that of hot-pressed Si3N4 (NC-132). The oxidation resistance at 1370 C was also higher than that of NC-132.

Dutta, S.↗

Oxidation of TD nickel at 1050 C and 1200 C as compared with three grades of nickel of different purity

The isothermal oxidation of three nickels of different purity, Ni-200, Ni-270, and JM-Ni, was compared with that of TD-Ni in air at 1050 and 1200 C. The samples were oxidized as ground, as polished, or as annealed and polished. Weight change, metal loss, scale thickness, oxide morphology, and scale texture were determined. In degree of oxidation, TD-Ni was nearly the same as the higher purity materials, Ni-270 and JM-Ni; and less pure Ni-200 oxidized more than the others. However, in microstructure and scale texture the TD-Ni more closely resembled Ni-200. Grinding only charged the texture of the oxides of Ni_200 and TD-Ni.

Lowell, C. E.↗

Delayed Alumina Scale Spallation on Rene'n5+y: Moisture Effects and Acoustic Emission

The single crystal superalloy Rene'N5 (with or without Y-doping and hydrogen annealing) was cyclically oxidized at 1150 C for 1000 hours. After considerable scale growth (>= 500 hours), even the adherent alumina scales formed on Y-doped samples exhibited delayed interfacial spallation during subsequent water immersion tests, performed up to one year after oxidation. Spallation was characterized by weight loss, the amount of spalled area, and acoustic emission response. Hydrogen annealing (prior to oxidation) reduced spallation both before and after immersion, but without measurably reducing the bulk sulfur content of the Y-doped alloys. The duration and frequency of sequential, co-located acoustic emission events implied an interfacial crack growth rate at least 10(exp -3) m/s, but possibly higher than 10(exp 2) m/s. This is much greater than classic moisture-assisted slow crack growth rates in bulk alumina (10(exp -6) to 10(exp -3) m/s), which may still have occurred undetected by acoustic emission. An alternative failure sequence is proposed: an incubation process for preferential moisture ingress leads to a local decrease in interfacial toughness, thus allowing fast fracture driven by stored strain energy.

Smialek, James L.↗

Oxidation of TaSi2-Containing ZrB2-SiC Ultra-High Temperature Materials

Hot pressed coupons of composition ZrB2-20 v% SiC-5 v% TaSi2 and ZrB2-20 v% SiC-20 v% TaSi2 were oxidized in stagnant air at temperatures of 1627 and 1927C for one, five and ten 10-minute cycles. The oxidation reactions were characterized by weight change kinetics, x-ray diffraction, and SEM/EDS. Detailed WDS/microprobe quantitative analyses of the oxidation products were conducted for the ZrB2-20 v% SiC-20 v% TaSi2 sample oxidized for five 10-minute cycles at 1927C. Oxidation kinetics and product formation were compared to ZrB2-20 v% SiC with no TaSi2 additions. It was found that the 20 v% TaSi2 composition exhibited improved oxidation resistance relative to the material with no TaSi2 additions at 1627C. However, for exposures at 1927C less oxidation resistance and extensive liquid phase formation were observed compared to the material with no TaSi2 additions. Attempts to limit the liquid phase formation by reducing the TaSi2 content to 5 v% were unsuccessful. In addition, the enhanced oxidation resistance at 1627C due to 20 v% TaSi2 additions was not achieved at the 5 v% addition level. The observed oxidation product evolution is discussed in terms of thermodynamics and phase equilibria for the TaSi2-containing ZrB2-SiC material system. TaSi2-additions to ZrB2-SiC at any level are not recommended for ultra-high temperature (>1900C) applications due to excessive liquid phase formation.

Opila, Elizabeth J.↗

Resin/fiber thermo-oxidative interactions in PMR polymide/graphite composites

The amounts of resin weight loss and fiber weight loss in four PMR-polyimide graphite fiber composites were calculated from the composite weight losses and the fiber/resin ratios of the composites after long term thermo-oxidative aging in 600 F air. The accelerating effect of graphite fiber on resin weight loss, compared to neat resin weight loss, indicated the presence of a deleterious resin/fiber thermo-oxidative interaction, presumably due to fiber impurities. Similarly, the decelerating effect of the protective matrix resin on fiber weight loss, compared to bare fiber weight loss, was also demonstrated. The amount of hydrazine-indigestible resin and the amount of loose surface graphite fiber that formed during 600 deg F exposure of the composites were quantitatively determined. The indigestible residual resin was also qualitatively studied by scanning electron microscopy.

Alston, W. B.↗

Effect of thermal cycling in a Mach 0.3 burner rig on properties and structure of directionally solidified gamma/gamma prime-delta eutectic

An experimental study was carried out to evaluate the effect of cyclic thermal exposures on the mechanical properties of a gamma/gamma prime-delta eutectic alloy parallel to the growth direction. The alloy had a nominal composition by weight of Ni-20 Nb-6 Cr-2.5 Al and was directionally solidified at 3 cm/hr in a furnace with a thermal gradient of at least 200 C/cm. Bars of the alloy were exposed in a Mach 0.3 burner rig and cycled 300 times between 1100 and 425 C. Oxidation-erosion characteristics of the alloy were determined by weight loss measurements at 300-cycle intervals. After cyclic exposure, stress rupture and tensile tests were performed at both 760 and 1040 C. Microstructural changes from cyclic exposure were determined. Thermal cycling resulted in gamma prime coarsening and Widmanstaetten delta precipitation in the gamma phase. An unidentified precipitate, presumably gamma prime, was observed within the delta phase. These microstructural changes did not affect the mechanical properties of the eutectic. High oxidation-erosion weight loss rate was observed.

Gray, H. R.↗

Thermal fatigue and oxidation data of TAZ-8A and M22 alloys and variations

Thermal fatigue and oxidation data were obtained on 36 specimens, representing 18 distinct variations (including the base systems) of TAZ-8A and M22 alloys. Double-edge wedge specimens for these systems were cycled between fluidized beds maintained at 1088 C and 316 C with a 180 s immersion in each bed. The systems included alloys TAZ-8A, M22, and 16 variations of these alloys. Each alloy variation consisted of a unique composition with an alternation in the percentage of carbon (C1 and C2), molydenum (M1 and M2), tungsten (W1 and W2), columbium (CB1, CB2, and CB3), tantalium (T1, T2, and T3), or boron (B1, B2, and B3) present. All of the alloys showed little weight change due to oxidation compared with other alloys previously tested in fluidized beds. Only both C1 alloy variation specimens survived 3500 cycles without cracking in the small radius, although substantial cracks were present, emanating from the end notches which were used for holding the specimens.

Hofer, K. E.↗

Current EBC Development and Testing at NASA

SiC SiC Ceramic Matrix Composites (CMCs) are a game changer for advanced power generation equipment because of their high temperature capability, oxidation resistance, and light weight that translate to significant reduction in fuel consumption and emission. Limitations of SiC SiC CMCs include surface recession and component cracking and associated chemical and physical degradation in the CMC. The solution pursued to mitigate surface recession of SiC SiC CMCs is the incorporation of coating systems that provide surface protection, which has become known as an Environmental Barrier Coating (EBC). The development of EBCs for the protection of SiC SiC CMCs was a continuation of coating development work for corrosion protection of silicon-based monolithics. The first and second generation EBCs developed in mid 1990s-early 2000s laid the foundation for current EBCs. Environmental degradation that limits EBC life includes surface recession by steam, oxidation in steam environments, and CMAS-EBC reactions. Many engine tests have been conducted since late 1990s and a first CMC component entered into service in 2016 in a commercial engine. The introduction of CMCs represents significant challenges as failure of the EBC means rapid reduction in component life. A reliable lifing method and engine-relevant testing methods to validate life need to be developed. This paper will current activities on EBC development and testing at NASA.

CMC↗

The effects of Cr, Al, Ti, Mo, W, Ta, and Cb on the cyclic oxidation behavior of cast Ni-base superalloys at 1100 and 1150 C

Fifty Ni-base superalloys with concentrations of Cr, Al, Ti, Mo, W, Ta, and Cb systematically varied between two nonzero levels, were tested for cyclic oxidation resistance at 1100 and 1150 C. Oxidation resistance was interpreted in terms of the rate of specific weight change and the types of oxides formed. It is found that the resistance of the alloys to cyclic oxidation is largely determined by Al content, with a sharp increase in the oxidation resistance observed in the Al concentration range 5-8 at. pct. The effects of the other elements studied were small compared with that of aluminum. Best oxidation resistance characteristics were predicted for high Al (13 at. pct), low Cr (10 at. pct), low Ti (2 at. pct), low Cb (1 at. pct), and high Mo, W, and Ta (3 at. pct each). The effects of the refractory metals, however, are somewhat ambiguous and should be investigated further. Higher boron contents, which were unintentionally varied, were clearly detrimental even for the most resistant compositions.

Barrett, C. A.↗

Global Impact of Lightning-Produced Oxidants

Lightning plays a major role in tropospheric oxidation, and its role on modulating tropospheric chemistry was thought to be emissions of nitrogen oxides (NOx). Recent field and laboratory measurements demonstrate that lightning generates extremely large amounts of oxidants, including hydrogen oxides (HOx) and O3. Here we implement these lightning-produced oxidants in a global chemical transport model to examine its global impact on tropospheric composition. We find that lightning-produced oxidants can increase global mass weighted OH by 0.3-10%, and affect CO, O3, and reactive nitrogen substantially, depending on the emission strength of oxidants from lightning. Our work highlights the importance and uncertainties of lightning-produced oxidants, as well as the need for rethinking the role of lightning in tropospheric oxidation chemistry.

Jingqiu Mao↗

The degradation of space shuttle TPS metals in dissociated oxygen.

The interaction of space shuttle orbiter Thermal Protection System (TPS) metals with the chemical environment to which it is exposed during reentry is considered with emphasis on the effects of dissociated oxygen. Experimental results comparing the interactions of atomic (dissociated) and molecular oxygen with five candidate shuttle TPS metals, Ni-20Cr-2ThO2, Ni-20Cr-3.5Al-2ThO2, Ni-16Cr-15Fe-2Mn-.5Si-.3La-2ThO2, Haynes Alloy Number 188, and Ti-6Al-4V at their maximum planned use temperature are presented. As measured by metal recession, weight change, rate of oxide scale formation, and scale spalling, the first four metals show enhanced degradation in a dissociated oxygen environment. The enhanced degradation appears to result from differing rates of alloy constituent reactions in the two environments. The dissociated oxygen environmental tests are found to better assess the usefulness of shuttle skin materials for the planned mission than do conventional molecular (either flowing or static) oxidation experiments.-

Gilbreath, W. P.↗