Comparison of high frequency, high temperature core loss and B-H loop characteristics of an 80 Ni-Fe crystalline alloy and two iron-based amorphous alloys
Limited experimental data exists for the specific core loss and dynamic B-H loops for soft magnetic materials for the combined conditions of high frequency and high temperature. This experimental study investigates the specific core loss and dynamic B-H characteristics of a nickel-iron crystalline magnetic alloy (Supermalloy) and two iron-based amorphous magnetic materials (Metglas 2605S-3A and Metglas 2605SC) over the frequency range of 1-50 kHz and temperature range of 23-300 C under sinusoidal voltage excitation. The effects of maximum magnetic flux density, frequency, and temperature on the specific core loss and on the size and shape of the B-H loops are examined. The Supermalloy and Metglass 2605S-3A and 2605SC data are used to compare the core loss of transformers with identical kVA and voltage ratings.