A Study on Vitrification for LLW Radioactive Wastes - 16235

Ash and ion exchange resin wastes to be vitrified were considered among various radioactive wastes in the Japanese nuclear industry. The appropriate glass composition for the waste is calculated using the computer program. The glass composition is systematically studied using a ternary diagram, considering viscosity, electrical conductivity, and durability. The optimized glass composition based on calculated parameters of vitrification process and the convenience of mixing wastes is selected for crucible experiment. Since differences between calculated values and measured values may occur upon evaluation of glass formulations using glass formulation computer simulation program, the calculated glass formulations should be verified through experiments on a laboratory scale for more meticulous development of glass formulations. For the follow-up development of glass formulations, several glass formulations are planned to be developed. The candidate glasses for treatment of ash and ion exchange resin were melted and fabricated using reagents, respectively. The chemicals were weighed out to produce the desired batch compositions and mixed thoroughly and then put into clay crucibles for melting. Next, the crucibles were introduced into an electric furnace at 1,150 deg. C in the ambient atmosphere and pressure with occasional stirring by a quartz rod. A hold time of 1 hour was introduced to promote homogenization. Finally, the melted material was poured on a graphite plate to be rapidly cooled. The viscosities of all fabricated glasses were in the desired range. After rapid cooling, the micro-structure of the glasses was analyzed using the SEM. They exhibited amorphous structure with good homogeneity. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Formulation and Characterization of Waste Glasses with Varying Processing Temperature

This report documents the preliminary results of glass formulation and characterization accomplished within the finished scope of the EM-31 technology development tasks for WP-4 and WP-5, including WP-4.1.2: Glass Formulation for Next Generation Melter, WP-5.1.2.3: Systematic Glass Studies, and WP-5.1.2.4: Glass Formulation for Specific Wastes. This report also presents the suggested studies for eventual restart of these tasks. The initial glass formulation efforts for the cold crucible induction melter (CCIM), operating at {approx}1200 C, with selected HLW (AZ-101) and LAW (AN-105) successfully developed glasses with significant increase of waste loading compared to that is likely to be achieved based on expected reference WTP formulations. Three glasses formulated for AZ-101HLW and one glass for AN-105 LAW were selected for the initial CCIM demonstration melter tests. Melter tests were not performed within the finished scope of the WP-4.1.2 task. Glass formulations for CCIM were expanded to cover additional HLWs that have high potential to successfully demonstrate the unique advantages of the CCIM technologies based on projected composition of Hanford wastes. However, only the preliminary scoping tests were completed with selected wastes within the finished scope. Advanced glass formulations for the reference WTP melter, operating at {approx}1200 C, were initiated with selected specific wastes to determine the estimated maximum waste loading. The incomplete results from these initial formulation efforts are summarized. For systematic glass studies, a test matrix of 32 high-aluminum glasses was completed based on a new method developed in this study.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Ion-Exchange Interdiffusion Model with Potential Application to Long-Term Nuclear Waste Glass Performance

Ion exchange is an integral mechanism influencing the corrosion of glasses. Due to the formation of alteration layers in aqueous conditions, it is difficult to conclusively deconvolute the process of ion exchange from other processes, principally dissolution of the glass matrix. Therefore, we have developed a method to isolate alkali diffusion that involves contacting glass coupons with a solution of 6 LiCl dissolved in functionally inert dimethyl sulfoxide. Here, we employ the method at temperatures ranging from 25 to 150 °C with various glass formulations. Glass compositions include simulant nuclear waste glasses, such as SON68 and the international simple glass (ISG), glasses in which the nature of the alkali element was varied, and glasses that contained more than one alkali element. An interdiffusion model based on Fick’s second law was developed and applied to all experiments to extract diffusion coefficients. The model expands established models of interdiffusion to the case where multiple types of alkali sites are present in the glass. Activation energies for alkali ion exchange were calculated and the results are in agreement with those obtained in glass strengthening experiments but are nearly five times higher than values reported for diffusion-controlled processes in nuclear waste glass corrosion experiments. A discussion of the root causes for this apparent discrepancy is provided. The interdiffusion model derived from laboratory experiments is expected to be useful for modeling glass corrosion in a geological repository when the silicon concentration is high.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Final Report Summary of DM1200 Operation at VSL

The principal objective of this report was to summarize the testing experience on the DuraMelter 1200 (DMI200), which is the High Level Waste (HLW) Pilot Melter located at the Vitreous State Laboratory (VSL). Further objectives were to provide descriptions of the history of all modifications and maintenance, methods of operation, problems and unit failures, and melter emissions and performance while processing a variety of simulated HL W and low activity waste (LAW) feeds for the Hanford Waste Treatment and Immobilization Plant (WTP) and employing a variety of operating methods. All of these objectives were met. The River Protection Project - Hanford Waste Treatment and Immobilization Plant (RPP-WTP) Project has undertaken a 'tiered' approach to vitrification development testing involving computer-based glass formulation, glass property-composition models, crucible melts, and continuous melter tests of increasing, more realistic scales. Melter systems ranging from 0.02 to 1.2 m{sup 2} installed at the Vitreous State Laboratory (VSL) have been used for this purpose, which, in combination with the 3.3 m{sup 2} low activity waste (LAW) Pilot Melter at Duratek, Inc., span more than two orders of magnitude in melt surface area. In this way, less-costly small-scale tests can be used to define the most appropriate tests to be conducted at the larger scales in order to extract maximum benefit from the large-scale tests. For high level waste (HLW) vitrification development, a key component in this approach is the one-third scale DuraMelter 1200 (DM 1200), which is the HLW Pilot Melter that has been installed at VSL with an integrated prototypical off-gas treatment system. That system replaced the DM1000 system that was used for HLW throughput testing during Part B1. Both melters have similar melt surface areas (1.2 m{sup 2}) but the DM1200 is prototypical of the present RPP-WTP HLW melter design whereas the DM1000 was not. In particular, the DM1200 provides for testing on a vitrification system with the specific train of unit operations that has been selected for both HLW and LAW RPP-WTP off-gas treatment.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Glass Ceramic Formulation Data Package

A glass ceramic waste form is being developed for treatment of secondary waste streams generated by aqueous reprocessing of commercial used nuclear fuel (Crum et al. 2012b). The waste stream contains a mixture of transition metals, alkali, alkaline earths, and lanthanides, several of which exceed the solubility limits of a single phase borosilicate glass (Crum et al. 2009; Caurant et al. 2007). A multi-phase glass ceramic waste form allows incorporation of insoluble components of the waste by designed crystallization into durable heat tolerant phases. The glass ceramic formulation and processing targets the formation of the following three stable crystalline phases: (1) powellite (XMoO 4 ) where X can be (Ca, Sr, Ba, and/or Ln), (2) oxyapatite Y x, Z (10-x) Si 6 O 26 where Y is alkaline earth, Z is Ln, and (3) lanthanide borosilicate (Ln 5 BSi 2 O 13 ). These three phases incorporate the waste components that are above the solubility limit of a single-phase borosilicate glass. The glass ceramic is designed to be a single phase melt, just like a borosilicate glass, and then crystallize upon slow cooling to form the targeted phases. The slow cooling schedule is based on the centerline cooling profile of a 2 foot diameter canister such as the Hanford High-Level Waste canister. Up to this point, crucible testing has been used for glass ceramic development, with cold crucible induction melter (CCIM) targeted as the ultimate processing technology for the waste form. Idaho National Laboratory (INL) will conduct a scaled CCIM test in FY2012 with a glass ceramic to demonstrate the processing behavior. This Data Package documents the laboratory studies of the glass ceramic composition to support the CCIM test. Pacific Northwest National Laboratory (PNNL) measured melt viscosity, electrical conductivity, and crystallization behavior upon cooling to identify a processing window (temperature range) for melter operation and cooling profiles necessary to crystallize the targeted phases in the waste form.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

HIGH ALUMINUM HLW (HIGH LEVEL WASTE ) GLASSES FOR HANFORDS WTP (WASTE TREATMENT PROJECT)

This paper presents the results of glass formulation development and melter testing to identify high waste loading glasses to treat high-Al high level waste (HLW) at Hanford. Previous glass formulations developed for this HLW had high waste loadings but their processing rates were lower that desired. The present work was aimed at improving the glass processing rate while maintaining high waste loadings. Glass formulations were designed, prepared at crucible-scale and characterized to determine their properties relevant to processing and product quality. Glass formulations that met these requirements were screened for melt rates using small-scale tests. The small-scale melt rate screening included vertical gradient furnace (VGF) and direct feed consumption (DFC) melter tests. Based on the results of these tests, modified glass formulations were developed and selected for larger scale melter tests to determine their processing rate. Melter tests were conducted on the DuraMelter 100 (DMIOO) with a melt surface area of 0.11 m{sup 2} and the DuraMelter 1200 (DMI200) HLW Pilot Melter with a melt surface area of 1.2 m{sup 2}. The newly developed glass formulations had waste loadings as high as 50 wt%, with corresponding Al{sub 2}O{sub 3} concentration in the glass of 26.63 wt%. The new glass formulations showed glass production rates as high as 1900 kg/(m{sup 2}.day) under nominal melter operating conditions. The demonstrated glass production rates are much higher than the current requirement of 800 kg/(m{sup 2}.day) and anticipated future enhanced Hanford Tank Waste Treatment and Immobilization Plant (WTP) requirement of 1000 kg/(m{sup 2}.day).

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Advanced High-Level Waste Glass Research and Development Plan

The U.S. Department of Energy Office of River Protection (ORP) has implemented an integrated program to increase the loading of Hanford tank wastes in glass while meeting melter lifetime expectancies and process, regulatory, and product quality requirements. The integrated ORP program is focused on providing a technical, science-based foundation from which key decisions can be made regarding the successful operation of the Hanford Tank Waste Treatment and Immobilization Plant (WTP) facilities. The fundamental data stemming from this program will support development of advanced glass formulations, key process control models, and tactical processing strategies to ensure safe and successful operations for both the low-activity waste (LAW) and high-level waste (HLW) vitrification facilities with an appreciation toward reducing overall mission life. The purpose of this advanced HLW glass research and development plan is to identify the near-, mid-, and longer-term research and development activities required to develop and validate advanced HLW glasses and their associated models to support facility operations at WTP, including both direct feed and full pretreatment flowsheets. This plan also integrates technical support of facility operations and waste qualification activities to show the interdependence of these activities with the advanced waste glass (AWG) program to support the full WTP mission. Figure ES-1 shows these key ORP programmatic activities and their interfaces with both WTP facility operations and qualification needs. The plan is a living document that will be updated to reflect key advancements and mission strategy changes. The research outlined here is motivated by the potential for substantial economic benefits (e.g., significant increases in waste throughput and reductions in glass volumes) that will be realized when advancements in glass formulation continue and models supporting facility operations are implemented. Developing and applying advanced glass formulations will reduce the cost of Hanford tank waste management by reducing the schedule for tank waste treatment and reducing the amount of HLW glass for storage, transportation, and disposal. Additional benefits will be realized if advanced glasses are developed that demonstrate more tolerance for key components in the waste (such as Al 2 O 3 , Cr 2 O 3 , SO 3 and Na 2 O) above the currently defined WTP constraints. Tolerating these higher concentrations of key waste loading limiters may reduce the burden on (or even eliminate the need for) leaching to remove Cr and Al and washing to remove excess S and Na from the HLW fraction. Advanced glass formulations may also make direct vitrification of the HLW fraction without significant pretreatment more cost effective. Finally, the advanced glass formulation efforts seek not only to increase waste loading in glass, but also to increase glass production rate. When coupled with higher waste loading, ensuring that all of the advanced glass formulations are processable at or above the current contract processing rate leads to significant improvements in waste throughput (the amount of waste being processed per unit time),which could significantly reduce the overall WTP mission life. The integration of increased waste loading, reduced leaching/washing requirements, and improved melting rates provides a system-wide approach to improve the effectiveness of the WTP process.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effects of High Spinel and Chromium Oxide Crystal Contents on Simulated HLW Vitrification in DM100 Melter Tests (Final Report)

The principal objective of the work was to evaluate the effects of spinel and chromium oxide particles on WTP HLW melter operations and potential impacts on melter life. This was accomplished through a combination of crucible-scale tests, settling and rheological tests, and tests on the DM100 melter system. Crucible testing was designed to develop and identify HLW glass compositions with high waste loadings that exhibit formation of crystalline spinel and/or chromium oxide phases up to relatively high crystal contents (i.e., > 1 vol%). Characterization of crystal settling and the effects on melt rheology was performed on the HLW glass formulations. Appropriate candidate HLW glass formulations were selected, based on characterization results, to support subsequent melter tests. In the present work, crucible melts were formulated that exhibit up to about 4.4 vol% crystallization.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Glass Property Models, Constraints, and Formulation Approaches for Vitrification of High-Level Nuclear Wastes at the US Hanford Site

The legacy nuclear wastes stored in underground tanks at the US Department of Energy’s Hanford site is planned to be separated into high-level waste and low-activity waste fractions and vitrified separately. Formulating optimized glass compositions that maximize the waste loading in glass is critical for successful and economical treatment and immobilization of nuclear wastes. Glass property-composition models have been developed and applied to formulate glass compositions for various objectives for the past several decades. The property models with associated uncertainties and combined with composition and property constraints have been used to develop preliminary glass formulation algorithms designed for vitrification process control and waste form qualification at the planned waste vitrification plant. This paper provides an overview of current status of glass property-composition models, constraints applicable to Hanford waste vitrification, and glass formulation approaches that have been developed for vitrification of hazardous and highly radioactive wastes stored at the Hanford site.

composition constraint↗

Advanced waste form and Melter development for treatment of troublesome high-level wastes

A number of waste components in US defense high level radioactive wastes (HLW) have proven challenging for current Joule heated ceramic melter (JHCM) operations and have limited the ability to increase waste loadings beyond already realized levels. Many of these “troublesome" waste species cause crystallization in the glass melt that can negatively impact product quality or have a deleterious effect on melter processing. Recent efforts at US Department of Energy laboratories have focused on understanding crystallization behavior within HLW glass melts and investigating approaches to mitigate the impacts of crystallization so that increases in waste loading can be realized. Advanced glass formulations have been developed to highlight the unique benefits of next-generation melter technologies such as the Cold Crucible Induction Melter (CCIM). Crystal-tolerant HLW glasses have been investigated to allow sparingly soluble components such as chromium to crystallize in the melter but pass out of the melter before accumulating.The Hanford site AZ-101 tank waste composition represents a waste group that is waste loading limited primarily due to high concentrations of Fe 2 O 3 (also with high Al 2 O 3 concentrations). Systematic glass formulation development utilizing slightly higher process temperatures and higher tolerance to spinel crystals demonstrated that an increase in waste loading of more than 20% could be achieved for this waste composition, and by extension higher loadings for wastes in the same group. An extended duration CCIM melter test was conducted on an AZ-101 waste simulant using the CCIM platform at the Idaho National Laboratory (INL). The melter was continually operated for approximately 80 hours demonstrating that the AZ-101 high waste loading glass composition could be readily processed using the CCIM technology. The resulting glass was close to the targeted composition and exhibited excellent durability in both the as poured state and after being slowly cooled according to the canister centerline cooling (CCC) profile. Glass formulation development was also completed on other Hanford tank wastes that were identified to further challenge waste loading due to the presence of appreciable quantities (>750 g) of plutonium in the waste tanks. In addition to containing appreciable Pu quantities, the C-102 waste tank and the 244-TX waste tank contain high concentrations of aluminum and iron, respectively that will further challenge vitrification processing. Glass formulation testing also demonstrated that high waste loadings could be achieved with these tank compositions using the attributes afforded by the CCIM technology.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

High Level Waste Vitrification System Improvements (Final Report)

This report describes work conducted to support the development and testing of new glass formulations that extend beyond those that have been previously investigated for the Hanford Waste Treatment and Immobilization Plant (WTP). The principal objective was to investigate maximization of the incorporation of several waste components that are expected to limit waste loading and, consequently, high level waste (HLW) processing rates and canister count. The work was performed with four waste compositions specified by the Office of River Protection (ORP); these wastes contain high concentrations of bismuth, chromium, aluminum, and aluminum plus sodium. The tests were designed to identify glass formulations that maximize waste loading while meeting all processing and product quality requirements. The work included preparation and characterization of crucible melts in support of subsequent DuraMelter 100 (DM100) tests designed to examine the effects of enhanced glass formulations, increased glass processing temperature, increased crystallinity, and feed solids content on waste processing rate and product quality.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

The WTP Immobilized LAW Formulation Algorithm: Recent Efforts Toward Software Development - 17342

The immobilized low-activity waste (ILAW) product from WTP must meet certain requirements and processing constraints. The strategy for controlling ILAW product composition uses the ILAW formulation algorithm. This algorithm is approved by the DOE Office of River Protection (ORP) for use in calculating melter feed recipes that will produce acceptable ILAW product during Low-Activity Waste (LAW) Facility commissioning. The calculations performed by the algorithm have been demonstrated using a sophisticated spreadsheet, but this spreadsheet is not expected to support continuous operation. Efforts are underway to develop software that will support glass formulation during operation. Recent work toward software development includes an examination of assumptions made in the algorithm about expected LAW Facility operation, and spreadsheet calculations to formulate glass for potential LAW compositions under the direct feed LAW (DFLAW) strategy that ORP has adopted. The documentation of the ILAW algorithm is the planned basis for software development. However, some assumptions made in the current algorithm's mass balance logic do not match the matured design and expected operation of the LAW Facility. A self-assessment effort evaluated the validity of these assumptions by reviewing design documents, in order to identify opportunities to align the algorithm's mass balance logic with the matured design and ensure that the developed software supports continuous LAW Facility operation. Several improvement opportunities were identified and are discussed. The results of ILAW algorithm calculations to formulate glass for eighteen challenging LAW compositions indicate that the current WTP baseline LAW glass models are sufficiently robust to accommodate DFLAW. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

WASTE LOADING ENHANCEMENTS FOR HANFORD LAW GLASSES VLS-10R1790-1 FINAL REPORT REV 0 12/1/2010

About 50 million gallons of high-level mixed waste is currently stored in underground tanks at The United States Department of Energy's (DOE's) Hanford site in the State of Washington. The Hanford Tank Waste Treatment and Immobilization Plant (WTP) will provide DOE's Office of River Protection (ORP) with a means of treating this waste by vitrification for subsequent disposal. The tank waste will be separated into low- and high-activity waste fractions, which will then be vitrified respectively into Immobilized Low Activity Waste (ILAW) and Immobilized High Level Waste (IHLW) products. The ILAW product will be disposed in an engineered facility on the Hanford site while the IHLW product will likely be directed to a national deep geological disposal facility for high-level nuclear waste. The ILAW and IHLW products must meet a variety of requirements with respect to protection of the environment before they can be accepted for disposal. The Office of River Protection is currently examining options to optimize the Low Activity Waste (LAW) Facility and LAW glass waste form. One option under evaluation is to enhance the waste processing rate of the vitrification plant currently under construction. It is likely that the capacity of the LAW vitrification plant can be increased incrementally by implementation of a variety of low-risk, high-probability changes, either separately or in combination. These changes include: (1) Operating at the higher processing rates demonstrated at the LAW pilot melter; (2) Increasing the glass pool surface area within the existing external melter envelope; (3) Increasing the glass waste loading; and (4) Operating the melter at a slightly higher temperature. The Vitreous State Laboratory (VSL) of The Catholic University of America (CUA) and Energy Solutions, Inc. have evaluated several of these potential incremental improvements for ORP in support of its evaluation of WTP LAW facility optimization. Some of these incremental improvements have been tested at VSL including increasing the waste loading, increasing the processing temperature, and increasing the fraction of the sulfur in the feed that is partitioned to the off-gas (in the event that a decision is made to break the present WTP recycle loop). These approaches successfully demonstrated increases in glass production rates and significant increases in sulfate incorporation at the nominal melter operating temperature of 1150 C and at slightly higher than nominal glass processing temperatures. Subsequent tests demonstrated further enhancement of glass formulations for all of the LAW waste envelopes, thereby reducing the amount of glass to be produced by the WTP for the same amount of waste processed. The next phase of testing determined the applicability of these improvements over the expected range of sodium and sulfur concentrations for Hanford LAW. This approach was subsequently applied to an even wider range of LAW wastes types, including those with high potassium concentration. The feasibility of formulating higher waste loading glasses using SnO{sub 2} and V{sub 2}O{sub 5} in place of Fe{sub 2}O{sub 3} and TiO{sub 2} as glass former additives was also evaluated. The present report provides data from investigation of the effects of magnesium content (up to {approx}10 wt%) on LAW glass properties and from work to identify improved high waste loading glass formulations that meets all processing and product quality requirements for two waste compositions. The scope of testing is detailed in the Test Plan for this work. A glass composition previously developed and tested at VSL for LAW from tank AN-105 (LAWA187) was varied by substituting Mg for other glass former additives such as Ca, B and Si in an attempt to formulate a glass with improved properties, such as higher waste loading and greater sulfur tolerance. The results were used to reformulate another glass (ORPLG9) developed for LAW from tank AP-101 that contains high concentrations of alkalis (Na and K). Glass formulation goals for this waste were to increase the sulfur tolerance of the glass as well as to decrease refractory corrosion. Each of the two final glass compositions was evaluated to determine the maximum amount of sulfur that can be incorporated into the glass through melter testing. The results from these tests together with earlier work for ORP were evaluated to develop recommendations for the work scope necessary to modify and update the WTP LAW glass formulation correlation algorithm.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

HLW Processing for Complementary Disposition Strategy: Development and Testing of Glass and Feed Formulations

The objective of the work described herein was to develop and identify HLW glass compositions and glass forming additive blends for vitrification of selected HLW streams, which have undergone various degrees of washing but no other pretreatment, while maintaining high WLs, high processing rates, and acceptable glass properties. The glass formulations were actively designed and based on previous formulation experience and testing at VSL. The WTP baseline HLW property-composition models were used to select glass formulations for testing and to predict various glass properties. Crucible-scale fabrication of the HLW glasses that were formulated was performed and the product glasses were characterized with respect to select properties. A total of 10 HLW glasses were developed and tested for five fully washed waste batches and one singly washed waste batch.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Candidate Low-Temperature Glass Waste Forms for Technetium-99 Recovered from Hanford Effluent Management Facility Evaporator Concentrate

Alternative treatment and disposition options may exist for technetium-99 (99Tc) in secondary liquid waste from the Hanford Direct-Feed Low-Activity Waste (DFLAW) process. One approach includes development of an alternate glass waste form that is suitable for on-site disposition of technetium, including salts and other species recovered by ion exchange or precipitation from the EMF evaporator concentrate. By recovering the Tc content from the stream, and not recycling the treated concentrate, the DFLAW process can potentially be operated in a more efficient manner that lowers the cost to the Department of Energy. This report provides a survey of candidate glass formulations and glass-making processes that can potentially incorporate technetium at temperatures <700 °C to avoid volatilization. Three candidate technetium feed streams are considered: (1) dilute sodium pertechnetate loaded on a non-elutable ion exchange resin; (2) dilute sodium-bearing aqueous eluent from ion exchange recovery of pertechnetate, or (3) technetium(IV) oxide precipitate containing Sn and Cr solids in an aqueous slurry. From the technical literature, promising candidate glasses are identified based on their processing temperatures and chemical durability data. The suitability and technical risk of three low-temperature glass processing routes (vitrification, encapsulation by sintering into a glass composite material, and sol-gel chemical condensation) for the three waste streams was assessed, based on available low-temperature glass data. For a subset of candidate glasses, their long-term thermodynamic behavior with exposure to water and oxygen was modeled using Geochemist’s Workbench, with and without addition of reducing stannous ion. For further evaluation and development, encapsulation of precipitated TcO2/Sn/Cr in a glass composite material based on lead-free sealing glasses is recommended as a high priority. Vitrification of pertechnetate in aqueous anion exchange eluent solution using a high lead content borate glass, or other low melting glass is also recommended for further evaluation and development. Additional laboratory studies of phase behavior and chemical durability of low-temperature glasses is also recommended to provide risk mitigation if one of the primary development paths proves infeasible. This report is a deliverable for the task “Candidate Low-T Glass Waste Forms for EMF Bottoms On-Site Disposition Alternative Option.”

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Glass Crystallization Constraints for WTP LAW Operations: Assessment of Isothermal Treatments on Crystal Formation

Much work has been done to expand the glass composition region available for operation of the Hanford Tank Waste Treatment and Immobilization Plant. This includes the development of updated glass property-composition models as well as constraints. This report supports this effort by suggesting constraints for avoiding excessive, and likely detrimental, crystallization during melter operation while processing advanced low-activity glasses. The constraints target Cassiterite and ZrO 2 -containing phases (ZCP, e.g., Baddeleyite and Zircon) that can form when melter temperatures drop below 1100 °C. These types of crystals were found to be potentially detrimental during processing as they are denser than low-activity waste glass melts; with densities of 6.95 g/cm 3 for Cassiterite and 5.68 g/cm 3 for Baddeleyite (the most prevalent ZCP). Compared to melt densities of approximately 2.65 g/cm 3 . Thus, they have the potential to form during melter idling and settle to the bottom of the melter or inside the melter. If the crystals are present in appreciable amounts, they can result in blockages of the pour-spout riser, which impacts glass pouring and melter operation. Additionally, SnO 2 and ZrO 2 are added to glass formulations to improve glass durability. Their precipitation from the melt may reduce overall glass durability. Using previously acquired results and results from testing during this effort, the following constraints (Table S.1) were determined and are recommended to reduce the risk of forming crystals of the types and concentrations that are likely detrimental to melter operation.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

OFFGAS GENERATION FROM THE DISPOSITION OF SCRAP PLUTONIUM BY VITRIFICATION SIMULANT TESTS

The Department of Energy Office of Environmental Management is supporting R&D for the conceptual design of the Plutonium Disposition Project at the Savannah River Site in Aiken, SC to reduce the attractiveness of plutonium scrap by fabricating a durable plutonium oxide glass form and immobilizing this form within the high-level waste glass prepared in the Defense Waste Processing Facility. A glass formulation was developed that is capable of incorporating large amounts of actinides as well as accommodating many impurities that may be associated with impure Pu feed streams. The basis for the glass formulation was derived from commercial glasses that had high lanthanide loadings. A development effort led to a Lanthanide BoroSilicate (LaBS) glass that accommodated significant quantities of actinides, tolerated impurities associated with the actinide feed streams and could be processed using established melter technologies. A Cylindrical Induction Melter (CIM) was used for vitrification of the Pu LaBS glass. Induction melting for the immobilization of americium and curium (Am/Cm) in a glass matrix was first demonstrated in 1997. The induction melting system was developed to vitrify a non-radioactive Am/Cm simulant combined with a glass frit. Most of the development of the melter itself was completed as part of that work. This same melter system used for Am/Cm was used for the current work. The CIM system used consisted of a 5 inch (12.7 cm) diameter inductively heated platinum-rhodium (Pt-Rh) containment vessel with a control system and offgas characterization. Scrap plutonium can contain numerous impurities including significant amounts of chlorides, fluorides, sodium, potassium, lead, gallium, chromium, and nickel. Smaller amounts of additional elements can also be present. The amount of chlorides present is unusually high for a melter feed. In commercial applications there is no reason to have chloride at such high concentrations. Because the melter operates at 1400-1475 C, many of the impurities present are extremely volatile. An alternative being considered is to pre-treat the impure PuO{sub 2} by water washing to remove the soluble salts, which would significantly reduce the melter emissions. The disadvantage of the washing alternative is the criticality concerns of using water with plutonium. In this paper, the testing that has been conducted at the Savannah River National Laboratory (SRNL) to demonstrate induction melting of impure plutonium simulants will be described. The work described concentrates on quantification of the gaseous and particulate emissions from the induction melter. The Pt-Rh melter vessel is a cylinder with a conical bottom and a tubular drain as shown in Figure 1. A 5-inch (12.7 cm) diameter CIM was used for all of the emissions tests. A 6-inch (15.24 cm) diameter CIM, which is the size of the full-scale melter, has since been constructed for further testing. The 5-inch CIM is heated by three induction coils: one for the 5 inch cylinder, one for the conical section, and one for the 1/4-inch (6.35 mm) drain tube. The 6-inch CIM is similar except the cylinder heater extends lower and also heats the cone. The induction heating system is manufactured by Ameritherm{trademark}. The heating system is controlled by a PC to maintain a specific heat up profile and then maintain a constant energy input that maintains a constant temperature. The CIM is operated in batch mode where the plutonium simulant and the glass-forming frit are first thoroughly mixed in an attrittor mill, then added to the melter. Hafnium oxide (HfO{sub 2}) is used as a simulant for the radioactive PuO{sub 2}. The melter is heated until the mixture begins to melt at about 1100 C, then completely melts at about 1400-1450 C. This temperature is maintained for about three hours. While the temperature is maintained at {approx} 1400 C, an air bubbler is normally used to promote mixing of the glass-forming frit and the waste simulant.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Improved Alumina Loading in High-Level Waste Glasses

Recent tank retrieval, blending, and treatment strategies at both the Savannah River Site (SRS) and Hanford have identified increased amounts of high-Al{sub 2}O{sub 3} waste streams that are scheduled to be processed through their respective high-level waste (HLW) vitrification facilities. It is well known that the addition of small amounts of Al{sub 2}O{sub 3} to borosilicate glasses generally enhances the durability of the waste glasses. However, at higher Al{sub 2}O{sub 3} concentrations nepheline (NaAlSiO{sub 4}) formation can result in a severe deterioration of the chemical durability of the slowly cooled glass near the center of the canister. Additionally, higher concentrations of Al{sub 2}O{sub 3} generally increase the liquidus temperature of the melt and decrease the processing rate. Pacific Northwest National Laboratory (PNNL), Savannah River National Laboratory (SRNL), and Khlopin Radium Institute (KRI) are jointly performing laboratory and scaled-melter tests, through US Department of Energy, EM-21 Office of Waste Processing program, to develop glass formulations with increased Al{sub 2}O{sub 3} concentrations. These glasses are formulated for specific DOE waste compositions at Hanford and Savannah River Site. The objectives are to avoid nepheline formation while maintaining or meeting waste loading and/or waste throughput expectations as well as satisfying critical process and product performance related constraints such as viscosity, liquidus temperature, and glass durability. This paper summarizes the results of recent tests of simulated Hanford HLW glasses containing up to 26 wt% Al{sub 2}O{sub 3} in glass. In summary: Glasses with Al{sub 2}O{sub 3} loading ranging from 25 to 27 wt% were formulated and tested at a crucible scale. Successful glass formulations with up to 26 wt% Al{sub 2}O{sub 3} that do not precipitate nepheline during CCC treatment and had spinel crystals 1 vol% or less after 24 hr heat treatment at 950 deg. C were obtained. The selected glass, HAL-17 with 26 wt% Al{sub 2}O{sub 3}, had viscosity and electrical conductivity within the boundaries for adequate processing in the Joule heated melters operated at 1150 deg. C. This HAL-17 glass was successfully processed using small-scale (SMK) and larger scale (EP-5) melters. There was no indication of spinel settling during processing. The product glass samples from these melter tests contained 1 to 4 vol% spinel crystals that are likely formed during cooling. The PCT tests on the product glasses are underway. The present study demonstrated that it is possible to formulate the glasses with up to 26 wt% Al{sub 2}O{sub 3} that satisfy the property requirements and is processable with Joule-heated melters operated at 1150 deg. C. The 'nepheline discriminator' for HAL-17 glass is 0.45, which supports that claim that the current rule ('nepheline discriminator' < 0.62) is too restrictive. Considering that the cost of HLW treatment is highly dependent on loading of waste in glass, this result provides a potential for significant cost saving for Hanford. The maximum Al{sub 2}O{sub 3} loading that can be achieved will also depend on concentrations of other components in wastes. For example, the loading of waste used in this study was also limited by the spinel crystallization after 950 deg. C 24 hr heat treatment, which suggests that the concentrations of spinel-forming components such as Fe{sub 2}O{sub 3}, Cr{sub 2}O{sub 3}, NiO, ZnO, and MnO would be critical in addition to Al{sub 2}O{sub 3} for the maximum Al{sub 2}O{sub 3} loading achievable. The observed glass production rate per unit melter surface area of 0.75 MT/(d.m{sup 2}) for SMK test is comparable to the design capacity of WTP HLW melters at 0.8 MT/(d.m{sup 2}). However, the test with EP-5 melter achieved 0.38 MT/(d.m{sup 2}), which is roughly a half of the WTP design capacity. This result may imply that the glass with 26 wt% Al{sub 2}O{sub 3} may not achieve the WTP design production rate. However, this hypothesis is not conclusive because of unknown effects of melter size and operational differences. Further testing is needed to quantify the effect of high Al{sub 2}O{sub 3} loading on glass production rate. (authors)