Demonstration of the Reproducibility Challenges in the Sintering Behavior of Lithium‐Stuffed Garnets in Scaling up Synthesis

Lithium-stuffed garnets, such as Li 7 La 3 Zr 2 O 12 (LLZO), are promising candidates for next-generation solid-state batteries because of their high room-temperature ionic conductivity and chemical stability against lithium metal anodes, which are crucial for achieving higher energy density. However, realizing LLZO's potential in practical devices requires synthesis methods that can be scaled reliably to large batch sizes for manufacturing. Herein, we investigate the sintering reproducibility of LLZO synthesized at larger scales using ultrasonic spray pyrolysis, a cost-effective and scalable synthesis route. Two 100 g batches of Al-doped LLZO are prepared and their sintering behavior is examined in detail. Both Al-LLZO batches contain over 90 wt.% cubic-phase LLZO, and both batches exhibit room temperature conductivities greater than 1 × 10 −4 S cm −1 at a relative density above 0.8. However, variations in secondary phases and subtle differences in Al content lead to significant differences in densification and microstructure. These results demonstrate that LLZO's sintering behavior is highly sensitive to small changes in secondary phases and Al content, creating reproducibility challenges when moving from laboratory- to manufacturing-scale synthesis.

36 MATERIALS SCIENCE↗

Efficacy of Gadolinium Gallium Garnet (GGG) as a High-Impedance Optical Window for Shock Wave Experiments

We conducted a series of plate impact experiments to examine the efficacy of < 111>-oriented gadolinium gallium garnet (GGG) single crystals as high-impedance optical window for Photonic Doppler velocimetry (PDV) under shock and double-shock loading. At ~ 123 GPa, shocked GGG remains fully transparent to 1550 nm light for at least 250 ns without any signal degradation. Above 135 GPa, PDV data measured through GGG exhibit a gradual loss of fringe contrast following shock entrance, which eventually leads to transparency loss. The duration for which shocked GGG remains transparent decreases with increasing pressure, and at ~ 148 GPa, it becomes opaque within ~ 20–30 ns. This limits the use of GGG as an interferometry window between ~ 110–140 GPa under single shock loading. Within this pressure range, the refractive index of GGG increases linearly with density: n = 1.552 + 0.054ρ. In contrast to single shock loading, where GGG becomes opaque rapidly above ~ 140 GPa, double-shocked GGG remains optically transparent for over 100 ns when it is first shocked to ~ 123 GPa and then reshocked to significantly higher pressures (215–233 GPa). Our findings raise the exciting possibility of GGG being used as a high-impedance optical window in multi-shock and shock-ramp loading experiments.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Robust perpendicular magnetic anisotropy in off-axis sputtered europium iron garnet (EuIG) thin films

In this study, the rare earth iron garnet (REIG), Eu 3 Fe 5 O 12 (EuIG) has emerged as a promising material for ferrimagnetic insulator based spintronics. Earlier studies have shown that perpendicular magnetic anisotropy (PMA) in EuIG and other REIGs can be achieved by magnetostriction and misfit strain at the film-substrate interface. Typically, the strain relaxes significantly with thickness, limiting the thickness of films that can be grown using this strategy. Here we show PMA that does not reduce substantially with thickness in epitaxial EuIG films grown by off-axis sputtering; The PMA remains robust in films > 100 nm thick. Epitaxially induced strain with minimal relaxation is confirmed using high resolution symmetric and asymmetric x-ray diffraction reciprocal space maps.

36 MATERIALS SCIENCE↗

Detecting Magnon-phonon coupling in yttrium iron garnet with variable temperature STEM-EELS

Magnons, quanta of spin wave excitations in magnetically ordered materials, have been identified as candidates for several potentially transformative technologies in recent years. Macroscopic techniques, such as neutron scattering or Raman spectroscopy, can be used to identify and analyze magnons, but provide relatively delocalized information about the sample. Understanding how the bonding and local structure of a material interacts with, and influences, the magnon population in a material is a crucial step toward the ability to produce any real-world application utilizing magnons. By leveraging the combined spatial resolution of scanning transmission electron microscopy (STEM) and the energy resolution of monochromated electron energy-loss spectroscopy (EELS) nanoscale analysis of magnons can be performed. While the weak interaction of magnons with the electron beam makes magnon EELS challenging on reasonable timescales, magnon-phonon coupling can be leveraged to understand magnons through their effect on the more easily measured phonons. Here, we examine yttrium iron garnet (YIG) flakes, and demonstrate non-linear, temperature-dependent shifts in the phonon frequencies, consistent with previously described magnon-phonon coupling effects. The ability to measure the temperature-dependence of vibrational frequencies with high precision in individual nanoscale flakes, demonstrates the ability to study magnon-phonon coupling in the STEM with unprecedented spatial resolution.

Reifsnyder, Alexander [ORNL]↗

Effect of H + Exchange and Surface Impurities on Bulk and Interfacial Electrochemistry of Garnet Solid Electrolytes

Contact loss and current constriction pose significant challenges at the Li metal interface of solid-state batteries. For garnet-structured Li 7 La 3 Zr 2 O 12 (LLZO), these effects are amplified by Li + /H + exchange and surface contamination reactions, which lead to conductivity losses and poor Li wetting. In this study, we utilize a variety of surface treatment processes across 37 cells to selectively induce proton exchange and contamination reactions in LLZO. The resulting bulk and surface chemistry is systematically characterized and correlated to changes in electrochemical properties. Additionally, we combine impedance analysis and finite element method modeling to deconvolute sources of impedance contributions at the Li metal interface. Specifically, we show that constriction impedance at the Li metal interface arises not solely from voids, but also from ionically-resistive surface contaminants. Further, these findings emphasize the connection between ionic conductivity and constriction, demonstrating that micron-scale ionically-resistive components increase constriction even with identical contact geometries. Finally, we leverage our comprehensive dataset to highlight unstable overpotential growth as a failure mechanism, additionally showing that the phase of a cell’s impedance is a sensitive indicator for the onset of interfacial instability. Overall, this study clarifies the impacts of proton exchange and surface contamination on electrochemical properties at the Li|solid electrolyte interface and elucidates insights that are generalizable to other solid-state battery systems.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrochemical Oxidation in Garnet-Type Solid Electrolyte by Formation of Point Defects

All-solid-state batteries hold greater promise for improving safety and energy density over conventional battery technology employing organic liquid electrolytes. One of the required features of a Li + conducting solid electrolyte is electrochemical stability, attained thermodynamically or kinetically, within the targeted operating voltage and temperature ranges. Therefore, understanding of the oxidative or reductive degradation mechanism is important to allow the design of stable solid electrolyte materials. This work contributes to building an understanding of the oxidative degradation mechanism in lithium solid electrolytes at cell operating conditions. Here, we have focused on resolving the oxidative decomposition mechanism of Al-doped lithium garnet Li 6.28 Al 0.24 La 3 Zr 2 O 12 (LLZO) as a state-of-the-art inorganic ceramic electrolyte. By combining experimental and computational analyses, we show that oxidation of LLZO occurs by simultaneous loss of oxygen and lithium from the structure, resulting in substoichiometric LLZO, at a moderate temperature (80 °C) and a high electrode potential (4.3 V vs Li/Li + ). Based on X-ray absorption and diffraction analyses, we find that the zirconium coordination shells in LLZO contract while the crystal structure experiences positive chemical strain upon electrochemical oxidation. The results from ex situ structural characterization of both the local structure and crystal symmetry are supported by a substoichiometric LLZO with lithium and oxygen vacancies, modeled by density functional theory (DFT) calculations. These chemical and structural changes in LLZO suppress effective lithium-ion conductivity by an order of magnitude. Formation of lithium and oxygen vacancies in LLZO upon electrochemical oxidation is different from prior thermodynamic predictions of phase decomposition of LLZO. The difference here is that the experiments were conducted at near-room temperature, which can hinder the kinetics of phase separation, and thus, the resultant LLZO solid electrolyte is still single-phase but substoichiometric in Li and O. In conclusion, these findings contribute an important degradation mechanism of the electrolyte, relevant for practical operational conditions of solid-state batteries.

36 MATERIALS SCIENCE↗

La 2 Zr 2 O 7 Nanoparticle-Mediated Synthesis of Porous Al-Doped Li 7 La 3 Zr 2 O 12 Garnet

In this work, we modified the reaction pathway to quickly (minutes) incorporate lithium and stabilize the ionic conducting garnet phase by decoupling the formation of a La–Zr–O network from the addition of lithium. To do this, we synthesized La 2 Zr 2 O 7 (LZO) nanoparticles to which LiNO 3 was added. This method is a departure from typical solid-state synthesis methods that require high-energy milling to promote mixing and intimate particle–particle contact and from sol–gel syntheses as a unique porous microstructure is obtained. We show that the reaction time is limited by the rate of nitrate decomposition and that this method produces a porous high-Li-ion-conducting cubic phase, within an hour, that may be used as a starting structure for a composite electrolyte.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electro-Chemo-Mechanical Evolution at the Garnet Solid Electrolyte–Cathode Interface

Solid-state batteries promise higher energy density and improved safety compared with lithium-ion batteries. However, electro-chemomechanical instabilities at the solid electrolyte interface with the cathode and the anode hinder their large scale implementation. Here, in this study, we focus on resolving electro-chemo-mechanical instability mechanisms and their onset conditions between a state-of-the-art cathode, LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622), and the garnet Li 7 La 3 Zr 2 O 12 (LLZO) solid electrolyte. We used thin-film NMC622 on LLZO pellets to place the interfacial region within the detection depth of the X-ray characterization techniques. The experimental probes of the near-interface region included in operando X-ray absorption spectroscopy and ex situ focused ion beam scanning electron microscopy. Electrochemical degradation was not observable during cycling at room temperature with 4.3 V versus Li/Li + charge voltage cutoff, or with stepwise potentiostatic hold up to 4.1 V versus Li/Li + . In contrast, secondary phases including reduced transition metal species (Ni 2+ , Co 2+ ) were found after cycling up to 4.3 V versus Li/Li + at 80 °C and during potentiostatic hold at 4.3 V versus Li/Li + (Ni 2+ ). Intergranular cracks between NMC622 grains and delamination at the NMC622|LLZO interface occurred readily after the first charge. These interface reaction products and mechanical failure lowered the capacity and cell efficiency due to partial loss of the NMC622 phase, partial loss of contact at the interface, and a higher polarization resistance. Electrochemical instability between delithiated NMC622 and LLZO could be mitigated by using a low charge voltage cutoff or cycling at lower temperature. Ways to engineer the mechanical properties to avoid crack deflection and delamination at the interface are also discussed for enhancing mechanical stability.

36 MATERIALS SCIENCE↗

CO 2 Laser Sintering of Garnet-Type Solid-State Electrolytes

We report the processing of garnet-type solid-state electrolytes remains challenging as densification conventionally requires high sintering temperatures and long processing times, which can result in severe Li loss, the formation of secondary phases, and thus high porosity and low ionic conductivity. Here, we report an ultrafast sintering method based on CO 2 laser scanning with the assistance of a heating stage. We demonstrate the rapid densification of low-packing-density Li 6.4 La 3 Zr 1.4 Ta 0.6 O 12 (LLZTO) films, which are difficult to densify by conventional furnace sintering methods. This unique approach has three fingerprint characteristics: (1) mitigation of Li loss through ultrafast sintering (dwelling time $\ll$1 s); (2) a unique anisotropic shrinkage behavior that greatly reduces film thickness; (3) wave-like surface topology from point scanning strategy that enables 3D interfacial contacts with electrode materials. Herein, highly dense (95.68%) and highly conductive (0.26 mS·cm –1 at 25 °C) LLZTO films are obtained through CO2 laser sintering. This work provides a unique, scalable, and widely applicable ultrarapid laser sintering technique to overcome the difficulties associated with classic methods for the integration of SSEs for practical all-solid-state Li-metal battery applications.

36 MATERIALS SCIENCE↗

Comparative Analysis of Reactivity of Al and Ga Doped Garnet Solid State Electrolyte at the Interface with Li Metal

Lithium garnet (Li 7 La 3 Zr 2 O 12 , LLZO) based solid electrolytes are leading candidate materials for all-solid-state batteries with lithium metal anodes because of their high ionic conductivity, high mechanical toughness, and superior electrochemical stability. While doping LLZO with Al and Ga increases its ionic conductivity by stabilizing the cubic phase, the impact of dopants on its (electro)chemical stability at the interfaces with Li metal is critical. Here, our study of differences between Al- and Ga-doped LLZO when interfaced with lithium metal using X-ray photoelectron spectroscopy and density functional theory shows a higher propensity of Ga to move across LLZO interface with Li metal and form Ga-Li alloy. Additionally, neutron diffraction reveals loss of cubic phase resulting from the loss of dopant that explains electrochemical behavior differences between Ga- and Al-doped LLZO. Overall, our study reveals the key role of dopant chemistry in enabling stable solid electrolyte materials for all-solid-state batteries.

Klenk, Matthew↗

Elimination of detrimental grain boundary segregation in garnets

Garnet Li 7 La 3 Zr 2 O 12 electrolyte is considered a key enabler of solid-state batteries with Li metal electrodes, but the grain boundaries impair its performance. To date, the understanding of grain boundary structures and its impact on performance remains elusive. Here, we show that element segregation at Li 7 La 3 Zr 2 O 12 grain boundaries critically governs Li transport and nucleation. During conventional sintering, Al, Ta, and La segregate at grain boundaries, locally depleting Li and creating space-charge layers that lower total ionic conductivity. Simultaneously, this segregation leads to higher electronic conductivity along grain boundaries, which promotes Li nucleation at grain boundary edges with increased risk of dendrite formation. The underlying mechanism of segregation is governed by both thermodynamic driving forces and diffusion kinetics. Building on this understanding, we develop a strategy to achieve segregation-free grain boundaries through a rapid sintering protocol that utilizes the onset of solid-state softening. This approach yields transparent, polycrystalline Li 7 La 3 Zr 2 O 12 with negligible grain boundary impedance and enhanced dendrite tolerance. By elucidating the structural origins and electrochemical consequences of grain boundary segregation, this work provides a guidance for the rational optimization of solid electrolytes.

Energy - Storage↗

Grain boundary zirconia-modified garnet solid-state electrolyte

Here, we report a method for promoting electrochemical stability in garnet Li 6.4 La 3 Zr 1.4 Ta 0.6 O 12 solid-state electrolyte based on a composite two-phase oxide–oxide microstructure. Grain boundary precipitation of the controlled distribution of amorphous zirconium oxide microparticles is achieved through the addition of reactive tantalum carbide. During ambient-atmosphere sintering, the carbide decomposes through an in situ reaction, the ‘extra’ Ta substituting for Zr within the Li 6.4 La 3 Zr 1.4 Ta 0.6 O 12 lattice. Density functional theory (DFT) calculations identify a thermodynamically favourable reaction path and show how substituting Ta 5+ at Zr 4+ sites affects the crystal structure as well as bulk ionic and electronic conductivities. Quantitative stereology highlights that zirconia also acts as a sintering aid, reducing compact porosity. Cryogenic focused-ion-beam scanning electron microscopy and fractography analysis of cycled solid-state electrolytes illustrates that near-universally observed intergranular Li-metal dendrite propagation is suppressed by the two-phase microstructure, favouring transgranular dendrites instead. Importantly, DFT demonstrates that compared with the Li 6.4 La 3 Zr 1.4 Ta 0.6 O 12 surface, the zirconium oxide surface per se is less electronically conductive and does not trap excess electrons to reduce Li ions. This is a key reason for the substantial improvement in the electrochemical properties over the single-phase baseline.

36 MATERIALS SCIENCE↗

Floating zone crystal growth, structure, and properties of a cubic Li 5.5 La 3 Nb 1.5 Zr 0.5 O 12 garnet-type lithium-ion conductor

As a promising candidate for solid-state electrolytes in Li-ion batteries, the garnet-type Li-ion conductor series Li 5+x La 3 Nb 2-x Zr x O 12 (LLNZO) (0 ≤ x ≤ 2) exhibits high ionic conductivity at room temperature. However, no previous single-crystal growth or characterization has been reported for LLNZO compositions 0 ≤ x ≤ 1. To obtain a complete understanding of the trend in the structure–property relationship in this class of materials, we used the floating zone (FZ) method to grow a single crystal of Li 5.5 La 3 Nb 1.5 Zr 0.5 O 12 that was 4 mm in diameter and 10 mm in length. Using Laue neutron single-crystal diffraction, two distinct Li sites were observed: tetrahedral 24d and octahedral 96h sites. The maximum entropy method (MEM) based on neutron single-crystal diffraction data was used to map Li nuclear density and estimate that the bottleneck of Li transport exists between neighboring tetrahedral and octahedral sites, and that Li is delocalized between split octahedral sites. Room-temperature Li-ion conductivity in Li 5.5 La 3 Nb 1.5 Zr 0.5 O 12 measured with electrochemical impedance spectroscopy (EIS) was 1.37 × 10 -4 S cm -1 . The Li migration activation energy was estimated to be 0.50 eV from EIS and 0.47 eV from dielectric relaxation measurements. The Li-ion jump attempt rate was estimated to be 1.47 × 10 12 Hz while the time scale of successful migration is 10 -7 to 10 -6 s.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of rare earth size on network structure and glass forming ability in binary aluminum garnets

Rare earth aluminate glasses are potentially useful for optical, luminescence, and laser applications. As reluctant glass formers, these materials exhibit unconventional atomic structures. To better understand how their structures correlate with glass formation, we investigate two rare earth aluminum garnet melts, La 3 Al 5 O 12 (LAG) and Yb 3 Al 5 O 12 (YbAG), which represent the relative extremes of good and poor glass forming ability in rare earth aluminates. Structural models have been refined to high-energy X-ray diffraction data over 1340–2740 K. Both melts contain mixtures of AlO 4 , AlO 5 , and AlO 6 polyhedra, with larger fractions of [5] Al and [6] Al in YbAG. Extrapolation of the Al–O coordination distributions to the glass transition match closely with 27 Al nuclear magnetic resonance measurements of (La 1−z Y z ) 3 Al 5 O 12 glasses, z = 0 to 1. During cooling, the mean coordination numbers increase for La–O in LAG from 6.45(8) to 6.98(8) and for Yb–O in YbAG from 6.02(8) to 6.21(8). Linkedness among Al–O polyhedra at ∼2450 K is mostly corner-sharing, with 9% edge-sharing in LAG and 19% in YbAG. Among [4] Al units, both melts have 6% edge-sharing that convert to all corner-sharing upon cooling. Network connectivity is compared using a newly defined metric, K n , that is similar to the Q n distribution but that accounts for the edge-sharing and triply bonded oxygen present in these melts. The lower glass forming ability in YbAG as compared to LAG correlates with more edge-sharing, associated with the larger fractions of [5] Al and [6] Al, and lower connectivity among [4] Al units.

Wilke, Stephen K. [Materials Development, Inc., Ar↗

Ferromagnetic resonances in single-crystal yttrium iron garnet nanofilms fabricated by metal-organic decomposition

Tunable microwave and millimeter wave oscillators and bandpass filters with ultra-low phase noise play a critical role in electronic devices, including wireless communication, microelectronics, and quantum computing. Magnetic materials, such as yttrium iron garnet (YIG), possess ultra-low phase noise and a ferromagnetic resonance tunable up to tens of gigahertz. Here, we report structural and magnetic properties of single-crystal 60 and 130 nm-thick YIG films prepared by metal-organic decomposition epitaxy. These films, consisting of multiple homoepitaxially grown monolayers, are atomically flat and possess magnetic properties similar to those grown with liquid-phase epitaxy, pulsed laser deposition, and sputtering. Our approach does not involve expensive high-vacuum deposition systems and is a true low-cost alternative to current commercial techniques that have the potential to transform the industry.

Wang, Szu-Fan (Paul)↗

Proton damage in (Y,Lu,Gd) 3 (Al,Ga) 5 O 12 :Ce mixed garnet scintillators

Scintillators are vital components for nuclear instrumentation and its applications, including plasma diagnostics and imaging. As yields in controlled fusion experiments increase, the radiation tolerance of scintillator candidates for use in instrumentation is of particular importance. High radiation exposure can damage scintillating materials and alter the optical properties. The effects of radiation damage in Ce-doped mixed garnet ceramics over the compositional range (Y,Gd,Lu) 3 (Al,Ga) 5 O 12 are investigated using optical techniques. The samples were exposed to 200 keV protons to an accumulated fluence of 10 16 protons per square centimeter, then characterized using diffuse reflectance spectroscopy (DRS). DRS with visible light can assess the radiation tolerance of opaque poly-crystalline samples, which can be easily sintered from powders and thus offer distinct advantages in characterization compared to single crystals. Qualitative trends in induced absorption are presented as a function of composition, and the ideal cerium dopant concentration for Y 2 LuAl 5 O 12 is determined to be 0.60–0.75 mol.%.

47 OTHER INSTRUMENTATION↗

Enhanced spin pumping in heterostructures of coupled ferrimagnetic garnets

Spin pumping has significant implications for spintronics, providing a mechanism to manipulate and transport spins for information processing. Understanding and harnessing spin currents through spin pumping is critical for the development of efficient spintronic devices. The use of a magnetic insulator with low damping enhances the signal-to-noise ratio in crucial experiments such as spin-torque ferromagnetic resonance (FMR) and spin pumping. A magnetic insulator coupled with a heavy metal or quantum material offers a more straightforward model system, especially when investigating spin-charge interconversion processes to greater accuracy. This simplicity arises from the absence of unwanted effects caused by conduction electrons unlike in ferromagnetic metals. Here, we investigate the spin pumping in coupled ferrimagnetic (FiM) Y 3 Fe 5 O 12 (YIG)/Tm 3 Fe 5 O 12 (TmIG) bilayers combined with heavy-metal (Pt) using the inverse spin Hall effect. It is observed that magnon transmission occurs at both of the FiMs FMR positions. The enhancement of spin pumping voltage (V sp ) in the FiM garnet heterostructures is observed. The plausible reason might be the interfacial exchange coupling between FiMs. The modulation of V sp is achieved by tuning the bilayer structure. Further, the spin mixing conductance for these coupled systems is found to be ≈ 10 18 m –2 . Furthermore, our findings describe a coupled FiM system for the investigation of magnon coupling providing opportunities for magnonic devices.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Magnon-magnon coupling in an all-oxide insulator garnet Y 3 ⁢Fe 5 ⁢O 12 /Tm 3 ⁢Fe 5⁢ O 12 heterostructure

Hybrid magnonic systems have recently attracted significant attention due to their intriguing physics and potential applications in coherent information processing. In this regard, we have investigated magnon-magnon coupling in the all-oxide insulator garnet Y 3⁢ Fe 5⁢ O 12 (YIG)/Tm 3 ⁢Fe 5 ⁢O 12 (TmIG) heterostructure. The presence of an avoided mode crossing region between the ferromagnetic resonance modes of YIG and TmIG indicates interfacial exchange coupling. This all-insulator system enables interfacial coupling via magnon-magnon interactions. The mode crossing occurs at 𝑓 𝑐 = 6.88 GHz, corresponding to the minimal resonance separation between the two hybrid modes. The coupling strength is determined to be 78 MHz (or 2.8 mT), providing clear evidence of magnon-magnon coupling between the two Kittel modes in the YIG/TmIG insulator system at 200 K. As a result, these findings pave the way for engineering magnonic band structures, tunable coherent magnonic interactions, and nonreciprocal spin transport, which are crucial for advancing ultralow-power magnonic devices.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗