Deciphering the influence of high-flux helium plasma exposure on tungsten nanostructure growth using real-time, in situ spectroscopic ellipsometry

In situ analysis of surfaces during high-flux plasma exposure represents a long-standing challenge in the study of plasma–material interactions. While post-mortem microscopy can provide a detailed picture of structural and compositional changes, in situ techniques can capture the dynamic evolution of the surface. In this study, we demonstrate how spectroscopic ellipsometry can be applied to the real-time characterization of W nanostructure (also known as “fuzz”) growth during exposure to low temperature, high-flux He plasmas. Strikingly, over a wide range of sample temperatures and helium fluences, the measured ellipsometric parameters (Ψ,Δ) collapse onto a single curve that can be directly correlated with surface morphologies characterized by ex situ helium ion microscopy. The initial variation in the (Ψ,Δ) parameters appears to be governed by small changes in surface roughness (<50 nm) produced by helium bubble nucleation and growth, followed by the emergence of 50 nm diameter W tendrils. This basic behavior appears to be reproducible over a wide parameter space, indicating that the spectroscopic ellipsometry may be of general practical use as a diagnostic to study surface morphologies produced by high-flux He implantation in refractory metals. An advantage of the methods outlined here is that they are applicable at low incident ion energies, even below the sputtering threshold. As an example of this application, we apply in situ ellipsometry to examine how W fuzz growth is affected both by varying ion energy and the temperature of the surface.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Continuum-scale modeling of helium bubble bursting under plasma-exposed tungsten surfaces

We present a comparison between a continuum-scale drift-diffusion-reaction cluster dynamics prediction of helium retention in low-energy helium plasma exposed tungsten and experimental measurements, in a temperature regime that did not produce tungsten fuzz. Our cluster dynamics model, Xolotl, has been successfully benchmarked to high helium implantation flux MD simulations at relatively low implanted fluence. In this article, we also describe the extension of the Xolotl DDR model to incorporate the effect of bubble bursting, which is observed in very high rate MD simulations, as well as MD simulations at longer times than simulated in our prior benchmarking comparison. The bursting model parameters have been tuned by comparing to MD simulations at a flux of 5.0 × 10 27 m –2 s –1 , and also compared to lower implanted fluence simulations performed at ~4.0 × 10 25 m –2 s –1 . This article then reports on the consistency of the Xolotl predictions with respect to the size of the simulated cluster phase space (i.e. the maximum cluster size), initial vacancy concentration, and bubble growth trajectory (maximum number of helium atoms per vacancy). Finally, our simulation results are compared to helium plasma experiments that did not produce fuzz. While the Xolotl predictions including bubble bursting are in quantitative agreement with high-flux MD simulations, the initial comparison to plasma exposure experiments at a flux on the order of 10 21 m –2 s –1 disagree by more than an order of magnitude, and in fact cannot reproduce the trends in helium retention with varying exposure temperature. Modifying the initial vacancy concentrations and helium cluster diffusion behavior in Xolotl leads to a reasonable agreement with the experimental observations, although the underlying physical explanation for these modifications remains unclear. The predicted helium content at experimentally relevant fluxes has been shown to be relatively insensitive to the parameters used in the bubble bursting model implemented in Xolotl, although these parameters have a larger influence at higher flux. As a result, more systematic comparisons between the modeling predictions with both experiments and MD simulation results is expected to improve the bubble bursting model in Xolotl in the future.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Nonlinear impact of the porous nanostructure on the net tungsten erosion in the linear plasma device PISCES-A

Abstract The tungsten fuzz growth under non-erosive and erosive helium plasmas in the linear plasma device PISCES-A has been investigated by experiments and simulations. The simulation results benchmarked against the experimental measurements indicate a decayed net physical sputtering yield during fuzz growth under the erosive helium plasma. Further, a nonlinear dependence of the net tungsten erosion on the ‘effective’ porous nanostructure that can be sputtered by incident helium particles has been found.

Physics↗

Final Progress Report The U.S. Department of Energy Research Grant No. DE-SC0008660 Plasma Surface Interactions: Bridging from the Surface to the Micron Frontier through Leadership Class Computing

The choice of material for the plasma facing components (PFC), in particular, for divertor targets, is one of the main issues for future tokamak reactors. There are two major requirements for the PFC’s material: acceptable level of tritium retention and durability in a harsh environment of fusion grade plasma. Based on these criteria, some years ago it was decided that tungsten is an acceptable material for divertor targets in ITER. However, further experimental studies reveal that the irradiation of tungsten even with low energetic (well below sputtering threshold!) He containing plasma causes significant modification of surface morphology, formation of the layer of He nano-bubbles (in the temperature range T<1000 K), “fuzz” (for 1000 K 2000 K) (e.g. see Fig. 1). Recall that He, being an ash of D-T fusion reactions, is an inherent impurity in fusion plasma. The goals of the UCSD Applied Plasma Theory Group was: i) investigate the mechanisms of the formation of He nano-bubble layer and fuzz growth under He irradiation, as well as the physics of transport of hydrogen species in tungsten lattice, and ii) develop physics understanding of the models suitable for the incorporation into the Xolotl-PSI code based on the reaction-diffusion approach, which is the flagship of the whole SciDAC project [8], which can guide both numerical simulations and experimental studies. Here we just highlight our major accomplishments.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Effects of surface vacancy-adatom pair formation on PFC tungsten surface morphological response

Abstract We report a simulation study of the effect of He-irradiation-induced surface vacancy-adatom pair formation on the surface morphological evolution of plasma-facing component (PFC) tungsten and examine a number of factors that impact such evolution. Our analysis is based on self-consistent dynamical simulations according to an atomistically-informed, continuum-scale surface evolution model that has been developed following a hierarchical multiscale modeling strategy and can access the spatiotemporal scales of relevance to fuzz formation. The model accounts for the flux of surface adatoms generated as a result of the surface vacancy-adatom pair formation effect upon He implantation, which contributes to the anisotropic growth of surface nanostructural features due to the different rates of adatom diffusion along and across step edges of islands on the tungsten surface. We have carried out atomic-scale computations of optimal diffusion pathways along and across island step edges on the W(110) surface and calculated Ehrlich–Schwoebel (ES) barriers in adatom diffusion along and across such step edges. This aspect of surface adatom diffusion contributes to anisotropic surface atomic fluxes, terrace and step diffusive currents, and has been incorporated into our PFC surface evolution model, which predicts the formation of preferentially aligned nanoridge stripe patterns on the PFC surface. We establish that these anisotropic diffusive currents accelerate nanotendril growth on the PFC surface and the onset of surface nanostructure pattern formation. We also explore systematically the dependence of the PFC surface morphological response on the surface temperature and He ion incident flux, characterize in detail the resulting surface topographies and growth kinetics, and compare the predicted surface morphologies with experimental observations. Our simulation predictions for the emerging surface nanostructure patterns under certain plasma exposure conditions are consistent with experimental findings in the literature.

36 MATERIALS SCIENCE↗

The influence of fusion-relevant D 2 -0.1He plasma on Be-W mixed-materials

We report compositionally homogeneous mixed-material layers of Be and W, ∼2 μm thick, and of various W contents (spanning 0–100 at.% W), are produced by thermionic vacuum arc deposition. The layers are exposed to low energy (∼50 eV), high ion flux (6–8 × 10 22 m −2 s −1 ) D 2 -0.1He (10% He) mixed species plasma at 473 K and 1073 K to simulate ITER-like first wall and divertor plasma-material interaction. Surface morphological and compositional analysis is conducted prior and subsequent to plasma exposure. The action of the plasma produces almost complete depletion of Be from the near surface, and this is found regardless of the exposure temperature or initial composition. In the exposure case of 473 K, thermal desorption spectrometry reveals decreased D retention in W rich compositions compared to similar exposure in D 2 plasma without He, but no discernable difference is noted in Be rich compositions. At 1073 K, surface enrichment in W, by depletion of the Be, results in He induced W “fuzz” structures for all Be-W compositions explored.

36 MATERIALS SCIENCE↗

High Flux Helium Irradiation of Dispersion-Strengthened Tungsten Alloys and Effects of Heavy Metal Impurity Layer Deposition

Tungsten has been chosen as the plasma-facing material (PFM) for the divertor region in ITER and also a candidate PFM for future plasma-burning nuclear fusion reactors. During fusion device operation, PFMs will be exposed to low-energy He irradiation at high temperatures, resulting in sub-surface bubbles and surface morphology changes such as pores and fuzz. Carbide dispersion-strengthened W materials may enhance the ductility of W, but their behavior under high flux He irradiation remains unclear. In this work, the response of dispersion-strengthened tungsten materials to high flux, low energy He irradiation at high temperature is examined. Tungsten alloyed with 1, 5, or 10 wt. % tantalum carbide or titanium carbide exposed to these conditions result in surface pores, coral-like feature growth and sub-surface helium bubbles. Reactor-relevant helium irradiation (5 x 10 26 m -2 fluence) combined with high powered laser pulses to simulate off-normal reactor events does not significantly alter the surface morphology, as the surface nanostructures appear stable and cracks are only observed on a localized region of one sample. However, specimens show the development of an impurity layer on the surface, likely impurity deposition from the sample holder during irradiation, resulting in a mixed material layer on the surface. Helium bubbles exist in this impurity layer, and obscure conclusions about helium interactions with the carbide dispersoids. Nonetheless, it is clear that the dispersoid microstructure limits He bubble formation and subsequent surface nanostructuring, attributed to the dispersoid composition.

36 MATERIALS SCIENCE↗

Intense cyclic heating effects on thermo-fracture and thermal shock of solid tungsten and open-cell tungsten foam

Here we investigate here the effects of transient (cyclic) arc-jet plasma and laser heating on fracture behavior of W-foam and solid tungsten. The two key parameters that control the foam thermomechanical response are its density and mean cell size expressed in Pores Per Inch (PPI). Tungsten foam samples were fabricated with Chemical Vapor Deposition (CVD) with variety of PPI and relative density. These were tested under two types of qualitatively different conditions: (1) high-enthalpy arc-jet, and (2) high-power cyclic laser heating. None of the foam samples showed macroscopic through-thickness cracks. However, distributed micro-cracks were observed on ligaments and their triple junctions. Under the same loading conditions, W-foam and solid tungsten showed similar crack network pattern and characteristic length-scale. However, Crack Opening Displacement (COD) was twice as large in solid W as compared to W-foam. Foam samples that have been previously exposed to a low-pressure helium plasma showed significant changes in their surface forming nano-texture fuzz which was removed by subsequent testing in the arc-jet. Extensive fracture and re-crystallization were observed in the thin solid W disk that was fully-constrained from expansion. Thicker and fully-constrained solid W disks did not display recrystallization, grain growth, and extensive cracking. However, thicker disks that were free to expand showed some recrystallization and extensive through-thickness cracks due to less effective cooling and thus higher temperatures. Laser beam testing showed no visible damage formation at 0.19 GW/m 2 and 0.38 GW/m 2 for both low-density (23%) and high-density (43%) foams at low pulses (100-1000). Micro-cracks were observed after 10,000 pulses at 0.19 GW/m 2 in both foams, and in low-density foam after 100,000 at 0.38 GW/m 2 . The nature of thermomechanical damage in W-foam exposed to extreme power (GW/m 2 ) short-duration laser pulses was found to be qualitatively similar to that of high power (MW/m 2 ) long-duration arc-jet.

36 MATERIALS SCIENCE↗

Mobility of tungsten clusters on tungsten surfaces

It is reported on an accelerated molecular dynamics investigation of surface transport mechanisms on W surfaces. These mechanisms likely influence the formation of nano-fuzz in fusion plasma-facing conditions. The simulations use an embedded-atom potential to investigate the diffusion mechanisms of W clusters (W n , n = 2–9) on W(1 1 0) and W(1 0 0) surfaces at 1000 K, reaching timescales beyond 10 microseconds. A number of fast moving adatom species, W n (n = 2–6), were observed. In contrast, slightly larger clusters W n (n = 7–9), especially W 8 , exhibit significantly lower diffusivities. The diffusion mechanisms of W n clusters on the W(1 1 0) surface are complex, with the most common elementary steps involving hops of monomers and dimers. Moreover, we observe tetramer hopping in the diffusion processes of W n (n = 4–7), trimer hopping in W n (n = 5, 6, 8), and pentamer hopping in W 5 on the W(1 1 0) surface. W n (n ≤ 3) and metastable W n (n > 3) clusters on the W(1 0 0) surface diffuse predominantly through monomer exchange with surface atoms. However, W clusters containing square tetramers are essentially immobile on the W(1 0 0) surface at 1000 K.

Instruments & Instrumentation↗

Deuterium and helium ion irradiation of nanograined tungsten and tungsten–titanium alloys

Tungsten (W), a primary candidate for the plasma-facing components of nuclear fusion reactors (e.g. the divertor region in ITER) is susceptible to cracks, blisters, bubbles, and other morphological changes when irradiated with energetic particles. This work investigated two new materials, nanograined W and a nanograined W–Ti alloy, for potential use as plasma-facing materials. Their retention properties and morphological changes after exposure to deuterium (D) and helium (He) plasma at 50 eV and surface temperatures of 500 and 1000 K were analyzed. Nanograined W was found to have smaller blisters and be less prone to fuzz formation than commonly-utilized micro-grain polycrystalline W. Additionally, the nanograined W–Ti alloy exhibited a lower concentration of blisters on its surface than pure W, including nanograined W.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Stability and mobility of tungsten clusters on tungsten (110) surface: Ab initio and atomistic simulations

Quantifying the surface transport properties of tungsten (W) is of prime importance to understand the formation of nano-fuzz in fusion plasma-facing conditions. The stability and mobility of W adatom clusters (W n , n = 2-9) on the W(110) surface has been investigated by computer simulations, including ab initio calculations using density functional theory (DFT) and molecular statics (MS) simulations with multiple W interatomic potentials. The DFT results demonstrate that the sequential binding energy generally increases with number of W adatoms, except for the 5 th and 7 th W adatoms. The most common elemental migration steps of W n (n>2) clusters are observed to consist of monomer and dimer hops, while larger W n clusters can also diffuse by dissociation and recombination of smaller clusters. The threshold migration energy of W 9 is the highest, then followed by W 8 , W 4 , and W 6 , while W 3 , W 5 , and W 7 have similar migration energies. Compared to DFT, each interatomic potential evaluated overestimates the binding energies of W n clusters. Additionally, the embedded-atom potential developed by Juslin and Wirth adequately predicts the threshold migration energy of W n (n>2) clusters, although it predicts different underlying migration mechanisms. The results show that interaction mechanism between W adatoms controls the stability and mobility of W n clusters on the W(110) surface.

36 MATERIALS SCIENCE↗

The mobility of small vacancy/helium complexes in tungsten and its impact on retention in fusion-relevant conditions

Tungsten is a promising plasma facing material for fusion reactors. Despite many favorable properties, helium ions incoming from the plasma are known to dramatically affect the microstructure of tungsten, leading to bubble growth, blistering, and/or to the formation of fuzz. In order to develop mitigation strategies, it is essential to understand the atomistic processes that lead to bubble formation and subsequent microstructural changes. In this work, we use large-scale Accelerated Molecular Dynamics simulations to investigate small (N=1,2) V N He M vacancy/helium complexes, which serve as the nuclei for larger helium bubble growth, over timescales reaching into the milliseconds under conditions typical of the operation of fusion reactors. These complexes can interconvert between different I L V N+L He M variants via Frenkel pair nucleation (leading to the creation of a additional vacancy/interstitial pair) and annihilation events; sequences of these events can lead to net migration of these embryonic bubbles. The competition between nucleation and annihilation produces a very complex dependence of the diffusivity on the number of heliums. Finally, through cluster dynamics simulations, we show that diffusion of these complexes provides an efficient pathway for helium release at fluxes expected in fusion reactors, and hence that accounting for the mobility of these complexes is crucial.

36 MATERIALS SCIENCE↗

Helium bubble bursting in tungsten

Molecular dynamics simulations have been used to systematically study the pressure evolution and bursting behavior of sub-surface helium bubbles and the resulting tungsten surface morphology. This study specifically investigates how bubble shape and size, temperature, tungsten surface orientation, and ligament thickness above the bubble influence bubble stability and surface evolution. The tungsten surface is roughened by a combination of adatom “islands,” craters, and pinholes. The present study provides insight into the mechanisms and conditions leading to various tungsten topology changes, which we believe are the initial stages of surface evolution leading to the formation of nanoscale fuzz.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Secondary electron emission of reticulated foam materials

Complex material surfaces can reduce secondary electron emission (SEE) and sputtering via geometric trapping. In this work, the SEE yields for a range of open-cell reticulated carbon foam geometries are characterized using scanning electron microscopy. The total reduction in the SEE yield from carbon foams with a 3% volume fill density and 10–100 pores per inch (PPI) is shown to be between 23.5% and 35.0%. Contributions of a foam backplate are assessed by experimentally and analytically defining the critical parameter, transparency. The transparency of a foam is quantified and is shown to affect the primary electron angular dependence on the SEE yield. For the same thickness of 6 mm, it is found that higher PPI decreases foam transparency from 32% to 0% and reduces the SEE yield. The SEE yield from carbon foams is also shown to have weaker dependence on the morphology of the surface compared with fuzzes and velvets and less variation across individual sample surfaces due to the rigidity of their ligament structures and isotropic geometries.

Physics↗

Accelerating plasma and radiation surface science using transient grating spectroscopy

A facility for the investigation of in situ radiation-materials and plasma-materials interaction is demonstrated with tungsten, using transient grating spectroscopy as a probe of thermal diffusivity and surface acoustic wave speed. Helium plasma exposure at 645 °C to 1.18 × 10 18 cm −2 helium, until the growth of tungsten fuzz, showed an increase in surface acoustic wave speed at the near-surface from 2542 ± 1 m s −1 up to 2565 ± 1 m s −1 , followed by a greater drop to 2499 ± 7 m s −1 . No observable change in thermal diffusivity was present for plasma exposure alone. A separate 10.26 MeV self-ion-irradiation of tungsten to a dose of 7.92 dpa showed a reduction in both thermal diffusivity from 61.4 ± 1.4 mm 2 s −1 to 36.0 ± 0.7 mm 2 s −1 , following trends seen in existing studies, and surface acoustic wave speed from 2647.8 ± 0.6 m s −1 to 2640.0 ± 0.4 m s −1 . Facilities like these are poised to rapidly close critical knowledge gaps regarding the coupled effects of plasma and radiation damage for materials in fusion systems.

Accelerated plasmas↗

Plasma-Material-Interaction Research Using PISCES Linear Plasma Devices

In this paper, recent plasma-material-interaction (PMI) studies of relevance to fusion PMI science are discussed. The results are a mix of science experiments and in situ diagnostic technology development. Scientific issues addressed include the nature of He and W atom migration in the evolution of W fuzz surfaces, understanding the nature of D retention in damaged W surfaces via modeling with the tritium migration and analysis program, and an examination of synergistic effects associated with D trapping on composite Be codeposit and W substrate surfaces. In situ diagnostic developments discussed include laser-induced desorption spectroscopy for the measurement of bulk hydrogen retention and laser-induced breakdown spectroscopy for the measurement of near-surface composition.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗