Internal wire guide for GTAW welding

A welding torch for gas tungsten arc welding apparatus has a filler metal wire guide positioned within the torch, and within the shielding gas nozzle. The wire guide is adjacent to the tungsten electrode and has a ceramic liner through which the wire is fed. This reduces the size of the torch and eliminates the outside clearance problems that exit with external wire guides. Additionally, since the wire is always within the shielding gas, oxidizing of the wire is eliminated.

Morgan, Gene E.↗

Electrode carrying wire for GTAW welding

A welding torch for gas tungsten arc welding apparatus has a hollow tungsten electrode including a ceramic liner and forms the filler metal wire guide. The wire is fed through the tungsten electrode thereby reducing the size of the torch to eliminate clearance problems which exist with external wire guides. Since the wire is preheated from the tungsten more wire may be fed into the weld puddle, and the wire will not oxidize because it is always within the shielding gas.

Morgan, Gene E.↗

Oxygen-Free Welding Contact Tips

Contact tips for gas/metal arc welding (GMAW) fabricated from oxygen-free copper. Prototype tips tested in robotic welding, for which application intended. Reduces electrical erosion, increases electrical conductivity, and reduces mechanical wear. Productivity of robotic welding increases while time during welding interrupted for removal and replacement of contact tips minimal. Improves alignment of joints and filler metal, reducing rate of rejection and repair of unacceptable weldments. Utility extends beyond aerospace industry to mass production of various types of hardware, including heavy off-highway construction equipment.

Pike, James F.↗

More About Brazing Or Welding NiAl Without Filler

Two reports present additional information about two processes for joining, brazing, or welding workpieces made of nickel aluminide alloys, without use of filler metal. Joining processes involve uniform heating in vacuum-controlled furnace. Eliminates internal thermal gradients in workpieces joined and greatly reduces tendency toward cracking.

Moore, Thomas J.↗

Evaluation of the Transient Liquid Phase (TLP) Bonding Process for Ti3Al-Based Honeycomb Core Sandwich Structure

The suitability of using transient liquid phase (TLP) bonding to fabricate honeycomb core sandwich panels with Ti-14Al-21Nb (wt%) titanium aluminide (T3Al) face sheets for high-temperature hypersonic vehicle applications was evaluated. Three titanium alloy honeycomb cores and one Ti3Al alloy honeycomb core were investigated. Edgewise compression (EWC) and flatwise tension (FWT) tests on honeycomb core sandwich specimens and tensile tests of the face sheet material were conducted at temperatures ranging from room temperature to 1500 F. EWC tests indicated that the honeycomb cores and diffusion bonded joints were able to stabilize the face sheets up to and beyond the face sheet compressive yield strength for all temperatures investigated. The specimens with the T3Al honeycomb core produced the highest FWT strengths at temperatures above 1000 F. Tensile tests indicated that TLP processing conditions resulted in decreases in ductility of the Ti-14Al-21Nb face sheets. Microstructural examination showed that the side of the face sheets to which the filler metals had been applied was transformed from equiaxed alpha2 grains to coarse plates of alpha2 with intergranular Beta. Fractographic examination of the tensile specimens showed that this transformed region was dominated by brittle fracture.

Bird, R. Keith↗

Filler Wire Development for 2195 Aluminum-Lithium

The objective of the research was to determine the susceptibility of submitted welded 2195 plate in an AI (Alternate Immersion) environment. Forty-day AI exposure was completed on 8 welded 2195 stress corrosion samples. No stress corrosion cracking (SCC) was found on any of the samples tested. All 8 samples experienced exfoliation corrosion attack in the heat-affected zone (HAZ) adjacent to the weld. All samples were examined metallographically and showed varying degrees of intergranular corrosion (IG). The filler metal on all samples showed moderate to heavy pitting.

Bjorkman, Gerald W.↗

Validation of Modified Wine-Rack Thermal Design for Nickel-Hydrogen Batteries in Landsat-7 Spacecraft Thermal Vacuum Test and in Flight

A heritage wine-rack thermal/mechanical design for the nickel-hydrogen batteries was the baseline at the Landsat-7 Preliminary Design Review. An integrated thermal and power analysis of the batteries performed by the author in 1994 revealed that the maximum cell-to-cell gradient was 6.6 C. The author proposed modifying the heritage wine-rack design by enhancing heat conduction from cells to cells, and from cells to battery frame. At the 1995 Intersociety Energy Conversion Engineering Conference (IECEC), the author presented a paper on methods of modifying the wine-rack design. It showed that the modified wine-rack option, which uses a metallic filler, could reduce the maximum cell-to-cell temperature gradient to 1.30 C, and could also reduce the maximum cell temperature by as much as 80 C. That design concept was adopted by the Landsat7 Project Office, and a design change was made at the Critical Design Review. Results of the spacecraft thermal vacuum and thermal balance tests, and temperature data in flight show that the temperatures of the battery cells are very uniform. The maximum cell-to-cell gradient is 1.50 C. They validate the modified wine-rack thermal design.

Choi, Michael K.↗

Friction stir welding process to repair voids in aluminum alloys

The present invention provides an in-process method to repair voids in an aluminum alloy, particularly a friction stir weld in an aluminum alloy. For repairing a circular void or an in-process exit hole in a weld, the method includes the steps of fabricating filler material of the same composition or compatible with the parent material into a plug form to be fitted into the void, positioning the plug in the void, and friction stir welding over and through the plug. For repairing a longitudinal void (30), the method includes machining the void area to provide a trough (34) that subsumes the void, fabricating filler metal into a strip form (36) to be fitted into the trough, positioning the strip in the trough, and rewelding the void area by traversing a friction stir welding tool longitudinally through the strip. The method is also applicable for repairing welds made by a fusing welding process or voids in aluminum alloy workpieces themselves.

Rosen, Charles D.↗

Evaluation of Margins of Safety in Brazed Joints

One of the essential steps in assuring reliable performance of high cost critical brazed structures is the assessment of the Margin of Safety (MS) of the brazed joints. In many cases the experimental determination of the failure loads by destructive testing of the brazed assembly is not practical and cost prohibitive. In such cases the evaluation of the MS is performed analytically by comparing the maximum design loads with the allowable ones and incorporating various safety or knock down factors imposed by the customer. Unfortunately, an industry standard methodology for the design and analysis of brazed joints has not been developed. This paper provides an example of an approach that was used to analyze an AlBeMet 162 (38%Be-62%Al) structure brazed with the AWS BAlSi-4 (Al-12%Si) filler metal. A practical and conservative interaction equation combining shear and tensile allowables was developed and validated to evaluate an acceptable (safe) combination of tensile and shear stresses acting in the brazed joint. These allowables are obtained from testing of standard tensile and lap shear brazed specimens. The proposed equation enables the assessment of the load carrying capability of complex brazed joints subjected to multi-axial loading.

Flom, Yury↗

Failure Assessment Diagram for Brazed 304 Stainless Steel Joints

Interaction equations were proposed earlier to predict failure in Albemet 162 brazed joints. Present study demonstrates that the same interaction equations can be used for lower bound estimate of the failure criterion in 304 stainless steel joints brazed with silver-based filler metals as well as for construction of the Failure Assessment Diagrams (FAD).

Flom, Yory↗

Failure Assessment Diagram for Titanium Brazed Joints

The interaction equation was used to predict failure in Ti-4V-6Al joints brazed with Al 1100 filler metal. The joints used in this study were geometrically similar to the joints in the brazed beryllium metering structure considered for the ATLAS telescope. This study confirmed that the interaction equation R(sub sigma) + R(sub Tau) = 1, where R(sub sigma) and R(sub Tau)are normal and shear stress ratios, can be used as conservative lower bound estimate of the failure criterion in ATLAS brazed joints as well as for construction of the Failure Assessment Diagram (FAD).

Flom, Yury↗

Continue Effort to Improve Alloy 800H Weldment

This memorandum formally documents the completion of the Level 3 milestone M3AT-22IN0604055 titled, “Continue effort to improve Alloy 800H weldment creep rupture performance,” by the transmittal of this deliverable document, entitled, “Issue memo ‘Preliminary assessment of UTP A 2133 Mn as a matching filler metal for Alloy 800H in Section III Division 5 applications.’” The deadline for this milestone is August 27, 2022. This milestone is part of the ART GCR work package AT-22IN060405, “Long-Term Very-High Temperature Reactor (VHTR) Material Qualification – INL.”

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

In situ measurement of phase transformations and residual stress evolution during welding using spatially distributed fiber-optic strain sensors

Welding of high-strength steels can result in large tensile strains as the base metal and filler material cool from their molten state. To combat these large tensile strains, low-transformation-temperature (LTT) metal fillers have been proposed. These fillers undergo a martensitic phase transformation at a lower temperature which can ultimately reduce the tensile strain or can even introduce compressive strain adjacent to the weld metal. However, the process for optimizing the composition of the LTT material, as well as various weld parameters for each unique weld geometry, can be quite expensive, especially if the acceptance criterion requires using neutrons, x-ray beams, or destructive techniques to characterize residual stresses. This work describes a simple, low-cost method for quantifying residual stresses and phase transformations in situ during welding. Spatially distributed fiber-optic sensors were bonded to a cast iron plate, along with tack-welded thermocouples, to measure temperature and strain during multiple passes with LTT filler metals. Results show that the fiber-optic sensors can successfully resolve compressive strain adjacent to the weld region caused by the martensitic phase transformations in the LTT filler material.

47 OTHER INSTRUMENTATION↗

Hierarchically structured metal carbides as conductive fillers in thermo-responsive polymer nanocomposites for battery safety

Integrating thermo-responsive polymer switching materials (TRPS) into lithium-ion batteries (LIBs) has been recognized as one of the most effective strategies to prevent thermal runaway under various abuse scenarios. However, the current methods to obtain TRPS cannot satisfy different practical applications. Herein, we develop a versatile strategy for the preparation of various metal carbides (e.g., tungsten carbide, molybdenum carbide) with controllable hierarchical structure that is featured with surface protrusion structure, which is critical for high conductivity and rapid thermal response. Systematic studies of the phase and morphology evolutions by advanced characterizations illustrate that the reducing agent and reduction rate are critical for developing the specific morphology. In conclusion, by using the above-mentioned carbides as the conductive fillers of TRPS, the resulting TRPS with a specially controlled shape exhibits over 5 order of conductivity improvement compared with common carbides with particulate morphology, in addition to reversible shutdown performance and effective thermal abuse protections toward safe LIB operation.

25 ENERGY STORAGE↗

Aluminum 4047 Vendor Review [Slides]

The selected filler wire manufacturer should have full control of the filler wire manufacturing process (i.e. ingot metal, green rod, filler wire manufacturing and packaging). LANL would like to purchase filler wire as an off-the-shelf product in small quantities over time to maintain a fresh stock and eliminate issues related to long-term storage of aluminum. The filler wire would be purchased in 0.047” dia. on small (ideally 5 lb.) spools, but no larger than 16 lbs.

36 MATERIALS SCIENCE↗

Assessment of Overmatched Filler (Alloy 617) to Improve Alloy 800H Stress Rupture Factors

Section III, Division 5 of the American Society of Mechanical Engineers (ASME) Boiler and Pressure Vessel Code (BPVC) specifies rules for elevated temperature nuclear reactors. Currently, only six metals are qualified in Section III, Division for construction of Class A metallic pressure boundary components for elevated-temperature service, one of these being Alloy 800H. There are only two permissible filler metals Alloy 800H is qualified to be welded with: Alloy A and Alloy 82. The stress rupture factors for these two filler metals are low near the maximum temperatures and service lives Alloy 800H is qualified for. This may preclude vendors from being able to use Alloy 800H for elevated-temperature nuclear construction. In this work, an overmatched filler metal, Alloy 617 is assessed to determine its potential to offer improved stress rupture factors. Scoping creep-rupture tests of cross-welds with Alloy 800H base metal and Alloy 617 filler metal were conducted. Preliminary results do not indicate that Alloy 617 will offer significantly improved stress rupture factors. Consequently, a matching filler metal, UTP A 2133, is now being investigated.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗