The development of S-13G-type thermal-control coatings based on silicate-treated zinc oxide.
Silicate treated zinc oxide thermal control coatings, discussing effective stabilization against UV induced degradation in IR region of solar spectrum
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Silicate treated zinc oxide thermal control coatings, discussing effective stabilization against UV induced degradation in IR region of solar spectrum
Zinc Oxide nanoparticles are synthesized using DNA as capping agent. Zinc oxide nanoparticles are synthesized using DNA as a capping agent. Structural and morphological characterizations are done using SEM, FTIR and XRD. The particle size and lattice parameters are calculated from the diffraction data. The optical properties are studied using UV-Vis absorption spectroscopy and bandgap variation with temperature is determined. The dielectric property of nanoparticles is studied by varying temperature and frequency. The dielectric constant and dispersion parameters are found out. Method of Cole-Cole analysis is used to study the high temperature dispersion of relaxation time. The variation of both AC and DC conductivity are studied and activation energy calculated.
The determination of individual dissolution behaviors of zinc and manganese in waste alkaline battery powders is an important subject from the points of the leaching yield, design of leaching reactor, and separation and recovery steps of hydrometallurgical process. In the current study, we investigated the dissolution kinetics of zinc oxide powder. Zinc oxide was obtained from waste alkaline batteries, and sodium hydroxide solutions were used as solvent. In the experiments, the effects of solution concentration, reaction temperature, stirring speed, solid-to-liquid ratio, and particle size on the dissolution of zinc oxide were investigated. It was demonstrated that the dissolution increased with the increasing concentration, reaction temperature, and stirring speed, and with the decreasing solid-to-liquid ratio and particle size. In consequence of the kinetic analysis performed, it was found that the dissolution kinetics of zinc powder obeyed the Avrami model. Activation energy for the process was determined to be 19.42 kJ/mol. Zinc ions in the resulting solution after dissolution process was recovered in the form of hydroxy-carbonate product by precipitation method. Zinc oxide was produced by isothermal decomposition of hydroxy-carbonate product.
Zinc oxide has justifiably been attracting attention in several fields, and the relatively new field of tribology is not left out. Aside from its already extensively researched and documented applications in materials science, semiconductor and electronics industry, zinc oxide nanoparticles and thin films appear to be gaining fast grounds as tribological materials, thereby justifying a zealous approach in further exploring their inherent properties in this area. In this work, zinc oxide thin films were deposited by MOCVD (metal-organic chemical vapour deposition) on soda lime glass andAISI304L stainless steel plates at temperatures of 300°C, 330°C, 360°C, 390°C and 420°C respectively, using anhydrous zinc acetate as the precursor. The carrier gas was air with a flow rate of 2.5 dm 3 min -1 at atmospheric pressure, and deposition time of 2 hours each. The thickness and tribological properties of the thin films produced were thereafter investigated. The thickness was measured by RBS (Rutherford backscattering spectroscopy) using a 1.7 MeV Tandem Accelerator, and the friction and wear properties were tested with a HFRR (high frequency reciprocating rig) under dry contact conditions, Olympus BH-2 Optical Microscope, and ADE Phase Shift MicroXam Optical Surface Profiler. The thickness was found to decrease with increasing deposition temperature, although for the 300°C deposition temperature there appeared to be a bloated thickness, which is attributable to such factors as incomplete precursor decomposition, turbulence in precursor flow, and energy straggling during RBS measurement. The friction tests highlighted coefficients of friction which were relatively low at the onset of the tests, but thereafter rapidly increased, owing possibly to temperature rise, attendant rapid oxidation and aided abrasion by worn debris. The average coefficient of friction of each test was computed, and the outcome (0.33 – 0.43) for all of them was a material still good enough for use in reducing friction at nanolevel, even with worn out matter and increased working temperature, with no noticeable trend regarding their varied deposition temperatures. Microscope and profilometer profiles vividly showed wear scars with material removal and material transfer. The average wear scar diameters as well as the wear volumes were compiled for both the test balls and the thin films. The result showed a largely correlated trend in the wear scar diameters and the wear volumes, and the thin film deposited at 330°C was the coating with the least wear scars, material removal cum transfer on the test ball and sample. This result is attributed to the enhanced thickness of the sample over the others, apart from sample X1 earlier reported to have a problem in its thickness. As a result, this temperature is therefore recommended as the optimum deposition temperature for the best tribologically applicable zinc oxide thin films, using zinc acetate precursor by MOCVD.
We have studied the effect of long time post-fabrication annealing on negative bias illumination stress (NBIS) of amorphous indium-gallium-zinc-oxide (a-IGZO) thin-film-transistors. Annealing for 100 h at 250 °C increased the field effect mobility from 14.7 cm{sup 2}/V s to 17.9 cm{sup 2}/V s and reduced the NBIS instability remarkably. Using X-ray photoelectron spectroscopy, the oxygen vacancy and OH were found to exist at the interfaces of a-IGZO with top and bottom SiO{sub 2}. Long time annealing helps to decrease the vacancy concentration and increase the metal-oxygen bonds at the interfaces; this leads to increase in the free carrier concentrations in a-IGZO and field-effect mobility. X-ray reflectivity measurement indicated the increment of a-IGZO film density of 5.63 g cm{sup −3} to 5.83 g cm{sup −3} (3.4% increase) by 100 h annealing at 250 °C. The increase in film density reveals the decrease of O vacancy concentration and reduction of weak metal-oxygen bonds in a-IGZO, which substantially helps to improve the NBIS stability.
Indium-gallium-zinc-oxide (IGZO) Schottky diodes exhibit excellent performance in comparison with conventional devices used in future flexible high frequency electronics. In this work, a high performance Pt IGZO Schottky diode was presented by using a new fabrication process. An argon/oxygen mixture gas was introduced during the deposition of the Pt layer to reduce the oxygen deficiency at the Schottky interface. The diode showed a high barrier height of 0.92 eV and a low ideality factor of 1.36 from the current–voltage characteristics. Even the radius of the active area was 0.1 mm, and the diode showed a cut-off frequency of 6 MHz in the rectifier circuit. Using the diode as a demodulator, a potential application was also demonstrated in this work.
Optical properties of zinc oxide analyzed by exposing samples to mechanical and thermal treatments and UV radiation
Aluminum doped zinc oxide (AZO) was grown via magnetron sputtering as a low-cost alternative to indium tin oxide (ITO) for organic photovoltaics (OPVs). Postdeposition ozone treatment resulted in devices with lower series resistance, increased open-circuit voltage, and power conversion efficiency double that of devices fabricated on untreated AZO. Furthermore, cells fabricated using ozone treated AZO and standard ITO displayed comparable performance.
Highlights: • Zinc oxides were synthetized using spent alkaline batteries as raw materials. • Both prepared samples present the wurzite structure and exhibits good optical properties. • The decrease in lattice parameters and the narrow band gap are associated with the formation of oxygen vacancies. • Recovered zinc oxides were active for photodegradation of methylene blue by UV irradiation. • The photocatalytic was correlates to the bulk/surface defects ratio. - Abstract: The structural, optical and photocatalytic properties of two zinc oxides prepared from spent alkaline batteries were analysed. After leaching the anode of alkaline batteries, zinc was precipitated from the leachate liquor by introducing oxalic acid (O-ZnO) or sodium carbonate (C-ZnO). The structure of ZnO samples were analysed by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), S{sub BET}, DRS-UV-vis spectroscopy and positron annihilation lifetime spectroscopy (PALS). Both oxides present the ZnO wurzite structure and similar morphology. C-ZnO presents a cell lower lattice parameters and bang gap energy (2.99 eV) than O-ZnO (3.05 eV), possibly due to higher concentration of oxygen vacancies. The photocatalytic activity in the degradation of methylene blue (MB) of O-ZnO (achieving 70% MB degradation at 90 min) was superior to C-ZnO, due to its higher surface area and degree of crystallinity and lower bulk/surface defects ratio.
The atomic layer deposition (ALD) of several metal oxides is selectivity inhibited on alkanethiol self-assembled monolayers (SAMs) on Au and the eventual nucleation mechanism is investigated. The inhibition ability of the SAM is significantly improved by the in situ H 2 -plasma pretreatment of the Au substrate prior to gas-phase deposition of a long-chain alkanethiol, 1-dodecanethiol (DDT). This more rigorous surface preparation inhibits even aggressive oxide ALD precursors, including trimethylaluminum and water, for at least 20 cycles. We study the effect that ALD precursor purge times, growth temperature, alkanethiol chain length, alkanethiol deposition time, and plasma treatment time have on Al 2 O 3 ALD inhibition. This is the first example of Al 2 O 3 ALD inhibition from a vapor-deposited SAM. Inhibition of Al 2 O 3 , ZnO, and MnO ALD processes are compared, revealing the versatility of this selective surface treatment. As a result, atomic force microscopy (AFM) and grazing incidence x-ray fluorescence (GIXRF) further reveals insight into the mechanism by which the well-defined surface chemistry of ALD may eventually be circumvented to allow metal oxide nucleation and growth on SAM-modified surfaces.
Silver films of varying thicknesses (25, 45, and 60 nm) were deposited on indium tin oxide (ITO) on silicon and zinc oxide (ZnO) on silicon. The films were annealed in vacuum for 1 h at different temperatures (300-650 deg. C). Four-point-probe measurements were used to determine the resistivity of the films. All films showed an abrupt change in resistivity beyond an onset temperature that varied with thickness. Rutherford backscattering spectrometry measurements revealed agglomeration of the Ag films upon annealing as being responsible for the resistivity change. X-ray pole figure analysis determined that the annealed films took on a preferential <111> texturing; however, the degree of texturing was significantly higher in Ag/ZnO/Si than in Ag/ITO/Si samples. This observation was accounted for by interface energy minimization. Atomic force microscopy (AFM) measurements revealed an increasing surface roughness of the annealed films with temperature. The resistivity behavior was explained by the counterbalancing effects of increasing crystallinity and surface roughness. Average surface roughness obtained from the AFM measurements were also used to model the agglomeration of Ag based on Ostwald ripening theory.
Highlights: • We have demonstrated nondegenerate n-type doping phenomenon of MoS{sub 2} by ZnO. • ZnO doping improved the electrical parameters of MoS{sub 2} transistor (I{sub on}↑, μ{sub FE}↑, n↑). • The reduction of ZnO doping effect (ΔV{sub TH}: ∼75% ↓) was observed in air. • The highest photoresponsivity of ZnO-doped MoS{sub 2} photodetector was 3.18 × 10{sup 3} A/W. • The highest detectivity of ZnO-doped MoS{sub 2} photodetector was 5.94 × 10{sup 12} Jones. - Abstract: In this paper, we have demonstrated nondegenerate n-type doping phenomenon of MoS{sub 2} by ZnO. The ZnO doping effects were systematically investigated by Raman spectroscopy and electrical/optical measurements (I{sub D}–V{sub G} with/without exposure to 520, 655, 785, and 850 nm laser sources). The ZnO doping improved the performance parameters of MoS{sub 2}-based electronics (I{sub on}↑, μ{sub FE}↑, n↑) owing to reduction of the effective barrier height between the source and the MoS{sub 2} channel. We also monitored the effects of ZnO doping during exposure to air; reduction in ΔV{sub TH} of about 75% was observed after 156 h. In addition, the optoelectronic performance of the MoS{sub 2} photodetector was enhanced due to the reduction of the recombination rate of photogenerated carriers caused by ZnO doping. In our results, the highest photoresponsivity (about 3.18 × 10{sup 3} A/W) and detectivity (5.94 × 10{sup 12} Jones) of the ZnO-doped photodetector were observed for 520 nm laser exposure.
Explore the source record for details and available documents.
Highlights: ► Amine-functionalized zinc oxide nanoparticle (AFZON) was synthesized. ► Isotherm and kinetics data followed Langmuir isotherm and pseudo-second order kinetic model, respectively. ► Q{sub 0} of ZON for AB25, DR23 and DR31 was 20, 12 and 15 mg/g, respectively. ► Q{sub 0} of AFZON for AB25, DR23 and DR31 was 1250, 1000 and 1429 mg/g, respectively. ► AFZON was regenerated at pH 12. -- Abstract: In this paper, the surface modification of zinc oxide nanoparticle (ZON) by amine functionalization was studied to prepare high capacity adsorbent. Dye removal ability of amine-functionalized zinc oxide nanoparticle (AFZON) and zinc oxide nanoparticle (ZON) was also investigated. The physical characteristics of AFZON were studied using Fourier transform infrared (FTIR), scanning electron microscopy (SEM) and X-ray diffraction (XRD). Acid Blue 25 (AB25), Direct Red 23 (DR23) and Direct Red 31 (DR31) were used as model compounds. The effect of operational parameters such as dye concentration, adsorbent dosage, pH and salt on dye removal was evaluated. The isotherm and kinetic of dye adsorption were studied. The maximum dye adsorption capacity (Q{sub 0}) was 20 mg/g AB25, 12 mg/g DR23 and 15 mg/g DR31 for ZON and 1250 mg/g AB25, 1000 mg/g DR23 and 1429 mg/g DR31 for AFZON. It was found that dye adsorption followed Langmuir isotherm. Adsorption kinetic of dyes was found to conform to pseudo-second order kinetics. Dye desorption tests (adsorbent regeneration) showed that the maximum dye release of 90% AB25, 86% for DR23 and 90% for DR31 were achieved in aqueous solution at pH 12. Based on the data of the present investigation, it can be concluded that the AFZON being an adsorbent with high dye adsorption capacity might be a suitable alternative to remove dyes from colored aqueous solutions.
The impact of humidity and temperature on a zinc oxide based transparent conducting oxide (TCO) was assessed under accelerated aging conditions. An in situ electroanalytical method was used to monitor the electrical properties for a conducting zinc oxide under controlled atmospheric (humidity, temperature and irradiation) conditions. A review of thin film photovoltaic (PV) literature has shown one major failure mode of cells/modules is associated with the ingress of water into modules in the field. Water contamination has been shown to degrade the performance of the TCO in addition to corroding interconnects and other conductive metals/materials associated with the module. Water ingress is particularly problematic in flexible thin film PV modules since traditional encapsulates such as poly(ethyl vinyl acetate) (EVA) have high water vapor transmission rates. The accelerated aging studies of the zinc oxide based TCOs will allow acceleration factors and kinetic parameters to be determined for reliability purposes.
Vertically aligned zinc oxide nanorods were grown on low and high temperature deposited aluminium doped zinc oxide seed layer by hydrothermal method and annealed to improve crystallinity. The morphology of the seed layer and the grown nanorods were studied by field emission scanning electron microscopy characterization technique. The properties of the zinc oxide nanorods were analyzed using laser spectroscopic studies. Resonant Raman spectroscopy reveals the unique increase in the A{sub 1}(LO) mode of vibration with increase in count. The luminescence property of the nanorods was studied with photoluminescence spectrometer. The vertically aligned zinc oxide nanorods show, the very high band edge emission in the ultraviolet region of the electromagnetic spectrum.
Optical properties of zinc oxide analyzed by exposing samples to mechanical and thermal treatments and UV radiation
Ultraviolet degradation of zinc oxide thin films