Pin Load Control Applied to Retractable Pin Tool Technology and its Characterization

Until the development of retractable pin tool (RPT) technology, friction stir welding (FSW) was limited to constant thickness joining of aluminum materials and the choices of keyhole elimination focused on traditional fusion and plug weld repair techniques. An invention, US Patent Number 5,893,507, "Auto-Adjustable Pin Tool for Friction Stir Welding" assigned to NASA, demonstrated an approach to resolve these serious drawbacks. This approach brings forth a technique that allows the crater, or keyhole, to be closed out automatically at the end of the weld joint without adding any additional equipment or material. Also the probe length can be varied automatically in the weld joint to compensate for material thickness changes, such as, in a tapered joint. This paper reports the effects of pin extension and retraction rates in the weld joint and its correlation to weld quality. The investigation utilized a pin load-detecting device that was integrated in the Phase 2A RPT designed by Boeing for NASA/MSFC. The RPT modification provided pin load data that was accessed and used to eliminate root side indications and determine pin manipulation rates necessary to produce consistence homogeneous joints.

Oelgoetz, Peter A.↗

Pin Load Control Applied to Retractable Pin Tool Technology and its Characterization

Until the development of retractable pin tool (RPT) technology, friction stir welding (FSW) was limited to constant thickness joining of aluminum materials and the choices of keyhole elimination focused on traditional fusion and plug weld repair techniques. An invention, US Patent Number 5,893.507, "Auto-Adjustable Pin Tool for Friction Stir Welding" assigned to NASA, demonstrated an approach to resolve these serious drawbacks. This approach brings forth a technique that allows the crater, or keyhole, to be closed out automatically at the end of the weld joint without adding any additional equipment or material. Also the probe length can be varied automatically in the weld joint to compensate for material thickness changes, such as, in a tapered joint. This paper reports the effects of pin extension and retraction rates in the weld joint and its correlation to weld quality. The investigation utilized a pin load-detecting device that was integrated in the Phase 2A RPT designed by Boeing for NASA/MSFC. The RPT modification provided pin load data that was accessed and used to eliminate root side indications and determine pin manipulation rates necessary to produce consistence homogeneous joints.

Oelgoetz, Peter↗

Use of photostress to characterize the mechanical behavior of weldments

Welded aluminum is an important part of many space structures. Knowledge of the properties and behavior of weld material and the material surrounding the weld is important for modeling and design of the structures. Photoelastic coatings (Photostress) and strain gages were used to determine behavior of heat treated and as welded joints made from 2219T87 parent material and 2319 weld material subjected to tensile loads. TIG welds of 1/8, 1/2, and 1.4 inches thickness were investigated. Discontinuous yielding was observed in all tests and highly non-uniform behavior through the weld thickness was observed in joints having welds 1.4 inches thick. Joints having welds 1/8 and 1/2 inches thick had only small differences in behavior through the thickness of the weld. Joints in the 1/2 inch thick material contained distinct zones of constant strain within the normal strain gradient extending outward from the weld centerline. These zones had different thickness and locations. Points at the weld centerline, and for a distance of nearly one inch from the centerline, exhibited very nonlinear behavior during the first loading but exhibited near perfect strain hardening during the second loading.

Gambrell, S. C., Jr.↗

Making Internal Molds Of Long, Curved Tubes

Mold material carried to internal weld joint and removed after impression taken. Remotely operated device makes impression mold of interior surface of tube at weld joint. Mold provides indication of extent of mismatch between members at joint. Maneuvered to weld inspected through curved tube 3 in. in diameter by 50 in. long. Readily adapted to making molds to measure depth of corrosion in boiler tubes or other pipes.

Burley, Richard K.↗

Development of sensor augmented robotic weld systems for aerospace propulsion system fabrication

In order to meet stringent performance goals for power and reuseability, the Space Shuttle Main Engine was designed with many complex, difficult welded joints that provide maximum strength and minimum weight. To this end, the SSME requires 370 meters of welded joints. Automation of some welds has improved welding productivity significantly over manual welding. Application has previously been limited by accessibility constraints, requirements for complex process control, low production volumes, high part variability, and stringent quality requirements. Development of robots for welding in this application requires that a unique set of constraints be addressed. This paper shows how robotic welding can enhance production of aerospace components by addressing their specific requirements. A development program at the Marshall Space Flight Center combining industrial robots with state-of-the-art sensor systems and computer simulation is providing technology for the automation of welds in Space Shuttle Main Engine production.

Jones, C. S.↗

Effect of high temperature aging on bonded and weld bonded joints

Development of adhesives for applications requiring long-term service at temperatures up to 600 F is discussed. This development work utilizes polyimide (PI) and polyphenylquinoxaline (PPQ) resin technology worked out previously. The resultant adhesives are evaluated in structural joints of titanium, steel and composite adherends and in honeycomb sandwich panels. Suitable adhesives also are evaluated in weld bonded titanium alloy joints. Testing includes determination of long-term aging of stressed and unstressed specimens at temperatures from about 450 F to 600 F as well as under dynamic fatigue conditions.

Vaughan, R. W.↗

Strength of Rewelded Inconel 718

Inconel 718, nickel-based alloy used extensively for high-temperature structural service, welded repeatedly without detriment to its strength. According to NASA report, tests show 12 repairs on same weld joint do not adversely affect ultimate tensile strenth, yield strength, fatigue strength, metallurgical grain structures, or ability of weld joint to respond to post weld heat treatments.

Bayless, E.↗

Electron Beam Welding of Pure Tungsten Hex Cans for Nuclear Thermal Propulsion Engines

Nuclear thermal propulsion (NTP) is an in-space propulsion method currently being developed at the NASA Marshall Space Flight Center (MSFC). NTP systems are a high specific impulse (750–1,100 s), high thrust (15,000–250,000 lbf ) method of propulsion which have the potential to allow for faster transit times when optimizing for high ΔV. In the nuclear rocket engine, the heat from the nuclear fission reaction is transferred to a low molecular mass propellant (such as hydrogen). Hot propellant is expanded through a nozzle to generate thrust. Development of ceramic metal (cermet) fuel systems for NTP applications is currently ongoing at MSFC. In cermet fuel systems, ceramic fissile fuel particles such as uranium nitride or uranium dioxide are dispersed within a net-shaped, high-density structural matrix. The composite material is cladded by a protective metal structure to make up an NTP fuel element. Cladding materials must be able to withstand the demanding operating conditions required of the engine as well as retain a hermetic seal to allow for retention of fuel element structural integrity, prevent hydrogen attack or migration of the ceramic fuel, and limit release of fission products during operation. For NTP applications, tungsten is a prime material for both the metal matrix and cladding in cermet fuel systems because of its high melting point, high temperature strength, and compatibility with hot hydrogen. If a weld in tungsten with the capability of holding a hermetic seal is achievable, tungsten becomes a strong candidate for NTP applications. This Technical Memorandum focuses on determining the weldability of pure tungsten using electron beam welding (EBW). Tungsten appears well suited for NTP applications, but it has a high ductile to brittle transition temperature (DBTT) dependent upon chemical composition, structure/stress distribution, and mechanical conditions. Therefore, it is highly subject to brittle fracture. Because of its high susceptibility to brittle fracture, it is very difficult to weld. EBW was chosen for joining pure tungsten because of its low heat input compared to gas tungsten arc welding. Reduced heat input can be directly correlated with an increase in ductility of a tungsten weld. EBW is a high energy density welding process in which a stream of electrons penetrates a weld joint in a deep, narrow spike in contrast to a broad gas tungsten arc weld pool. The investigation initially focused on EBW of tungsten plates of both 0.01 in and 0.03 in thickness to determine if EBW could weld pure tungsten without the presence of visual defects—particularly cracking—in the welds. Variation in the weld procedure and post-weld heat treatment (PWHT) was used to improve the surface appearance of flat EBWs on a pure tungsten sheet. The investigation moved on to weld 0.05-in-thick hexagonal tungsten cans with a weld joint thickness of 0.025 in. The goal for welding the pure tungsten hex cans was to avoid any visual surface defects and generate a weld capable of a hermetic seal. This proved difficult. Cold welds commonly exhibited porosity that leaked air. Hot welds exhibited cracks, typically observed immediately after welding. Later welds were preheated to increase ductility and decrease the likelihood of through-thickness cracking. PWHT was used to arrest microcrack growth both in the flat weld samples and hexagonal weld samples.

Courtright, Z. S.↗

Room temperature crack growth rates and -20 deg F fracture toughness of welded 1 1/4 inch A-285 steel plate

Data are presented which were developed in support of a structural assessment of NASA-LEWIS' 10-foot by 10-foot supersonic wind tunnel, critical portions of which are fabricated from rolled and welded 1 1/4 inch thick A-285 steel plate. Test material was flame cut from the tunnel wall and included longitudinal and circumferential weld joints. Parent metal, welds, and weld heat affected zone were tested. Tensile strength and fracture toughness were determined at -20 F, the estimated lowest tunnel operating temperature. Crack growth rates were measured at room temperature, where growth rates in service are expected to be highest.

Shannon, J. L., Jr.↗

Seam tracking performance of a Coaxial Weld Vision System and pulsed welding

This report describes a continuation of a series of tests on the Coaxial Weld Vision System at MSFC. The ability of the system to compensate for transients associated with pulsed current welding is analyzed. Using the standard image processing approach for root pass seam tracking, the system is also tested for the ability to track the toe of a previous weld bead, for tracking multiple pass weld joints. This Coaxial Weld Vision System was developed by the Ohio State University (OSU) Center for Welding Research and is a part of the Space Shuttle Main Engine Robotic Welding Development System at MSFC.

Gangl, K. J.↗

Wide Panel Testing Technique for Evaluating Repair Weld Strengths

This paper describes a new tensile testing technique for evaluating the overall effect of a repair weld on the strength of a welded joint. Previously, repair weld strengths have been evaluated using one-inch width tensile specimens, but this technique does not capture all of the effects that result from a repair. The new technique involves testing of "wide panel" tensile specimens which contain the full length of a repair weld within a longer initial weld, allowing the specimen to capture the combined effects of residual stresses, local strength degradation, and load redistribution around a repair. The development of strains in the repair area of standard aluminum alloy specimens and new high-performance aluminum-lithium alloy specimens was observed and evaluated using photoelastic material. The results of this evaluation show an increased sensitivity to repair welding residual stresses in the aluminum-lithium alloy specimens.

Rogers, Patrick R.↗

Strength of Welded Aircraft Joints

This investigation is a continuation of work started in 1928 and described in NACA-TR-348 which shows that the insertion of gusset plates was the most satisfactory way of strengthening a joint. Additional tests of the present series show that joints of this type could be improved by cutting out the portion of the plate between the intersecting tubes. T and lattice joints in thin-walled tubing 1 1/2 by 0.020 inch have somewhat lower strengths than joints in tubing of greater wall thickness because of failure by local buckling. In welding the thin-walled tubing, the recently developed "carburizing flux" process was found to be the only method capable of producing joints free from cracks. The "magnetic powder" inspection was used to detect cracks in the joints and flaws in the tubing.

Brueggeman, W C↗

Residual Stress Measurements of Ni-base Superalloys through Neutron Diffraction

Linear friction welding (LFW) is being considered for joining single crystal to polycrystalline nickel-base alloys for advanced high temperature gas turbine disks. Unfortunately, the transient thermal cycle during the welding generates undesirable residual stresses. Additionally, upon thermal treatment to relieve these residual stresses the weld joints often crack. To understand this issue, state-of-the-art neutron diffraction was performed near weld joints to quantify the residual stresses created by varying linear friction weld conditions. The residual stresses were measured along three orthogonal axes in both the polycrystalline LSHR and single crystal SC-180 alloys. Residual stress measurements using a contour method were used to compare the calculations obtained by neutron diffraction. The results suggest high residual stresses can be successfully reduced using both pre- and post-weld processing steps. Moreover, the effect of grain size and pre-heat temperatures on the LFW process were explored.

Superalloys↗

Gas tungsten arc welding and post weld heat treatment effects on microstructure and mechanical property of castable nanostructured alloy steel

Here, this paper details the first study of castable nanostructured alloy (CNA) steel gas tungsten arc weldability and the post-weld heat treatment (PWHT) effects. Effects of welding heat input, thermal cycles, and PWHT on microstructures, microhardness distributions, room temperature tensile properties, and fracture characteristics are discussed. Results show that CNA steel exhibits excellent weldability (i.e., no indication of welding defects and reasonable tensile properties). The welded joint exhibited heterogeneous microstructures with δ-ferrite as well as large microhardness variation and fluctuation. The welded joint yield and ultimate tensile strengths were similar to those of the base metal, but the elongations decreased by 30 %. However, with normalization and tempering PWHT, the δ-ferrite was eliminated, microstructure was modified, hardness was unified, and joint ductility was restored. The study indicated that the CNA reduced-activation ferritic-martensitic steel owns excellent weldability, and PWHT is needed for the industrial application of welded structures.

36 MATERIALS SCIENCE↗

Simulation Tools for Characterizing Stress Distribution in Laser Welded Dissimilar Joints

This project focuses on developing a thermo-metallurgical-mechanical modeling method to accurately predict the microstructural evolution and residual stress in laser welding between dissimilar metals, such as HSLA steel and high carbon equivalent (CE) gear steel. The method leverages a comprehensive material database to model the temperature and rate dependent phase transformations, along with their associated effects on material properties, such as thermal expansion and flow stress, throughout the welding process. A key innovation is the incorporation of phase transformation and phase-specific properties, which enhances the accuracy of residual stress predictions. The mixture material in the fusion zone due to the dissimilar metals will also be addressed in the numerical model. This is especially critical in scenarios involving phase transformations in the fusion zone and heat-affected zone (HAZ), where the phase changes can induce substantial residual stress variations. The material database has been generated using JMatPro. The modeling approach is implemented through a custom User Material (UMAT) subroutine, executed with the commercial finite element software Abaqus.

36 MATERIALS SCIENCE↗