At least 73 records · Page 4

Self-lubricating coatings for high-temperature applications

Some present-day aeropropulsion systems impose severe demands on the thermal and oxidative stability of lubricant, bearing, and seal materials. These demands will be much more severe for operational systems around the turn of the century. Solid lubricants with maximum temperature capabilities of about 1100 C are known. Unfortunately, none of the solid lubricants with the highest temperature capabilities are effective below approximately 400 C. However, research shows that silver and stable fluorides, such as calcium and barium fluoride act synergistically to provide lubrication from below room temperature to approximately 900 C. Plasma-sprayed, self-lubricating composite coatings that were developed at Lewis are described. Background information is given on coatings, designed as PS100 and PS101, that contain the solid lubricants in a Nichrome matrix. These coatings have low friction coefficients over a wide temperature range, but they have inadequate wear resistance for some long-duration applications. Wear resistance was dramatically improved in a recently developed coating PS200, by replacing the Nichrome matrix material with metal-bonded chromium carbide containing dispersed silver and calcium fluoride/barium fluoride eutectic (CaF2/BaF2). The lubricants control friction and the carbide matrix provides excellent wear resistance. Successful tests of these coatings are discussed.

Sliney, Harold E.↗

High-Sensitivity Low-Energy Ion Spectroscopy with Sub-Nanometer Depth Resolution Reveals Oxidation Resistance of MoS 2 Increases with Film Density and Shear-Induced Nanostructural Modifications of the Surface

For decades, density has been attributed as a critical aspect of the structure of sputter-deposited nanocrystalline molybdenum disulfide (MoS 2 ) coatings impacting oxidation resistance and wear resistance. Despite its importance, there are few examples in the literature that explicitly investigate the relationship between the density and oxidation behaviors of MoS 2 coatings. Aging and oxidation are primary considerations for the use of MoS 2 coatings in aerospace applications as they inevitably experience prolonged storage in water and oxygen-rich environments prior to use. Oxidation that is either limited to the first few nanometers or through the bulk of the coating can result in seizure due to high initial coefficients of friction or component failure from excessive wear. High-sensitivity low-energy ion spectroscopy (HS-LEIS) and Rutherford backscattering spectrometry (RBS) are both used to understand the extent of oxidation throughout the first ~10 nanometers of the surface of pure sputtered nanocrystalline MoS 2 coatings after high-temperature aging and how it is impacted by the density of coatings as measured by RBS. Results show that low-density coatings (ρ = 3.55 g/cm 3 ) exhibit a more columnar microstructure and voiding, which act as pathways for oxidative species to penetrate and interact with edge sites, causing severe surface and subsurface oxidation. Furthermore, HS-LEIS of surfaces sheared prior to oxidation reveals that the oxidation resistance of low-density MoS 2 coatings can be significantly improved by shear-induced reorientation of the surface microstructure to a basal orientation and elimination of pathways for oxygen into the bulk through compaction of surface and subsurface voids.

36 MATERIALS SCIENCE↗

Effect of annealing on the tribological behavior of Zr-based bulk metallic glass

Bulk Metallic Glasses (BMGs) are promising materials for several applications owing to their high elastic limit and resistance to permanent deformation. However, BMGs have lower wear resistance than their crystalline counterparts during dry sliding. The formation of a composite material with crystalline phases dispersed in the BMG matrix through devitrification and partial crystallization at elevated temperatures has recently been proposed as an effective way to improve the wear resistance. However, our understanding of the origin of the improved wear behavior of annealed BMGs is still elusive. Here, a systematic evaluation of the effect of annealing temperature (from temperatures lower than the BMG glass transition temperature to temperatures higher than the BMG recrystallization temperature) on the friction and wear response of a Zr-based BMG, namely Vit105 (Zr 52.5 Cu 17.9 Ni 14.6 Al 10 Ti 5 ), was performed. The results indicate that annealing Vit105 improves its wear resistance while also reducing the steady-state friction response when the annealing temperature is close to the glass transition temperature. Notably, the formation of a transfer film on the sapphire countersurface is highly dependent on the applied normal load and sliding time. Finally, the wear mechanism was found to be strongly dependent on the annealing temperature as a transition from a predominantly adhesive wear mechanism to an abrasive-dominated one was observed as the annealing temperature crossed the glass transition temperature. Altogether, the results of this work aid to our understanding of the tribological behavior of Zr-based BMGs in general, while also providing clues to strategies for the effective use of BMGs in tribological applications.

Lien, Hsu-Ming [Univ. of Texas, Austin, TX (United↗

Preparation of particle-dispersion alloys (M-6)

A particle dispersion alloy is one type of metal-ceramic composite material, and is used as heat resistance material, wear resistance material, and electrical material. This material consists of a metal matrix and dispersed particles, and for its unique structure it has both tenacity as a metal and hardness as a ceramic. Its properties improve when the particles become finer and disperse more uniformly. Most of the particle dispersion alloys are produced by the powder metallurgical process. This process is favorable for uniform dispersion of particles, but it consists of complicated techniques such as mechanical alloying and hot extrusion, and has the following drawbacks: (1) it is difficult to fabricate large-sized products; (2) the amount of particles is limited to a few percent; and (3) the process is complicated and expensive. To overcome these drawbacks, recently special attention has been paid to conventional melting process. However, under terrestrial conditions, dispersions separate immediately due to the different specific gravities of the metal matrix and the particles and thermal convection effects. The microgravity environment is, therefore, considered to be an attractive place for fabricating the dispersion alloy. This space experiment is carried out to clarify the influence of microgravity on the properties of the particle dispersion alloy and to obtain a deeper understanding of the experiment under the microgravity environment.

Muramatsu, Yuji↗

Quality optimization of thermally sprayed coatings produced by the JP-5000 (HVOF) gun using mathematical modeling

Currently, thermal barrier coatings (TBC) of gas-turbine blades and similar applications have centered around the use of zirconia as a protective coating for high thermal applications. The advantages of zirconia include low thermal conductivity and good thermal shock resistance. Thermally sprayed tungsten carbide hardface coatings are used for a wide range of applications spanning both the aerospace and other industrial markets. Major aircraft engine manufacturers and repair facilities use hardface coatings for original engine manufacture (OEM), as well as in the overhaul of critical engine components. The principle function of these coatings is to resist severe wear environments for such wear mechanisms as abrasion, adhesion, fretting, and erosion. The (JP-5000) thermal spray gun is the most advanced in the High Velocity Oxygen Fuel (HVOF) systems. Recently, it has received considerable attention because of its relative low cost and its production of quality coatings that challenge the very successful but yet very expensive Vacuum Plasma Spraying (VPS) system. The quality of thermal spray coatings is enhanced as porosity, oxidation, residual stress, and surface roughness are reduced or minimized. Higher densification, interfacial bonding strength, hardness and wear resistance of coating are desirable features for quality improvement.

Tawfik, Hazem↗

Investigating the Adhesion Force of Lunar Regolith Particulates on Air Plasma Sprayed Alumina Coatings

Ceramic materials, often used to protect components due to their high strength, and wear resistance, have added benefits of being lightweight and providing multifunctional properties. They are, therefore, significant to provide durability and support during long-duration missions to the moon’s surface for rovers, landers, robotic systems, habitats, and many other components. Materials such as aluminum oxide with high mechanical strength and hardness can help to improve the durability of structures used in space exploration. Devices used for space exploration require the use of materials with the ability to withstand exposure to extreme environments. Lunar regolith is a constituent with the ability to adhere electrostatically and damage the components used to perform these missions due to adhesion of lunar dust projectiles that can cause delamination on surfaces, which may not be physically visible. The particulates of lunar dust are classified as corrosive material, leading to the degradation of structures. Aluminum oxide presents excellent resistance to different types of wear due to its high strength and hardness. Air plasma sprayed (APS) aluminum oxide coatings have demonstrated the potential to protect the surface to which they are applied. However, the parameters of roughness and porosity of the coatings need to be considered to establish if they can protect the components from extreme environments. Considering the electrostatic forces that the components are exposed to, the adhesion between the lunar regolith and the surface of the components needs to be investigated. In this work, the adhesion forces of lunar dust simulants with an average size of 30 𝜇m are investigated considering the roughness of the surface of the APS aluminum oxide. The centrifugal technique utilized here offers the advantage of establishing the adhesion force between particles with different shapes on smooth or rough surfaces. The simulants were deposited on the surface of APS aluminum oxide using an aerosolization technique to achieve a monolayer coating in three different locations across the specimen to determine the increments in adhesion force at the centrifuge. The roughness of the APS aluminum oxide was determined to be 2.257 𝜇m. The specimen was tested under an incremental centrifugal speed from 100 rpm to 3000 rpm for 20 seconds. Low magnification microscopy images were collected to cover a larger surface area of the test coating. The adhesion force was measured considering the distance from the centrifugal axis and the rotational speed. Due to the coating roughness, and the distance from the centrifugal axis, the results demonstrated a larger adhesion force in locations closer to the centrifugal axis. Smaller particles were entrapped within the roughness of the coating, and a stronger adhesion force was measured. In order to continue designing wear-resistant coating for structural protection in space missions, press-on experiments using a centrifuge will be performed. Future experiments will allow us to determine the design parameters for APS aluminum oxide coating to protect the structures from harsh space environments.

Perla Latorre-Suarez↗

A Comparative Tribo-Mechanical Behavior Analysis of Laser Cladded Nitronic 60 Coating Against Wrought Nitronic 60 Alloy

In this study the tribological and mechanical behavior of a laser cladded Nitronic 60 coating on maraging steel is compared to that of a wrought Nitronic 60 alloy. A multi-layer Nitronic 60 coating was deposited using laser directed energy deposition, and its microstructure, porosity, and microhardness were characterized. The microhardness of the coated region in the laser cladded Nitronic 60 varied between 270-300 HV whereas that for wrought form was 230 HV. Controlled tribological tests under motor oil lubricated conditions were conducted at both room and elevated temperatures. The laser cladded Nitronic coating exhibited poorer wear resistance at room temperature but higher wear resistance at elevated temperature as compared to the wrought Nitronic alloy. Severe plastic deformation and fracture was observed on the laser cladded coating after the wear tests at both temperatures. Wear mechanisms were investigated based on the morphological and compositional characterization of the wear tracks.

36 MATERIALS SCIENCE↗

Tribological behaviors of nanotwinned Al alloys

Wear-induced damages cause significant materials loss each year. Al alloys are widely used by industry but usually have low wear resistance. Here, we compare the tribological behaviors of ultrafine grained Al, a nanoprecipitate hardened Al 7075 alloy and nanotwinned Al–Ni alloys using the nanoscratch. The nanotwinned Al–Ni alloys exhibit lower coefficient of friction and much greater wear resistance than the Al and Al 7075 alloys. Additionally, the enhanced wear properties of Al–Ni alloys arise from their high strength and the evolution of nanotwinned microstructures into gradient nanograins during wear. These findings on fundamental wear mechanisms in nanotwinned alloys may advance the discovery of wear-resistant metallic materials.

36 MATERIALS SCIENCE↗

Effect of 3D-printed surface textures on wear mechanism in 3-body abrasion of soil

This study systematically investigates the enhancement of wear resistance in 3D printed surface textures through both experimental and theoretical approaches. Three distinct surface morphologies (Smooth Surface, Surface with uniformly distributed Pits, and Surface with uniformly distributed Bumps) were fabricated using High-Impact Polystyrene, where the meso-scale textures were precisely controlled through the 3D printing process. Wear behavior was evaluated using a 3-body wear tester in an abrasive particle environment, analyzing the influence of surface textures under various operating conditions. Systematic wear tests revealed that optimally designed surface textures achieved a remarkable 77 % reduction in wear compared to the worst-performing sample. The wear mechanisms were comprehensively characterized through weight loss measurements, Scanning Electron Microscopy (SEM), and Energy Dispersive Spectroscopy (EDS) analyses, elucidating the surface morphology changes and their interaction with wear particles. Notably, the study identified how the geometric characteristics of surface textures influence the movement of wear particles and the distribution of contact stresses. Discrete element method simulations corroborated the experimental findings, providing theoretical validation for the enhanced wear resistance of the optimal structure. The high correlation between simulated wear patterns and experimental results validates the reliability of the proposed design methodology. In conclusion, these results demonstrate that 3D printed surface texturing offers a cost-effective and scalable approach to significantly improve wear resistance in engineering applications, presenting a practical alternative to conventional, high-cost surface engineering methods.

3-body abrasion↗

Measuring the Wear and Abrasive Resistance of Air Plasma Sprayed Aluminum Oxide for Lunar Exploration

Lunar regolith, especially finer dust particles traveling at high velocities, can cause significant wear and abrasive damage to structural components that ensure a prolongated presence on the surface of the Moon. With the absence of an atmosphere and lower gravity than on Earth, regolith particles maintain high velocities at large distances from where they were generated, for example next to lunar landers. Wear-resistant ceramic and ceramic composite materials can improve the durability of spacecraft components during long missions on the Moon’s surface. Aluminum oxide coatings are lightweight, have multifunctional properties, and have high strength including high hardness and wear resistance. These properties can help improve the durability of structures used in space exploration. Air plasma sprayed (APS) aluminum oxide coatings have demonstrated the potential to protect critical structures. This study investigated the abrasive wear resistance of APS aluminum oxide coatings via Taber abrasion experiments. Taber abrasion offers the advantage of quantifying the abrasive wear behavior of particles with different shapes on a surface. In this work, an abrasive wheel made of silicon carbide was utilized to evaluate wear properties of specimens progressively over 5000 cycles. This experiment focused on testing two series of specimens to determine whether a bond coat composed of nickel, chromium, aluminum, and yttrium (NiCrAlY) improved the protective behavior of the APS aluminum oxide coating. The specimens varied in topcoat thickness and were made with and without an approximately 100 µm bond coat layer. The mass of the specimens was measured at 400 cycles, 800 cycles, 3800 cycles, and 5000 cycles. Increasing thickness was found to result in higher wear for samples with and without a bond coat. Increased mass loss in samples with a bond coat was observed indicating a need for further studies on the overall impact of the use of a bond coat on the protective behavior of the coatings. To continue designing wear resistant coatings for structural protection in space missions, the multifunctional properties of the APS aluminum oxide coating will be studied. Future experiments will determine whether the APS aluminum oxide coating can protect the structures from other aspects of the harsh space environment, such as extreme temperature variations and ionizing radiation.

aluminum oxide↗

Tribological performance of Al2O3-B2O3 composites: Role of CuOand CaO constituents

Al2O3-B2O3 based composites for wear resistant applications (e.g., seal rings and bearings) were manufactured using powder metallurgy route. Four different compositions were considered to control amount of in situ phases, mainly aluminum borate, formed during sintering. The fabricated composites were characterized using X-ray diffraction to identify the phases. Hardness was measured in terms of micro-hardness. The tribological performance of the composites were evaluated by conducting dry sliding tests against alumina balls at different humidity levels (10 – 95% relative humidity). The X-ray spectrum revealed that increase in B2O3 content in the composites increased the amount of aluminum borate phase that enhanced the micro-hardness. Results revealed that aluminum borate enhanced the wear resistance of the composites, whereas the humidity-sensitive alumina phase reduced friction at higher humidity levels. Furthermore, CuO and CaO (2-5 wt.%) were added separately to the composite, resulting in increased density by 22-48 %. Athough the addition of CuO and CaO led to increase in hardness and wear resistance of the composites, the coefficient of friction was negatively affected. The friction and wear performance along with wear mechanism are discussed with respect to observed phases in the composites.

Ashish K. Kasar↗

Residual stresses in Cu matrix composite surface deposits after laser melt injection

Abstract Tungsten carbide particles reinforced metal matrix composite (MMC) coatings can significantly improve surface wear resistance owing to their increased surface hardness. However, the presence of macro‐ and micro‐residual stresses in MMC coatings can have detrimental effects, such as reducing service life. In this study, neutron diffraction was used to determine the residual stresses in spherical fused tungsten carbide (sFTC) reinforced Cu matrix composite surface deposits after laser melt injection. We also developed a thermo‐mechanical coupled finite element model to predict residual stresses. Our findings reveal that sFTC/Cu composite deposits produced with a preheating temperature of 400°C have low residual stresses, with a maximum tensile residual stress of 98 MPa in the Cu matrix on the top surface. In contrast, the sFTC/bronze (CuAl10Ni5Fe4) composite deposit exhibits very high residual stresses, with a maximum tensile residual stress in the Cu matrix on the top surface reaching 651 MPa. These results provide a better understanding of the magnitudes and distributions of residual stresses in sFTC‐reinforced Cu matrix composite surface deposits manufactured via laser melt injection.

Zhang, Xingxing↗

Friction and Wear Properties of As-deposited and Carbon Ion-implanted Diamond Films

Recent work on the friction and wear properties of as-deposited and carbon ion-implanted diamond films was reviewed. Diamond films were produced by the microwave plasma chemical vapor deposition (CVD) technique. Diamond films with various grain sizes and surface roughnesses were implanted with carbon ions at 60 ke V ion energy, resulting in a dose of 1.2310(exp 17) carbon ions/cm(exp 2). Various analytical techniques, including Raman spectroscopy, proton recoil analysis, Rutherford backscattering, transmission and scanning electron microscopy, x-ray photoelectron spectroscopy, and x-ray diffraction, were utilized to characterize the diamond films. Sliding friction experiments were conducted with a polished natural diamond pin in contact with diamond films in the three environments: humid air (40 percent relative humidity), dry nitrogen (less than 1 percent relative humidity), and ultrahigh vacuum (10(exp -7) Pa). The CVD diamond films indeed have friction and were properties similar to those of natural diamond in the three environments. The as-deposited, fine-grain diamond films can be effectively used as self-lubricating, wear-resistant coatings that have low coefficients of friction (0.02 to 0.04) and low wear rates (10(exp -7) to 10(exp -8)mm(exp 3)/N-m) in both humid air and dry nitrogen. However, they have high coefficients of friction (1.5 to 1.7) and a high wear rate (10(exp -4)mm(exp 3/N-m) in ultrahigh vacuum. The carbon ion implanation produced a thin surficial layer (less than 0.1 micron thick) of amorphous, nondiamond carbon on the diamond films. In humid air and dry nitrogen, the ion-implanted, fine- and coarse-grain diamond films have a low coefficient of friction (around 0.1) and a low wear rate (10(exp -7)mm(exp 3/N-m). Even in ultrahigh vacuum, the presence of the nondiamond carbon layer reduced the coefficient of friction of fine-grain diamond films to 0.1 or lower and the wear rate to 10(exp -6)mm(exp 3)/N-m. Thus, the carbon ion-implanted, fine-grain diamond films can be effectively used as wear-resistant, self-lubricating coatings not only in air and dry nitrogen, but also in ultrahigh vacuum. The wear mechanism of diamond films is that of small fragments chipping off the surface. The size of wear particles is related to the extent of wear rates.

Miyoshi, Kazuhisa↗

Friction and Wear Properties of As-Deposited and Carbon Ion-Implanted Diamond Films

Recent work on the friction and wear properties of as-deposited and carbon ion-implanted diamond films was reviewed. Diamond films were produced by the microwave plasma chemical vapor deposition (CVD) technique. Diamond films with various grain sizes and surface roughnesses were implanted with carbon ions at 60 keV ion energy, resulting in a dose of 1.2 x 10(exp 17) carbon ions per cm(exp 2). Various analytical techniques, including Raman spectroscopy, proton recoil analysis, Rutherford backscattering, transmission and scanning electron microscopy, X-ray photoelectron spectroscopy, and X-ray diffraction, were utilized to characterize the diamond films. Sliding friction experiments were conducted with a polished natural diamond pin in contact with diamond films in the three environments: humid air (40% relative humidity), dry nitrogen (less than 1 percent relative humidity), and ultrahigh vacuum (10(exp -7) Pa). The CVD diamond films indeed have friction and wear properties similar to those of natural diamond in the three environments. The as-deposited, fine-grain diamond films can be effectively used as self-lubricating, wear-resistant coatings that have low coefficients of friction (0.02 to 0.04) and low wear rates (10(exp -7) to lO(exp -8) mm(exp 3) N(exp -1) m(exp -1)) in both humid air and dry nitrogen. However, they have high coefficients of friction (1.5 to 1.7) and a high wear rate (10(exp -4) mm(exp 7) N(exp -1) m(exp -1)) in ultrahigh vacuum. The carbon ion implantation produced a thin surficial layer (less than 0.1 micron thick) of amorphous, non-diamond carbon on the diamond films. In humid air and dry nitrogen, the ion-implanted, fine and coarse-grain diamond films have a low coefficient of friction (around 0.1) and a low wear rate (10(exp -7) mm(exp 3) N(exp -1) m(exp-1)). Even in ultrahigh vacuum, the presence of the non-diamond carbon layer reduced the coefficient of friction of fine-grain diamond films to 0.1 or lower and the wear rate to 10(exp -6) mm(exp 3) N(exp -1) m(exp -1). Thus, the carbon ion-implanted, fine-grain diamond films can be effectively used as wear-resistant, self-lubricating coatings not only in air and dry nitrogen, but also in ultrahigh vacuum.

Miyoshi, Kazuhisa↗

Saltstone Paddles and Augers Materials of Construction Study

The Saltstone Production Facility (SPF) uses a 10-inch READCO continuous, co-rotating twin-screw mixer to mix the dry premix with the low-level radioactive waste (LLW) salt solution to produce fresh saltstone grout. The paddles and augers within the mixer degrade via erosion in the region where the salt solution is introduced into the mixer. After the paddles/augers erode to a point where the throughput impacts operations, the mixer is disassembled, the effected paddles/augers are replaced, and the mixer is reassembled. Saltstone Engineering indicated that this effort requires an approximately three-week outage. The objective of this task is to assess alternative materials of construction (MOCs) that will provide better erosion characteristics and decrease the frequency in which the paddles and augers need replacement. Previous Astralloy V studies looked only at Charpy Impact and Rockwell Hardness Testing. Each of these will be examined for different alloys as well as Miller Testing (abrasion to determine wear) which will provide a good assessment of an alloy’s erosion/wear characteristics. The following facts concerning the current and proposed alloys for Saltstone Paddles and Augers are provided in this report. • Current Astralloy V material and alloy E52100 had the most favorable Miller Testing Results. • Charpy Impact Testing did not correlate with Miller Testing Results. • Hardness Testing correlated with Miller Testing results meaning that higher hardness will provide more favorable wear resistance. • Further investigation of E52100 and various tool grade steels is recommended for achieving wear resistant properties.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Tribological Studies of Dynamic Thermal Seal Materials

Thermal seals are required on high-speed vehicles in many dynamic applications such as variable inlets in propulsion systems and control surfaces. These seals, often referred to as dynamic thermal seals, must not only mitigate inboard heat transfer, but must also exhibit sufficient durability when scrubbed against mating surfaces. For high-temperature high-speed vehicle applications, the mating surfaces are often made from thermal protection system (TPS) materials, which are typically rougher and more abrasive than TPS materials used at lower temperatures. The high-temperature TPS materials used can include non-ablative (e.g., lightweight porous oxides, ceramic matrix composites) andor ablative systems (e.g., phenolic systems). Due to the increased need for durable high-temperature dynamic seals, researchers working with the NASA Glenn Research Center embarked on an effort to (a) characterize the tribological performance of state-of-the-art thermal seal materials against a variety of TPS materials and (b) develop approaches for improved wear resistance. Tests were conducted using a recently upgraded high-temperature tribometer to assess wear resistance for a variety of tribopairs under multiple conditions. This data will begin to frame the challenges of using these materials and eventually permit an improved ability to design and implement these critical TPS components.

thermal protection↗

Sliding Wear and Fretting Wear of DLC-Based, Functionally Graded Nanocomposite Coatings

Improving the tribological functionality of diamondlike carbon (DLC) films--developing, good wear resistance, low friction, and high load-carrying capacity-was the aim of this investigation. Nanocomposite coatings consisting of an amorphous DLC (a-DLC) top layer and a functionally graded titanium-titanium carbon-diamondlike carbon (Ti-Ti(sub x) C(sub y)-DLC) underlayer were produced on AISI 440C stainless steel substrates by the hybrid technique of magnetron sputtering and pulsed-laser deposition. The resultant DLC films were characterized by Raman spectroscopy, scanning electron microscopy, and surface profilometry. Two types of wear experiment were conducted in this investioation: sliding friction experiments and fretting wear experiments. Unidirectional ball-on-disk sliding friction experiments were conducted to examine the wear behavior of an a-DLC/Ti-Ti(sub x) C(sub y)-DLC-coated AISI 440C stainless steel disk in sliding contact with a 6-mm-diameter AISI 440C stainless steel ball in ultrahigh vacuum, dry nitrogen, and humid air. Although the wear rates for both the coating and ball were low in all three environments, the humid air and dry nitrogen caused mild wear with burnishing, in the a-DLC top layer, and the ultrahigh vacuum caused relatively severe wear with brittle fracture in both the a-DLC top layer and the Ti-Ti(sub x) C(sub y)-DLC underlayer. For reference, amorphous hydrogenated carbon (H-DLC) films produced on a-DLC/Ti-Ti(sub x) C(sub y)-DLC nanocomposite coatings by using an ion beam were also examined in the same manner. The H-DLC films markedly reduced friction even in ultrahigh vacuum without sacrificing wear resistance. The H-DLC films behaved much like the a-DLC/Ti-Ti(sub x) C(sub y)-DLC nanocomposite coating in dry nitrogen and humid air, presenting low friction and low wear. Fretting wear experiments were conducted in humid air (approximately 50% relative humidity) at a frequency of 80 Hz and an amplitude of 75 micron on an a-DLC/Ti-Ti(sub x) C(sub y)-DLC-coated AISI 440C disk and on a titanium-6 wt % aluminum-4 wt% vanadium (Ti-6Al-4V) flat, both in contact with a 9.4-mm-diameter, hemispherical Ti-6Al-4V pin. The resistance to fretting wear and damage of the a-DLC/Ti-6Al-4V materials pair was superior to that of the Ti-6Al-4V/Ti-6AI-4V materials pair.

Miyoshi, K.↗