Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “WEAR”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Wear measurement of highly cross-linked UHMWPE using a 7 Be tracer implantation technique

The very low wear rates achieved with the current highly cross-linked ultra-high molecular weight polyethylenes (UHMWPE) used in joint prostheses have proven to be difficult to measure accurately by gravimetry. Tracer methods are therefore being explored. The purpose of this study was to effect a proof-of-concept on the use of the radioactive tracer beryllium-7 (7Be) for the determination of wear in a highly cross-linked orthopedic UHMWPE. Three crosslinked and four conventional UHMWPE pins made from compression-molded GUR 1050, were activated with 109 to 1010 7Be nuclei using a new implantation setup that produced a homogenous distribution of implanted nuclei up to 8.5 μm below the surface. The pins were tested for wear in a six-station pin-on-flat apparatus for up to 7.1 million cycles (178 km). A Germanium gamma detector was employed to determine activity loss of the UHMWPE pins at preset intervals during the wear test. The wear of the cross-linked UHMWPE pins was readily detected and estimated to be 17 ± 3 μg/Mc. The conventional-to-cross-linked ratio of the wear rates was 13.1 ± 0.8, in the expected range for these materials. It was estimated that implantation reduced the average wear rate by approximately 20%, and the oxidative degradation damage from implantation was negligible. Future applications of this tracer technology may include the analysis of location-specific wear, such as loss of material in the post or backside of a tibial insert.

Wimmer, Markus A.↗

Investigation of the Effect of Residual Stress Gradient on the Wear Behavior of PVD Thin Films

The control of residual stresses has been seldom investigated in multilayer coatings dedicated to improvement of wear behavior. Here, we report the preparation and characterization of superposed structures composed of Cr, CrN and CrAlN layers. Nano-multilayers CrN/CrAlN and Cr/CrN/CrAlN were deposited by Physical Vapor Deposition (PVD) onto Si (100) and AISI4140 steel substrates. The Cr, CrN and CrAlN monolayers were developed with an innovative approach in PVD coatings technologies corresponding to deposition with different residual stresses levels. Composition and wear tracks morphologies of the coatings were characterized by scanning electron microscopy, high-resolution transmission electron microscopy, atomic force microscopy, x-ray photoelectron spectroscopy, energy-dispersive x-ray spectroscopy, x-ray diffraction and 3D-surface analyzer. The mechanical properties (hardness, residual stresses and wear) were investigated by nanoindentation, interferometry and micro-tribometry (fretting-wear tests). Observations suggest that multilayer coatings are composed mostly of nanocrystalline. The residual stresses level in the films has practically affected all the physicochemical and mechanical properties as well as the wear behavior. Consequently, it is demonstrated that the coating containing moderate stresses has a better wear behavior compared to the coating developed with higher residual stresses. The friction contact between coated samples and alumina balls shows also a large variety of wear mechanisms. In particular, the abrasive wear of the coatings was a combination of plastic deformation, fine microcracking and microspallation. The application of these multilayers will be wood machining of green wood.

36 MATERIALS SCIENCE↗

Tribological Behavior and Wear Mechanism of TZ20 Titanium Alloy After Various Treatments

Abrasion is one of the most common failure forms of metals and alloys. The study of the friction and wear behavior of metals and alloys is greatly beneficial to improve their long life and safe service. The friction coefficient, weight loss, specific wear rate, and wear mechanism of Ti-20Zr-6.5Al-4V (TZ20) alloy after various treatments were investigated using a pin–disk-type wear apparatus at various normal loads. The wear results revealed that at a normal load, the friction coefficient steadily decreased, whereas the weight loss increased. By contrast, different specimens displayed distinct variation trends of specific wear rate with respect to the normal load. Further investigations indicated that the effects of hardness and toughness on the wear properties were markedly influenced by the normal load. The main characteristic of the abrasion surface gradually changed from grooves to plastic deformation as the normal load increased. The findings promote the practical application of TiZrAlV series alloys and expand wear theory.

36 MATERIALS SCIENCE↗

Grid-to-rod fretting wear study of SiC/SiC composite accident-tolerant fuel claddings using an autoclave fretting bench test

Grid-to-rod-fretting (GTRF) in pressurized water reactors (PWRs) is known to cause wear and surface damage on the fuel claddings, potentially leading to radioactive leakage. One of the accident-tolerant fuel (ATF) concepts is to use advanced cladding materials that could withstand higher temperatures. Here, we investigated the wear behavior of candidate silicon carbide (SiC)-based composite claddings with different levels of surface finish in fretting against a commercial ZIRLO alloy grid using a unique bench-scale autoclave GTRF rig. The experiments mimicked the environment in an industrial full-assembly PWR simulator. Fretting tests were conducted with a realistic load (~0.5 N) in deionized water under a pressure of 20–23 bar at 204 °C for 100 h. While the SiC/SiC composite claddings showed significantly higher wear resistance than the commercial ZIRLO alloy cladding as expected, the smoother versions experienced surprisingly higher wear than the much softer counterface, ZIRLO grid. The wear mechanism of the SiC/SiC cladding was attributed to the SiC wear debris that was trapped at the fretting interface causing both 3-body and 2-body (embedded into the grid surface) abrasion of the cladding. Rougher SiC/SiC claddings had less material loss but caused more wear on the ZIRLO grid. Finally, pre-oxidized ZIRLO grid showed better compatibility with the SiC/SiC cladding to protect both the cladding and grid as a result of reduced wear debris trapping.

36 MATERIALS SCIENCE↗

X-ray photoelectron spectroscopic study of surface chemistry of dibenzyl-disulfide on steel under mild and severe wear conditions

Wear tests were performed on 304 stainless steel lubricated with pure mineral oil with and without dibenzyl-disulfide. Both mild and severe wear were observed. The type of wear was distinguished by a marked change in wear rate, friction coefficient, and wear scar appearance. The chemical composition of the wear scar surface was examined with X-ray photoelectron spectroscopy in conjunction with argon ion sputter etching. In severe wear scars, a sulfide was formed at the expense of the normal oxide layer. In mild wear scars, there were only superficial sulfur compounds, but there was a substantial increase in the oxide thickness.

Wheeler, D. R.↗

Friction and Wear of Monolithic and Fiber Reinforced Silicon-Ceramics Sliding Against IN-718 Alloy at 25 to 800 C in Atmospheric Air at Ambient Pressure

The friction and wear of monolithic and fiber reinforced Si-ceramics sliding against the nickel base alloy IN-718 at 25 to 800 C was measured. The monolithic materials tested were silicon carbide (SiC), fused silica (SiO2), syalon, silicon nitride (Si3N4) with W and Mg additives, and Si3N4 with Y2O3 additive. At 25 C fused silica had the lowest friction while Si3N4 (W,Mg type) had the lowest wear. At 800 C syalon had the lowest friction while Si3N4 (W,Mg type) and syalon had the lowest wear. The SiC/IN-718 couple had the lowest total wear at 25 C. At 800 C the fused silica/IN-718 couple exhibited the least total wear. SiC fiber reinforced reaction bonded silicon nitride (RBSN) composite material with a porosity of 32 percent and a fiber content of 23 vol percent had a lower coefficient of friction and wear when sliding parallel to the fiber direction than in the perpendicular at 25 C. The coefficient of friction for the carbon fiber reinforced borosilicate composite was 0.18 at 25 C. This is the lowest of all the couples tested. Wear of this material was about two decades smaller than that of the monolithic fused silica. This illustrates the large improvement in tribological properties which can be achieved in ceramic materials by fiber reinforcement. At higher temperatures the oxidation products formed on the IN-718 alloy are transferred to the ceramic by sliding action and forms a thin, solid lubricant layer which decreases friction and wear for both the monolithic and fiber reinforced composites.

Deadmore, Daniel L.↗

Reciprocating sliding wear characteristics of copper-carbon fiber composites

The effect of fiber orientation and alloy composition on the reciprocating sliding wear behavior of Cu-C fiber composite was studied. The wear volume was smaller than that of Cu alloys. The wear volume increased with increasing sliding load and volume fraction of C fibers above 30 volume percent. The effectiveness of fiber orientation in decreasing the wear volume was the highest for random orientation, medium in the direction perpendicular to the fiber direction, and lowest in the fiber direction. The wear volume was decreased by the addition of Sn and Zr. However, the additions did not achieve isotropic wear characteristics of the composite. Isotropic wear was obtained by the addition of C powder. Isotropic and decreased composite wear were attained by adding Zr and C powder together.

Kuniya, Keiichi↗

Friction and Wear Properties of As-Deposited and Carbon Ion-Implanted Diamond Films

Recent work on the friction and wear properties of as-deposited and carbon ion-implanted diamond films was reviewed. Diamond films were produced by the microwave plasma chemical vapor deposition (CVD) technique. Diamond films with various grain sizes and surface roughnesses were implanted with carbon ions at 60 keV ion energy, resulting in a dose of 1.2 x 10(exp 17) carbon ions per cm(exp 2). Various analytical techniques, including Raman spectroscopy, proton recoil analysis, Rutherford backscattering, transmission and scanning electron microscopy, X-ray photoelectron spectroscopy, and X-ray diffraction, were utilized to characterize the diamond films. Sliding friction experiments were conducted with a polished natural diamond pin in contact with diamond films in the three environments: humid air (40% relative humidity), dry nitrogen (less than 1 percent relative humidity), and ultrahigh vacuum (10(exp -7) Pa). The CVD diamond films indeed have friction and wear properties similar to those of natural diamond in the three environments. The as-deposited, fine-grain diamond films can be effectively used as self-lubricating, wear-resistant coatings that have low coefficients of friction (0.02 to 0.04) and low wear rates (10(exp -7) to lO(exp -8) mm(exp 3) N(exp -1) m(exp -1)) in both humid air and dry nitrogen. However, they have high coefficients of friction (1.5 to 1.7) and a high wear rate (10(exp -4) mm(exp 7) N(exp -1) m(exp -1)) in ultrahigh vacuum. The carbon ion implantation produced a thin surficial layer (less than 0.1 micron thick) of amorphous, non-diamond carbon on the diamond films. In humid air and dry nitrogen, the ion-implanted, fine and coarse-grain diamond films have a low coefficient of friction (around 0.1) and a low wear rate (10(exp -7) mm(exp 3) N(exp -1) m(exp-1)). Even in ultrahigh vacuum, the presence of the non-diamond carbon layer reduced the coefficient of friction of fine-grain diamond films to 0.1 or lower and the wear rate to 10(exp -6) mm(exp 3) N(exp -1) m(exp -1). Thus, the carbon ion-implanted, fine-grain diamond films can be effectively used as wear-resistant, self-lubricating coatings not only in air and dry nitrogen, but also in ultrahigh vacuum.

Miyoshi, Kazuhisa↗

Friction and Wear Properties of Selected Solid Lubricating Films: Ion-Plated Lead Films - Part 2

To evaluate commercially developed dry solid film lubricants for aerospace bearing applications, an investigation was conducted to examine the friction and wear behavior of ion-plated lead films in sliding contact with 6-mm-diameter American Iron and Steel Institute (AISI) 440C stainless steel balls. Unidirectional sliding friction experiments were conducted with a load of 5.9 N (600 g), a mean Hertzian contact pressure of 0.79 GPa (maximum Hertzian contact pressure of 1.2 GPa), and a sliding velocity of 0.2 m/s. The experiments were conducted at room temperature in three environments: ultrahigh vacuum (vacuum pressure, 7 x 10(exp -7 Pa), humid air (relative humidity, approx. 20 percent), and dry nitrogen (relative humidity, less then 1 percent). The resultant films were characterized by scanning electron microscopy, energy-dispersive X-ray spectroscopy, and surface profilometry. Marked differences in the friction and wear of the ion-plated lead films investigated herein resulted from the environmental conditions. The main criteria for judging the performance of the ion-plated lead films were coefficient of friction and wear rate, which had to be less than 0.3 and on the order of 1(exp -6) cu mm/N.m or less, respectively. The ion-plated lead films met both criteria only in ultrahigh vacuum but failed in humid air and in dry nitrogen, where the coefficient of friction was higher than the criterion. Both the lead film wear rate and the ball wear rate met that criterion in all three environments. Adhesion and plastic deformation played important roles in the friction and wear of the ion-plated lead films in contact with 440C stainless steel balls in the three environments. All sliding involved adhesive transfer of materials: transfer of lead wear debris to the counterpart 440C stainless steel and transfer of 440C stainless steel wear debris to the counterpart lead.

Miyoshi, Kazuhisa↗

Carbon-Based Wear Coatings: Properties and Applications

The technical function of numerous engineering systems - such as vehicles, machines, and instruments - depends on the processes of motion and on the surface systems. Many processes in nature and technology depend on the motion and dynamic behavior of solids, liquids, and gases. Smart surface systems are essential because of the recent technological push toward higher speeds, loads, and operating temperatures; longer life; lighter weight and smaller size (including nanotechnology); and harsh environments in mechanical, mechatronic, and biomechanical systems. If proper attention is not given to surface systems, then vehicles, machines, instruments, and other technical systems could have short lives, consume excessive energy, experience breakdowns, result in liabilities, and fail to accomplish their missions. Surface systems strongly affect our national economy and our lifestyles. At the NASA Glenn Research Center, we believe that proper attention to surface systems, especially in education, research, and application, could lead to economic savings of between 1.3 and 1.6 percent of the gross domestic product. Wear coatings and surface systems continue to experience rapid growth as new coating and surface engineering technologies are discovered, more cost-effective coating and surface engineering solutions are developed, and marketers aggressively pursue, uncover, and exploit new applications for engineered surface systems in cutting tools and wear components. Wear coatings and smart surface systems have been used widely in industrial, consumer, automotive, aerospace, and biomedical applications. This presentation expresses the author's views of and insights into smart surface systems in wear coatings. A revolution is taking place in carbon science and technology. Diamond, an allotrope of carbon, joins graphite, fullerenes, and nanotubes as its major pure carbon structures. It has a unique combination of extreme properties: hardness and abrasion resistance; adhesion and friction; thermal conductivity; chemical and thermal inertness; corrosion and wear resistance; radiation resistance and biocompatibility; electronic, acoustic, and electrochemical characteristics; and environmental compatibility. These properties make diamond attractive for a wide range of diverse applications. In particular, chemical-vapor-deposited (CVD) diamond coatings offer a broad potential, since size and cost are not as limiting. The production of large, superhard diamond films or sheets at low cost make designer materials possible. This presentation is divided into two sections: properties and applications of hard coatings. The first section is concerned with the fundamental properties of the surfaces of CVD diamonds and related materials. The surface properties of hard coatings with favorable coefficients of friction (less than or equal to 0.1) and dimensional wear coefficients (less than or equal to 10(exp -6) cubic millimeters/N.m) in specific environments are discussed. The second section is devoted to applications. Examples of actual, successful applications and of potential challenging applications of the coatings.such as CVD diamond, diamondlike carbon, and cubic boron nitride-are described. Cutting tools coated with CVD diamond are of immediate commercial interest. Other applications, such as microelectromechanical systems (MEMS), valves, and bearings of CVD diamond, are being developed, but at a slow pace. There is a continually growing interest in commercializing diamondlike carbon for wear parts applications, such as biomedical parts and implants, forming dies, transport guides, magnetic tapes and disks, valves, and gears. Cubic boron nitride films are receiving attention because they can be used on tools to machine ferrous materials or on wear parts in sliding contact with ferrous materials.

Miyoshi, Kazuhisa↗

Optimizing Rate of Penetration and Tripping Decision-Making using Real-Time Bit Wear Monitoring While Drilling Geothermal Wells

Understanding bit wear while drilling is critical to minimizing non-productive time (NPT) and optimizing rate of penetration (ROP). Lengthening drilling runs with damaged bits does not only lower the ROP, but also elevates the risk of inducing severe bit damage, which could potentially lead to time-consuming fishing operations. When drillers believe the bit has worn off substantially, the bit is tripped out to be replaced. On geothermal wells, tripping can take up to 20% of the overall well construction time, and this is generally acknowledged as an opportunity for improvement. Ideally, a bit run should be terminated before the bit is damaged beyond repair. At the same time, premature bit pulls are to be avoided as well. This study aims to leverage bit and tooth wear metrics that can be obtained in real time to characterize bit condition in order to optimize ROP and determine the optimal time to pull the bit. Two metrics were explored in this study: a bit wear metric that incorporated depth-of-cut, and a tooth wear metric developed by Bourgoyne & Young characterizing the state of bit teeth dull. Both metrics were computed using recorded data from 12¼ inches roller cone insert bit runs in five geothermal wells targeting a granodiorite formation in the western United States. Together with the actual dull grades, determined after the bits were pulled to surface, the metric trends were interpreted to characterize the downhole bit condition and identify the point at which the bit should have optimally been tripped out. The insights from studying the actual dull grades and how they relate to the two metrics were used to establish a reliable bit pull criterion. The bit wear metric trend correctly showed a noticeable departure from baseline for bits experiencing major dulling behavior. Additionally, the tooth wear model predicted the cutter dull within two dull grades for most runs, with better performance in predicting the inner teeth dull. Moreover, the combination of the bit wear and tooth wear metrics was effective in revealing the cause of the bit performance impairment. Proactive tracking of these two metrics in real-time can facilitate geothermal drilling ROP optimization and better-informed tripping decision-making, thereby avoiding wasted time and cost.

Ashari, Rahmat↗

Fretting wear behaviors of a dual-cooled nuclear fuel rod under a simulated rod vibration

Recently, a dual-cooled fuel (i.e., annular fuel) that is compatible with current operating PWR plants has been proposed in order to realize both a considerable amount of power uprating and an increase of safety margins. As the design concept should be compatible with current operating PWR plants, however, it shows a narrow gap between the fuel rods when compared with current solid nuclear fuel arrays and needs to modify the spacer grid shapes and their positions. In this study, fretting wear tests have been performed to evaluate the wear resistance of a dual-cooled fuel by using a proposed spring and dimple of spacer grids that have a cantilever type and hemispherical shape, respectively. As a result, the wear volume of the spring specimen gradually increases as the contact condition is changed from a certain gap, just contact to positive force. However, in the dimple specimen, just contact condition shows a large wear volume. In addition, a circular rod motion at upper region of contact surface is gradually increased and its diametric size depends on the wear depth increase. Based on the test results, the fretting wear resistance of the proposed spring and dimple is analyzed by comparing the wear measurement results and rod motion in detail.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Wear of Spheroidal Graphite Cast Irons for Tractor Drive Train Components

The study was prompted by a desire to improve the wear resistance of power transmission components in rear axle drives on commercial farm tractors. Reciprocating wear tests were conducted under lubricated and non-lubricated conditions on three spheroidal cast irons which varied in strength and hardness (designated GGG450, GGG600, and GGG700). Hemispherically-tipped steel pins (designed 42CrMoS4/ 41CrS4) were used as the sliders. Except for the test duration, test procedures were similar to those described in ASTM Standard Test Method G133 for linearly-reciprocating sliding. Among the three cast irons tested, the harder and stronger the alloy, the lower was its wear rate. Wear factors were approximately four orders of magnitude lower for experiments lubricated in fresh, fully-formulated lubricating oil. There was a linear relationship between Brinell hardness of the alloys and the negative logarithm of the wear factors that were expressed in (mm3/N-m). Wear of lubricated test pins was not measurable due to the presence of deposits; however under non-lubricated sliding, the ratio of the wear of the flat specimen to that of the pin decreased as the hardness of the flat specimens approached that of the pin specimen.

24 POWER TRANSMISSION AND DISTRIBUTION↗

Characterization of Microstructure and Wear Resistance of PEO Coatings Containing Various Microparticles on Ti6Al4V Alloy

Titania-based composite coatings were prepared by plasma electrolytic oxidation (PEO) treatment of Ti6Al4V alloy in electrolyte with α-Al{sub 2}O{sub 3}, Cr{sub 2}O{sub 3} or h-BN microparticles in suspension. The microstructure, composition of PEO composite coatings were analyzed by SEM, EDS and XRD. The wear resistance of composite ceramic coatings was studied by ball-on-disk wear test at ambient temperature and 300 °C. The results showed that the addition of microparticles accelerated the growth rate of PEO coating and changed the microstructure and composition of PEO coating. PEO coating was porous and mainly composed of rutile-TiO{sub 2}, anatase-TiO{sub 2} and Al{sub 2}TiO{sub 5}. PEO/α-Al{sub 2}O{sub 3} (Cr{sub 2}O{sub 3} or h-BN) composite coating only had small micropores and appeared some α-Al{sub 2}O{sub 3} (Cr{sub 2}O{sub 3} or h-BN) phase. Besides, the addition of α-Al{sub 2}O{sub 3} (Cr{sub 2}O{sub 3} or h-BN) microparticles greatly improved the wear resistance of PEO coating. At ambient temperature, abrasive wear dominated the wear behavior of PEO coating, but abrasive wear and adhesive peel simultaneously happened at 300 °C. Whether at ambient temperature or 300 °C, PEO composite coating had better wear resistance than PEO coating. Besides, PEO/h-BN composite coating outperformed other composite coatings regardless of the temperature.

36 MATERIALS SCIENCE↗

Dry Sliding Wear Behavior of Hot-Dip Aluminized Ti-6Al-4V Alloy as a Function of Sliding Velocity

An aluminized coating was prepared on Ti-6Al-4V alloy by hot-dip aluminizing and subsequently diffusion treatment. Dry sliding wear tests were performed for the aluminized and uncoated Ti-6Al-4V alloy under the loads of 10-50 N at the sliding velocities of 0.5-4 m/s. The wear resistance of the titanium alloy was improved by the aluminized coating under various conditions, especially at 4 m/s. The improved wear performance was suggested to be attributed to the Ti-Al coating and tribo-oxide layer. Tribo-layers were identified to form on worn surfaces under various conditions but their influence on the wear behavior and mechanism was decided by the amount and kind of oxides. The outmost values of the microhardness distribution at subsurfaces as a function of load could be used to identify the property and stability of tribo-layers. At 4 m/s, oxide-containing tribo-layers (more TiO, TiO{sub 2} and trace Fe{sub 2}O{sub 3}) presented high hardness and stability, thus possessed an obvious wear-reduced function. Conversely at 2.68 m/s, no-oxide tribo-layers did not show the protection from wear because of their lower hardness and instability. The formation of tribo-layers under various sliding speeds was noticed to be a process including wear debris production, oxidation and accumulation and densification, even sintering.

36 MATERIALS SCIENCE↗

Cathodic Cage Plasma Pre-treatment of TiN-Coated AISI-304 Stainless Steel for Enhancement of Mechanical Strength and Wear Resistance

Although austenitic stainless steels (ASSs) are known for their superior corrosion resistance properties, the use of such materials in motion contact parts is limited due to their low wear resistance. Previous studies reveal that titanium nitride (TiN) coating of ASS significantly improves its hardness and surface morphology but not the wear resistance due to weak interfacing with the substrate. Since plasma nitriding is a flexible and multifunctional case-hardening process, an attempt was made to improve the wear resistance of TiN-coated AISI-304 stainless steel by subjecting it to pre-treatment by pulsed DC cathodic cage plasma nitriding (CCPN) in the abnormal glow region. The hardness of the TiN-coated steel samples (with and without CCPN pre-treatment) was measured using Vickers micro-hardness tester. This test revealed maximum hardness of 2284 HV after plasma treatment of TiN-coated steel. The untreated TiN-coated steel exhibited 10.6 times lower hardness than the plasma pre-treated TiN-coated steel (CCPN-TiN). XRD analysis of the untreated TiN-coated steel showed strong diffraction peaks of TiN (311) and (400) in the spectrum, whereas plasma pre-treated sample contained dominant peaks of TiN (111), (200) and (220). The ball-on-disk wear tester was used to investigate the wear behavior of the samples. Very small wear rate and friction coefficient were reported for CCPN-TiN-coated steel. The observed low wear rate was probably due to the development of a subsurface (i.e., nitrided surface) on TiN-coated steel during CCPN pre-treatment.

36 MATERIALS SCIENCE↗

Structure and Anticorrosion, Friction, and Wear Characteristics of Pure Diamond-Like Carbon (DLC), Cr-DLC, and Cr-H-DLC Films on AZ91D Mg Alloy

This study evaluated the protection against corrosion and wear afforded to AZ91D Mg alloy by coatings of hydrogen-free and low-Cr-doped hydrogenated diamond-like carbon (DLC) films. The microstructure and corrosion resistance were evaluated using scanning electron microscopy, atomic force microscopy, Raman spectroscopy, polarization curves, and neutral salt spraying tests. Wear tests were performed to investigate the friction and wear behaviors of the samples against 9Cr18 in humid air, deionized water, and 3.5 wt.% NaCl solution using a reciprocating sliding test in the ball-on-disk mode. The results showed that the more compact Cr-H-DLC film improved the corrosion resistance of the Mg alloy, whereas the Cr-DLC film accelerated the corrosion in the 3.5 wt.% NaCl solution. All Mg alloy samples coated with DLC films exhibited low coefficient of friction (COF) values and smaller wear volumes compared with those of bare substrate in air, water, or NaCl solution. The Cr-DLC film presented the lowest COF and wear rate in air, but the worst corrosion protection in air and NaCl solution, whereas the converse was found for the Cr-H-DLC film. Unfortunately, all coated samples showed limited protection ability because of pore defects in the films, high galvanic potential between the substrate and the buffer layer or film, and high electrical conductivity, which caused severe tribocorrosion of the Mg alloy during the wear tests in NaCl solution. The corrosion protection ability of DLC films is key to the wear resistance protection of Mg alloys in water or NaCl solution.

36 MATERIALS SCIENCE↗

Investigating grid-to-rod fretting wear of nuclear fuel claddings using a unique autoclave fretting rig

Fuel rods in a pressurized water nuclear reactor (PWR) experience coolant flow-induced relative motion against the grid support features, a phenomenon called grid-to-rod fretting (GTRF), which may cause progressive fretting wear damage. Wear-through of the cladding on fuel rods will leak the radioactive fuel into the coolant loop to significantly increase the radiation level in PWR primary loop and often trigger expensive Post Irradiation Examination. In this work, a unique autoclave fretting test rig was designed and fabricated to allow studying GTRF using actual cladding and grid materials. Water temperature was up to 220 °C, which was designed to mimic the environment in an industry full-assembly reactor core simulator. The contact load (0.1–1 N), oscillation frequency (20–30 Hz) and stroke (50–150 µm), and work rate (1–3 mW) were defined based on simulations of GTRF in an actual reactor. Using this autoclave GTRF rig, tests were conducted to learn the effect of water temperature and to investigate the wear behavior of different cladding-grid material combinations currently used in actual PWRs, including Zr alloy claddings without and with pre-oxidation against Zr alloy and Inconel grids. Higher water temperature evidently increased the cladding wear, and pre-oxidation of the Zr alloy and/or using the Inconel grid effectively reduced the wear rate. In conclusion, results were correlated with the data of a full-size industry reactor core simulator in terms of both wear rate and wear scar morphology.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗