Creep and Fatigue Characterization of High Strength Alloy Thin Sections in Advanced CO2 Heat Exchangers

The objective of this work was to characterize and model elevated temperature creep and fatigue behavior for thin sheet and foil forms of gamma-prime strengthened alloys in wrought form and as-processed folded and brazed constructions. This work was motivated by the demanding temperature and pressure service conditions of the GEN3 Concentrated Solar Power (CSP) and supercritical CO2 (sCO2) power cycle working fluid. More specifically, the possibility of leveraging the superior creep strength of gamma-prime alloys in folded-fin and brazed-plate heat exchanger constructions. Gamma-prime alloys represent a step-change in raw-material strength over solid-solution strengthened alloys. And the folded-fin and brazed-plate heat exchanger architecture is lightweight and leverages cost-effective material stock forms. The investigation contained two parallel paths. (1) The first is referred to as a fundamental investigation where Oak Ridge National Laboratory conducts uniaxial creep testing on thin sheet and foil in wrought form. This effort aimed to serve as a benchmark against a relatively sparse existing database and a baseline comparison for path number 2. (2) The second path is referred to as the practical investigation where Brayton Energy manufactures plate-fin heat exchangers and performs pressurized creep and fatigue testing. This effort aimed to de-risk heat exchanger manufacturing process for service under sCO2 CSP conditions. A total of 14 uniaxial creep tests were completed using Haynes 282 thin sheet and foil. A variety of heat treatments were specified to coincide with path number 2. Baseline metallography of test samples and creep strength performance are contained. Benchmarks relatively to existing thick-form Haynes 282 are made, as well as to other thin-form Nickel-based superalloys. Description of a wrought-form modeling approach for thin gamma-prime alloys is also discussed. A total of 11 pressurized creep and fatigue tests were completed successfully with Haynes 282 heat exchanger prototypes. Manufacturing processing details, testing details, testing results, and failure analysis are discussed. Additionally, creep modeling techniques to predict failure are discussed, and modeling to support technological-to-market. In conclusion, Haynes 282 foils were demonstrated to yield rupture two-to-three orders of magnitude higher than Haynes 230 foils under similar conditions. And the manufactured heat exchanger prototypes demonstrated strength similar to the wrought constituents. Both of which contribute to elevated performance potential or cost savings in practice. Discussion is included.

14 SOLAR ENERGY↗

Charges on a suspended silicon nitride membrane under a high-energy electron beam

Thin silicon nitride (SiN x ) membranes are widely used in gas and liquid phase transmission electron microscopy (TEM) and as phase plates to enhance imaging contrast. SiN x contains trap sites for both positive and negative charges, which can be manipulated by high-energy electron irradiation, external potential biasing, or light exposure. Charge accumulation on the membrane can significantly affect in situ TEM processes, including chemical and electrochemical reactions, nanoparticle dynamics, and catalytic activity, or introduce unwanted phase shifts when used as a phase plate. Here, in this study, charge accumulation on suspended SiN x membranes was investigated using off-axis electron holography combined with model-free charge analysis, supported by custom finite element analysis (FEA) simulations. An average residual positive charge density of approximately 2.8 × 10 −4 C m −2 was measured. Localized and stable regions of both positive and negative charges were identified on the membrane. The global positive and localized positive/negative charges give rise to strong electric fields and electroosmotic slip velocities at the membrane surface, which are sufficient to induce non-Brownian particle behavior and directional fluid flow, offering a physical explanation for previously observed anomalies in particle dynamics, nucleation, and growth during gas and liquid phase TEM experiments. These results provide a benchmark for understanding charge behavior at SiNx interfaces in gas and liquid phase TEM. Furthermore, the FEA simulations establish a framework for future investigations into charge distribution, electrostatic potentials, and electrical double layers at solid–liquid interfaces, particularly in complex geometries and chemically dynamic environments.

Suspended silicon↗

Element-specific first order reversal curves measured by magnetic transmission x-ray microscopy

The first-order reversal curve (FORC) method is a macroscopic measurement technique that can be used to extract quantitative and microscopic properties of hysteretic systems. Using magnetic transmission x-ray microscopy (MTXM), local element-specific FORC measurements are performed on a 20 nm thick film of CoTb. The FORCs measured with microscopy reveal a step-by-step domain evolution under the magnetic field cycling protocol and provide a direct visualization of the mechanistic interpretation of FORC diagrams. They are compared with magnetometry FORCs and show good quantitative agreement. Furthermore, the high spatial resolution and element-specific sensitivity of MTXM provide new capabilities to measure FORCs in small regions or specific phases within multicomponent systems, including buried layers in heterostructures. The ability to perform FORCs on very small features is demonstrated with the MTXM-FORC measurement of a rectangular microstructure with vortex-like Landau structures. This work demonstrates the confluence of two uniquely powerful techniques to achieve quantitative insight into nanoscale magnetic behavior.

36 MATERIALS SCIENCE↗

A critical review of the history of fabricating monolithic U-Mo fuel plates

The fabrication of monolithic uranium-molybdenum alloy fuels, specifically those developed for high-performance research and test reactors, began in the early 2000s. The primary fuel form consists of uranium alloyed with 10-wt% molybdenum in a thin foil coated with zirconium and encapsulated in aluminum-6061 cladding. Over the years, the process has evolved with different types of casting, heat treatments, rolling schedules, and cladding applications. This review examines the history of these fabrication processes and their impact on microstructure and fuel-swelling performance. Even though various fabrication methods were used, we found little correlation between fabrication variation and fuel swelling. This insensitive relationship between fabrication variation and fuel swelling is primarily due to inhomogeneous microstructures that formed during casting and grain refinement that occurred during rolling. We conclude that the fabrication processes we examined produced similar microstructures, indicating that the fuel microstructure is somewhat insensitive to the fabrication parameters evaluated. However, the relatively small amount of historic data, such as those for grain sizes, limited this analysis. More recently fabricated materials, such as those from ongoing irradiation experiment, Mini-Plate-1 and Mini-Plate-2, were also excluded from this analysis and are intended to be reviewed separately. The findings, that fuel microstructure is somewhat insensitive to the fabrication parameters, do not imply that any fabrication method is acceptable, given the uncertainties in data and fuel-swelling observations. For example, only arc melting and vacuum induction melting casting processes were previously explored in the historic fabrication efforts. In conclusion, the findings should not be extrapolated to other casting processes.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

An experimental and computational study of thin-layer Rayleigh–Taylor instability development during deceleration with and without an externally applied magnetic field

The importance of mitigating the Rayleigh–Taylor instability (RTI) in inertial confinement fusion (ICF) is critical to successfully achieve high gain fusion yield. Consequently, understanding the seed mechanisms of RTI and the potential evolution of RTI in ICF relevant conditions is crucial. Single feature perturbations consistently demonstrate non-linear RTI evolution, for which an experimental platform on OMEGA-EP is developed. Manufacturing defects introduced into the target design require exploration of unanticipated changes to RTI development and an identification of targets that will still render quantifiable physics results. Consequently, it is presented that the inherent 3D nature of experimental targets necessitates 3D modeling for accurate design work and predictive modeling of experimental targets, especially when high resolution imaging diagnostics, like Fresnel Zone Plates, are utilized. A study of the morphology of the RTI evolution due to changing initial conditions and the presence of an externally applied magnetic field are also explored. Experimental data show thin-layer RTI morphology comparable to resistive magneto hydrodynamic 3D results. A discussion on the impacts of an externally applied magnetic field makes the case for continued efforts to observe a magnetic field's impact on RTI morphology.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Controlled lithium stripping enables a stable interface for long-cycling anode-free solid-state batteries

Anode-free solid-state batteries (AFSSBs) are a promising route toward achieving high energy density. In these cells, the anode contains no pre-stored lithium (Li). Instead, the entire Li inventory originates from the cathode and is freshly deposited onto a bare current collector during charging. However, achieving uniform and defect-free Li plating on this bare current collector remains a major challenge, often resulting in low Li plating/stripping efficiency and rapid capacity decay. Here, for the first time, operando neutron imaging is employed to visualize Li plating/stripping behavior in an anode-free full cell with LiNi0.82Mn0.07Co0.11O2 (NMC) as the cathode. Operando measurements reveal that complete stripping of Li leaves isolated Li residues on the current collector, which degrades the interfacial contact between the current collector and the solid-state electrolyte. To mitigate this interfacial issue and promote more uniform Li deposition, we implement a discharge-cutoff-voltage strategy that intentionally retains a thin residual Li layer after stripping. This preserved Li-containing interfacial reservoir not only improves interfacial contact but also serves as an in situ formed seed layer that enables more homogeneous subsequent Li plating. As a result, the optimized anode-free cell with limited stripping depth exhibits excellent long-term cycling stability, maintaining a discharge capacity of 112.1 mAh g−1 with a capacity retention of 80.6% and an average coulombic efficiency of approximately 99.9% after 500 cycles at 0.25 C. In contrast, the cell with a conventional discharge cutoff voltage of 2.8 V exhibits rapid capacity decay, retaining only 59.7 mAh g−1 after 50 cycles with a capacity retention of 40.7%. This work demonstrates that limiting deep stripping to preserve a thin Li-containing interfacial layer can effectively improve the cycling stability of sulfide-based AFSSBs.

Wang, Jiwei [Northeastern University, Boston]↗

The passivity of lithium electrodes in liquid electrolytes for secondary batteries

Rechargeable Li metal batteries are currently limited by electrolyte decomposition and rapid Li consumption. Li plating and stripping greatly depend on the solid electrolyte interphase formed at the Li metal-liquid electrolyte interface. This Review discusses the reactions occurring at this interface from a corrosion science perspective, highlighting the requirements for an ideal passivation layer. Rechargeable Li metal batteries are currently limited by safety concerns, continuous electrolyte decomposition and rapid consumption of Li. These issues are mainly related to reactions occurring at the Li metal-liquid electrolyte interface. Additionally, the formation of a passivation film (that is, a solid electrolyte interphase) determines ionic diffusion and the structural and morphological evolution of the Li metal electrode upon cycling. In this Review, we discuss spontaneous and operation-induced reactions at the Li metal-electrolyte interface from a corrosion science perspective. We highlight that the instantaneous formation of a thin protective film of corrosion products at the Li surface, which acts as a barrier to further chemical reactions with the electrolyte, precedes film reformation, which occurs during subsequent electrochemical stripping and plating of Li during battery operation. Finally, we discuss solutions to overcoming remaining challenges of Li metal batteries related to Li surface science, electrolyte chemistry, cell engineering and the intrinsic instability of the Li metal-electrolyte interface.

25 ENERGY STORAGE↗

Effects of shielding gas and spot reduction on humping suppression in high-speed laser welding

High-speed laser welding is a crucial process to enhance the production rate of fuel cell fabrication. However, exceeding a critical welding speed leads to defect formation such as humps and root concavities, which degrade weld quality and mechanical performance. This study employed shielding gas and spot reduction approaches to suppress these defects. The relationships between individual defect types and their influence on weld strength were systematically examined. Moreover, in situ high-speed synchrotron X-ray imaging was employed to comprehend the mechanisms of humping mitigation by shielding gas through analysis of instantaneous keyhole and melt pool dynamics. The observations reveal that shielding gas mitigates humping by shortening the molten pool through enhanced surface heat convection and by altering surface tension to prevent melt flow collisions. The effects of shielding gas and spot reduction were further incorporated into the dimensionless humping index (π h ) that describes the humping formation tendency. These findings provide mechanistic insights and quantitative guidance for defect control strategies in high-speed laser welding.

08 HYDROGEN↗

HIGHER EFFICIENCY FISSION COUNTER FOR NEUTRON DETECTION

Fission chambers containing 235U have been used for detection of neutrons for many decades. In these chambers 235U is electroplated on a metal which is one plate of an ionization chamber. Since the range of fission products from induced fission in the chamber is extremely short, these deposits from electroplating are so thin that the amount of 235U results in low neutron detection efficiency and the chamber needs high internal 235U surface area to increase efficiency. A typical ~8 in. long, ~2 in. diameter fission counter only contains < 2 g of 235U total, resulting in very low detection efficiency per incident neutron impinging on the outer surface of the detector. However, because of their large electronic pulses from fission products compared to gamma rays it is very easy to discriminate against gamma rays impinging on the detector. These types of chambers are produced commercially and are used worldwide in nuclear research and nuclear power reactors. ORNL has made a higher efficiency fission ionization chamber by using many thin concentric annuli to increase the area. A higher efficiency fission counter would be useful and can be made by incorporating 235U into a glass or ceramic scintillator. For nearly 100 years the green color in antique glass was produced by incorporation of depleted uranium (up to 20 wt. %) into a glass. The concept for this scintillation-optical-based fission detector is to dope a scintillator (either ceramic or glass) with 235U. Glass scintillators are commercially available doped with as much as 8 wt. % 6Li for neutron detection. In the 235U doped scintillator the fission product pulses would be double the size of those in an ion chamber since all fission products produce light in the scintillator whereas in the ionization chamber half do not go into the ionizing gas volume. These higher efficiency fission chambers would be very useful for a wide variety of research, nuclear research, and nuclear power reactor applications. Because of their smaller size and weight, they should be useful for space application such as monitoring of space nuclear power reactors. This report reviews existing fission chamber technology and suggests the development of these small high-efficiency fission chambers. Other fission isotopes could be used for other research applications.

Mihalczo, John [ORNL] (ORCID:0000000254292681)↗

Combined, time-resolved, in situ neutron reflectometry and X-ray diffraction analysis of dynamic SEI formation during electrochemical N 2 reduction

One means of improving performance for electrochemical ammonia production through the Li-mediated N 2 reduction reaction (Li-NRR) is by cycling the current driving the reaction between open-circuit conditions and periods of applied current density. Herein, we have investigated the dynamics of the electrode–electrolyte interface under Li-NRR conditions during current cycling using in situ time-resolved neutron reflectometry and grazing-incidence synchrotron X-ray diffraction. During cycling, measured neutron reflectivity curves indicated bilayer formation in which Li-containing species such as LiOH, Li 2 O, and small quantities of Li 3 N and metallic Li primarily appeared in a thin layer at the cathode surface, above which formed a much larger, porous, ‘solid–electrolyte interface’ (SEI) layer. Upon return to open-circuit conditions, Li-containing species quickly moved out of the thin layer, leaving a compact, stable layer of decomposition products underneath the SEI layer. This SEI layer concomitantly filled with electrolyte or dissolved, becoming indistinguishable from the electrolyte via contrast in scattering-length density (SLD). During the second current cycle, Li-containing species again preferentially deposited directly atop the cathode, with the thick SEI-like layer again appearing within a minute. This SEI layer exhibited a lower SLD more quickly than in the first cycle, which might suggest that Li-containing species become distributed within the porous SEI layer. Furthermore, these time-resolved observations of SEI and plated layers during current cycling suggest that benefits associated with return to open-circuit conditions between periods of applied current density may be related to the concomitant loss of Li-containing species from a thin layer at the cathode surface into a porous SEI layer that becomes filled with electrolyte or dissolves.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Novel imaging technique for thermal neutrons using a fast optical camera

A novel imaging technique for thermal neutrons using a fast optical camera is presented. Thermal neutrons are reacted with 6 Lithium to produce a pair of 2.73 MeV tritium and 2.05 MeV alpha particles, which in turn interact in a thin layer of LYSO crystal scintillator to produce a localized flash of light. These photons are directed by a pair of lenses to a micro-channel plate intensifier, and its output is connected to the optical camera, TPX3CAM. The results from the camera are reconstructed through a custom algorithm. Various cutting parameters were found through data analysis to eliminate the background, and they were shown effective in matching the simulated rate of the neutron source. The system is fast with 40 ns decay time and allows free-space light collection, both vastly enhances flexibility of neutron detection.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Computational Modeling of Multi-Pass Rolling Parameters Effect on Resulting Fuel Foil Shape

A focus of the U.S. Department of Energy is to improve production yield and reduce the cost of Low Enriched Uranium (LEU)-molybdenum alloy (U-10Mo) monolithic fuel plates that will be replacing High Enriched Uranium (HEU) oxide dispersion fuels used currently in the United States High Performance Research Reactors (USHPRR). One area of improvement is lowering the high transverse waviness and longitudinal waviness currently present within rolled foils prior to cladding to produce fuel plates. Traditional rolling manufacturing techniques for other metal foils use winders to pull and straighten the foil as it is rolled back and forth to the final thickness. This approach cannot be used to roll thin U-10Mo foils (0.008-0.025” thick) because only small castings can be rolled due to nuclear criticality safety concerns. As a result, the fuel foils are too short (1 m in length) to use traditional winders. Therefore, it is crucial to identify other rolling parameters (i.e., roller friction, axial tension load, roller diameter, and roll pass reduction percent) that might reduce transverse waviness and longitudinal waviness in the rolled fuel foil and develop a high-yield, low-cost multi-pass rolling manufacturing process. This report documents a systematic finite element modeling study to investigate the effects of numerous rolling parameters to reduce resulting transverse waviness and longitudinal waviness in the fuel foil during multi-pass rolling of U-10Mo foils. The rolling of a U-10Mo plate with initial dimensions of 1”x1”x 0.048” is modeled using Abaqus CAE. This rolling is modeled to undergo eight 20% reduction roll passes to a final fuel foil thickness of 0.01”. The elastic-plastic constitutive model of the U-10Mo alloy was input to the fuel foil rolling model. The rollers were modeled as rigid bodies. A comparison of rolling friction coefficients of 0.3 and 0.7 over a wide range of applied axial tension loads were investigated in order to evaluate the effect of using a lubricant during rolling. The effect of roller diameter on the resulting transverse waviness and longitudinal waviness of the fuel foil over a wide range of axial tension loads were also investigated by modeling rollers 7/8” and 3.75” in diameter. The results of this systematic finite element method study will aid manufacturers in producing low transverse waviness and reduced longitudinal waviness in U-10Mo fuel foils.

U-10Mo, FEA, Rolling, Residual Stress, Fuel Foil↗

Unveiling mechanisms and onset threshold of humping in high-speed laser welding

The fabrication of fuel cells relies on a rapid laser welding process. However, challenges arise with the occurrence of humping when the welding speed surpasses a critical threshold, which poses difficulties in achieving a smooth surface finish and a consistent weld strength. This study aims to elucidate the humping mechanisms by analyzing the morphology of molten pool and the characteristics of melt flow at varying welding speeds via in situ synchrotron high-speed X-ray imaging and computational fluid dynamics simulations. Our findings indicate that the short keyhole rear wall, the high backward melt velocity, and the prolonged tail of molten pool are the primary factors contributing to the onset of humping. Furthermore, a dimensionless humping index (π h ) was introduced, which successfully captured the onset threshold of humping across different literatures. This index not only provides a quantitative description of the humping formation tendency but also serves as a valuable tool for optimizing the laser welding process.

42 ENGINEERING↗

High-rate heavy-ion tracking using MWPCs and PPACs with an Anti-Discharge Unit

This work reports on the development of two robust, heavy-ion beam tracking concepts operating at low pressure (< 15 Torr) for high rate applications (> 200 kHz). The first concept consists of a Multi-Wire Proportional Counter (MWPC) with a central anode consisting of 12 μm Au-plated Tungsten wires spaced 1 mm from each other. The anode grid is sandwiched between two segmented cathodes aligned orthogonally in the two dimensions for (x,y) particle localization. The second detector is a Parallel-Plate Avalanche Counter (PPAC) that uses the same readout geometry as the MWPC, but replaces the wire anode with a 150 nm silver layer deposited on both sides of a thin (< 1 mg/cm 2 ) polypropylene foil. Additionally, the bias circuitry for the PPAC anode central foil is equipped with an Anti-Discharge Unit (ADU) to prevent transitions from proportional operation to streamer formation, thereby avoiding damaging discharges. The localization capability of both detectors was tested with a low-rate alpha-particle source (241-Am). A position resolution of < 1 mm (FWHM) was achieved under stable, high-gas-gain (> 1000) operating conditions. Their performance in terms of detection efficiency as a function of the isotope charge (Z) was determined by irradiating the detectors with a cocktail beam (Z ≤ 15) with energy of ∼ 100 MeV/u. Full detection efficiency is maintained for all available fragments under optimal operational conditions (i.e., voltage bias). Full detection efficiency was achieved at rates above 200 kHz by irradiating the detectors with a 1 cm diameter 238 U beam at an energy of 143 MeV/u.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Highly Permeable Rubbery Thin Film Composite Membranes for CO2 Capture from Steel Mills

This presentation will report the rational design and fabrication of NETL’s highly permeable non-aging thin film composite (TFC) membranes for CO2 capture from various industrial point sources. This talk will also cover the design, computational fluid dynamic simulation, 3D printing, and permeation testing of plate-and-frame membrane modules for an upcoming field demonstration at U. S. Steel’s Edgar Thomson Plant in Braddock, PA. The field test will demonstrate membrane-based CO2 capture from a blast furnace for decarbonization of steel manufacturing for the first time in the U.S. A mobile gas permeation test unit is currently under design and construction for the field test, which is scheduled to take place in 2025.

Zhu, Lingxiang↗

Metallurgical Analysis of the High Flux Isotope Reactor (HFIR) Carrier Lifting Bails (Rev.1)

The dissolution rates of the aluminum alloys in the High Flux Isotope Reactor (HFIR) element carriers and the Material Test Reactor (MTR) L-bundles in the H-Canyon facility have been identified as the possible cause of extended dissolutions that result in significant time and financial expenditures. A study, carried out by Savannah River National Laboratory (SRNL) to determine relationships between the dissolution rates and the metallurgical properties of the aluminum alloy materials of construction of the HFIR carriers and the L-bundles, considered the dissolution rates of aluminum alloy (AA) series 1100, 6061, and 6063. The study determined that the aluminum alloy compositions played a principal role in the dissolution rate of the carrier/bundle components. Higher dissolution rates were correlated with lower concentrations of the minor element additions in the alloys and with specific element concentrations. Aluminum alloys 1100 and 6063 were found to have similar dissolution rates that were approximately two orders of magnitude (100X) greater than those of AA6061. Based on the results of the dissolution behavior study, a Technical Assistance Request (TAR) was first issued to determine if the replacement of AA6061-T6 with AA6063-T6 is feasible for the HFIR carrier lifting bails. A Technical Task Request was then issued to consider AA6063-T5 as well as other alloys to improve possible supply chain issues. The metallurgical properties of the L-bundle (specifically the end caps) were not evaluated in this report because L-Bundle drawings already allow for the use of AA6063-T6 in all structural components. The HFIR carriers are composed of thin-walled components with significant surface areas that allow for relatively quick overall dissolution times. Conversely, the carrier lifting bails and the supporting constituents are composed of solid bars and thick plate regions with relatively small surface areas that experience longer overall dissolution times. While the MTR L-bundle design includes allowances for the materials of construction to be either AA6061-T6 or AA6063-T6, the HFIR carriers are specified to be constructed fully with AA6061-T6 alloy. This report analyzes the recommendations of the dissolution behavior study to replace the materials of construction of the HFIR carrier lifting bails. The analysis considers the operational requirements of the lifting bail and its supporting structures. To decrease dissolution times, the analysis considers direct replacement of the material as well as reductions in the thicknesses of the components to decrease the mass of the elements. Material reductions are considered on options for using either AA6061 and/or AA6063. The calculations are based on specifications from the American Society of Mechanical Engineer (ASME) and The Aluminum Association, Inc. design codes. The analysis finds that direct replacement of the lifting bail material of construction with AA6063-T6, and AA6063-T5 as well as reductions in the dimensions of the lifting bail components are acceptable. Note that this study considers the structural suitability of the alloys. It does not consider their dissolution rates in the dissolvers.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Laser Shock Modeling Archival Discussion

The purpose of this discussion is to provide archival information related to the Laser Shock finite element modeling effort. As discussed in Laser Shock System, Assessing bond strength in layered materials (see Section 8.0), the Laser Shock System creates a high-amplitude shockwave on the frontside of a structure (i.e. an aluminum 6061-T6 plate for this discussion) via a high-energy pulsed laser. The shock wave is monitored on the back surface of the structure as a velocity time history. It is a compressive wave as it comes to the back surface but reflects as a tensile wave. If a bond exists in the structure and the reflected tensile wave exceeds its interface threshold stress, then bond rupture occurs. The desire of the Laser Shock effort is to establish (with multiple tests) an ultimate bond strength which can be used for fuel plate design calculations. In this process, the finite element modeling effort is the catalyst to mimic the Laser Shock tests and provide the damage information at the bond that is useful for fuel plate design calculations.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microjet printing of metal salt or oxide targets for nuclear reaction studies on radionuclides

Radioactive targets for direct measurements of neutron-induced reactions are required to improve evaluated cross-section data and, ultimately, the fidelity of neutron reaction network simulations. Electrodeposition and molecular plating are the current state-of-the-art radioactive target production techniques, but not all metals can be electrodeposited or molecular plated with high yields. Alternative techniques can be expensive or may produce targets that are unsatisfactory in terms of thickness, yield, or purity. Microjet printing is a new, rather inexpensive technique that utilizes equipment with a small footprint and has the potential to produce thin, highly radioactive targets with good uniformity and minimal impurities from the target fabrication process. This study involved optimizing the process of producing microjet printed targets to allow for the fabrication of a stable vanadium(V) oxide (V 2 O 5 ) target that was compared with an analogous electrodeposition V 2 O 5 target manufactured via the application of a vanadium chemical conversion coating on aluminum (Al) foil. Finally, the results from these studies suggest microjet printing could be used to produce relatively uniform target layers with adequate film thicknesses (< 15 μm). V 2 O 5 microjet printed targets, when compared with chemical conversion coating V 2 O 5 targets, appeared to be qualitatively less uniform and quantitatively larger in thickness (11.7(27) μm vs. 5.3(18) μm). However, the conversion coating target contained more impurities and the Al backing had a higher background contribution to measurements of neutron-induced reactions as opposed to targets produced via microjet printing. Overall, the results from this study suggest microjet printing has the capability to be an excellent alternative target production technique to the electrodeposition and molecular plating methods.