Garnet-Type Solid-State Electrolytes: Materials, Interfaces, and Batteries

Solid-state batteries with desirable advantages, including high-energy density, wide temperature tolerance, and fewer safety-concerns, have been considered as a promising energy storage technology to replace organic liquid electrolyte-dominated Li-ion batteries. Solid-state electrolytes (SSEs) as the most vital component in solid-state batteries largely lead the future battery development. Among different types of solid-state electrolytes, garnet-type Li 7 La 3 Zr 2 O 12 (LLZO) solid-state electrolytes have particularly high ionic conductivity (10 –3 to 10 –4 S/cm) and good chemical stability against Li metal, offering a great opportunity for solid-state Li-metal batteries. Since the discovery of garnet-type LLZO in 2007, there has been an increasing interest in the development of garnet-type solid-state electrolytes and all solid-state batteries. Garnet-type electrolyte has been considered one of the most promising and important solid-state electrolytes for batteries with potential benefits in energy density, electrochemical stability, high temperature stability, and safety. In this Review, we will survey recent development of garnet-type LLZO electrolytes with discussions of experimental studies and theoretical results in parallel, LLZO electrolyte synthesis strategies and modifications, stability of garnet solid electrolytes/electrodes, emerging nanostructure designs, degradation mechanisms and mitigations, and battery architectures and integrations. We will also provide a target-oriented research overview of garnet-type LLZO electrolyte and its application in various types of solid-state battery concepts (e.g., Li-ion, Li–S, and Li–air), and we will demonstrate opportunities and perspectives as guides for future development of solid electrolytes and solid-state batteries.

25 ENERGY STORAGE↗

In Situ Formation of Li 3 P Layer Enables Fast Li + Conduction across Li/Solid Polymer Electrolyte Interface

Abstract Solid‐state polymer electrolytes provide better flexibility and electrode contact than their ceramic counterparts, making them a worthwhile pursuit for all‐solid‐state lithium‐metal batteries. However, their large Li/solid state electrolyte interfacial resistance, small critical current density, and rapid lithium dendrite growth during cycling still limit their viability. Owing to these restrictions, all‐solid‐state cells with solid polymer electrolytes must be cycled above room‐temperature and with a small current density. These problems can be mitigated with an in situ formed artificial solid electrolyte interphase that rapidly conducts Li + ions. Herein, a Li 3 P layer formed in situ at the Li‐metal/solid polymer electrolyte interphase is reported that significantly reduces the electrode/electrolyte interfacial resistance. Additionally, this layer increases the wettability of the solid polymer by the metallic lithium anode, allowing for the critical current density of lithium symmetric cells to be doubled by homogenizing the current density at the interface. All‐solid‐state Li/Li symmetric cells and Li/LiFePO 4 cells with the Li 3 P layer show improved cycling performance with a high current density.

Wu, Nan↗

Improved electrochemical and thermal performances of layered Li[Li 0.2 Ni 0.17 Co 0.07 Mn 0.56 ]O 2 via Li 2 ZrO 3 surface modification

We successfully coated a conductive Li 2 ZrO 3 layer on the surface of Li-rich layered cathode Li[Li 0.2 Ni 0.17 Co 0.07 Mn 0.56 ]O 2 in order to enhance its electrochemical performances. For the crystal structures, electrochemical properties and thermal stabilities of the bare and coated materials are studied by X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), high resolution transmission electron microscopy (HRTEM), electron diffraction spectroscopy (EDS), inductively coupled plasma (ICP), galvanostatic cycling, cyclic voltammetry (CV), electrochemical impedance spectroscopy (EIS), Fourier transform infrared spectroscopy (FTIR) and differential scanning calorimetry (DSC). We found that the electrochemical performances of Li-rich cathode material are obviously improved by Li 2 ZrO 3 surface modification. Especially, the 1 wt.% Li 2 ZrO 3 -coated material demonstrates the best cycling performance, with capacity retention of 89% after 50 cycles, much better than that of the pristine one, 64%. Intensive explorations indicate that the improved electrochemical properties can be attributed to the Li 2 ZrO 3 surface layer, which not only stabilizes the cathode structure by decreasing the loss of oxygen, but also protects the Li-rich cathode material from side reaction(s) with the electrolyte and thus suppressing the fast growth of solid electrolyte interface (SEI) film on the surface of oxide particles.

25 ENERGY STORAGE↗

Design principles for self-forming interfaces enabling stable lithium-metal anodes

Significance It is possible to nearly double the energy density of existing lithium-ion batteries by using lithium metal anodes. However, it has been known for decades that the lithium dendrites and mossy lithium formed during charging (electrodeposition) limit the cycle life of the batteries. It is important to change the growth behavior of lithium metal, which is closely related to the properties of the solid–electrolyte interface (SEI) formed via spontaneous reactions between the lithium metal and the electrolyte. In this experimental-modeling integrated study, we reveal the design principles of the SEI that facilitates the dendrite-free and dense deposition of lithium and demonstrate one of the best cycling performances of lithium metal anode to date under practically relevant conditions.

25 ENERGY STORAGE↗

Role of Solution Structure in Solid Electrolyte Interphase Formation on Graphite with LiPF 6 in Propylene Carbonate

An investigation of the interrelationship of cycling performance, solution structure, and electrode surface film structure has been conducted for electrolytes composed of different concentrations of LiPF6 in propylene carbonate (PC) with a binderfree (BF) graphite electrode. Varying the concentration of LiPF6 changes the solution structure, altering the predominant mechanism of electrolyte reduction at the electrode interface. The change in mechanism results in a change in the structure of the solid electrolyte interface (SEI) and the reversible cycling of the cell. At low concentrations of LiPF6 in PC (1.2 M), electrochemical cycling and cyclic voltammetry (CV) of BF graphite electrodes reveal continuous electrolyte reduction and no lithiation/delithiation of the graphite. The solution structure is dominated by solvent-separated ion pairs (Li+(PC)4// PF6 -), and the primary reduction product of the electrolyte is lithium propylene dicarbonate (LPDC). At high concentrations of LiPF6 in PC (3.0-3.5 M), electrochemical cycling and CV reveal reversible lithiation/delithiation of the graphite electrode. The solution structure is dominated by contact ion pairs (Li+(PC)3PF6 -), and the primary reduction product of the electrolyte is LiF.

36 MATERIALS SCIENCE↗

Superoxide (Electro)Chemistry on Well-Defined Surfaces in Organic Environments

Efficient chemical transformations in energy conversion and storage systems depend on understanding superoxide anion (O 2 – ) electrochemistry at atomic and molecular levels. Here, in this work, a combination of experimental and theoretical techniques are used for rationalizing, and ultimately understanding, the complexity of superoxide anion (electro)chemistry in organic environments. By exploring the O 2 + e – ↔ O 2 – reaction on well-characterized metal single crystals (Au, Pt, Ir), Pt single crystal modified with a single layer of graphene (Graphene@Pt(111)), and glassy carbon (GC) in 1,2 dimethoxyethane (DME) electrolytes, we demonstrate that (i) the reaction is an outer-sphere process; (ii) the reaction product O 2 – can “attack” any part of the DME molecule, i.e., the C–O bond via nucleophilic reaction and the C–H bond via radical hydrogen abstraction; (iii) the adsorption of carbon-based decomposition products and the extent of formation of a “solid electrolyte interface” (“SEI”) increases in the same order as the reactivity of the substrate, i.e., Pt(hkl)/Ir(hkl) » Au(hkl)/GC > Gaphene@Pt(111); and (iv) the formation of the “SEI” layer leads to irreversible superoxide electrochemistry on Pt(hkl) and Ir(hkl) surfaces. In conclusion, we believe this fundamental insight provides a pathway for the rational design of stable organic solvents that are urgently needed for the development of a new generation of reliable and affordable battery systems.

25 ENERGY STORAGE↗

Understanding the Role of SEI Layer in Low-Temperature Performance of Lithium-Ion Batteries

Low-temperature electrolytes (LTEs) have been considered as one of the most challenging aspects for the wide adoption of lithium-ion batteries (LIBs) since the SOA electrolytes cannot sufficiently support the redox reactions at LT resulting in dramatic performance degradation. Although many attempts have been taken by employing various noncarbonate solvent electrolytes, there was a lack of fundamental understanding of the limiting factors for low-temperature operations (e.g., -20 to -40 degrees C). Here, the crucial role of the solid-electrolyte-interface (SEI) in LIB performance at low temperature using a butyronitrile (BN)-based electrolyte was demonstrated. These results suggested that an additive formed SEI with low resistance and low charge transfer dictates the LT performance in terms of capacity and cycle life, presenting a useful guideline in designing new electrolytes to address the LT issue.

25 ENERGY STORAGE↗

Understanding the Origin of the Ultrahigh Rate Performance of a SiO 2 -Modified LiNi 0.5 Mn 1.5 O 4 Cathode for Lithium-Ion Batteries

LiNi 0.5 Mn 1.5 O 4 (LNMO) is one of the most promising cathode materials for next-generation lithium-ion batteries for rapid charging-discharge applications. The surfaces of LNMO samples are coated with different amounts (0.5-2.0 wt. %) of silica (SiO 2 ) using a cost-effective and scalable ball milling process, and the surface-modified samples showing excellent electrochemical stability with conventional liquid electrolyte. The advantage of this coating is clearly demonstrated by the improved electrochemical performance at ambient and elevated temperatures (25 °C and 55 °C) using half- and full-cell configurations. The solid electrolyte interface (SEI) and coating properties have been highlighted by Ex situ TEM analysis, which indicates the close attachment and good wetting of the SiO 2 layer with the LNMO active particles. Importantly, the 1 wt. % SiO 2 -coated material cycled at 10 C, 40 C and 80 C rates for 400 cycles and excellent cycling stability with capacity retentions of 96.7, 87.9 and 82.4 %, respectively. The 1 wt. % SiO 2 -coated material also shows excellent cycling stability when charged at 6C (10 min.) and discharged at C /3 for 500 cycles. Here, the interfacial resistances of the SiO 2 -coated LiNi 0.5 Mn 1.5 O 4 is found to be much lower compared to bare material and does not considerably increase with the amount of coating. Overall, the scalable and cost-effective strategy of SiO 2 coating applied to LiNi 0.5 Mn 1.5 O 4 lowers the interfacial charge transfer resistance and enables the materials to be suitable for extremely fast-charging electric vehicle battery applications.

25 ENERGY STORAGE↗

Atomistic Modeling of the Electrode–Electrolyte Interface in Li-Ion Energy Storage Systems: Electrolyte Structuring

The solid electrolyte interface (SEI) forms as a result of side reactions between the electrolyte and electrode surfaces in Li-ion batteries and can adversely impact performance by impeding Li-ion transport and diminishing the storage capacity of the battery. To gain a detailed understanding of the impact of the SEI on electrolyte structure, atomistic molecular dynamics simulations of the electrode/electrolyte interface were performed in the presence and absence of the SEI under applied voltages. The composition of the SEI was guided by a wealth of data from experiments and allowed to vary across the simulations. A novel computational approach was implemented that showed significant computational speedup compared to fully polarizable electrode simulations, yet, retained the correct qualitative physics for the electrolyte. A force-matching algorithm was used to construct a new force field for the pure electrolyte, LiPF6 in ethylene carbonate, which was developed from ab initio molecular dynamics simulations. The electrode/electrolyte interface was included using a simple, physically motivated model, which includes the polarization of the conducting graphitic electrode by the electrolyte and the application of an external voltage. Changes in the structure of the electrolyte at the interface as a function of applied voltage, the thickness of the SEI layer, and composition of the SEI provide molecular level insight into the species present at these interfaces and potential clues to the effect of the SEI on transport. It is noted that, with increasing SEI thickness and LiF content, lithium ions are drawn closer to the SEI surface, which implies that these interfaces favor desolvation and promote more rapid lithium transport.

Jorn, Ryan↗

Delineating the Roles of Mn, Al, and Co by Comparing Three Layered Oxide Cathodes with the Same Nickel Content of 70% for Lithium-Ion Batteries

High-nickel layered oxides continue to prevail in the energy storage market as the frontmost cathode candidates for next-generation lithium-ion batteries. Demand and development of LiNi 1–x–y Mn x Co y O 2 (NMC) and LiNi 1–x–y Co x Al y O 2 (NCA) cathodes are rampantly increasing, particularly for the electric vehicle (EV) industry. However, the continued presence of cobalt in NMC and NCA cathodes raises global concerns due to geopolitical and ethical issues attributed to Co sourcing. We herein introduce a novel cobalt-free, high-nickel cathode LiNi 0.7 Mn 0.25 Al 0.05 O 2 (NMA70) and benchmark it against Co-containing LiNi 0.7 Mn 0.15 Co 0.15 O 2 (NMC70) as well as Co- and Al-free LiNi 0.7 Mn 0.3 O 2 (NM70) cathodes with equivalent 70% Ni contents that are all synthesized in-house. NMA70 displays a high initial C/10 capacity of 210 mA h g –1 , matching that of NMC70 in half cells with a cutoff voltage of 4.5 V. NMA70 also exhibits an impressive high-voltage full cell cycling performance with a cutoff voltage of 4.4 V with a nearly identical capacity retention of 83% compared to that of 82% for NMC70 after 300 cycles. Postmortem X-ray photoelectron spectroscopy (XPS), high-angle annular dark-field scanning transmission electron microscopy (HAADF-STEM), and electron energy loss spectroscopy (EELS) analyses indicate a thinner cathode–electrolyte interface (CEI) developed in NMA70 compared to that in NM70 and unveil a more robust solid-electrolyte interface (SEI) passivation on the graphite anode among all samples. The benefits of Al doping are additionally highlighted with enhanced high-voltage CEI and thermal stabilities in NMA70. Furthermore, this work assesses the roles of Mn, Al, and Co to demonstrate both the practicality and feasibility of synthesizing cobalt-free, high-nickel cathodes that are promising alternatives to current NMC- and NCA-based cathodes.

25 ENERGY STORAGE↗

Interface potentials inside solid-state batteries: Origins and implications

Interface resistance has become a significant bottleneck for solid-state batteries (SSBs). Most studies of interface resistance have focused on extrinsic mechanisms such as interface reactions and imperfect contact between electrodes and solid electrolytes. Interface potentials are an important intrinsic mechanism that is often ignored. Here, we highlight Kelvin probe force microscopy (KPFM) as a tool to image the local potential at interfaces inside SSBs, examining the existing literature and discussing challenges in interpretation. Drawing analogies with electron transport in metal/semiconductor interfaces, we showcase a formalism that predicts intrinsic ionic resistance based on the properties of the contacting phases, and we emphasize that future battery designs should start from material pairs with low intrinsic resistance. Here, we conclude by outlining future directions in the study of interface potentials through both theory and experiment.

25 ENERGY STORAGE↗

Thermally Driven Interfacial Degradation between Li 7 La 3 Zr 2 O 12 Electrolyte and LiNi 0.6 Mn 0.2 Co 0.2 O 2 Cathode

Solid-state batteries offer higher energy density and enhanced safety compared to the present lithium-ion batteries using liquid electrolytes. A challenge to implement them is the high resistances, especially at the solid electrolyte interface with the cathode. Sintering at elevated temperature is needed in order to get good contact between the ceramic solid electrolyte and oxide cathodes and thus to reduce contact resistances. Many solid electrolyte and cathode materials react to form secondary phases. It is necessary to find out which phases arise as a result of interface sintering and evaluate their effect on electrochemical properties. Herein, we assessed the interfacial reactions between LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) and Li 7 La 3 Zr 2 O 12 (LLZO) as a function of temperature in air. We prepared model systems by depositing thin-film NMC622 cathode layers on LLZO pellets. The thin-film cathode approach enabled us to use interface-sensitive techniques such as X-ray absorption spectroscopy in the near-edge as well as the extended regimes and identify the onset of detrimental reactions. We found that the Ni and Co chemical environments change already at moderate temperatures, on-setting from 500 °C and becoming especially prominent at 700 °C. By analyzing spectroscopy results along with X-ray diffraction, we identified Li 2 CO 3 , La 2 Zr 2 O 7 , and La(Ni,Co)O 3 as the secondary phases that formed at 700 °C. The interfacial resistance for Li transfer, measured by electrochemical impedance spectroscopy, increases significantly upon the onset and evolution of the detected interface chemistry. Our findings suggest that limiting the bonding temperature and avoiding CO 2 in the sintering environment can help to remedy the interfacial degradation.

36 MATERIALS SCIENCE↗

Avoiding CO 2 Improves Thermal Stability at the Interface of Li 7 La 3 Zr 2 O 12 Electrolyte with Layered Oxide Cathodes

Abstract Solid‐state batteries promise higher energy densities and better safety than Li‐ion batteries with liquid electrolytes. However, the interface between solid electrolyte and cathode is unstable at the elevated temperatures that are needed while sintering to achieve good bonding between ceramic components. Here, the hypothesis is that, the gas environment, especially the presence of CO 2, is critical in determining the stability of the solid electrolyte–cathode interface. The effect of gas species on the interface is systematically probed, by a using Li 7 La 3 Zr 2 O 12 (LLZO) solid electrolyte with a thin film LiNi 0.6 Mn 0.2 Co 0.2 O 2 cathode as a model system to enable interface sensitivity. Detrimental phases formed at the interface and their onset conditions are identified by X‐ray absorption spectroscopy, X‐ray diffraction, and Gibbs free energy analysis. As a result, removing CO 2 and minimizing H 2 O(g) during sintering is necessary to obtain good contact at the LLZO|cathode interface without forming secondary phases. Sintering in O 2 is ideal, yielding excellent chemical stability and low interfacial resistance. Secondary phases also do not form in N 2, but oxygen loss occurs at elevated temperatures. The interfacial resistance obtained upon sintering in pure O 2 is comparable to the lowest values at LLZO interfaces with protective coatings, but here without the need for interface coatings.

25 ENERGY STORAGE↗

Multidimensional visualization of the dynamic evolution of Li metal via in situ/operando methods

The growing demands for high-energy density electrical energy storage devices stimulate the coupling of conversion-type cathodes and lithium (Li) metal anodes. While promising, the use of these “Li-free” cathodes brings new challenges to the Li anode interface, as Li needs to be dissolved first during cell operation. In this study, we have achieved a direct visualization and comprehensive analysis of the dynamic evolution of the Li interface. The critical metrics of the interfacial resistance, Li growth, and solid electrolyte interface (SEI) distribution during the initial dissolution/deposition processes were systematically investigated by employing multidimensional analysis methods. They include three-electrode impedance tests, in situ atomic force microscopy, scanning electrochemical microscopy, and cryogenic scanning transmission electron microscopy. The high-resolution imaging and real-time observations show that a loose, diffuse, and unevenly distributed SEI is formed during the initial dissolution process. This leads to the dramatically fast growth of Li during the subsequent deposition, deviating from Fick’s law, which exacerbates the interfacial impedance. The compactness of the interfacial structure and enrichment of electrolyte species at the surface during the initial deposition play critical roles in the long-term stability of Li anodes, as revealed by operando confocal Raman spectroscopic mapping. In conclusion, our observations relate to ion transfer, morphological and structural evolution, and Li (de)solvation at Li interfaces, revealing the underlying pathways influenced by the initial dissolution process, which promotes a reconsideration of anode investigations and effective protection strategies.

25 ENERGY STORAGE↗

The Effect of Artificial SEIs on Lithium Metal Anode Morphology and Conductivity

Lithium metal has often been termed the “holy grail” of battery technology, due to its high capacity (2,061 mAh/cm3) and low electrochemical potential (-3.04 V vs. SHE). However, lithium’s beneficially low potential also causes it to be highly reactive in the presence of organic solvents, making it difficult to harness the high energy capabilities for rechargeable batteries. Common failure of lithium metal batteries occurs by rapid dendrite growth leading to a hazardous short-circuit. Various methods have been brought forth to better understand the fundamental mechanisms of lithium metal batteries, as well as modifications made to better stabilize lithium metal. A common route of modification is done through interface engineering, with attempts to artificially provide a stable, homogeneous solid-electrolyte interface (SEI). The stability of the SEI has direct effects on the heterogeneity of the electrode surface, which initiates a waterfall effect of for progressive reactions such as dendrite growth, dead lithium accumulation, and electrolyte consumption. This work aims to produce a mixed LiI-LiF artificial SEI to improve ionic conductivity while retaining a high elastic modulus.

25 ENERGY STORAGE↗

MATERIALS AND INTERFACIAL ENGINEERING FOR HIGH- PERFORMANCE ALL-SOLID-STATE BATTERIES

Developing advanced energy storage systems may address the increasing concerns of energy shortage and environmental issues. Among many energy storage technologies, electrochemical energy storage systems such as lithium-ion batteries have been widely used in various applications. However, current lithium-ion batteries using flammable liquid electrolytes may cause a safety risk. All-solid-state sodium batteries (ASSSBs) have been attracting considerable attention as safe and low-cost alternatives to Li-ion batteries. However, the performance of ASSSBs falls short of the requirements for commercial applications mainly due to the challenges at the electrode-solid electrolyte interface. The goal of this dissertation is to develop new materials and interfacial engineering methods for high-performance ASSSBs with favorable electrode-electrolyte interfaces. In this dissertation, I demonstrate three effective strategies to address the interfacial challenges, namely through the use of organic cathode materials, new solid electrolyte development, and interfacial engineering.

Hao, Fang↗

Tension‐Induced Cavitation in Li‐Metal Stripping

Abstract Designing stable Li metal and supporting solid structures (SSS) is of fundamental importance in rechargeable Li‐metal batteries. Yet, the stripping kinetics of Li metal and its mechanical effect on the supporting solids (including solid electrolyte interface) remain mysterious to date. Here, through nanoscale in situ observations of a solid‐state Li‐metal battery in an electron microscope, two distinct cavitation‐mediated Li stripping modes controlled by the ratio of the SSS thickness ( t ) to the Li deposit's radius ( r ) are discovered. A quantitative criterion is established to understand the damage tolerance of SSS on the Li‐metal stripping pathways. For mechanically unstable SSS ( t / r < 0.21), the stripping proceeds via tension‐induced multisite cavitation accompanied by severe SSS buckling and necking, ultimately leading to Li “trapping” or “dead Li” formation; for mechanically stable SSS ( t / r > 0.21), the Li metal undergoes nearly planar stripping from the root via single cavitation, showing negligible buckling. This work proves the existence of an electronically conductive precursor film coated on the interior of solid electrolytes that however can be mechanically damaged, and it is of potential importance to the design of delicate Li‐metal supporting structures to high‐performance solid‐state Li‐metal batteries.

36 MATERIALS SCIENCE↗