Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Solid dissolution”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

NUCLEAR WASTE VITRIFICATION EFFICIENCY COLD CAP REACTIONS

The cost and schedule of nuclear waste treatment and immobilization are greatly affected by the rate of glass production. Various factors influence the performance of a waste-glass melter. One of the most significant, and also one of the least understood, is the process of batch melting. Studies are being conducted to gain fundamental understanding of the batch reactions, particularly those that influence the rate of melting, and models are being developed to link batch makeup and melter operation to the melting rate. Batch melting takes place within the cold cap, i.e., a batch layer floating on the surface of molten glass. The conversion of batch to glass consists of various chemical reactions, phase transitions, and diffusion-controlled processes. These include water evaporation (slurry feed contains as high as 60% water), gas evolution, the melting of salts, the formation of borate melt, reactions of borate melt with molten salts and with amorphous oxides (Fe{sub 2}O{sub 3} and Al{sub 2}O{sub 3}), the formation of intermediate crystalline phases, the formation of a continuous glass-forming melt, the growth and collapse of primary foam, and the dissolution of residual solids. To this list we also need to add the formation of secondary foam that originates from molten glass but accumulates on the bottom of the cold cap. This study presents relevant data obtained for a high-level-waste melter feed and introduces a one-dimensional (1D) mathematical model of the cold cap as a step toward an advanced three-dimensional (3D) version for a complete model of the waste glass melter. The 1D model describes the batch-to-glass conversion within the cold cap as it progresses in a vertical direction. With constitutive equations and key parameters based on measured data, and simplified boundary conditions on the cold-cap interfaces with the glass melt and the plenum space of the melter, the model provides sensitivity analysis of the response of the cold cap to the batch makeup and melter conditions. The model demonstrates that batch foaming has a decisive influence on the rate of melting. Understanding the dynamics of the foam layer at the bottom of the cold cap and the heat transfer through it appears crucial for a reliable prediction of the rate of melting as a function of the melter-feed makeup and melter operation parameters. Although the study is focused on a batch for waste vitrification, the authors expect that the outcome will also be relevant for commercial glass melting.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

RESULTS OF PHYSICOCHEMICAL CHARACTERIZATION AND CAUSTIC DISSOLUTION TESTS ON TANK 241-C-108 HEEL SOLIDS

Based on an ENRAF waste surface measurement taken February 1, 2009, double-shell tank (DST) 241-AN-106 (AN-106) contained approximately 278.98 inches (793 kgal) of waste. A zip cord measurement from the tank on February 1, 2009, indicated a settled solids layer of 91.7 inches in height (280 kgal). The supernatant layer in February 2009, by difference, was approximately 187 inches deep (514 kgal). Laboratory results from AN-106 February 1, 2009 (see Table 2) grab samples indicated the supernatant was below the chemistry limit that applied at the time as identified in HNF-SD-WM-TSR-006, Tank Farms Technical Safety Requirements, Administrative Control (AC) 5.16, 'Corrosion Mitigation Controls.' (The limits have since been removed from the Technical Safety Requirements (TSR) and are captured in OSD-T-151-00007, Operating Specifications for the Double-Shell Storage Tanks.) Problem evaluation request WRPS-PER-2009-0218 was submitted February 9, 2009, to document the finding that the supernatant chemistry for grab samples taken from the middle and upper regions of the supernatant was noncompliant with the chemistry control limits. The lab results for the samples taken from the bottom region of the supernatant met AC 5.16 limits.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Nuclear waste vitrification efficiency: cold cap reactions

The cost and schedule of nuclear waste treatment and immobilization are greatly affected by the rate of glass production. Various factors influence the performance of a waste-glass melter. One of the most significant, and also one of the least understood, is the process of batch melting. Studies are being conducted to gain fundamental understanding of the batch reactions, particularly those that influence the rate of melting, and models are being developed to link batch makeup and melter operation to the melting rate. Batch melting takes place within the cold cap, i.e., a batch layer floating on the surface of molten glass. The conversion of batch to glass consists of various chemical reactions, phase transitions, and diffusion-controlled processes. These include water evaporation (slurry feed contains as high as 60% water), gas evolution, the melting of salts, the formation of borate melt, reactions of borate melt with molten salts and with amorphous oxides (Fe2O3 and Al2O3), the formation of intermediate crystalline phases, the formation of a continuous glass-forming melt, the growth and collapse of primary foam, and the dissolution of residual solids. To this list we also need to add the formation of secondary foam that originates from molten glass but accumulates on the bottom of the cold cap. This study presents relevant data obtained for a high-level-waste melter feed and introduces a one-dimensional (1D) mathematical model of the cold cap as a step toward an advanced three-dimensional (3D) version for a complete model of the waste glass melter. The 1D model describes the batch-to-glass conversion within the cold cap as it progresses in a vertical direction. With constitutive equations and key parameters based on measured data, and simplified boundary conditions on the cold-cap interfaces with the glass melt and the plenum space of the melter, the model provides sensitivity analysis of the response of the cold cap to the batch makeup and melter conditions. The model demonstrates that batch foaming has a decisive influence on the rate of melting. Understanding the dynamics of the foam layer at the bottom of the cold cap and the heat transfer through it appears crucial for a reliable prediction of the rate of melting as a function of the melter-feed makeup and melter operation parameters. Although the study is focused on a batch for waste vitrification, the authors expect that the outcome will also be relevant for commercial glass melting.

Hrma, Pavel R↗

Laser-driven hydrothermal process studied with excimer laser pulses

Previously, we discovered [Mariella et al., J. Appl. Phys. 114, 014904 (2013)] that modest-fluence/modest-intensity 351-nm laser pulses, with insufficient fluence/intensity to ablate rock, mineral, or concrete samples via surface vaporization, still removed the surface material from water-submerged target samples with confinement of the removed material, and then dispersed at least some of the removed material into the water as a long-lived suspension of nanoparticles. We called this new process, which appears to include the generation of larger colorless particles, “laser-driven hydrothermal processing” (LDHP) [Mariella et al., J. Appl. Phys. 114, 014904 (2013)]. Now, we report that we have studied this process using 248-nm and 193-nm laser light on submerged concrete, quartzite, and obsidian, and, even though light at these wavelengths is more strongly absorbed than at 351 nm, we found that the overall efficiency of LDHP, in terms of the mass of the target removed per Joule of laser-pulse energy, is lower with 248-nm and 193-nm laser pulses than with 351-nm laser pulses. Given that stronger absorption creates higher peak surface temperatures for comparable laser fluence and intensity, it was surprising to observe reduced efficiencies for material removal. We also measured the nascent particle-size distributions that LDHP creates in the submerging water and found that they do not display the long tail towards larger particle sizes that we had observed when there had been a multi-week delay between experiments and the date of measuring the size distributions. This is consistent with transient dissolution of the solid surface, followed by diffusion-limited kinetics of nucleation and growth of particles from the resulting thin layer of supersaturated solution at the sample surface.

36 MATERIALS SCIENCE↗

Laser Driven Hydrothermal Processing (LDHP) for Rapid Dissolution of Glassy Nuclear Debris

Discovered in 2009 on the SLAB laser system at LLNL, Laser-Driven Hydrothermal Processing (LDHP) both spalls and transiently dissolves a wetted surface (e.g., rock, concrete, paint) when that surface is struck by a laser beam pulse under specific conditions. Previous projects have explored the application of LDHP to expediting sample dissolution for post-detonation nuclear forensics. Early results were very promising, indicating that this method could decrease material dissolution time by a factor of 10 or more. However, the large and complicated lasers previously used are impractical for this application. Under the R^3 venture we aimed to benchmark the LDHP capabilities of turn-key commercial off-the-shelf (COTS) lasers, and to establish how this process could be integrated into an analytical workflow for nuclear forensic analysis. We demonstrated that geological rock standards could be quickly processed into fine powder by LDHP followed by complete acid digestion in 15 minutes, without elemental fractionation that would skew analytical results. We determined that the COTS laser can be used for LDHP that could potentially reduce dissolution time for solid nuclear debris samples in post detonation nuclear forensics. One downside to this approach, however, is that the laser interactions are different with every material, so extensive method validation would be required for all likely material compositions. The LDHP processing rates of several materials were tested and determined to be favorable in the beginning with significant slowdown due to particulate scattering. This could be mitigated either by stopping and centrifuging the sample at specific intervals, or through design of a continuous solvent flow through mechanism.

36 MATERIALS SCIENCE↗

Experimental determination of zirconium hydride precipitation and dissolution in zirconium alloy

In this study, synchrotron X-Ray transmission diffraction experiments were performed to study hydride precipitation and dissolution in the zirconium/zirconium-hydride system while it occurs. Evidence was found that the hysteresis between the terminal solid solubility for precipitation and dissolution is not observed when hydride particles are already present at the beginning of sample cooldown. Additionally, experimental results show that, during a temperature hold, the concentration of hydrogen in solid solution becomes lower than the terminal solid solubility for hydride precipitation and eventually reaches the terminal solid solubility for hydride dissolution, indicating that the latter is the actual thermodynamic solubility limit.

36 MATERIALS SCIENCE↗

Real-Time Atomic-Scale Structural Analysis Resolves the Amorphous to Crystalline CaCO 3 Mechanism Controversy

Amorphous calcium carbonate (ACC) occurs as a precursor to geological and biogenic calcium carbonate (CaCO 3 ), yet its transformation pathways and reaction mechanisms remain inconsistent and controversial. In this study, we investigated the transformation of ACC to calcite under both solution and dry conditions, in the presence and absence of impurity ions, utilizing operando time-resolved synchrotron X-ray diffraction (TRXRD) and reactive transport modeling. Results demonstrate that TRXRD techniques allow us to differentiate dissolution-reprecipitation versus solid-state transformation mechanisms for amorphous to crystalline phase transitions. Specifically, we observe that in environments with abundant water, ACC transforms to calcite through a dissolution-reprecipitation mechanism. This features an activation energy of 63 ± 2 kJ/mol and unit cell volume contraction during calcite crystal growth. Conversely, under water-limited conditions, ACC to calcite transformation proceeds via a solid-state transformation mechanism, with an activation energy of 210 ± 2 kJ/mol, three times greater than the dissolution-reprecipitation route, and a unit cell expansion during crystalline calcite growth. Further, to illustrate the magnitude of these effects, the rates of calcite growth were similar during dissolution-reprecipitation at 3 °C [0.00207(35) s –1 ] and solid-state transformation at 280 °C [0.00134(11) s –1 ]. Moreover, the incorporation of an impurity, strontium, significantly retards the rate of calcite growth while expanding its unit cell but whose incorporation is history dependent. Reactive transport modeling of the dissolution–precipitation kinetics suggests that ACC must be dissolving as compact aggregates. These various transformation mechanisms drive diverse geological and biological carbonate formations, impacting their use as paleoenvironmental markers and functional materials synthesis.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Simulation of mineral dissolution at the pore scale with evolving fluid-solid interfaces: review of approaches and benchmark problem set

This manuscript presents a benchmark problem for the simulation of single-phase flow, reactive transport, and solid geometry evolution at the pore scale. The problem is organized in three parts that focus on specific aspects: flow and reactive transport (part I), dissolution-driven geometry evolution in two dimensions (part II), and an experimental validation of three-dimensional dissolution-driven geometry evolution (part III). Five codes are used to obtain the solution to this benchmark problem, including Chombo-Crunch, OpenFOAM-DBS, a lattice Boltzman code, Vortex, and dissolFoam. These codes cover a good portion of the wide range of approaches typically employed for solving pore-scale problems in the literature, including discretization methods, characterization of the fluid-solid interfaces, and methods to move these interfaces as a result of fluid-solid reactions. A short review of these approaches is given in relation to selected published studies. Results from the simulations performed by the five codes show remarkable agreement both quantitatively--based on upscaled parameters such as surface area, solid volume, and effective reaction rate--and qualitatively--based on comparisons of shape evolution. This outcome is especially notable given the disparity of approaches used by the codes. Therefore, these results establish a strong benchmark for the validation and testing of pore-scale codes developed for the simulation of flow and reactive transport with evolving geometries. They also underscore the significant advances seen in the last decade in tools and approaches for simulating this type of problem.

58 GEOSCIENCES↗

Leaching behaviour of low Ca:Si ratio CaO–SiO{sub 2}–H{sub 2}O systems

A dynamic leaching study of the dissolution of low calcium to silicon ratio (C/S) calcium–silicate–hydrate (C–S–H) systems with initial C/S ranging from 0.2 to 0.6 has been undertaken. Dissolution was studied in demineralised water at 25 °C to a degree of leaching of 2.5 m{sup 3} kg{sup −1}. These C–S–H gels show remarkably similar behaviour during early leaching stages, giving an equilibrated pH of ~ 9.9 and a solution phase C/S of ~ 0.29. Over longer times, C–S–H gels with C/S > 0.29 evolve, on leaching, towards a congruent dissolution point with a solid C/S close to 0.84 (consistent with tobermorite) and pH ~ 10.8. C–S–H gels with C/S < 0.29 become increasingly silica-rich on leaching but maintain an alkaline pH > 9.5 down to at least C/S = 0.07 (the lowest ratio reached). For C/S < 0.7, chemical modelling and X-ray diffraction data support an explanation of the incongruent dissolution behaviour of the low C/S C–S–H gels based on the congruent dissolution of distinct amorphous silica and tobermorite-like C–S–H phases. Above C/S of 0.7, the dissolution data are well described by an ideal solid solution model for the C–S–H phases. These results are of relevance to the consideration of the disposal of silica-rich vitrified intermediate-level radioactive wastes in cement-based concepts for geological disposal, where maintenance of alkaline pH values forms a key component of the chemical barrier to radionuclide migration. The implications are that the long-term pH buffering capacity provided by cementitious backfill materials would not be significantly affected by interactions with silica-rich wasteforms, which may lower the net C/S ratio of C–S–H phases, due to the natural tendency of these systems to restore congruent dissolution at pH 10.8.

36 MATERIALS SCIENCE↗

Artificial Solid Electrolyte Interphase for Suppressing Surface Reactions and Cathode Dissolution in Aqueous Zinc Ion Batteries

Vanadium-based compounds have been widely used as electrode materials in aqueous zinc ion batteries (ZIBs) due to the multiple oxidation states of vanadium and their open framework structure. However, the solubility of vanadium in aqueous electrolytes and the formation of byproducts during the charge/discharge process cause severe capacity fading and limit cycle life. Here in this paper, we report an ultrathin HfO 2 film as an artificial solid electrolyte interphase (SEI) that is uniformly and conformally deposited by atomic layer deposition (ALD). The inactive hafnium(IV) oxide (HfO 2 ) film not only decreases byproduct (Zn 4 SO 4 (OH) 6 ·xH 2 O) formation on the surface of Zn 3 V 2 O 7 (OH) 2 ·2H 2 O (ZVO) but also suppresses the ZVO cathode dissolution in the electrolyte. As a result, the obtained HfO 2 -coated ZVO cathodes deliver higher capacity and better cycle life (227 mAh g –1 @100 mA g –1 , 90% retention over 100 cycles) compared with pristine ZVO (170 mAh g –1 @100 mA g –1 , 45% retention over 100 cycles). A mechanistic investigation of the role of HfO 2 is presented, along with data showing that our method constitutes a general strategy for other cathodes to enhance their performance in aqueous ZIBs.

25 ENERGY STORAGE↗

Morphology selection in dealloying: A phase field study of the coupling among kinetic mechanisms

A phase field model is used to investigate how the corrosion rate and morphology of a dealloying metal is controlled by the kinetic rates of bulk solid diffusion, interfacial diffusivity, and interface dissolution. A specific focus is investigating the manner by which variations in these kinetic parameters synergistically influence the onset of a morphological instability at the solid-liquid interface, which is known to precede rapid dealloying corrosion towards highly topologically complex structures such as bicontinuous porous solids. This work demonstrates that this instability can be suppressed by either an increase of interdiffusion in the solid alloy, or by a decreasing rate of dissolution at the solid-liquid interface. When the instability is suppressed, the result is a relatively planar, passivated dealloying front. Importantly, however, coupled changes in kinetic parameters can also promote the morphological instability and sustain fine-scale ligament and pore formation. Finally, the relevance of the solid-liquid interfacial diffusion for determining the rate of dealloying and ligament formation is highlighted. By elucidating the mechanistic influence of bulk and interfacial kinetic factors on the dealloyed morphology, this work helps to rationalize the contrasting morphologies observed in various dealloying systems.

Diffusion↗

Peculiarities of CsPbBr3 perovskites melting in quasi-equilibrium conditions

The melting behavior of CsPbBr3 perovskite was studied by differential thermal analysis (DTA). It was found that melting of CsPbBr3 occurs non-isothermally in the temperature range of 561-570 °C. From the temperature dependence of the solid-phase melting rate, it was established that at 567±1 °C the change in the mechanism of the solid-phase melting goes from fragmentation to dissolution at the surface. The obtained values of the activation energy of the melting of the solid phase in CsPbBr3 show that the activation energy of the dissolution of the solid-phase fragments is 4 times greater than the energy of the fragmentation of the solid phase.

Kopach, O.↗

Transformation of Gibbsite to Boehmite in Caustic Aqueous Solution at Hydrothermal Conditions

Phase transformations among aluminum (oxyhydr)oxide minerals play important roles across a wide range of natural and industrial settings. In highly caustic aqueous solutions, uncertainty persists regarding whether solid-state or dissolution-reprecipitation pathways dominate. We explored transformation of gibbsite [a Al(OH)3] to boehmite (? AlOOH) in caustic NaOH solution at hydrothermal conditions as a function of temperature, Al(III) and NaOH concentrations, and reaction time. Comparison of detailed structural and morphological solids characterization by XRD, SEM/TEM, AFM, Raman spectroscopy, and high field 27Al MAS NMR to predictions from equilibrium thermodynamics calculations suggests the critical importance of dissolution-reprecipitation across our range of system conditions. The yield and physical properties of the boehmite product was found to be sensitive to the hydrothermal treatment temperature and the Al/OH- ratio, controlled by the loading of gibbsite with respect to NaOH. Experiments at lower Al/OH- ratios (e.g., 0.64) indicate that the dissolution of the gibbsite reaches an aqueous aluminate saturation state sufficient to overcome the nucleation barrier for boehmite. Higher Al/OH- ratios (e.g., 3.2) are found to slow the phase transformation, leaving residual unreacted gibbsite in the final product. Higher temperatures appear to improve the phase transformation rate, but also typically yield smaller sized boehmite particles. Particle morphological analyses compared to thermodynamic expectations suggest an important role of kinetics at mineral/solution interfaces, both in the gibbsite dissolution rate as well as the growth rate of boehmite nanocrystals.

Zhang, Xin↗

COMPILATION OF LABORATORY SCALE ALUMINUM WASH AND LEACH REPORT RESULTS

This report compiles and analyzes all known wash and caustic leach laboratory studies. As further data is produced, this report will be updated. Included are aluminum mineralogical analysis results as well as a summation of the wash and leach procedures and results. Of the 177 underground storage tanks at Hanford, information was only available for five individual double-shell tanks, forty-one individual single-shell tanks (e.g. thirty-nine 100 series and two 200 series tanks), and twelve grouped tank wastes. Seven of the individual single-shell tank studies provided data for the percent of aluminum removal as a function of time for various caustic concentrations and leaching temperatures. It was determined that in most cases increased leaching temperature, caustic concentration, and leaching time leads to increased dissolution of leachable aluminum solids.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Characterization of Tank 16 Annulus Samples

The closure of Tank 16H will require removal of material from the annulus of the tank. Samples from Tank 16H annulus were characterized and tested to provide information to evaluate various alternatives for removing the annulus waste. The analysis found all four annulus samples to be composed mainly of Si, Na, and Al and lesser amounts of other elements. The XRD data indicate quartz (SiO 2 ) and sodium aluminum nitrate silicate hydrate (Na 8 (Al 6 Si 6 O 24 )(NO 3 ) 2 .4H 2 O) as the predominant crystalline mineral phases in the samples. The XRD data also indicate the presence of crystalline sodium nitrate, sodium nitrite, gibbsite, hydrated sodium bicarbonate, and muscovite. Based on the weight of solids remaining at the end of the test, the water leaching test results indicate approximately 20-35% of the solids dissolved after three contacts with an approximately 3:1 volume of water at 45 C. The chemical analysis of the leachates and the XRD results of the remaining solids indicate sodium salts of nitrate, nitrite, sulfate, and possibly carbonate/bicarbonate make up the majority of the dissolved material. The majority of these salts were dissolved in the first water contact and simply diluted with each subsequent water contact. The water leaching removed large amounts of the uranium in two of the samples and {approx}1/3 of the {sup 99}Tc from all four samples. Most of the other radionuclides analyzed showed low solubility in the water leaching test. The preliminary data on the oxalic acid leaching test indicate the three acid contacts at 45 C dissolved from {approx}34-47% of the solids. The somewhat higher dissolution found in the oxalic acid leaching test versus the water leaching test might be offset by the tendency of the oxalic acid solutions to take on a gel-like consistency. The filtered solids left behind after three oxalic acid contacts were sticky and formed large clumps after drying. These two observations could indicate potential processing difficulties with solutions and solids from oxalic acid leaching. The gel formation might be avoided by using larger volumes of the acid. Further testing would be recommended before using oxalic acid to dissolve the Tank 16H annulus waste to ensure no processing difficulties are encountered in the full scale process.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Microstructural Characterization and Electrochemical Behavior of AA2014 Al-Cu-Mg-Si Alloy of Various Tempers

AA2014 Al-Cu-Mg-Si alloy is subjected to aging heat treatment, and microstructural features and electrochemical behavior of the AA2014 Al-Cu-Mg-Si alloy of various tempers have been characterized. Hardness measurement of the alloy of different tempers showed typical age hardening behavior. X-ray diffraction and transmission electron microscopy studies revealed the presence of characteristic phases. Differential scanning calorimetry study displayed the sequence of solid-state precipitation and dissolution reactions in the AA2014 alloy of various tempers. Electrochemical behavior was assessed by measurement of variation of open-circuit voltage with time, potentiodynamic polarization and potentiodynamic cyclic polarization of the AA2014 alloy of various tempers in 3.5 wt.% NaCl solution at near neural (pH ~ 7) and at alkaline (pH 12) conditions. Potentiodynamic polarization studies of different tempers in 3.5 wt.% NaCl solution at pH ~ 7 showed that the corrosion potential (E{sub corr}) value has shifted toward more negative (active) direction with increasing aging time. The cyclic polarization in 3.5 wt.% NaCl solution at pH ~ 7 displayed active–passive behavior and also showed a large hysteresis loop indicating high pit growth damage.

36 MATERIALS SCIENCE↗