Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Secondary Waste Form”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Evaluation of Technetium Getters to Improve the Performance of Cast Stone

Cast Stone has been selected as the preferred waste form for solidification of aqueous secondary liquid effluents from the Hanford Tank Waste Treatment and Immobilization Plant (WTP) process condensates and low-activity waste (LAW) melter off-gas caustic scrubber effluents. Cast Stone is also being evaluated as a supplemental immobilization technology to provide the necessary LAW treatment capacity to complete the Hanford tank waste cleanup mission in a timely and cost effective manner. One of the major radionuclides that Cast Stone has the potential to immobilize is technetium (Tc). The mechanism for immobilization is through the reduction of the highly mobile Tc(VII) species to the less mobile Tc(IV) species by the blast furnace slag (BFS) used in the Cast Stone formulation. Technetium immobilization through this method would be beneficial because Tc is one of the most difficult contaminants to address at the U.S. Department of Energy (DOE) Hanford Site due to its complex chemical behavior in tank waste, limited incorporation in mid- to high-temperature immobilization processes (vitrification, steam reformation, etc.), and high mobility in subsurface environments. In fact, the Tank Closure and Waste Management Environmental Impact Statement for the Hanford Site, Richland, Washington (TC&WM EIS) identifies technetium-99 ( 99 Tc) as one of the radioactive tank waste components contributing the most to the environmental impact associated with the cleanup of the Hanford Site. The TC&WM EIS, along with an earlier supplemental waste-form risk assessment, used a diffusion-limited release model to estimate the release of different contaminants from the WTP process waste forms. In both of these predictive modeling exercises, where effective diffusivities based on grout performance data available at the time, groundwater at the 100-m down-gradient well exceeded the allowable maximum permissible concentrations for 99 Tc. (900 pCi/L). Recent relatively short-term (63 day) leach tests conducted on both LAW and secondary waste Cast Stone monoliths indicated that 99 Tc diffusivities were at or near diffusivities where the groundwater at the 100-m down-gradient well would exceed the allowable maximum permissible 99 Tc concentrations. There is, therefore, a need and an opportunity to improve the retention of Tc in the Cast Stone waste form. One method to improve the performance of the Cast Stone waste form is through the addition of “getters” that selectively sequester Tc inside Cast Stone.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

EVALUATION AND SELECTION OF 99TC GETTERS FOR SEQUESTRATION OF LIQUID SECONDARY WASTE RESULTING FROM VITRIFICATION OF RADIOACTIVE WASTE FROM HANFORD

Getters are most commonly inorganic materials that selectively adsorb radionuclide and metallic contaminants. Typically, these materials have been deployed in two different modes to immobilize and retard contaminant release from monolithic waste forms. One mode is to first use getters to selectively scavenge the radionuclide of interest from a liquid waste stream, and then incorporate the radionuclide-loaded getters in cementitious or other monolithic waste forms. The other mode consists of mixing getters and liquid waste together during formulation of monolithic waste forms. Desirable characteristics for a getter material include, (1) specific adsorption of radionuclide of interest and very high selectivity toward radionuclides of concern in concentrations that would be several orders of magnitude less than the concentrations of competing anions and cations, (2) adsorption capacity that should be sufficient for the mass and volume of the material that will be deployed to be within practicable limits, (3) long-term adsorption and retention of radionuclide, (4) sufficient physical and chemical stability that its radionuclide retention performance will not degrade significantly during the designed life span of the waste form, (5) chemical stability under the range of Eh, pH, and solution conditions that exist in the waste form environment, and (6) should not adversely affect chemical and physical integrity of waste forms. We conducted a literature review to identify getters that are suitable for effectively sequestering 99Tc in monolithic waste forms that are being evaluated for stabilizing secondary liquid waste streams resulting from treatment and vitrification of radioactive tank wastes at Hanford. As a result of this review, we identified a set of getters that warrant further evaluation for this specific application.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Glass Ceramic Formulation Data Package

A glass ceramic waste form is being developed for treatment of secondary waste streams generated by aqueous reprocessing of commercial used nuclear fuel (Crum et al. 2012b). The waste stream contains a mixture of transition metals, alkali, alkaline earths, and lanthanides, several of which exceed the solubility limits of a single phase borosilicate glass (Crum et al. 2009; Caurant et al. 2007). A multi-phase glass ceramic waste form allows incorporation of insoluble components of the waste by designed crystallization into durable heat tolerant phases. The glass ceramic formulation and processing targets the formation of the following three stable crystalline phases: (1) powellite (XMoO 4 ) where X can be (Ca, Sr, Ba, and/or Ln), (2) oxyapatite Y x, Z (10-x) Si 6 O 26 where Y is alkaline earth, Z is Ln, and (3) lanthanide borosilicate (Ln 5 BSi 2 O 13 ). These three phases incorporate the waste components that are above the solubility limit of a single-phase borosilicate glass. The glass ceramic is designed to be a single phase melt, just like a borosilicate glass, and then crystallize upon slow cooling to form the targeted phases. The slow cooling schedule is based on the centerline cooling profile of a 2 foot diameter canister such as the Hanford High-Level Waste canister. Up to this point, crucible testing has been used for glass ceramic development, with cold crucible induction melter (CCIM) targeted as the ultimate processing technology for the waste form. Idaho National Laboratory (INL) will conduct a scaled CCIM test in FY2012 with a glass ceramic to demonstrate the processing behavior. This Data Package documents the laboratory studies of the glass ceramic composition to support the CCIM test. Pacific Northwest National Laboratory (PNNL) measured melt viscosity, electrical conductivity, and crystallization behavior upon cooling to identify a processing window (temperature range) for melter operation and cooling profiles necessary to crystallize the targeted phases in the waste form.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Technetium Getters to Improve Cast Stone Performance

The cementitious material known as Cast Stone has been selected as the preferred waste form for solidification of aqueous secondary liquid effluents from the Hanford Tank Waste Treatment and Immobilization Plant (WTP) process condensates and low-activity waste (LAW) melter off-gas caustic scrubber effluents. Cast Stone is also being evaluated as a supplemental immobilization technology to provide the necessary LAW treatment capacity to complete the Hanford tank waste cleanup mission in a timely and cost effective manner. Two radionuclides of particular concern in these waste streams are technetium-99 (99Tc) and iodine-129 (129I). These radioactive tank waste components contribute the most to the environmental impacts associated with the cleanup of the Hanford site. A recent environmental assessment of Cast Stone performance, which assumes a diffusion controlled release of contaminants from the waste form, calculates groundwater in excess of the allowable maximum permissible concentrations for both contaminants. There is, therefore, a need and an opportunity to improve the retention of both 99Tc and 129I in Cast Stone. One method to improve the performance of Cast Stone is through the addition of “getters” that selectively sequester Tc and I, therefore reducing their diffusion out of Cast Stone. In this paper, we present results of Tc and I removal from solution with various getters with batch sorption experiments conducted in deionized water (DIW) and a highly caustic 7.8 M Na Ave LAW simulant. In general, the data show that the selected getters are effective in DIW but their performance is comprised when experiments are performed with the 7.8 M Na Ave LAW simulant. Reasons for the mitigated performance in the LAW simulant may be due to competition with Cr present in the 7.8 M Na Ave LAW simulant and to a pH effect.

Cast Stone↗

Influences on Subsurface Plutonium and Americium Migration

Plutonium (Pu) has been released to the environment worldwide, including approximately 1.85 × 1015 Bq (200 kg) of Pu from process waste solutions to unconfined soil structures at the Hanford Site in Washington State. The subsurface mobility of Pu is influenced by complex interactions with sediments, groundwater, and any co-contaminants within the waste stream. Previous investigations at Hanford have shown that Pu exists as discrete PuO 2 particles forming before or after disposal, as secondary solid phases formed from waste interactions with sediments as adsorbed/incorporated species, and/or as dissolved species. In this research, new evidence is presented for the existence of PuO 2 , PuO 2 -Bi 2 O 3 composites, and particles from burnt Pu metal in near-surface sediments where Pu-laden acidic process waste was disposed to sediments. Pu and americium (Am) L3 X-ray absorption spectroscopy and density functional theory suggest that, in larger, more crystalline PuO 2 particles, Am formed from radioactive decay is retained in the Pu IV O 2 structure as Am IV . The Pu and Am that were disposed of in an acidic waste stream have since migrated deeper into the subsurface with detection to at least 37 meters below ground surface. In contrast, Pu deposited near the ground surface from neutral pH waste is found to be homogeneously distributed and relatively immobile. Groundwater extractions performed on contaminated sediments indicate that both Pu and Am are recalcitrant, with Am being fractionally less extractable than Pu on a molar basis. These results suggest that the more mobile fraction of Am has migrated from the near-surface and may be present in the deeper sediments as a different phase than Pu. From these results, it is suggested that Pu and Am deposited from acidic wastes were initially mobile and became significantly less mobile as wastes were neutralized within the soil profile.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Technetium and iodine getters to improve Cast Stone performance - 15420

Technetium-99 ({sup 99}Tc) and iodine-129 ({sup 129}I) have been determined to be tank waste components contributing most to the environmental impacts associated with the cleanup of the Hanford site. Cast Stone, which has the ability to immobilize {sup 99}Tc, {sup 129}I, and other contaminants of concern, is being considered as a low temperature waste form for solidification of aqueous secondary liquid effluents from the Hanford Tank Waste Treatment and Immobilization Plant (WTP) An environmental assessment of Cast Stone performance, using measured diffusivities of the radionuclides from the Cast Stone product, calculates groundwater at the 100 m down-gradient in excess of the allowable maximum permissible concentrations for both radionuclides. Therefore, an opportunity exists to improve the performance of Cast Stone. One method for improvement is through the addition of immobilizing agents known as 'getters' that selectively sequester Tc and I. In the present paper, we report on seven getter materials that have been tested for Tc and five materials that have been tested for I to determine their effectiveness for radionuclide removal in a series of batch sorption tests in 18.2 MΩ DI H{sub 2}O and a 7.8 M Na Ave LAW waste simulant. Contact experiments have been carried out in anoxic conditions at room temperature, with varying solid-to-solution ratios, and in the presence and absence of competing species. Results indicate that most materials perform better in the 18.2 MΩ DI H{sub 2}O compared to the 7.8 M Na LAW waste simulant for both Tc and I getter. Radionuclide sequestration may be affected by the presence of the redox sensitive Cr(VI) in the simulant. The top performing Tc getter materials, Sn(II)-apatite, BFS-2, KMS-2 and Sn-hydroxyapatite, were examined through various solid-state characterization techniques such as SEM/XEDS, XANES and EXAFS. Tc removal is theorized to occur through reduction of the highly soluble Tc(VII) species to the less soluble Tc(IV). Solution results from the series of I tests show that iodide is effectively removed from solution via, most likely, a precipitation reaction of AgI. A wide range of I getter materials and the silver exchanged zeolite getter performed well in both DI water and the simulant. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

The effect of concentration on the structure and crystallinity of a cementitious waste form for caustic wastes

Cement-based waste forms have long been considered economical technologies for disposal of various types of waste. A solidified cementitious waste form, Cast Stone, was developed to immobilize the radioactive secondary waste from vitrification processes. In this work, Cast Stone was considered for a Na-based caustic liquid waste, and its physical properties were analyzed as a function of liquid waste loading up to 2 M Na. Differences in crystallinity (phase composition), microstructure, mesostructure (pore size distribution, surface area), and macrostructure (density, compressive strength) were investigated using various analytical techniques, in order to assess the suitability of Cast Stone as a chemically durable waste. It was found that the concentration of secondary waste simulant (caustic waste) had little effect on the relevant engineering properties of Cast Stone, showing that Cast Stone could be an effective and tolerant waste form for a wide range of concentrations of high sodium waste.

Cast Stone↗

New Formulation of Cast Stone for {sup 99}Tc Immobilization in Sulfate Rich Secondary Waste Stream - 16098

A low-temperature, cementitious waste form called Cast Stone (or grout) has been selected for solidification of the Effluent Treatment Facility (ETF)-treated wastes at the Hanford Site. Because the waste stream to be solidified may be relatively high in sulfate, the current Cast Stone dry blend formulation with ordinary Portland cement (OPC), fly ash (FA), and blast furnace slag (BFS) (47% BFS, 45% FA, and 8% OPC) may not be adequate. Thus a new formulation, called secondary waste grout, was proposed and tested. The secondary waste grout uses hydrated lime [Ca(OH){sub 2}] to tie up the sulfate initially such that ettringite [Ca{sub 6}Al{sub 2}(SO{sub 4}){sub 3}(OH){sub 12}.26(H{sub 2}O)] forms rapidly instead of forming as the cementitious waste form cures. Three different liquid waste simulants (242-A evaporator, Environmental Restoration Disposal Facility [ERDF] leachates, and Hanford Tank Waste Treatment and Immobilization Plant [WTP] off-gas condensates) were prepared and solidified using this new dry blend formulation. Baseline grout dry mixes were 20 wt% hydrated lime (HL), 35 wt% OPC, and 45 wt% BFS, and two different water-to-dry mix (w/dm) ratios (0.5 and 0.6) of free water mass to mass of dry blend were tested. After curing for a minimum of 28 days, the grout solidified waste forms were characterized and used for Tc leachability testing using the EPA 1315 Method. X-ray diffraction analysis confirmed that ∼12-15% of ettringite was formed in early stage of 28-day curing for the grouts prepared with the high sulfate WTP simulant and HL addition. In addition, the new formulation of secondary waste grout prepared with HL (20%), OPC (35%), and BFS (45%) at either 0.5 or 0.6 water to dry mix ratio yields higher average Tc interval leachability index (LI) values (12.5 to 13.9) after 28 to 90 days of leaching using deionized water, which is higher than the desired {sup 99}Tc LI value of 12 for grout destined for burial in the Integrated Disposal Facility at the Hanford Site. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Diffusion and Leaching Behavior of Radionuclides in Category 3 Waste Encasement Concrete and Soil Fill Material – Summary Report

One of the methods being considered for safely disposing of Category 3 low-level radioactive wastes is to encase the waste in concrete. Such concrete encasement would contain and isolate the waste packages from the hydrologic environment and would act as an intrusion barrier. The current plan for waste isolation consists of stacking low-level waste packages on a trench floor, surrounding the stacks with reinforced steel, and encasing these packages in concrete. These concrete-encased waste stacks are expected to vary in size with maximum dimensions of 6.4 m long, 2.7 m wide, and 4 m high. The waste stacks are expected to have a surrounding minimum thickness of 15 cm of concrete encasement. These concrete-encased waste packages are expected to withstand environmental exposure (solar radiation, temperature variations, and precipitation) until an interim soil cover or permanent closure cover is installed, and to remain largely intact thereafter. Any failure of concrete encasement may result in water intrusion and consequent mobilization of radionuclides from the waste packages. The mobilized radionuclides may escape from the encased concrete by mass flow and/or diffusion and move into the surrounding subsurface environment. Therefore, it is necessary to assess the performance of the concrete encasement structure and the ability of the surrounding soil to retard radionuclide migration. The retardation factors for radionuclides contained in the waste packages can be determined from measurements of diffusion coefficients for these contaminants through concrete and fill material. Some of the mobilization scenarios include (1) potential leaching of waste form before permanent closure cover is installed; (2) after the cover installation, long-term diffusion of radionuclides from concrete waste form into surrounding fill material; (3) diffusion of radionuclides from contaminated soils into adjoining concrete encasement and clean fill material. Additionally, the rate of diffusion of radionuclides may be affected by the formation of structural cracks in concrete, the carbonation of the buried waste form, and any potential effect of metallic iron (in the form of rebars) on the mobility of radionuclides. The radionuclides iodine-129 ({sup 129}I), technetium-99 ({sup 99}Tc), and uranium-238 ({sup 238}U) are identified as long-term dose contributors in Category 3 waste (Mann et al. 2001; Wood et al. 1995). Because of their anionic nature in aqueous solutions, {sup 129}I, {sup 99}Tc, and carbonate-complexed {sup 238}U may readily leach into the subsurface environment (Serne et al. 1989, 1992a, b, 1993, and 1995). The leachability and/or diffusion of radionuclide species must be measured to assess the long-term performance of waste grouts when contacted with vadose-zone pore water or groundwater. Although significant research has been conducted on the design and performance of cementitious waste forms, the current protocol conducted to assess radionuclide stability within these waste forms has been limited to the Toxicity Characteristic Leaching Procedure, Method 1311 Federal Registry (EPA 1992) and ANSI/ANS-16.1 leach test (ANSI 1986). These tests evaluate the performance under water-saturated conditions and do not evaluate the performance of cementitious waste forms within the context of waste repositories which are located within water-deficient vadose zones. Moreover, these tests assess only the diffusion of radionuclides from concrete waste forms and neglect evaluating the mechanisms of retention, stability of the waste form, and formation of secondary phases during weathering, which may serve as long-term secondary hosts for immobilization of radionuclides. The results of recent investigations conducted under arid and semi-arid conditions (Al-Khayat et al. 2002; Garrabrants et al. 2002; Garrabrants and Kosson 2003; Garrabrants et al. 2004; Gervais et al. 2004; Sanchez et al. 2002; Sanchez et al. 2003) provide valuable information suggesting structural and chemical changes to concrete waste forms which may affect contaminant containment and waste form performance. However, continued research is necessitated by the need to understand: the mechanism of contaminant release; the significance of contaminant release pathways; how waste form performance is affected by the full range of environmental conditions within the disposal facility; the process of waste form aging under conditions that are representative of processes occurring in response to changing environmental conditions within the disposal facility; the effect of waste form aging on chemical, physical, and radiological properties, and the associated impact on contaminant release. Recent reviews conducted by the National Academies of Science recognized the efficacy of cementitious materials for waste isolation, but further noted the significant shortcomings in our current understanding and testing protocol for evaluating the performance of various formulations.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Improving the Estimates of Waste from the Recycling of Used Nuclear Fuel - 13410

Estimates are presented of wastes arising from the reprocessing of 50 GWD/tonne, 5 year and 50 year cooled used nuclear fuel (UNF) from Light Water Reactors (LWRs), using the 'NUEX' solvent extraction process. NUEX is a fourth generation aqueous based reprocessing system, comprising shearing and dissolution in nitric acid of the UNF, separation of uranium and mixed uranium-plutonium using solvent extraction in a development of the PUREX process using tri-n-butyl phosphate in a kerosene diluent, purification of the plutonium and uranium-plutonium products, and conversion of them to uranium trioxide and mixed uranium-plutonium dioxides respectively. These products are suitable for use as new LWR uranium oxide and mixed oxide fuel, respectively. Each unit process is described and the wastes that it produces are identified and quantified. Quantification of the process wastes was achieved by use of a detailed process model developed using the Aspen Custom Modeler suite of software and based on both first principles equilibrium and rate data, plus practical experience and data from the industrial scale Thermal Oxide Reprocessing Plant (THORP) at the Sellafield nuclear site in the United Kingdom. By feeding this model with the known concentrations of all species in the incoming UNF, the species and their concentrations in all product and waste streams were produced as the output. By using these data, along with a defined set of assumptions, including regulatory requirements, it was possible to calculate the waste forms, their radioactivities, volumes and quantities. Quantification of secondary wastes, such as plant maintenance, housekeeping and clean-up wastes, was achieved by reviewing actual operating experience from THORP during its hot operation from 1994 to the present time. This work was carried out under a contract from the United States Department of Energy (DOE) and, so as to enable DOE to make valid comparisons with other similar work, a number of assumptions were agreed. These include an assumed reprocessing capacity of 800 tonnes per year, the requirement to remove as waste forms the volatile fission products carbon-14, iodine-129, krypton-85, tritium and ruthenium-106, the restriction of discharge of any water from the facility unless it meets US Environmental Protection Agency drinking water standards, no intentional blending of wastes to lower their classification, and the requirement for the recovered uranium to be sufficiently free from fission products and neutron-absorbing species to allow it to be re-enriched and recycled as nuclear fuel. The results from this work showed that over 99.9% of the radioactivity in the UNF can be concentrated via reprocessing into a fission-product-containing vitrified product, bottles of compressed krypton storage and a cement grout containing the tritium, that together have a volume of only about one eighth the volume of the original UNF. The other waste forms have larger volumes than the original UNF but contain only the remaining 0.1% of the radioactivity. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Computational Investigation of Technetium(IV) Incorporation into Inverse Spinels: Magnetite (Fe 3 O 4 ) and Trevorite (NiFe 2 O 4 )

Iron oxides and oxyhydroxides play an important role in minimizing the mobility of redox-sensitive elements in engineered and natural environments. For the radionuclide technetium-99 (Tc), these phases hold promise as primary hosts for increasing Tc loading into glass waste form matrices, or as secondary sinks during the long-term storage of nuclear materials. Recent experiments show that the inverse spinel, magnetite [Fe(II)Fe(III)2O4], can incorporate Tc(IV) into its octahedral sub-lattice, and in that same class of materials, trevorite [Ni(II)Fe(III)2O4] is also being investigated for its ability to host Tc(IV). However, questions remain regarding the most energetically favorable charge-compensation mechanism for Tc(IV) incorporation in each structure, which will affect Tc behavior under changing waste processing or storage conditions. Here, quantum-mechanical methods were used to evaluate incorporation energies and optimized lattice bonding environments for three different, charge-balanced Tc(IV) incorporation mechanisms in magnetite and trevorite. In both cases, the removal of two octahedral Fe(II) or Ni(II) ions upon the addition of Tc(IV) to an octahedral site is the most stable mechanism, relative to the creation of octahedral Fe(III) defects or increasing octahedral Fe(II) content. Following hydration-energy corrections, Tc(IV) incorporation into magnetite is energetically favorable while an energy barrier exists for trevorite.

Environmental Molecular Sciences Laboratory↗

GeoMelt{sup R} In-Container Vitrification (ICV){sup TM} for Fukushima Daiichi Water Treatment Secondary Wastes - 20212

The Japanese government is supporting development work implemented jointly by Veolia subsidiaries Kurion Japan, K.K., Veolia Nuclear Solutions (VNS), Inc., and Veolia Nuclear Solutions Federal Services, LLC for treating radioactive waste generated from Fukushima Daiichi Nuclear Power Station (NPS) water treatment using the GeoMelt{sup TM} In-Container Vitrification (ICV){sup TM} technology. The initial work consisted of glass formulation and engineering-scale testing which was completed in 2018, in the frame of an IRID (International Research Institute for Nuclear Decommissioning) program as part of a project subsidized by Japan's Ministry of Economy, Trade and Industry (METI). The Fukushima Daiichi NPS Mid- and Long-Term Road-map requires investigation of methods to stabilize solid wastes (and to immobilize radioisotopes in the wastes) generated as a result of emergency response and decommissioning activities. Cooling water treatment has resulted in a significant amount of solid and slurry secondary wastes (mostly adsorbents and ion-exchange materials) which will require processing at some point. GeoMelt{sup R} ICV{sup TM} is a joule-heated melter technology which uses a refractory-lined single-use container combining the melter and disposal container. There is no pouring required nor concerns with refractory corrosion which allows the process to accommodate a wide range of waste chemistries and high waste loadings. The testing described here consisted of three engineering-scale melts, each processing between 212 kg and 240 kg of waste simulants, glass formers, and non-radioactive cesium (Cs) and strontium (Sr) tracers. Continuous isokinetic stack sampling of off-gas emissions was performed for each test in order to calculate Cs and Sr retention in the glass wasteform. Single-pass retention of Cs in the final glass wasteform ranged from 91.46 to 99.30%, and single-pass retention of Sr ranged from 99.76 to 100%. Planned particulate recycle will increase these retention levels. Melt 1 processed a mixture of KUR-EH (a zeolite-based ion-exchange material), simulated Advanced Liquid Processing System (ALPS) Carbonate and Iron Slurries, and glass additives. Melt 2 processed a mixture of KUR-EH, KUR-TSG (a titanate-based adsorbent), and glass additives. Melt 3 processed a mixture of KUR-EH, simulated barium sulfate/iron ferrocyanide sludge (AREVA sludge), and glass additives. Waste loadings for these melts ranged from 70 weight percent (wt%) to 82 wt%. Vitrification produces a waste form much denser than the stored water treatment secondary waste wastes, resulting in significant volume reduction. Volume reductions for the three tests ranged from 74 to 79 vol%. Vitrification produces a chemically durable wasteform. Pacific Northwest National Laboratory (PNNL) tested three glass samples from each engineering-scale melt) by the Materials Characterization Center 1 (MCC-1) test, an international standard leach test of the chemical durability of nuclear waste glasses. PNNL also obtained one U.S. reference glass (EA Glass) and two Japan reference glasses P0798) and tested these under the same MCC-1 conditions (90 deg. C, 10 m-1, DIW, and 7, 14, 28-day) as the GeoMelt{sup R} ICV{sup TM} glasses. The GeoMelt{sup R} ICV{sup TM} glasses exhibited lower total normalized releases and 14- to 28-day normalized release rates than the three reference glasses. These results suggest that the GeoMelt{sup R} ICV{sup TM} glasses have durabilities on par with high-level waste glasses under standard test conditions. Post-melt process sampling and analysis indicated no Cs migration into the melter refractory materials and very little deposition of Cs or Sr onto the melter hood or off-gas piping internals. The results of the testing indicated good Cs retention in the glass, high volume reduction and waste loadings, and excellent chemical durability. These factors are important to minimize treatment costs and to protect workers and the environment. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Alloying of Pu-Al with Stainless Steel for Material Disposition

The Savannah River National Laboratory (SRNL) has evaluated several options for the disposition of stainless-steel clad plutonium metal alloy. One of the technologies under consideration is alloying of the material with stainless steel (SS). The resulting SS-Pu alloy would be a non-proliferable waste form consisting of a secondary Pu composition region microencapsulated in the refractory stainless steel. Two 8-kg ingots were made at SS-1.8Zr-0.4Pu alloys (wt %); 8 kg was determined in a previous study to be the maximum mass of SS ingot at the maximum target Pu loading of 350-g that would result in a SS-4.4Pu alloy (wt %). Two smaller 500-g ingots were also produced at SS-1.6Zr-1.4Pu and SS-1.4Pu (wt %). The 500-g ingots evaluated alloying at a higher Pu concentration than in the 8 kg ingots, and they evaluated the necessity of adding Zr metal to incorporate the Pu and control Pu oxidation. Zr addition was found to be unnecessary to incorporate the Pu and control Pu oxidation. Drill turnings were collected from the large and small ingots and metallographic samples were directly cut from the small ingots. Both were analyzed to validate the structure and composition region formation. Chemical analyses of turnings proved that the Pu was dispersed within the SS ingots.

36 MATERIALS SCIENCE↗

Corrosion Behavior and Microstructure Influence of Glass-Ceramic Nuclear Waste Forms

Glass ceramic waste forms present a potentially viable technology for the long term immobilization and disposal of liquid nuclear wastes. Through control of chemistry during fabrication, such waste forms can have designed secondary crystalline phases within a borosilicate glass matrix. In this work, a glass ceramic containing powellite and oxyapatite secondary phases was tested for its corrosion properties in dilute conditions using single pass flow through testing (SPFT). Three glass ceramic samples were prepared using different cooling rates to produce samples with varying microstructure sizes. In testing at 90 °C in buffered pH 7 and pH 9 solutions, it was found that increasing pH and decreasing microstructure size (resulting from rapid cooling during fabrication) both led to a reduction in overall corrosion rate. The phases of the glass ceramic were found, using a combination of solutions analysis, SEM and AFM, to corrode preferably in the order of powellite > bulk glass matrix > oxyapatite.

Environmental Molecular Sciences Laboratory↗

Drying Spent Magnox Fuel for Interim Dry Storage

Spent Magnox fuel is usually stored under water for shielding and cooling following use in-reactor, but the storage water can react with Magnox clad fuel and cause corrosion and forms a sludge which generates a secondary waste product. One option to prevent unwanted corrosion and avoid expensive waste management is to dry the wet fuel. This project aims to test a drying process which will convert wet and corroded Magnox fuel to a stable form to demonstrate viability for conversion from wet to dry storage. Samples of corroded Magnox supplied by National Nuclear Laboratory. Corrosion product retrieved by various methods including dry scraping, ultrasonic treatment to form sludge and sludge drying to isolate suspension. TGA undertaken on Sample 1 and Sample 2, with brucite and hydromagnesite for comparison. Both samples showed ∼10% mass loss up to 250 deg. C attributable to water held in sample. Mass loss from dehydroxylation which liberates further water in both samples. TGA data plotted alongside chemically pure brucite and hydromagnesite shows expected similarities/differences between Sample 1(mostly brucite) and Sample 2 (brucite/hydromagnesite mixture). Following treatment, dried samples observed to slowly gain mass in ambient conditions. Presumed to be hygroscopic absorption of air water vapour as effect is reversible, with similar effect observed for hydromagnesite and brucite. Etched Magnox vacuum dried for 3.5 h at 90 deg. C to test for reaction with residual water - some discoloration but no noticeable corrosion observed. Drying etched Magnox metal to observe surface effects/corrosion during drying process.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

SRNL CRP progress report [Development of Melt Processed Ceramics for Nuclear Waste Immobilization]

A multi-phase ceramic waste form is being developed at the Savannah River National Laboratory (SRNL) for treatment of secondary waste streams generated by reprocessing commercial spent nuclear. The envisioned waste stream contains a mixture of transition, alkali, alkaline earth, and lanthanide metals. Ceramic waste forms are tailored (engineered) to incorporate waste components as part of their crystal structure based on knowledge from naturally found minerals containing radioactive and non-radioactive species similar to the radionuclides of concern in wastes from fuel reprocessing. The ability to tailor ceramics to mimic naturally occurring crystals substantiates the long term stability of such crystals (ceramics) over geologic timescales of interest for nuclear waste immobilization [1]. A durable multiphase ceramic waste form tailored to incorporate all the waste components has the potential to broaden the available disposal options and thus minimize the storage and disposal costs associated with aqueous reprocessing.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Melt Processed Crystalline Ceramic Waste Forms for Advanced Nuclear Fuel Cycles: CRP T21027 1813: Processing technologies for high level waste, formulation of matrices and characterization of waste forms, Task 17208 (Final Report)

A multi-phase ceramic waste form is being developed at the Savannah River National Laboratory (SRNL) for treatment of secondary waste streams generated by reprocessing commercial spent nuclear. The envisioned waste stream contains a mixture of transition, alkali, alkaline earth, and lanthanide metals. Ceramic waste forms are tailored (engineered) to incorporate waste components as part of their crystal structure based on knowledge from naturally found minerals containing radioactive and non-radioactive species similar to the radionuclides of concern in wastes from fuel reprocessing. The ability to tailor ceramics to mimic naturally occurring crystals substantiates the long term stability of such crystals (ceramics) over geologic timescales of interest for nuclear waste immobilization [1]. A durable multi-phase ceramic waste form tailored to incorporate all the waste components has the potential to broaden the available disposal options and thus minimize the storage and disposal costs associated with aqueous reprocessing. This report summarizes results from three years of work on the IAEA Coordinated Research Project on “Processing technologies for high level waste, formulation of matrices and characterization of waste forms” (T21027), and specific task “Melt Processed Crystalline Ceramic Waste Forms for Advanced Nuclear Fuel Cycles” (17208).

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Melt Processed Crystalline Ceramic Waste Forms for Advanced Nuclear Fuel Cycles CRP T21027 1813: Processing technologies for high level waste, formulation of matrices and characterization of waste forms, Task 17208 (Final Report)

A multi-phase ceramic waste form is being developed at the Savannah River National Laboratory (SRNL) for treatment of secondary waste streams generated by reprocessing commercial spent nuclear. The envisioned waste stream contains a mixture of transition, alkali, alkaline earth, and lanthanide metals. Ceramic waste forms are tailored (engineered) to incorporate waste components as part of their crystal structure based on knowledge from naturally found minerals containing radioactive and non-radioactive species similar to the radionuclides of concern in wastes from fuel reprocessing. The ability to tailor ceramics to mimic naturally occurring crystals substantiates the long term stability of such crystals (ceramics) over geologic timescales of interest for nuclear waste immobilization. A durable multi-phase ceramic waste form tailored to incorporate all the waste components has the potential to broaden the available disposal options and thus minimize the storage and disposal costs associated with aqueous reprocessing. This report summarizes results from three years of work on the IAEA Coordinated Research Project on “Processing technologies for high level waste, formulation of matrices and characterization of waste forms” (T21027), and specific task “Melt Processed Crystalline Ceramic Waste Forms for Advanced Nuclear Fuel Cycles” (17208).

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗