ESD Test Apparatus for Soldering Irons

ESDA (Electrostatic Discharge Association) ESD STM 13.1-2000 requires frequent testing of the voltage leakage from the tip of a soldering iron and the resistance from the tip of the soldering iron to the common point ground. Without this test apparatus, the process is time-consuming and requires several wires, alligator clips, or test probes, as well as additional equipment. Soldering iron tips must be tested for electrostatic discharge risks frequently, and this typically takes a lot of time in setup and testing. This device enables the operator to execute the full test in one minute or less. This innovation is a simple apparatus that plugs into a digital multimeter (DMM) and the Common Point Ground (CPG) reference. It enables the user to perform two of the electrostatic discharge tests required in ESD STM 13.1-2000. The device consists of a small black box with two prongs sticking out of one end, two inputs on the opposite end (one of the inputs is used to connect the reference CPG to the DMM), and a metal tab on one side. Inside the box are wires, several washers of various materials, and assembly hardware (nuts and screws/bolts). The device is a passive electronic component that is plugged into a DMM. The operator sets the DMM to read voltage. The operator places the heated tip of the soldering iron onto the metal tab with a small amount of solder to ensure a complete connection. The voltage is read and recorded. The operator switches the DMM to read resistance. The operator places the heated tip of the soldering iron onto the metal tab with a small amount of solder to ensure a complete connection. The resistance is recorded. If the recorded voltage and resistance are below a number stated in ESDA ESD STM 13.1-2000, the test is considered to pass. The device includes all the necessary wiring internal to its body so the operator does not need to do any independent wiring, except for grounding. It uses a stack of high-thermal-resistance washers to minimize the heat transfer from the soldering iron to the wiring used to measure the resistance and voltages. This minimizes thermal error. The device allows very rapid execution of a test that is performed frequently.

Sancho, Jose↗

Understanding the Reliability of Solder Joints Used in Advanced Structural and Electronics Applications: Part 2 - Reliability Performance.

Whether structural or electronic, all solder joints must provide the necessary level of reliability for the application. The Part 1 report examined the effects of filler metal properties and the soldering process on joint reliability. Filler metal solderability and mechanical properties, as well as the extents of base material dissolution and interface reaction that occur during the soldering process, were shown to affect reliability performance. The continuation of this discussion is presented in this Part 2 report, which highlights those factors that directly affect solder joint reliability. There is the growth of an intermetallic compound (IMC) reaction layer at the solder/base material interface by means of solid-state diffusion processes. In terms of mechanical response by the solder joint, fatigue remains as the foremost concern for long-term performance. Thermal mechanical fatigue (TMF), a form of low-cycle fatigue (LCF), occurs when temperature cycling is combined with mismatched values of the coefficient of thermal expansion (CTE) between materials comprising the solder joint “system.” Vibration environments give rise to high-cycle fatigue (HCF) degradation. Although accelerated aging studies provide valuable empirical data, too many variants of filler metals, base materials, joint geometries, and service environments are forcing design engineers to embrace computational modeling to predict the long-term reliability of solder joints.

42 ENGINEERING↗

Rapidly solidifying Pb-free Sn-Ag-Cu-Al or Sn-Cu-Al solder

A solder alloy includes Sn, optional Ag, Cu, and Al wherein the solder alloy composition together with the solder alloy superheat temperature and rapid cooling rate from the superheat temperature are controlled to provide a dispersion of fine hard Cu—Al intermetallic particles in an as-solidified solder alloy microstructure wherein the particles are retained even after multiple solder reflow cycles often used in modern electronic assembly procedures to provide a particle strengthening to the solder joint microstructure as well as exert a grain refining effect on the solder joint microstructure, providing a strong, impact- and thermal aging-resistant solder joint that has beneficial microstructural features and is substantially devoid of Ag3Sn blades.

36 MATERIALS SCIENCE↗

Effect of Ag3Sn nanoparticles and temperature on Cu6Sn5 IMC growth in Sn-xAg/Cu solder joints

Highlights: • The number density of Ag{sub 3}Sn grains precipitated upon Cu{sub 6}Sn{sub 5}, increases with Ag content and reflow temperature (T). • Raising of wt. % of Ag in solder and lowering of T can cause an increase in grain diameter of Ag{sub 3}Sn nanoparticles. • The blockading effect of Ag{sub 3}Sn particles on Cu{sub 6}Sn{sub 5} IMC growth is more pronounced in Sn-3Ag and Sn-3.5Ag alloys. • IMC suppressing nanoparticles can be utilized for solder materials design. - Abstract: The growing importance of Pb-free Sn-xAg solders and high cost of Ag has attracted the attention of researchers to perform experiment with solders with varied content of Ag element. In this study, Sn-xAg(0,1,2,3.5) solder balls on Cu substrate have been reflowed at 250/275/300 °C for 60 s and air cooled. Finite element method has been utilized to simulate the concentration and temperature during cooling. The experimental results suggest that the Cu flux through grain boundary diffusion is the dominant mechanism for Cu{sub 6}Sn{sub 5} intermetallic compound growth in Pure Sn and Sn-1Ag solders. When the Ag content is increased, as in case of Sn-3Ag and Sn-3.5Ag alloys; the shielding effect of Ag{sub 3}Sn nanoparticles is the determinant factor for affecting the thickness of Cu{sub 6}Sn{sub 5} IMC. Both Cu influx rate and shielding effect of Ag{sub 3}Sn nanoparticles are enhanced with the raise in pre-cooled isothermal reflow temperature. Sn-1Ag solder is observed to have the thickest Cu{sub 6}Sn{sub 5} IMC.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Comparison of Extensive Thermal Cycling Effects on Microstructure Development in Micro-alloyed Sn-Ag-Cu Solder Joints

Pb-free solder alloys based on the Sn-Ag-Cu (SAC) ternary eutectic have promise for widespread adoption across assembly conditions and operating environments, but enhanced microstructural control is needed. Micro-alloying with elements such as Zn was demonstrated for promoting a preferred solidification path and joint microstructure earlier in simple (Cu/Cu) solder joints studies for different cooling rates. This beneficial behavior now has been verified in reworked ball grid array (BGA) joints, using dissimilar SAC305 (Sn-3.0Ag-0.5Cu, wt.%) solder paste. After industrial assembly, BGA components joined with Sn-3.5Ag-0.74Cu-0.21Zn solder were tested in thermal cycling (-55 C/+125 C) along with baseline SAC305 BGA joints beyond 3000 cycles with continuous failure monitoring. Weibull analysis of the results demonstrated that BGA components joined with SAC + Zn/SAC305 have less joint integrity than SAC305 joints, but their lifetime is sufficient for severe applications in consumer, defense, and avionics electronic product field environments. Failure analysis of the BGA joints revealed that cracking did not deviate from the typical top area (BGA component side) of each joint, in spite of different Ag3Sn blade content. Thus, SAC + Zn solder has not shown any advantage over SAC305 solder in these thermal cycling trials, but other characteristics of SAC + Zn solder may make it more attractive for use across the full range of harsh conditions of avionics or defense applications.

36 MATERIALS SCIENCE↗

Development of Sn-Ag-Cu-X Solders for Electronic Assembly by Micro-Alloying with Al

Of Pb-free solder choices, an array of solder alloys based on the Sn-Ag-Cu (SAC) ternary eutectic (T eut = 217°C) composition have emerged with potential for broad use, including ball grid array (BGA) joints that cool slowly. This work investigated minor substitutional additions of Al (<0.25 wt.%) to Sn-3.5Ag-0.95Cu (SAC3595) solders to promote more consistent solder joint microstructures and to avoid deleterious product phases, e.g., Ag3Sn “blades,” for BGA cooling rates, since such Al additions to SAC had already demonstrated excellent thermal aging stability. Consistent with past work, blade formation was suppressed for increased Al content (>0.05Al), but the suppression effect faded for >0.20Al. Undercooling suppression did not correlate specifically with blade suppression since it became significant at 0.10Al and increased continuously with greater Al to 0.25Al. Surprisingly, an intermediate range of Al content (0.10 wt.% to 0.20 wt.% Al) promoted formation of significant populations of 2-μm to 5-μm faceted Cu-Al particles, identified as Cu33Al17, that clustered at the top of the solder joint matrix and exhibited extraordinary hardness. Clustering of Cu33Al17 was attributed to its buoyancy, from a lower density than Sn liquid, and its early position in the nucleation sequence within the solder matrix, permitting unrestricted migration to the top interface. Joint microstructures and implications for the full nucleation sequence for these SAC + Al solder joints are discussed, along with possible benefits from the clustered particles for improved thermal cycling resistance.

36 MATERIALS SCIENCE↗

Imaging and Analysis of Void-defects in Solder Joints Formed in Reduced Gravity using High-Resolution Computed Tomography

As a part of efforts to develop an electronics repair capability for long duration space missions, techniques and materials for soldering components on a circuit board in reduced gravity must be developed. This paper presents results from testing solder joint formation in low gravity on a NASA Reduced Gravity Research Aircraft. The results presented include joints formed using eutectic tin-lead solder and one of the following fluxes: (1) a no-clean flux core, (2) a rosin flux core, and (3) a solid solder wire with external liquid no-clean flux. The solder joints are analyzed with a computed tomography (CT) technique which imaged the interior of the entire solder joint. This replaced an earlier technique that required the solder joint to be destructively ground down revealing a single plane which was subsequently analyzed. The CT analysis technique is described and results presented with implications for future testing as well as implications for the overall electronics repair effort discussed.

Easton, John W.↗

Microstructural Evaluation and Comparison of Solder Samples Processed Aboard the International Space Station

Samples from the In-Space Soldering Investigation (ISSI), conducted aboard the International Space Station (ISS), are being examined for post-solidification microstructural development and porosity distribution. In this preliminary study, the internal structures of two ISSI processed samples are compared. In one case 10cm of rosin-core solder was wrapped around a coupon wire and melted by conduction, whereas, in the other a comparable length of solder was melted directly onto the hot wire; in both cases the molten solder formed ellipsoidal blobs, a shape that was maintained during subsequent solidification. In the former case, there is clear evidence of porosity throughout the sample, and an accumulation of larger pores near the hot end that implies thermocapillary induced migration and eventual coalescence of the flux vapor bubbles. In the second context, when solder was fed onto the wire. a part of the flux constituting the solder core is introduced into and remains within the liquid solder ball, becoming entombed upon solidification. In both cases the consequential porosity, particularly at a solder/contact interface, is very undesirable. In addition to compromising the desired electrical and thermal conductivity, it promotes mechanical failure.

Grugel, R. N.↗

Long-term reliability of hand-soldering M55365 Ta capacitors

This is a continuation of the report “Effects of Hand Soldering MIL-PRF-55365 Tantalum Capacitors,” which discusses the parametric effects of convection reflow soldering, JPL standard hand soldering, and optimized hand soldering on solid tantalum capacitors. The current focus is determining the long-term reliability effects of the various soldering techniques. Unfortunately, the 100-piece sample size chosen for the highly accelerated life tests was too small to reliably determine the effects of the different soldering techniques on the lifespan of the parts. In hindsight, this likely could have been predicted based on the large alphas and small betas of the Weibull failure distributions discovered during the scouting trials. Now that the effects of inadequate sample size are better understood, an opportunity exists to not only discover whether there are real differences in the reliability associated with the various soldering techniques, but also the potential to discover the voltage acceleration model and the temperature acceleration effect for these capacitors. It is recommended that the testing be repeated with a more appropriate sample size to capture this useful information.

Spence, Penelope↗

Effect of Preconditioning on Post-Soldering Failures in Tantalum Capacitors

Soldering have a strong effect on performance and reliability of most surface mount technology components, including tantalum capacitors. High quality tantalum capacitors are likely the only type of components where soldering simulation is the first step during screening. Nevertheless, post-soldering failures of tantalum capacitors do happen and require additional analysis. Popcorning is a well-known effect in plastic encapsulated microcircuits (PEM) and it occurs also in chip tantalum capacitors. The sensitivity of parts to the presence of moisture during soldering is characterized by the moisture sensitivity level (MSL); however, contrary to PEMs, there is no standard procedure for establishing MSL for tantalum capacitors, and standard J-STD-020 is applicable partially only. In this work, the effect of absorbed moisture on soldering related degradation and failures in tantalum capacitors have been studied using 22 types of polymer and 11 types of MnO2 cathodes tantalum capacitors including single and multianode parts. The amount of moisture released during soldering has been estimated by measurements of mass and capacitance variations. Results show that moisture uptake in similar parts is approximately two times greater in polymer than in MnO2 capacitors. Cracking of the case and degradation of parameters can occur in both types of parts, but MnO2 capacitors are much more susceptible to catastrophic short circuit failures and their ignition is possible during the first power-on cycle. This type of failure in MnO2 capacitors is lot-related, can occur even at derated voltages and relatively low levels of moisture sorption corresponding to room conditions. Baking before soldering is an effective measure to prevent failures even in lots susceptible to popcorning damage. Recommendations for testing to establish MSL and for baking to reduce the probability of failures are suggested.

tantalum polymer capacitors↗

Interconnection of thermal parameters, microstructure and mechanical properties in directionally solidified Sn–Sb lead-free solder alloys

Considerable effort is being made to develop lead-free solders for assembling in environmental-conscious electronics, due to the inherent toxicity of Pb. The search for substitute alloys of Pb–Sn solders has increased in order to comply with different soldering purposes. The solder must not only meet the expected levels of electrical performance but may also have appropriate mechanical strength, with the absence of cracks in the solder joints. The Sn–Sb alloy system has a range of compositions that can be potentially included in the class of high temperature solders. This study aims to establish interrelations of solidification thermal parameters, microstructure and mechanical properties of Sn–Sb alloys (2 wt.%Sb and 5.5 wt.%Sb) samples, which were directionally solidified under cooling rates similar to those of reflow procedures in industrial practice. A complete high-cooling rate cellular growth is shown to be associated with the Sn–2.0 wt.%Sb alloy and a reverse dendrite-to-cell transition is observed for the Sn–5.5 wt.%Sb alloy. Strength and ductility of the Sn–2.0 wt.%Sb alloy are shown not to be affected by the cellular spacing. On the other hand, a considerable variation in these properties is associated with the cellular region of the Sn–5.5 wt.%Sb alloy casting. - Graphical abstract: Display Omitted - Highlights: • The microstructure of the Sn–2 wt.%Sb alloy is characterized by high-cooling rates cells. • Reverse dendrite > cell transition occurs for Sn–5.5 wt.%Sb alloy: cells prevail for cooling rates > 1.2 K/s. • Sn–5.5 wt.%Sb alloy: the dendritic region occurs for cooling rates < 0.9 K/s. • Sn–5.5 wt.%Sb alloy: tensile properties are improved with decreasing cellular spacing.

36 MATERIALS SCIENCE↗

Effect of gamma radiation on micromechanical hardness of lead-free solder joint

Lead-free solders are important material in nano and microelectronic surface mounting technology for various applications in bio medicine, environmental monitoring, spacecraft and satellite instrumentation. Nevertheless solder joint in radiation environment needs higher reliability and resistance to any damage caused by ionizing radiations. In this study a lead-free 99.0Sn0.3Ag0.7Cu wt.% (SAC) solder joint was developed and subjected to various doses of gamma radiation to investigate the effects of the ionizing radiation to micromechanical hardness of the solder. Averaged hardness of the SAC joint was obtained from nanoindentation test. The results show a relationship between hardness values of indentations and the increment of radiation dose. Highest mean hardness, 0.2290 ± 0.0270 GPa was calculated on solder joint which was exposed to 5 Gray dose of gamma radiation. This value indicates possible radiation hardening effect on irradiated solder. The hardness gradually decreased to 0.1933 ± 0.0210 GPa and 0.1631 ± 0.0173 GPa when exposed to doses 50 and 500 gray respectively. These values are also lower than the hardness of non irradiated sample which was calculated as 0.2084 ± 0.0.3633 GPa indicating possible radiation damage and needs further related atomic dislocation study.

36 MATERIALS SCIENCE↗

Dark Lock-in Thermography Identifies Solder Bond Failure as the Root Cause of Series Resistance Increase in Fielded Solar Modules

Correlating the electrical performance of photovoltaic modules to the spatially resolved photoluminescence, electroluminescence, and dark lock-in thermography (DLIT) images is an important long-term goal for developing solar cell technology. These images offer highly sophisticated and detailed information about the spatial distribution and (if imaged at successive time intervals) temporal degradation of local series and shunt resistances. There have been extensive studies to correlate these imaging techniques to local characteristics at the cell level. However, it has been difficult to extract and quantify module-level information from the techniques. In this study, we interpret module current-voltage (I-V) measurements along with corresponding DLIT images within a module-scale simulation framework, demonstrating that series resistance degradation of the module I-V characteristics, in this case, can be attributed to solder bond failures. Our simulations highlight how current crowding associated with a failed solder joint (or a section of the solder pad) translates to the characteristic point-like (asymmetric doublet) heating pattern in neighboring solder joints (or the neighboring regions of the solder pad). Overall, the correlation between series resistance and solder joint degradation could inform expedited diagnosis of field degradation of solar modules.

42 ENGINEERING↗

An analysis of the pull strength behaviors of fine-pitch, flip chip solder interconnections using a Au-Pt-Pd thick film conductor on Low-Temperature, Co-fired Ceramic (LTCC) substrates.

The assembly of the BDYE detector requires the attachment of sixteen silicon (Si) processor dice (eight on the top side; eight on the bottom side) onto a low-temperature, co-fired ceramic (LTCC) substrate using 63Sn-37Pb (wt.%, Sn-Pb) in a double-reflow soldering process (nitrogen). There are 132 solder joints per die. The bond pads were gold-platinum-palladium (71Au-26Pt-3Pd, wt.%) thick film layers fired onto the LTCC in a post-process sequence. The pull strength and failure modes provided the quality metrics for the Sn-Pb solder joints. Pull strengths were measured in both the as-fabricated condition and after exposure to thermal cycling (-55/125 C; 15 min hold times; 20 cycles). Extremely low pull strengths--referred to as the low pull strength phenomenon--were observed intermittently throughout the product build, resulting in added program costs, schedule delays, and a long-term reliability concern for the detector. There was no statistically significant correlation between the low pull strength phenomenon and (1) the LTCC 'sub-floor' lot; (2) grit blasting the LTCC surfaces prior to the post-process steps; (3) the post-process parameters; (4) the conductor pad height (thickness); (5) the dice soldering assembly sequence; or (5) the dice pull test sequence. Formation of an intermetallic compound (IMC)/LTCC interface caused by thick film consumption during either the soldering process or by solid-state IMC formation was not directly responsible for the low-strength phenomenon. Metallographic cross sections of solder joints from dice that exhibited the low pull strength behavior, revealed the presence of a reaction layer resulting from an interaction between Sn from the molten Sn-Pb and the glassy phase at the TKN/LTCC interface. The thick film porosity did not contribute, explicitly, to the occurrence of reaction layer. Rather, the process of printing the very thin conductor pads was too sensitive to minor thixotropic changes to ink, which resulted in inconsistent proportions of metal and glassy phase particles present during the subsequent firing process. The consequences were subtle, intermittent changes to the thick film microstructure that gave rise to the reaction layer and, thus, the low pull strength phenomenon. A mitigation strategy would be the use of physical vapor deposition (PVD) techniques to create thin film bond pads; this is multi-chip module, deposited (MCM-D) technology.

36 MATERIALS SCIENCE↗

Investigation of Solder Cracking Problems on Printed Circuit Boards

A Solder Committee designated to investigate a solder cracking phenomena occurring on the SATURN electrical/electronic hardware found the cause to be induced stress in the soldered connections rather than faulty soldering techniques. The design of the printed circuit (PC) board assemblies did not allow for thermal expansion of the boards that occurred during normal operation. The difference between the thermal expansion properties of the boards and component lead materials caused stress and cracking in the soldered connections. The failure mechanism and various PC boards component mounting configurations are examined in this report. Effective rework techniques using flanged tubelets, copper tubelets, and soft copper wiring are detailed. Future design considerations to provide adequate strain relief in mounting configurations are included to ensure successful solder terminations.

CIRCUIT BOARD↗

Evaluation of advanced microelectronic fluxless solder-bump contacts for hybrid microcircuits

Technology for interconnecting monolithic integrated circuit chips with other components is investigated. The advantages and disadvantages of the current flip-chip approach as compared to other interconnection methods are outlined. A fluxless solder-bump contact technology is evaluated. Multiple solder-bump contacts were formed on silicon integrated circuit chips. The solder-bumps, comprised of a rigid nickel under layer and a compliant solder overlayer, were electroformed onto gold device pads with the aid of thick dry film photomasks. Different solder alloys and the use of conductive epoxy for bonding were explored. Fluxless solder-bump bond quality and reliability were evaluated by measuring the effects of centrifuge, thermal cycling, and high temperature storage on bond visual characteristics, bond electrical continuity, and bond shear tests. The applicability and suitability of this technology for hybrid microelectronic packaging is discussed.

Mandal, R. P.↗

Effects of hand soldering MIL-PRF 55365 tantalum capacitors

Different values of MIL-PRF-55365 tantalum capacitors were subjected to three different types of soldering conditions— Convection Reflow, JPL Standard Hand Soldering, and Optimized Hand Soldering. The electrical parameters for a large number of capacitors of each value were measured before and after thermal soldering stress. The results indicate that tantalum capacitors subjected to convection reflow conditions experience detectable changes in electrical parameters; capacitors subjected to hand solder conditions show reduced changes in electrical parameters when compared to the reflow samples. Optimized hand solder conditions are shown to have a minimal effect on electrical parameters.

Sheldon, Douglas↗

An Accelerated Method for Testing Soldering Tendency of Core Pins

An accelerated method for testing die soldering has been developed. High intensity ultrasonic vibrations has been used to simulate the die casting conditions such as high pressure and high impingement speed of molten metal on the pin. Soldering tendency of steels and coated pins has been examined. The results indicate that in the low carbon steel/Al system, the onset of soldering is 60 times faster with ultrasonic vibration than that without ultrasonic vibration. In the H13/A380 system, the onset of soldering reaction is accelerated to 30-60 times. Coating significantly reduces the soldering tendency of the core pins.

36 MATERIALS SCIENCE↗