At least 73 records · Page 4

Material characterization of seven photovoltaic backsheets using seven accelerated test conditions

A variety of polymeric backsheet materials can be found in fielded photovoltaic (PV) modules, mostly based on fluoropolymer and polyethylene terephthalate (PET) materials. Cost reduction and sustainability considerations drive the recent development of alternative backsheet materials and designs [1]. In some fielded PV installations, polymeric materials are susceptible to environmental degradation in the form of backsheet cracking. To prevent backsheet degradation that can result in a module failure, thorough laboratory reliability testing is needed. In this report we studied the durability of seven commercial and experimental PV backsheets through accelerated stress testing using seven photolytic, hygrometric, and custom tests with the goal to understand if novel fluoropolymer-free backsheets are sufficiently environmentally durable to be commercialized. We divided the mechanisms observed during aging into two categories: core degradation and surface degradation. Although core degradation due to hydrolysis was observed in all commercial PET-, and polyamide (PA)-based backsheets aged with 85 degrees C/85% relative humidity, this test is unlikely to be field relevant. Photo-oxidative reactions on the exposed surface during UV weathering affected all seven backsheets regardless of the outer layer polymer material and additives. This degradation was limited to the outermost micrometers of the surface, except for backsheets containing PA-12, which resulted in surface cracking. A custom test combining UV with water spray caused the most severe backsheet degradation, including surface erosion and loss of insulating properties in polyolefin (PO)- and PA-based backsheets. This highlights the importance of combined accelerated stress testing to screen for complex backsheet degradation mechanisms. We also showed that, with material and design optimization, coextruded experimental PO-based backsheets have the potential to be a durable alternative to commercial PET- and fluoropolymer-based PV backsheets.

14 SOLAR ENERGY↗

Improved analysis of arabinoxylan-bound hydroxycinnamate conjugates in grass cell walls

Background: Arabinoxylan in grass cell walls is acylated to varying extents by ferulate and p-coumarate at the 5-hydroxy position of arabinosyl residues branching off the xylan backbone. Some of these hydroxycinnamate units may then become involved in cell wall radical coupling reactions, resulting in ether and other linkages amongst themselves or to monolignols or oligolignols, thereby crosslinking arabinoxylan chains with each other and/or with lignin polymers. This crosslinking is assumed to increase the strength of the cell wall, and impedes the utilization of grass biomass in natural and industrial processes. A method for quantifying the degree of acylation in various grass tissues is, therefore, essential. We sought to reduce the incidence of hydroxycinnamate ester hydrolysis in our recently introduced method by utilizing more anhydrous conditions. Results: The improved methanolysis method minimizes the undesirable ester-cleavage of arabinose from ferulate and p-coumarate esters, and from diferulate dehydrodimers, and produces more methanolysis vs. hydrolysis of xylan-arabinosides, improving the yields of the desired feruloylated and p-coumaroylated methyl arabinosides and their diferulate analogs. Free ferulate and p-coumarate produced by ester-cleavage were reduced by 78% and 68%, respectively, and 21% and 39% more feruloyl and p-coumaroyl methyl arabinosides were detected in the more anhydrous method. The new protocol resulted in an estimated 56% less combined diferulate isomers in which only one acylated arabinosyl unit remained, and 170% more combined diferulate isomers conjugated to two arabinosyl units. Conclusions: Overall, the new protocol for mild acidolysis of grass cell walls is both recovering more ferulate- and p-coumarate-arabinose conjugates from the arabinoxylan and cleaving less of them down to free ferulic acid, p-coumaric acid, and dehydrodiferulates with just one arabinosyl ester. This cleaner method, especially when coupled with the orthogonal method for measuring monolignol hydroxycinnamate conjugates that have been incorporated into lignin, provides an enhanced tool to measure the extent of crosslinking in grass arabinoxylan chains, assisting in identification of useful grasses for biomass applications.

09 BIOMASS FUELS↗

Production and Evaluation of Fluorophore-Doped Polymer Substrates to Screen for Plastic-Degrading Enzymes

Fast and sensitive analytical methods are the key to efficient screening of plastic-degrading enzymes. Here, we present a streamlined and affordable approach to assess the enzymatic deconstruction of insoluble synthetic polymers by blending them with a fluorescent dye, rhodamine 6G, and we evaluate this screening method using poly(ethylene terephthalate) (PET) as a model material. Our results indicate that enzymatic depolymerization of the rhodamine-doped PET can be observed in a high-throughput fashion by following release of the fluorophore. The fluorescence data obtained during the hydrolysis of rhodamine-doped PET by 14 PET hydrolases, produced with a robotic platform, correlated with the quantitative chromatographic analysis of PET degradation products. Remarkably, the use of the rhodamine-loaded PET substrate resulted in negligibly low background signals even when detecting PETase activity in crude cell lysates, suggesting suitability for screening of a wide variety of samples. Encouraged by these results, we next produced a selection of polyethylene- and nylon-based materials loaded with rhodamine 6G. While rapid leaching of fluorophore observed with nylon substrates limits the utility of the method for detecting nylonase activity, the rhodamine-loaded polyethylene showed promising performance in passive diffusion tests, indicating that this latter substrate may be used to screen for polyolefin-degrading enzymes.

09 BIOMASS FUELS↗

A DNA packaging motor inchworms along one strand allowing it to adapt to alternative double-helical structures

Abstract Ring ATPases that translocate disordered polymers possess lock-washer architectures that they impose on their substrates during transport via a hand-over-hand mechanism. Here, we investigate the operation of ring motors that transport ordered, helical substrates, such as the bacteriophage ϕ29 dsDNA packaging motor. This pentameric motor alternates between an ATP loading dwell and a hydrolysis burst wherein it packages one turn of DNA in four steps. When challenged with DNA-RNA hybrids and dsRNA, the motor matches its burst to the shorter helical pitches, keeping three power strokes invariant while shortening the fourth. Intermittently, the motor loses grip on the RNA-containing substrates, indicating that it makes optimal load-bearing contacts with dsDNA. To rationalize these observations, we propose a helical inchworm translocation mechanism in which, during each cycle, the motor increasingly adopts a lock-washer structure during the ATP loading dwell and successively regains its planar form with each power stroke during the burst.

59 BASIC BIOLOGICAL SCIENCES↗

Role of Amorphous Chains in Nanoplastic Formation from Semicrystalline Polymers

Semicrystalline polymers, e.g., polyethylene terephthalate (PET), release micro- (100 nm to 1 mm) and nanoplastics (up to 100 nm) [MNPL] when they are degraded under quiescent conditions. However, the exact molecular mechanisms leading to material fragmentation into MNPL are unknown. Here, we monitor the evolution of chain molecular weight and the MNPL production kinetics during hydrolysis of PET pellets. We find that only ~0.6% of the amorphous phase ester bonds are hydrolyzed at the onset of MNPL release. Then, by combining a random scission model with measured amorphous spacings, we estimate that only ~15% of the stress transmitters in the amorphous phase, namely, bridges and entangled loops, have failed by this point. Thus, spontaneous fragmentation of the semicrystalline nanostructure occurs despite significant intercrystalline connectivity. We resolve this apparent contradiction by proposing that fragmentation can only occur when progressive tie-chain scission causes the material to undergo the ductile/brittle transition. Mechanistically, we speculate that the internal stresses responsible for material fragmentation are caused by processing (i.e., residual stresses) and/or sample densification induced by chemi-crystallization. We discuss additional factors that may affect our analysis and thus require further investigation, such as skin-core effects, preferential degradation of stress transmitters and/or recrystallization processes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Assembly of Metalloporphyrin Peptoids into Crystalline Nanomaterials as a Multifunctional System for Biomimetic Catalysis and Sensing

While natural enzymes excel at catalysis and sensing, they often suffer from high cost and low stability in applications outside living systems. Among tremendous efforts made toward the design and synthesis of catalytic biomimetic materials, the approach of using crystalline nanomaterials assembled from sequence-defined polymers has emerged as a promising strategy. Herein, we report the assembly of metalloporphyrin peptoids into crystalline nanomaterials as a multifunctional system for biomimetic catalysis and sensing. The precise spatial positioning of covalently attached porphyrins within crystalline peptoid nanomaterials enables the mimicry of several enzyme active sites, including phosphotriesterase and horseradish peroxidase, for efficient catalytic hydrolysis and oxidation reactions. Additionally, the high programmability of these peptoid crystalline materials enables the creation and tuning of the active site microenvironment for enhanced catalytic activity. We further demonstrate the integration of responsive organic dyes into catalytic peptoid assemblies to achieve both detection and degradation of chemical warfare agent (CWA) mimics, even in the vapor phase. In conclusion, we expect this multifunctional system to provide tremendous opportunities in biomimetic catalysis and sensing, including the detoxification and detection of CWAs.

Catalysts↗

Mechanistic insights into the colloidal assembly of mesoporous silica using in-operando cross-scale X-ray scattering and spectroscopic measurements

Advancing a mechanistic understanding of the colloidal to solid-phase transformations of silica allows us to tune these meso-scale structures. In this study, we probe the structural transformations associated with the formation of mesoporous silica particles, SBA-15 using in-operando Small Angle X-ray Scattering (SAXS) and Grazing Incidence-Small Angle X-ray Scattering (GI-SAXS). The chemical transformations associated with the hydrolysis and condensation of silica particles is investigated using Attenuated Total Reflection – Fourier Transform Infrared Spectroscopy (ATR-FTIR) measurements. Fast polymerization of Si-O-Si species to form mesoporous silica is noted when SBA-15 is synthesized in the presence of nitrate salts, due to the “salting-in” effect or enhanced solubility of polymers. However, aging the silica particles resulted in plate-like morphologies in the absence of the nitrate salt and spherical morphologies in the presence of nitrate salt. Early onset of nucleation of silica particles in the presence of nitrate salts was captured using GI-SAXS measurements. These studies show that the rational basis for developing new synthesis routes for accelerated kinetics or specific meso-scale structures can be informed by detailed characterization of the evolution in chemistry and meso-scale structure of these materials.

36 MATERIALS SCIENCE↗

A Combined Thermochemical and Microbial Process for Recycling Polylactic Acid Polymer to Optically Pure L-Lactic Acid for Reuse

Polylactic acid polymer (PLA) produced from renewable resources can be recycled at the end of life to constituent monomer, optically pure lactic acid (LA), by a combination of chemical and biological processes. Efficient application of this closed loop of LA-PLA plastics-LA can minimize accumulation of plastics waste that pollute land and oceans. Temperature-dependent hydrolysis of PLA in water to LA follows apparent first order decay kinetics after a short lag. A modified Gompertz equation can explain the overall hydrolysis process. Alkali increased the rate of hydrolysis of PLA and reduced the length of lag period compared to water alone. The stoichiometry of base added to LA released was 1.0. The highest lactic acid yield was 0.95 g g -1 of PLA. D-LA in the syrup obtained after hydrolysis of PLA-plastics was removed using an engineered Escherichia coli to produce a L-LA syrup with an optical purity ≥ 99%. Here, these results show that thermochemical hydrolysis of PLA-based plastics to LA with optimum amount of base followed by bio-based purification to L-LA is an effective method of recycling PLA-plastics for reuse.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Sourcing thermotolerant poly(ethylene terephthalate) hydrolase scaffolds from natural diversity

Enzymatic deconstruction of poly(ethylene terephthalate) (PET) is under intense investigation, given the ability of hydrolase enzymes to depolymerize PET to its constituent monomers near the polymer glass transition temperature. To date, reported PET hydrolases have been sourced from a relatively narrow sequence space. Here, we identify additional PET-active biocatalysts from natural diversity by using bioinformatics and machine learning to mine 74 putative thermotolerant PET hydrolases. We successfully express, purify, and assay 51 enzymes from seven distinct phylogenetic groups; observing PET hydrolysis activity on amorphous PET film from 37 enzymes in reactions spanning pH from 4.5–9.0 and temperatures from 30–70 °C. We conduct PET hydrolysis time-course reactions with the best-performing enzymes, where we observe differences in substrate selectivity as function of PET morphology. We employed X-ray crystallography and AlphaFold to examine the enzyme architectures of all 74 candidates, revealing protein folds and accessory domains not previously associated with PET deconstruction. Overall, this study expands the number and diversity of thermotolerant scaffolds for enzymatic PET deconstruction.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Dihydroxyterephthalate—A Trojan Horse PET Counit for Facile Chemical Recycling

Abstract Here, low‐energy poly(ethylene terephthalate) (PET) chemical recycling in water: PET copolymers with diethyl 2,5‐dihydroxyterephthalate (DHTE) undergo selective hydrolysis at DHTE sites, autocatalyzed by neighboring group participation, is demonstrated. Liberated oligomeric subchains further hydrolyze until only small molecules remain. Poly(ethylene terephthalate‐ stat ‐2,5‐dihydroxyterephthalate) copolymers were synthesized via melt polycondensation and then hydrolyzed in 150–200 °C water with 0–1 wt% ZnCl 2 , or alternatively in simulated sea water. Degradation progress follows pseudo‐first order kinetics. With increasing DHTE loading, the rate constant increases monotonically while the thermal activation barrier decreases. The depolymerization products are ethylene glycol, terephthalic acid, 2,5‐dihydroxyterephthalic acid, and bis(2‐hydroxyethyl) terephthalate dimer, which could be used to regenerate virgin polymer. Composition‐optimized copolymers show a decrease of nearly 50% in the Arrhenius activation energy, suggesting a 6‐order reduction in depolymerization time under ambient conditions compared to that of PET homopolymer. This study provides new insight to the design of polymers for end‐of‐life while maintaining key properties like service temperature and mechanical properties. Moreover, this chemical recycling procedure is more environmentally friendly compared to traditional approaches since water is the only needed material, which is green, sustainable, and cheap.

36 MATERIALS SCIENCE↗

Bottlebrush Block Copolymer Thin Films

The self-assembly of block copolymers (BCPs) in thin films is governed by interfacial interactions (enthalpy) between the blocks and interfaces (at both the substrate and the surface). Advantage can also be taken of entropy to control the polymer orientation. Here, we synthesized a series of bottlebrush block copolymers (BBCPs), with deuterated polystyrene (DPS) as the core block and poly­(solketal acrylate) (PSA) as the corona block, where the backbone length (N BB) and grafting densities (GDs) were varied. The hydrophobic PSA block was converted to a hydrophilic poly­(glyceryl acrylate) (PGA) block by solid-state hydrolysis, bringing the BBCP from a disordered state into an ordered state with a lamellar microdomain morphology. The orientation of the morphology as a function of distance from the interfaces was systematically investigated by atomic force microscopy (AFM), interference microscopy, grazing-incidence small-angle X-ray scattering (GISAXS), and grazing-incidence small angle neutron scattering (GISANS). For N BB = 1 (diblock BCP), a mixed lamellar orientation was found. For N BB = 5 (star-like BBCP), a vertical orientation of the lamellar microdomains was found dominantly at the interfaces that propagated into the bulk of the film due to the entropic penalty associated with constraints on the junction points. Increasing the N BB to 50 (rod-like BBCP) and 100 (worm-like BBCP) yielded a random orientation, as the side chains became overcrowded when aligned in the same direction. By reducing the grafting density (GD) of a N BB = 50 BBCP from 100% to 75% and 50% by the incorporation of spacers into the backbone, the steric hindrance of side chains is reduced markedly, facilitating a vertical orientation of the lamellar microdomains. However, the vertical orientation becomes more random within the bulk of the thin film for different BBCP architectures. By modifying the substrate with a layer of PS, the preferential interactions between the core block of the BBCP and the interfaces induce a reconfiguration of the BBCP, drawing the core block out to contact substrate directly driven by enthalpy. Under these conditions, N BB = 5 showed a predominantly parallel orientation of the lamellar microdomains with the corona block minimizing contact with the substrate. Higher N BB values of 50 and 100 showed a more random orientation of the lamellar microdomains at different depths on the PS-modified substrate. Overall, thin-film morphology was regulated by tuning the configuration of the BBCP, varying the entropic contribution to the microdomain orientation.

Chen, Zhan↗

Degradation Studies of Silicone Rubbers in Direct Contact with Corrosive Solids Under Compression

Silicone elastomers are polymer materials widely used within the complex, serving as cushions, adhesives, binders, and potting compounds. Excellent high-temperature resistance combined with low-temperature flexibility, high resistance to chemicals and long-term age-related stability, make silicones first-choice materials in many application areas. However, the siloxane bonds comprising the backbone of silicone elastomers are susceptible to hydrolysis when catalytic amounts of acid or base are present. Hydrolysis is a form of degradation that results in chain-cleavage and rearrangement reactions, which can manifest in changes to the physical response and mechanical properties of the elastomer. This task aims to assess and quantify the extent of degradation and/or corrosion of silicone elastomer materials when placed in direct compressive contact with an Arrhenius base under varying environments (oxidative/nonoxidative, relative humidity, temperature, time, etc.).

36 MATERIALS SCIENCE↗

Identification and characterization of substrate- and product-selective nylon hydrolases

Enzymes can rapidly and selectively hydrolyze diverse natural and anthropogenic polymers, but few have been shown to hydrolyze synthetic polyamides. Here, in this work, we synthesized and characterized a panel of 95 enzymes from the N-terminal nucleophile hydrolase superfamily with 30%–50% pairwise amino acid identity. We found that nearly 40% of the enzymes had substantial nylon hydrolase activity, but there was no relationship between phylogeny and activity, nor any evidence of prior evolutionary selection for nylon hydrolysis. Several newly identified hydrolases showed substrate selectivity, generating up to 20-fold higher product titers with nylon-6,6 versus nylon-6. However, the yield was still less than 1%, necessitating further optimization before potential applications. Finally, we determined the crystal structure and oligomerization state of a nylon-6,6-selective hydrolase to elucidate structural factors that could affect activity and selectivity. These new enzymes provide insights into nylon hydrolase evolution and opportunities for analysis and engineering of improved hydrolases.

nylon↗

Multiscale Modeling and Experimental Insights into High-Temperature Soil Biodegradation Dynamics of Semi-Crystalline Poly(Lactic Acid) Nonwoven Fabrics

This study investigates the biodegradation of semi-crystalline poly(lactic acid) (PLA) nonwovens (NWs) in soil at 58 °C using both experimental and mathematical modeling approaches. The model utilizes a system of parabolic diffusion-reaction partial differential equations (PDEs) to elucidate chemical transformations over time and in space. It accounts for phenomena such as the diffusion of water and lactic acid monomers through the polymer matrix and into the surrounding soil, along with their microbial breakdown. It also accounts for the initial PLA crystallinity and predicts its evolution in time. The model is solved numerically for a single filament, and the results were used to shed light on PLA NW transformations observed in soil over a 180-day incubation period. Various characterization techniques, including scanning electron microscopy (SEM), differential scanning calorimetry (DSC), and Raman spectroscopy, were employed to assess morphological changes, crystallinity, and molecular changes in the NWs throughout the experiment. By comparing the experimental data with the model predictions, the hydrolysis rate coefficient was found to be 3.37 × 10 -7 s -1 , while the rate of microbial degradation of lactic acid monomers was faster, of the order of 9.63 × 10 -7 s -1 . The findings highlight the significant role of crystallinity in the biodegradation process. The PLA degradation ceases when no amorphous material remains, and the crystallinity reaches 0.8, as observed in the experiments by day 120. Furthermore, this research contributes to a deeper understanding of PLA biodegradation dynamics and offers insights for effectively managing biodegradable materials in environmental settings.

Diffusion−reaction modeling↗

Janus bottlebrush compatibilizers

Bottlebrush random copolymers (BRCPs), consisting of a random distribution of two homopolymer chains along a backbone, can segregate to the interface between two immiscible homopolymers. BRCPs undergo a reconfiguration, where each block segregates to one of the homopolymer phases, adopting a Janus-type structure, reducing the interfacial tension and promoting adhesion between the two homopolymers, thereby serving as a Janus bottlebrush copolymer (JBCP) compatibilizer. Here, we synthesized a series of JBCPs by copolymerizing deuterated or hydrogenated polystyrene (DPS/PS) and poly(tert-butyl acrylate) (PtBA) macromonomers using ruthenium benzylidene-initiated ring-opening metathesis polymerization (ROMP). Subsequent acid-catalyzed hydrolysis converted the PtBA brushes to poly(acrylic acid) (PAA). The JBCPs were then placed at the interface between DPS/PS homopolymers and poly(2-vinyl pyridine) (P2VP) homopolymers, where the degree of polymerization of the backbone (N BB ) and the grafting density (GD) of the JBCPs were varied. Neutron reflectivity (NR) was used to determine the interfacial width and segmental density distributions (including PS homopolymer, PS block, PAA block and P2VP homopolymer) across the polymer-polymer interface. Our findings indicate that the star-like JBCP with N BB = 6 produces the largest interfacial broadening. Increasing N BB to 100 (rod-like shape) and 250 (worm-like shape) reduced the interfacial broadening due to a decrease in the interactions between blocks and homopolymers by stretching of blocks. Decreasing the GD from 100% to 80% at N BB = 100 caused an increase the interfacial width, yet further decreasing the GD to 50% and 20% reduced the interfacial width, as 80% of GD may efficiently increase the flexibility of blocks and promote interactions between homopolymers, while maintaining relatively high number of blocks attached to one molecule. The interfacial conformation of JBCPs was further translated into compatibilization efficiency. Thin film morphology studies showed that only the lower N BB values (N BB = 6 and N BB = 24) and the 80% GD of N BB = 100 had bicontinuous morphologies, due to a sufficient binding energy that arrested phase separation, supported by mechanical testing using asymmetric double cantilever beam (ADCB) tests. These provide fundamental insights into the assembly behavior of JBCPs compatibilizers at homopolymer interfaces, opening strategies for the design of new BCP compatibilizers.

36 MATERIALS SCIENCE↗

Fundamental Studies of Bifunctional Catalysts for Tandem Reactions

During the past few years of our funding from DOE Basic Energy Sciences, we have focused on the catalytic conversion of biomass-derived 5-hydroxymethyl furfural (HMF) as a platform molecule for sustainable synthesis of value-added chemicals. The combination of the diene and aldehyde functionalities in HMF enables catalytic production of acetalized HMF derivatives with diol or epoxy reactants to allow reversible synthesis of norcantharimide derivatives upon Diels-Alder reaction with maleimides. Whereas the electron-withdrawing nature of aldehyde group inhibits the reactivity of diene group in HMF to undergo Diels-Alder reactions with dienophiles, by converting the aldehyde group in HMF to an electron-donating hydroxyl group, HMF can append maleimide-based chemicals through Diels-Alder coupling. Acetalization of HMF not only produces an electron-rich diene for Diels-Alder reaction, but it also alters the reversibility of acetal formation and thereby allows for the controlled release of chemicals by hydrolysis. Therefore, we synthesized various norcantharimide derivatives from biomass-derived HMF by acetalization over an acid catalyst, Amberlyst-15, followed by Diels-Alder reaction with maleimide. The norcantharimides release the starting materials by retro Diels-Alder reaction that is triggered by acetal hydrolysis under acidic (≤pH 3) conditions. In subsequent work, we explored the synthesis and properties of functional polyurethanes and polyesters with tunable properties from biomass-derived (HMF)-Acetone-HMF (HAH) monomers. HAH can be selectively hydrogenated over Cu and Ru catalysts to produce partially-hydrogenated HAH (PHAH) and fully-hydrogenated HAH (FHAH). HAH contains functional groups, including hydroxyl, furan, enone, and ketone functionalities, that can be exploited to further tune the polymer properties. The π-electron conjugation between the enone and furan groups in HAH monomer stabilizes the furan group to prevent the uncontrolled degradation of furans during reactions, such as etherification. Therefore, HAH is a renewable monomer that can be used to synthesize polymers, having high molecular weight, symmetric functionalities, an inexpensive production price, and being derived from renewable resources without competition with food resources. We demonstrated the synthesis of functional polyurethanes and a renewable polyester from HAH-derived monomers, and 4,4’-methylenebis(phenyl isocyanate) (MDI). We showed that it is essential to be able to selective hydrogenate C=C double bonds in HAH to be able to achieve effective Diels Alder reactions of the furan ring. Therefore, we studied the hydrogenation at temperatures from 313 – 393 K of HAH over Pd, Ru, and Cu based catalysts. HAH was selectively hydrogenated to produce partially-hydrogenated monomers (PHAH) over Cu and Ru catalysts and to fully-hydrogenated HAH monomers (FHAH) over the Ru catalyst. Pd based catalysts yielded a mixture of partially and fully hydrogenated monomers. Reaction kinetics models were employed to quantify the kinetic behavior for hydrogenation over Ru, Cu, and Pd catalysts. A 5-step pathway exhibited over Pd and Ru catalysts consists of both series and parallel reaction steps, where HAH is both converted to fully hydrogenated products sequentially via series reactions of partially hydrogenated intermediates, as well as converted directly in parallel reactions to form the fully hydrogenated products. In contrast, a 3-step pathway over the Cu catalyst consists only of the consecutive reaction steps, where the final product was formed via series reactions of intermediate products. Additionally, reaction over the Cu catalyst did not hydrogenate the furan rings of the HAH molecule and yielded a different final product than those hydrogenation over Pd and Ru catalysts. Using the results from our detailed reaction kinetics studies, we developed universal conditions for the maximum production of the various hydrogenated products for both batch and plug flow systems. In subsequent work, we employed reaction schemes to optimize the yields of products from selective hydrogenations of HAH in isopropanol solvent and in the presence of liquid water. Reaction schemes consisting of 7, 9, and 11 steps were examined to describe the rates of formation of the observed products and reaction intermediates for hydrogenation of HAH over Ru and Pd catalysts, and a 3-step scheme was studied over Cu catalysts. Rate constants and activation energies were calculated using these reaction schemes, and we then apply these reaction schemes to explore the effects of water addition on the hydrogenation pathways. The effects of water addition to isopropanol (IPA) solvents on the hydrogenation of HAH were markedly different over Pd, Ru, and Cu catalysts. Over the Pd catalyst, the addition of water to IPA increased hydrogenation rates and promoted hydrogenation of furan rings. The addition of water to IPA yielded significant carbon losses over the Ru catalyst, and slowed hydrogenation steps over Cu, while significantly inhibiting hydrogenation of the ketone group. This behavior opened routes toward increased production rates of PHAH=O (a partially hydrogenated form of HAH containing a C=O bond), a product in which the diene groups of the furan rings were not hydrogenated. Addition of water also allowed increased feed concentrations of HAH that were previously not possible in pure IPA solvents.

09 BIOMASS FUELS↗

First principles modeling of polymer encapsulant degradation in Si photovoltaic modules

An outstanding issue in the longevity of photovoltaic (PV) modules is the accelerated degradation caused by the presence of moisture. Moisture leads to interfacial instability, de-adhesion, encapsulant decomposition, and contact corrosion. However, experimental characterization of moisture in PV modules is not trivial and its impacts can take years or decades to establish in the field, presenting a major obstacle to designing high-reliability modules. First principles calculations provide an alternative way to study the ingress of water and its detrimental effect on the structure and decomposition of the polymer encapsulant and interfaces between the encapsulant and the semiconductor, the metal contacts, or the dielectric layer. Here, we use density functional theory (DFT) computations to model single chain, crystalline and cross-linked structures, infrared (IR) signatures, and degradation mechanisms of ethylene vinyl acetate (EVA), the most common polymer encapsulant used in Si PV modules. IR-active modes computed for low energy EVA structures and possible decomposition products match well with reported experiments. The EVA decomposition energy barriers computed using the Nudged Elastic Band (NEB) method show a preference for acetic acid formation as compared to acetaldehyde, are lowered in the presence of a water solvent or hydroxyl ion catalyst, and match well with reported experimental activation energies. This systematic study leads to a clear picture of the hydrolysis-driven decomposition of EVA in terms of energetically favorable mechanisms, possible intermediate structures, and IR signatures of reactants and products.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High-Throughput Characterization and Optimization of Polyamide Hydrolase Activity Using Open Port Sampling Interface Mass Spectrometry

Enzymatic biodegradation of polymers, such as polyamides (PA), has the potential to cost-effectively reduce plastic waste, but enhancements in degradation efficiency are needed. Engineering enzymes through directed evolution is one pathway toward identification of critical domains needed for improving activity. However, screening such enzymatic libraries (100s-to-1000s of samples) is time-consuming. Here we demonstrate the use of robotic autosampler (PAL) and immediate drop on demand technology (I.DOT) liquid handling systems coupled with open-port sampling interface-mass spectrometry (OPSI-MS) to screen for PA6 and PA66 hydrolysis by 6-aminohexanoate-oligomer endo-hydrolase (nylon hydrolase, NylC) in a high-throughput (8–20 s/sample) manner. The OPSI-MS technique required minimal sample preparation and was amenable to 96-well plate formats for automated processing. Enzymatic hydrolysis of PA characteristically produced soluble linear oligomer products that could be identified by OPSI-MS. Incubation temperatures and times were optimized for PA6 (65 °C, 24 h) and PA66 (75 °C, 24 h) over 108 experiments. In addition, the I.DOT/OPSI-MS quantified production of PA6 linear dimer (8.3 ± 1.6 μg/mL) and PA66 linear monomer (13.5 ± 1.5 μg/mL) by NylC with a lower limit of detection of 0.029 and 0.032 μg/mL, respectively. For PA6 and PA66, linear oligomer production corresponded to 0.096 ± 0.018% and 0.204 ± 0.028% conversion of dry pellet mass, respectively. The developed methodology is expected to be utilized to assess enzymatic hydrolysis of engineered enzyme libraries, comprising hundreds to thousands of individual samples.

47 OTHER INSTRUMENTATION↗