Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Luminescence properties of core-shell structured SiO{sub 2}-CaMoO{sub 4}:Eu{sup 3+} phosphor

Uniform SiO{sub 2}-CaMoO{sub 4}:Eu{sup 3+} red phosphor has been synthesized by sol-gel method, and its luminescence properties have been studied by fluorescence spectrometer. The structure and morphology of the SiO{sub 2}-CaMoO{sub 4}:Eu{sup 3+} red phosphor have been investigated by transmission electron microscopy (TEM), scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS), X-ray diffraction (XRD), and FT-IR spectrometer. Results indicate that phosphor particles have a core-shell structure and the thickness of the SiO{sub 2}-shell is about 60 nm. In addition, the luminescent intensity of SiO{sub 2}-CaMoO{sub 4}:Eu{sup 3+} red phosphor has been greatly enhanced with respect to CaMoO{sub 4}:Eu{sup 3+} phosphor. But the lifetime {tau} value of SiO{sub 2}-coated CaMoO{sub 4}:Eu{sup 3+} is slightly smaller than that of non-coated CaMoO{sub 4}:Eu{sup 3+}. - Graphical abstract: A SiO{sub 2} nano-layer with thickness of 60 nm and good uniformity was successfully coated on the surface of CaMoO{sub 4}:Eu{sup 3+} phosphor. This coating greatly increases luminescent intensity of the phosphor. Highlights: Black-Right-Pointing-Pointer SiO{sub 2}-CaMoO{sub 4}:Eu{sup 3+} was successfully synthesized by sol-gel method. Black-Right-Pointing-Pointer The SiO{sub 2} nano-layer increases luminescent intensity of the phosphor. Black-Right-Pointing-Pointer The SiO{sub 2} nano-layer reduces fluorescence lifetime of the phosphor.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Synthesis and luminescent properties of spindle-like CaWO{sub 4}:Sm{sup 3+} phosphors

Graphical abstract: In this paper, spindle-like CaWO{sub 4}:Sm{sup 3+} phosphors were prepared via a polyvinylpyrrolidone (PVP)-assisted sonochemical process. Dependence of emission intensity on Sm{sup 3+} ions concentration in the CaWO{sub 4}:Sm{sup 3+} phosphor were also calculated via a nonlinear fitting by using the formula y = ax/(1 + bx{sup c}). Highlights: Black-Right-Pointing-Pointer The samples were prepared via a PVP assisted sonochemical process. Black-Right-Pointing-Pointer The color coordinates for 1 mol% Sm{sup 3+} doped CaWO{sub 4} phosphor were calculated. Black-Right-Pointing-Pointer The D-D interaction is responsible for concentration quenching between Sm{sup 3+} ions. Black-Right-Pointing-Pointer The critical energy transfer distances (R{sub c}) were obtained. -- Abstract: Spindle-like CaWO{sub 4}:Sm{sup 3+} phosphors were prepared via a Polyvinylpyrrolidone (PVP)-assisted sonochemical process, and characterized by using X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM) and photoluminescence spectroscopy (PL). The XRD results suggested that the prepared samples are single-phase. The FE-SEM images indicated that the prepared CaWO{sub 4}:Sm{sup 3+} phosphors are composed of many spindles with maximum average diameter of 150 nm and maximum average length of 500 nm. Under 404 nm excitation, the characteristic emissions corresponding to {sup 4}G{sub 5/2} {yields} {sup 6}H{sub J} (J = 5/2, 7/2, 9/2 and 11/2) transitions of Sm{sup 3+} in CaWO{sub 4} phosphors were observed. The color coordinates for 1 mol% Sm{sup 3+} doped CaWO{sub 4} phosphor were calculated to be (0.595, 0.404). The fluorescent concentration quenching of Sm{sup 3+} doped spindle-like phosphors was studied based on the Van Uitert's model, and it was found that the electric dipole-dipole (D-D) interaction is the dominant energy transfer mechanism between Sm{sup 3+} ions in the CaWO{sub 4}:Sm{sup 3+} phosphors. The critical energy transfer distance was estimated.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The imaging performance of compact Lu{sub 2}O{sub 3}:Eu powdered phosphor screens: Monte Carlo simulation for applications in mammography

In medical mammographic imaging systems, one type of detector configuration, often referred to as indirect detectors, is based on a scintillator layer (phosphor screen) that converts the x-ray radiation into optical signal. The indirect detector performance may be optimized either by improving the structural parameters of the screen or by employing new phosphor materials with improved physical characteristics (e.g., x-ray absorption efficiency, intrinsic conversion efficiency, emitted light spectrum). Lu{sub 2}O{sub 3}:Eu is a relatively new phosphor material that exhibits improved scintillating properties indicating a promising material for mammographic applications. In this article, a custom validated Monte Carlo program was used in order to examine the performance of compact Lu{sub 2}O{sub 3}:Eu powdered phosphor screens under diagnostic mammography conditions (x-ray spectra: 28 kV Mo, 0.030 mm Mo and 32 kV W, 0.050 mm Rh). Lu{sub 2}O{sub 3}:Eu screens of coating weight in the range between 20 and 40 mg/cm{sup 2} were examined. The Monte Carlo code was based on a model using Mie-scattering theory for the description of light propagation within the phosphor. The overall performance of Lu{sub 2}O{sub 3}:Eu powdered phosphor screens was investigated in terms of the (i) quantum detection efficiency, (ii) luminescence efficiency, (iii) compatibility with optical sensors, (iv) modulation transfer function, (v) the Swank factor, and (vi) zero-frequency detective quantum efficiency. Results were compared to the traditional rare-earth Gd{sub 2}O{sub 2}S:Tb phosphor material. The increased packing density and therefore the light extinction properties of Lu{sub 2}O{sub 3}:Eu phosphor were found to improve the x-ray absorption (approximately up to 21% and 16% at 40 mg/cm{sup 2} for Mo and W x-ray spectra, respectively), the spatial resolution (approximately 2.6 and 2.4 cycles/mm at 40 mg/cm{sup 2} for Mo and W x-ray spectra, respectively), as well as the zero-frequency detective quantum efficiency (approximately up to 8% and 18% at 20 mg/cm{sup 2} for Mo and W x-ray spectra, respectively) of the screens in comparison to the Gd{sub 2}O{sub 2}S:Tb screens. Data obtained by the simulations indicate that certain optical properties of Lu{sub 2}O{sub 3}:Eu make this material a promising phosphor which, under appropriate conditions, could be considered for use in x-ray mammography imagers.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

High-Temperature Sprayable Phosphor Coating Developed for Measuring Surface Temperatures

The use of phosphor thermography for noncontact temperature measurements in harsh environments has been proven over the last decade, but it has suffered from difficult application procedures such as vapor deposition or sputtering techniques. We have developed a high-temperature-sensitive paint that is easily applied with commercially available paint-spraying equipment and have successfully demonstrated it to temperatures up to 1500 C. Selected phosphors have also shown measurable signals to 1700 C, thus allowing a combination of phosphors to be used in high-temperature binders to make surface temperature measurements from ambient to over 1500 C. Phosphor thermography is an optical technique that measures the time response of fluorescence light, which is a function of the phosphor temperature. The phosphors are excited with short wavelength light (ultraviolet or blue), and they emit light at a longer wavelength. This technique has a benefit over other temperature measurements, such as thermocouples and infrared thermography, in difficult environments such as high blackbody backgrounds, vibration, flames, high electromagnetic noise, or where special windows may be needed. In addition, the sprayable phosphor paints easily cover large or complicated structures, providing full-surface information with a single measurement. Oak Ridge National Laboratories developed and tested the high-temperature binders and phosphors under the direction of the NASA Glenn Research Center. Refractory materials doped with rare earth metals were selected for their performance at high temperature. Survivability, adhesion, and material compatibility tests were conducted at high temperatures in a small furnace while the fluorescent response from the phosphors was being measured. A painted sample in a furnace with a clearly visible fluorescing dot excited by a pulsed laser is shown. Measuring the decay time of this fluorescence yields the surface temperature. One new paint was recently tested in a rocket test stand at Glenn. The floor of a square duct nozzle was painted, and full-field lifetime decay measurements were acquired for multiple firings of the rocket. Good agreement with predicted results was obtained, matching temperature gradients along the length of the nozzle and clearly showing shock structures. These good results were very satisfactory given that the measurements were made looking through the combustion plume. Infrared pyrometry was incapable of making the surface measurements because of the interference from the rocket exhaust, which contaminated the infrared signature.

Bencic, Timothy J.↗

Synthesis of high efficient Ca{sub 2}SiO{sub 4}:Eu{sup 2+} green emitting phosphor by a liquid phase precursor method

Green emitting Eu{sup 2+}-doped Ca{sub 2}SiO{sub 4} phosphors were synthesized by three different methods (a conventional solid state reaction (SSR) method, a novel liquid phase precursor approach using SiO{sub 2} sol (LPP-SiO{sub 2}(sol)) and water-soluble silicon compound (LPP-WSS)). The obtained phosphors exhibited a broad excitation spectrum ranging from 225 to 450 nm and a strong green emission peak at 502 nm due to the 4f{sup 6}5d{sup 1}{yields}4f{sup 7}({sup 8}S{sub 7/2}) transition of Eu{sup 2+}. The highest luminescent intensity was obtained for the samples fired at 1100 Degree-Sign C. The dependence of luminescence properties on Eu{sup 2+} concentration for the phosphors synthesized using LPP-WSS method was also examined from 0.1 to 5.0 mol% and the maximum emission intensity was observed at 3.0 mol% Eu{sup 2+}. A detailed analysis using various characterizations revealed that phosphors produced by the LPP-WSS process exhibited more homogenous phase distribution and higher luminescence intensity than those from the other two processes, which suggested the potential application of Ca{sub 2}SiO{sub 4}:Eu{sup 2+} in white light-emitting diodes and fluorescence lamps. - Graphical abstract: The synthesis of Eu{sup 2+} doped Ca{sub 2}SiO{sub 4} green emitting phosphors were carried out using LPP-SiO{sub 2}(sol), LPP-WSS and SSR methods. The adequate reaction of starting materials base on solution mixing and cellulose impregnating during LPP-WSS procedure resulted in single crystalline structure as well as fine morphology, and finally determined a superior luminescent intensity. Highlights: Black-Right-Pointing-Pointer Ca{sub 2}SiO{sub 4}:Eu{sup 2+} phosphor was synthesized by three methods (SSR, LPP-SiO{sub 2} and LPP-WSS). Black-Right-Pointing-Pointer Effect of different processes on the property of phosphor was studied. Black-Right-Pointing-Pointer Phosphor produced by LPP-WSS showed better homogenous phase and fluorescent property. Black-Right-Pointing-Pointer LPP-WSS approach was identified as the best method among these three approaches.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Crystal structure and luminescence properties of a novel red-emitting phosphor BaAlBO{sub 3}F{sub 2}:Eu{sup 3+}

A series of novel red-emitting phosphors BaAlBO{sub 3}F{sub 2}:xEu{sup 3+} (0.001≤x≤0.08) were first synthesized via a high temperature solid-state reaction. X-ray diffraction and photoluminescence spectroscopy were used to characterize the crystal structure and photoluminescence properties of the phosphor, respectively. The phosphor can be effectively excited with a 395 nm light, and shows a dominant {sup 5}D{sub 0}−{sup 7}F{sub 2} emission with chromatic coordination of 0.628 and 0.372. The optimal doping concentration is about 0.04. Rietveld refinement results and the luminescence behavior of Eu{sup 3+} indicate that the Eu{sup 3+} ion occupies a C{sub 3} symmetry site, and the host BaAlBO{sub 3}F{sub 2} has a hexagonal structure with P-6 space group. In addition, the phosphor could be a potential candidate as red-emitting phosphor for application in white light-emitting diode. - Graphical abstract: The luminescence behavior and Rietveld refinement of BaAlBO{sub 3}F{sub 2}:Eu{sup 3+} indicate that the red-emitting phosphor has potential application in white LED and the host has a hexagonal structure with P-6 space group. - Highlights: • A novel red-emitting phosphor BaAlBO{sub 3}F{sub 2}:Eu{sup 3+} is first synthesized. • The crystal structure of BaAlBO{sub 3}F{sub 2} is confirmed. • The phosphor shows potential application in white LED.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Crystal structure, thermally stability and photoluminescence properties of novel Sr{sub 10}(PO{sub 4}){sub 6}O:Eu{sup 2+} phosphors

A series of novel luminescent phosphors Sr{sub 10}(PO{sub 4}){sub 6}O:Eu{sup 2+} with apatite structure were synthesized via a high temperature solid-state reaction. The phase structure, photoluminescence (PL) properties, the PL thermal stability, as well as the fluorescence decay curves of the samples were investigated to characterize the resulting samples, and the selected Sr{sub 9.97}(PO{sub 4}){sub 6}O:0.03Eu{sup 2+} phosphor exhibits strong thermal quenching resistance, retaining the luminance of 88.73% at 150 °C. The quenching concentration of Eu{sup 2+} in Sr{sub 10}(PO{sub 4}){sub 6}O was about 0.03 attributing to the dipole–quadrupole interaction. The Sr{sub 10}(PO{sub 4}){sub 6}O:Eu{sup 2+} phosphor exhibited a broad-band blue emission at 439 nm upon excitation at 346 nm. The results indicate that Sr{sub 10}(PO{sub 4}){sub 6}O:Eu{sup 2+} phosphors have potential applications as near UV-convertible phosphors for white-light UV LEDs. - Graphical abstract: Sr{sub 10}(PO{sub 4}){sub 6}O:Eu{sup 2+} phosphors have potential applications as near UV-convertible phosphors for white-light UV LEDs. - Highlights: • Sr{sub 9.97}(PO{sub 4}){sub 6}O:0.03Eu{sup 2+} phosphor exhibits strong thermal quenching resistance. • Two different Eu{sup 2+} emission centers exists in Sr{sub 10}(PO{sub 4}){sub 6}O. • The activation energy was also estimated for the Eu{sup 2+} luminescence center.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Photoluminescence properties of a new orange–red emitting Sm{sup 3+}-doped Y{sub 2}Mo{sub 4}O{sub 15} phosphor

A series of novel Y{sub 2}Mo{sub 4}O{sub 15}:xSm{sup 3+} ( (0.01 ≤ x ≤ 0.20) phosphors for white light-emitting (W-LEDs) were successfully prepared by the solid state reaction technology at 973 K for 12 h. X-ray diffraction and photoluminescence spectra were utilized to characterize the structure and luminescence properties of the as-synthesized phosphors. The emission spectra of the Y{sub 2}Mo{sub 4}O{sub 15}:Sm{sup 3+} phosphors consisted of some sharp emission peaks of Sm{sup 3+} ions centered at 565 nm, 605 nm, 650 nm, and 712 nm. The strongest one is located at 605 nm due to {sup 4}G{sub 5/2}–{sup 6}H{sub 7/2} transition of Sm{sup 3+}, generating bright orange–red light. The optimum dopant concentration of Sm{sup 3+} ions in Y{sub 2}Mo{sub 4}O{sub 15}:xSm{sup 3+} is around 5 mol% and the critical transfer distance of Sm{sup 3+} is calculated as 23.32 Å. The CIE chromaticity coordinates of the Y{sub 2}Mo{sub 4}O{sub 15}:0.05Sm{sup 3+} phosphors were located in the orange reddish region. The Y{sub 2}Mo{sub 4}O{sub 15}:Sm{sup 3+} phosphors may be potentially used as red phosphors for white light-emitting diodes. - Graphical abstract: The excitation spectrum of Y{sub 2}Mo{sub 4}O{sub 15}:Sm{sup 3+} is composed of a broad band and some sharp f–f transitions. Under 407 nm excitation, the phosphor presents some sharp emission peaks of Sm{sup 3+} ions. - Highlights: • An orange–red emitting Y{sub 2}Mo{sub 4}O{sub 15}:Sm{sup 3+} phosphor has been firstly synthesized. • Their structures, luminescent properties have also been investigated. • The optical absorption edge for the molybdate lies around 325 nm. • The CIE chromaticity coordinates were located in the orange reddish region.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The charge transfer transition phenomenon and microstructure of Eu{sup 3+}-doped NaCaPO{sub 4} phosphors sintered with NH{sub 4}Cl flux via solid-state reaction

Graphical abstract: This paper describes: The charge transfer transition phenomenon and microstructure of Eu{sup 3+}-doped NaCaPO{sub 4} phosphors sintered with NH{sub 4}Cl flux via solid-state reaction. The emission intensity of NaCa{sub 0.95}PO{sub 4}:0.05Eu{sup 3+} phosphors with 2 wt.% NH{sub 4}Cl flux is enhanced as the sintering temperature was increased from 800 °C to 1000 °C and reveals the maximum value at 1000 °C. Photoluminescence emission spectra of NaCa{sub 0.95}PO{sub 4}:0.05Eu{sup 3+} phosphors with 2 wt.% NH{sub 4}Cl flux sintered at various sintering temperature for 3 h via solid state reaction method (λ{sub ex} = 270 nm). Highlights: ► NH{sub 4}Cl flux is helpful for enhancing the crystallization degree and decreasing surface defects. ► A single phase of NaCaPO{sub 4}:Eu{sup 3+} phosphor was observed as the sintering temperature was increased from 800 °C to 1000 °C. ► The intensity of the excitation peaks displays a maximum value at 1000 °C. ► The NaCaPO{sub 4} host added with NH{sub 4}Cl flux and sintered at the different temperature can affect the morphology. ► The NaCaPO{sub 4} host added with NH{sub 4}Cl flux and sintered at the different temperature can affect fluorescent properties. - Abstract: NaCa{sub 0.95}PO{sub 4}:0.05Eu{sup 3+} phosphors with 2 wt.% NH{sub 4}Cl flux sintered at various sintering temperature (800, 900, 1000, 1100 °C) for 3 h under air atmosphere were synthesized successfully via solid state reaction method. It is found that the addition of NH{sub 4}Cl flux and different sintering temperatures can affect the morphology and fluorescent properties of NaCa{sub 0.95}PO{sub 4}:0.05Eu{sup 3+} phosphor. The X-ray diffractions show a single phase and the microstructure observations show uniform morphologies for NaCa{sub 0.95}PO{sub 4}:0.05Eu{sup 3+} phosphors sintered at the range from 900 °C to 1000 °C, indicating that addition of 2 wt.% NH{sub 4}Cl flux is helpful for enhancing the crystallization, thus improving the luminescence intensity of the charge transfer transition. The intensity of the excitation peaks displayed a maximum value at 1000 °C. The chromaticity (x, y) is in the orange-red region (0.54, 0.39) and the lifetime value is about 2.1 ms, suitable for the remote phosphor packages.

36 MATERIALS SCIENCE↗

The effects of re-firing process under oxidizing atmosphere and temperatures on the properties of strontium aluminate phosphors

Graphical abstract: The comparative emission spectra of standard and re-fired Phosphor A under oxidizing atmosphere at various temperatures. The colour of Phosphor A re-fired at higher temperatures above 900 °C shifted from yellowish-green to bluish-green in the dark. But, the bluish-green emission could only be seen when it was exposed to UV and disappeared as soon as the light source was removed. Moreover, the emission intensities decreased as the re-firing temperatures increased. This could be attributed to the oxidation of Eu{sup 2+} during the re-firing process. It is well known fact from the literature that the reduction of Eu{sup 3+} to Eu{sup 2+} in appropriate host materials needs an annealing process in a reducing atmosphere such as H{sub 2}, H{sub 2}/N{sub 2} mixture or CO. Up to now, the reduction phenomena of Eu{sup 3+} → Eu{sup 2+} in air have been found in phosphates (Ba{sub 3}(PO{sub 4}){sub 2}:Eu), sulphates (BaSO{sub 4}:Eu), borates (SrB{sub 4}O{sub 7}:Eu, SrB{sub 6}O{sub 10}:Eu and BaB{sub 8}O{sub 13}:Eu) and aluminates (Sr{sub 4}Al{sub 14}O{sub 25}:Eu). Interestingly, an apparent blue shift in the phosphorescence spectrum was observed in the samples re-fired at 1000 °C and above, indicating a minimal effect on the oxidation state or the electronic energy levels of the co-doped Dy{sup 3+} ions, which were thought to act as long-lived hole traps resulting in long afterglow. - Highlights: • This study examines the effects re-firing at oxidizing atmosphere of photoluminescence of three different commercial SrAl{sub 2}O{sub 4}:Eu{sup 2+},Dy{sup 3+}-phosphors. • All the commercial SrAl{sub 2}O{sub 4}:Eu{sup 2+},Dy{sup 3+}-phosphors completely lost their phosphorescence after being re-fired at 1300 °C. • Oxidizing environment and re-firing temperature naturally affecting the valance of Eu{sup 2+} may cause the basic lattice structure to be modified and also limit their applications at higher temperatures, such as third firing vetrosa décor or glaze applications in ceramic industry. • It was thought that this kind of study may be promising to provide many outcome studies, may act to encourage additional efforts along these lines. - Abstract: Inorganic phosphorescent pigments have a very wide application, consisting of ceramic decoration and glazes. Therefore, in the present study 3 different commercially available strontium aluminate phosphors (coded Phosphor A, B and C) emitting yellowish-green light were investigated to determine their behaviour when re-fired under oxidizing atmosphere. The phosphors were re-fired at 10 different temperatures and consequent effects were studied. All the samples were characterized by X-ray fluorescence (XRF), X-ray diffraction (XRD), laser particle size, scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDX) and fluorescence spectrometer analysis. It was found that firing them under oxidizing atmosphere strongly affected their phosphorescence abilities especially over 800–900 °C, because doped europium ions (Eu{sup 2+}) in their structures are oxidized to Eu{sup 3+}. It was also concluded that the phosphor powders clumped as the temperature rose, leading to their particle size distributions to change.

36 MATERIALS SCIENCE↗

Sol–gel synthesis, structure and luminescence properties of Ba{sub 2}ZnMoO{sub 6}:Eu{sup 3+} phosphors

Graphical abstract: The phosphor powders of Ba{sub 2}ZnMoO{sub 6}:Eu{sup 3+} were prepared by sol–gel method. The dependence of luminescence intensity on the Eu{sup 3+} concentration was investigated. - Highlights: • We synthesize Ba{sub 2}ZnMoO{sub 6}:Eu{sup 3+} phosphors by the sol–gel method. • The effect of temperature on the crystallinity and morphology is investigated. • The phosphor presents an intense CT band in near UV range (370–410 nm). • The concentration quenching mechanism is the exchange interaction. - Abstract: Double-perovskite Ba{sub 2}Zn{sub 1−x}MoO{sub 6}:xEu{sup 3+} (x = 0, 0.02, 0.04, 0.06, 0.08, 0.1) orange–red emitting phosphors were synthesized by using the sol–gel method. The crystalline structure and photoluminescence properties of the phosphors were investigated. The X-ray diffraction (XRD) patterns indicate that the structure of matrix Ba{sub 2}ZnMoO{sub 6} is cubic double-perovskite with space group Fm-3m. The Ba{sub 2}ZnMoO{sub 6}:Eu{sup 3+} phosphors present an intense broad charge transfer (CT) band absorption in near UV range (370–410 nm), which attributes to the charge transfer state of MoO{sub 6}, and performs orange–red emission of Eu{sup 3+} ({sup 5}D{sub 0} → {sup 7}F{sub 1} transition) at around 596 nm. A low concentration quenching occurs in Ba{sub 2}ZnMoO{sub 6}:Eu{sup 3+} and the optimal doping concentration is about 6 mol%. The Ba{sub 2}ZnMoO{sub 6}:Eu{sup 3+} phosphors are considered to be a promising orange–red emitting phosphor for near ultraviolet GaN-based white light emitting diode.

36 MATERIALS SCIENCE↗

Photoluminescence and cathodoluminescence properties of Eu{sup 3+} ions activated AMoO{sub 4} (A = Mg, Ca, Sr, Ba) phosphors

Highlights: • Under 393 nm excitation, strong red emission located at 615 nm was observed in all the samples. • The Eu{sup 3+}-activated CaMoO{sub 4} phosphor exhibited the strongest PL properties. • The CIE chromaticity coordinate of Eu{sup 3+}-activated CaMoO{sub 4} phosphor was (0.647,0.352). • The color purity of Eu{sup 3+}-activated CaMoO{sub 4} phosphor was 92.8%. • Strong CL properties were observed in the Eu{sup 3+}-activated CaMoO{sub 4} phosphor. - Abstract: Eu{sup 3+}-activated AMoO{sub 4} (A = Mg, Ca, Sr, Ba) phosphors were synthesized by a solid-state reaction method. Photoluminescence and cathodoluminescence (CL) spectra as well as X-ray diffraction patterns were measured to characterize the fabricated samples. Under 393 nm excitation, strong red emissions located at ∼615 nm corresponding to the {sup 5}D{sub 0} → {sup 7}F{sub 2} transition of Eu{sup 3+} ions were observed in all the samples. Compared with other Eu{sup 3+} ions activated AMoO{sub 4} (A = Mg, Sr, Ba) phosphors, Eu{sup 3+}-activated CaMoO{sub 4} phosphor exhibited the strongest red emission intensity with better Commission Internationale de L’Eclairage chromaticity coordinate and higher color purity. Furthermore, the CL results indicated that the Eu{sup 3+}-activated CaMoO{sub 4} phosphor had excellent luminescence properties.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

White light emission and effect of annealing on the Ho{sup 3+}–Yb{sup 3+} codoped BaCa{sub 2}Al{sub 8}O{sub 15} phosphor

Graphical abstract: The upconversion emission spectra of the Ho{sup 3+}/Yb{sup 3+} doped/codoped BaCa{sub 2}Al{sub 8}O{sub 15} phosphors with different doping concentrations of Ho{sup 3+}/Yb{sup 3+} ions along with UC emission spectrum of the white light emitting phosphor annealed at 800 °C. - Highlights: • BaCa{sub 2}Al{sub 8}O{sub 15} phosphors codoped with Ho{sup 3+}–Yb{sup 3+} have been prepared by combustion method. • Phosphor annealed at 800 °C, illuminate an intense white light upon NIR excitation. • The sample annealed at higher temperatures emits in the pure green region. • The colour emitted persists in the white region even at high pump power density. • Developed phosphor is suitable for making upconverters and WLEDs. - Abstract: The BaCa{sub 2}Al{sub 8}O{sub 15} (BCAO) phosphors codoped with suitable Ho{sup 3+}–Yb{sup 3+} dopant concentration prepared by combustion method illuminate an intense white light upon near infrared diode laser excitation. The structural analysis of the phosphors and the detection of impurity contents have been performed by using the X-Ray Diffraction, FESEM and FTIR analysis. The purity of white light emitted from the sample has been confirmed by the CIE chromaticity diagram. Also, the white light emitted from the sample persists with the variation of pump power density. The phosphors emit upconversion (UC) emission bands in the blue, green and red region (three primary colours required for white light emission) along with one more band in the near infrared region of the electromagnetic spectrum. On annealing the white light emitting sample at higher temperatures, the sample starts to emit green colour and also the intensity of green and red UC emission bands get enhanced largely.

36 MATERIALS SCIENCE↗

Enhancing luminescence of Lu{sub 2}MoO{sub 6}:Eu{sup 3+} phosphors by doping with Li{sup +} ions for near ultraviolet based solid state lighting

Graphical abstract: The emission spectra of Lu{sub 2}MoO{sub 6}:3%Eu{sup 3+}, x%Li{sup +} phosphors under 365 nm excitation. The inset represents emission intensity of 610 nm as a function of Li{sup +} molar concentration. - Highlights: • Lu{sub 2}MoO{sub 6}:3%Eu{sup 3+}, x%Li{sup +} phosphors were synthesized by solid-state reaction method. • All the prepared phosphors can be assigned to its monoclinic phase. • The optimal concentration of Li{sup +} ions is 30mol%. • The luminescent intensity of Lu{sub 2}MoO{sub 6}:Eu{sup 3+} phosphors has been greatly enhanced by codoping Li{sup +} ions. - Abstract: Lu{sub 2}MoO{sub 6}: 3% Eu{sup 3+} co-doped with x% Li{sup +} (x = 0–40 mol) phosphors were synthesized by high-temperature solid-state reaction method. The structure and luminescent properties of these phosphors were investigated. The X-ray diffraction (XRD) results show that all prepared phosphors can be assigned to monoclinic phase and codoping with Li{sup +} ions does not change their crystallographic structure. The excitation and emission spectra show that the samples can be effectively excited by the near ultraviolet light at 365 nm and exhibit strong red emission centered at 610 nm. The experimental results indicate the red luminescent intensity of Lu{sub 2}MoO{sub 6}:Eu{sup 3+} phosphors has been greatly enhanced by codoping with Li{sup +} ions. The enhancement of the luminescent intensity can be the consequence of the modification of the local field symmetry around the Eu{sup 3+} ion, improved crystallization, and the enlarged grain size induced by the Li{sup +} ions.

36 MATERIALS SCIENCE↗

Luminescent properties and energy transfer studies of color-tunable LuBO{sub 3}: Ce{sup 3+}/Tb{sup 3+}/Eu{sup 3+} phosphors

Highlights: • A series of color-tunable LuBO{sub 3}: Ce{sup 3+}/Tb{sup 3+}/Eu{sup 3+} phosphors were synthesized. • Phosphors exhibit strong blue/green/red emission under UV excitation. • The reason of high Tb{sup 3+} content required for Ce{sup 3+} → Tb{sup 3+} → Eu{sup 3+} energy transfer is unveiled. • Green and red LED prototypes were fabricated and characterized. - Abstract: A series of LuBO{sub 3}: Ce{sup 3+}/Tb{sup 3+}/Eu{sup 3+} phosphors were synthesized via solid state reaction. The Ce{sup 3+}/Tb{sup 3+} co-doped and Ce{sup 3+}/Tb{sup 3+}/Eu{sup 3+} tri-doped phosphors absorb near UV light through 4f-5d transitions of Ce{sup 3+}, followed by sensitized Tb{sup 3+} green and Eu{sup 3+} red emission. Decay curves investigations for samples with various Tb{sup 3+} and Eu{sup 3+} contents reveal the occurrence of Ce{sup 3+} → Tb{sup 3+} → Eu{sup 3+} energy transfer. It is found that due to relative low Tb{sup 3+} → Eu{sup 3+} energy transfer rate, a high Tb{sup 3+} content (>40%) is required for efficient Ce{sup 3+} → Tb{sup 3+} → Eu{sup 3+} energy transfer. Emission color of LuBO{sub 3}: Ce{sup 3+}, Tb{sup 3+}, Eu{sup 3+} varies from blue through green to red with Ce{sup 3+}/Tb{sup 3+}/Eu{sup 3+} ratio. The quantum efficiency of LuBO{sub 3}: Ce{sup 3+}, Tb{sup 3+} green phosphor and LuBO{sub 3}: Ce{sup 3+}, Tb{sup 3+}, Eu{sup 3+} red phosphor is 50% and 30%, respectively. Green and red LED prototypes were fabricated. The results show that the obtained phosphors are potential candidates as down-converted phosphors for NUV LEDs.

36 MATERIALS SCIENCE↗

The GdF3 phosphors with enhanced multicolor luminescence via multi-channel excitation and energy migration procedure

Highlights: • Core-shell structured GdF{sub 3} phosphors were synthesized by hydrothermal method. • SiO{sub 2} coating layers prevent aggregation and sintering during thermal annealing. • The annealed CSS nanophosphors were highly dispersible. • The inserted PMA significantly enhances multicolor luminescence. • The annealed CSS phosphors exhibit enhanced multicolor luminescence properties. - Abstract: A collection of GdF{sub 3} core-shell structured (CSS) phosphors were synthesized by hydrothermal method. The as-prepared (AP) phosphors were coated with SiO{sub 2} layers to avoid aggregation and sintering during thermal annealing at 800 °C, after which the SiO{sub 2} layers were etched off and the annealed phosphors became highly dispersible. The annealed CSS phosphor aGdF{sub 3}:Eu{sup 3+}@GdF{sub 3}:Ce{sup 3+},Dy{sup 3+} shows excellent multicolor luminescence performance with the aid of dual-channel excitation and energy migration (EM) procedure of Gd{sup 3+} ions. By inserting pyromellitic acid (PMA) organic ligands into the interfaces between annealed core and AP shell layer regions, the so-called antenna effect of organic ligands of PMA forms a new excitation channel, which makes the CSS phosphor aGdF{sub 3}:Eu{sup 3+}@PMA@GdF{sub 3}:Ce{sup 3+},Dy{sup 3+} exhibit significantly enhanced multicolor luminescence via multi-channel excitation and EM process. The prepared CSS phosphors in this work are excellent candidates for applications in solid-state lighting.

36 MATERIALS SCIENCE↗

Visible emission spectra of thermographic phosphors under x-ray excitation

Thermographic phosphors have been employed for temperature sensing in challenging environments, such as on surfaces or within solid samples exposed to dynamic heating, because of the high temporal and spatial resolution that can be achieved using this approach. Typically, UV light sources are employed to induce temperature-sensitive spectral responses from the phosphors. However, it would be beneficial to explore x-rays as an alternate excitation source to facilitate simultaneous x-ray imaging of material deformation and temperature of heated samples and to reduce UV absorption within solid samples being investigated. Here, the phosphors BaMgAl 10 O 17 :Eu (BAM), Y 2 SiO 5 :Ce, YAG:Dy, La 2 O 2 S:Eu, ZnGa 2 O 4 :Mn, Mg 3 F 2 GeO 4 :Mn, Gd 2 O 2 S:Tb, and ZnO were excited using incident synchrotron x-ray radiation. These materials were chosen to include conventional thermographic phosphors as well as x-ray scintillators (with crossover between these two categories). X-ray-induced thermographic behavior was explored through the measurement of visible spectral response with varying temperature. The incident x-rays were observed to excite the same electronic energy level transitions in these phosphors as UV excitation. Similar shifts in the spectral response of BAM, Y 2 SiO 5 :Ce, YAG:Dy, La 2 O 2 S:Eu, ZnGa 2 O 4 :Mn, Mg 3 F 2 GeO 4 :Mn, and Gd 2 O 2 S:Tb were observed when compared to their response to UV excitation found in literature. Some phosphors were observed to thermally quench in the temperature ranges tested here, while the response from others did not rise above background noise levels. This may be attributed to the increased probability of non-radiative energy release from these phosphors due to the high energy of the incident x-rays. These results indicate that x-rays can serve as a viable excitation source for phosphor thermometry.

42 ENGINEERING↗

Narrow spectral emission CaMoO{sub 4}: Eu{sup 3+}, Dy{sup 3+}, Tb{sup 3+} phosphor crystals for white light emitting diodes

Alkaline earth metal molybdates are promising candidates as a host material for high efficiency narrow spectral emission phosphors. These phosphors could potentially be used for the fabrication of phosphor-converted light emitting diodes (pc-LEDs). Phosphor crystals of calcium molybdate doped with rare earth dopant Ln{sup 3+}(Ln=Eu, Dy, Tb) grown using flux growth method have been shown to exhibit higher excitation efficiency than the powders synthesized by solid-state reaction process. Molybdenum (VI) oxide has been found to be a suitable flux for growing large size optically transparent high quality crystals at a temperature around 1100 Degree-Sign C. Using the excitation wavelengths of 465 nm, 454 nm and 489 nm for CaMoO{sub 4}: Eu{sup 3+}, CaMoO{sub 4}: Dy{sup 3+} and CaMoO{sub 4}: Tb{sup 3+}, respectively, intense emission lines at wavelengths of 615 nm, 575 nm and 550 nm were observed. The optimized doping concentrations of 12%, 2% and 5% for Eu{sup 3+}, Dy{sup 3+} and Tb{sup 3+}, respectively, provided the highest luminescence intensity. - Graphical Abstract: CaMoO{sub 4}: Eu{sup 3+} phosphor crystals grown using a molybdenum (VI) oxide flux exhibited around 1.5 times the emission intensity of powders obtained from solid-state reaction at the same synthesis temperature. These crystals were found to efficiently emit 615 nm red light when excited by near UV light up to a wavelength of 395 nm. Highlights: Black-Right-Pointing-Pointer CaMoO{sub 4}: Ln{sup 3+} (Ln=Eu{sup 3+}, Dy{sup 3+}, Tb{sup 3+}) phosphor crystals were successfully grown using high temperature flux (solutions) containing molybdenum (VI) oxide or lithium chloride. Black-Right-Pointing-Pointer Narrow spectral emission at 615 nm, 575 nm and 550 nm, respectively, was observed from CaMoO{sub 4}: Ln{sup 3+} (Ln=Eu{sup 3+}, Dy{sup 3+}, Tb{sup 3+}) phosphor crystals. Black-Right-Pointing-Pointer The optimized doping concentrations of Eu{sup 3+}, Dy{sup 3+}, Tb{sup 3+} in CaMoO{sub 4} for highest emission intensity were determined to be 12%, 2% and 5%, respectively. Black-Right-Pointing-Pointer The CaMoO{sub 4}: Ln{sup 3+} (Ln=Eu{sup 3+}, Dy{sup 3+}, Tb{sup 3+}) phosphor crystals grown with molybdenum (VI) oxide flux exhibited 50% higher emission intensity compared to the crystals grown with lithium chloride flux and the powders synthesized by solid-state reaction.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗