Study of Chromium-Frit-Type Coatings for High-Temperature Protection of Molybdenum

The achievement of more compact and efficient power plants for aircraft is dependent, among other factors, on the perfection of heat-resisting materials that are superior to those in current use. Molybdenum is one of the high-melting metals (melting point, 4750 F). It is fairly abundant and also can be worked into many of the shapes required in modern power plants. To permit its widespread use at elevated temperatures, however, some means must first be found to prevent its rapid oxidation. The application of a protective coating is one method that might be used to achieve this goal. In the present work, a number of chromium-frit-type coatings were studied. These were bonded to molybdenum specimens by firing in controlled atmospheres to temperatures in the range of 2400 to 2700 F.

CERAMICS↗

Methods for the Identification of Aircraft Tubing of Plain Carbon Steel and Chromium-Molybdenum Steel

The survey of the possibilities for distinguishing between plain carbon and chromium-molybdenum steel tubing included the Herbert pendulum hardness, magnetic, sparks, and chemical tests. The Herbert pendulum test has the disadvantages of all hardness tests in being limited to factory use and being applicable only to scale-free, normalized material. The small difference in the range of hardness values between plain carbon and chromium-molybdenum steels is likewise a disadvantage. The Rockwell hardness test, at present used in the industry for this purpose, is much more reliable. It may be concluded on the basis of the experiments performed that of all methods surveyed, spark testing appears to be, at present, the most suitable for factory use from the standpoint of speed, accuracy, nondestructiveness and reliability. It is also applicable for field use.

Mutchler, W H↗

Rapid chemical test for the identification of chromium-molybdenum steel

This note describes a simple, rapid, qualitative test which can be applied to solutions of drilling or chips for the identification of chromium-molybdenum steel. The test is based on the orange-red compound which is formed when thiocyanate and inequivalent molybdenum react. This test is much more reliable than the potassium ethylxanthate test which has been recommended for a like purpose. A list of the apparatus and reagents which are required, and a description of the procedure follows.

Redmond, John C↗

Effect of Prestraining of Recrystallization Temperature and Mechanical Properties of Commercial, Sintered, Wrought Molybdenum

Given three presumably identical lots of commercial, sintered, wrought molybdenum, the 1-hour recrystallization temperature of one lot remained above 2900 F by limiting the amount of effective restraining to 35 percent or less. Different recrystallization temperatures were obtained in various atmospheres, the highest in argon and the lowest in hydrogen. Metal thus fabricated and then stress-relieved possessed an ultimate tensile strength at room temperature within 10 percent of metal swaged 99 percent and also possessed equivalent ductility. At 1800 F, equivalent strength and ductility was obtained irrespective of the amount of swaging over the range of 10 to 99 percent. The amount of swaging greatly influenced the recrystallized grain size but the difference in grain size is not the major controlling factor which determines whether recrystallized molybdenum is ductile or brittle at room temperature.

MATERIALS, PROPERTIES - TENSILE↗

Oxidation-resistance Mechanism and Other Properties of Molybdenum Disilicide

The outstanding oxidation resistance of molybdenum disilicide at 2400 F and above was found to depend on the formation of a protective siliceous coating which a-cristobalie has been identified. Molybdenum disilicide is not inherently resistant to oxidation and in powdered form burns at low temperatures.Melting and casting experiments have demonstrated the decomposition of the material at the melting point. The room-temperature modulus of elasticity has been determined and electric-resistivity data are given to 2000 F.

MATERIALS, PROPERTIES-CORROSION RESISTANCE↗

Reactive melt infiltration of silicon-molybdenum alloys into microporous carbon preforms

Investigations on the reactive melt infiltration of silicon-1.7 and 3.2 at.% molybdenum alloys into microporous carbon preforms have been carried out by modeling, differential thermal analysis (DTA), and melt infiltration experiments. These results indicate that the pore volume fraction of the carbon preform is a very important parameter in determining the final composition of the reaction-formed silicon carbide and the secondary phases. Various undesirable melt infiltration results, e.g. choking-off, specimen cracking, silicon veins, and lake formation, and their correlation with inadequate preform properties are presented. The liquid silicon-carbon reaction exotherm temperatures are influenced by the pore and carbon particle size of the preform and the compositions of infiltrants. Room temperature flexural strength and fracture toughness of materials made by the silicon-3.2 at.% molybdenum alloy infiltration of medium pore size preforms are also discussed.

Singh, M.↗

Investigation of Problems Associated with the Use of Alloyed Molybdenum Sheet in Structures at Elevated Temperatures

The results of an experimental study to explore the capabilities and limitations of thin Mo-0.5Ti molybdenum-alloy sheet for structural applications at high temperatures are presented. Evaluation tests at temperatures ranging from room temperature,to 3000 F were made on resistance-welded corrugated-core sandwiches that were coated with a commercially available oxidation resistant coating known as W-2 and on coated oxidation and tensile specimens. The performance of the corrugated-core sandwiches in compressive strength and static oxidation tests, tensile properties of the coated molybdenum sheet, and the life of the coated specimens in static oxidation tests are given. A description of the equipment and procedures utilized in performing the evaluation tests is included.

Mathauser, Eldon E.↗

Investigation of Oxidation-Resistant Coatings on Graphite and Molybdenum in Two Arc-Powered Facilities

A number of leading-edge specimens of ATJ graphite and 0.5-percent titanium-molybdenum alloy were tested in a 6-inch subsonic low-pressure arc-powered tunnel and a 1,500-kw subsonic arc jet to determine the effectiveness of several refractory coatings in preventing the oxidation of these materials. The results indicate that the siliconized coating for the ATJ graphite and the W-2 and Durak MG coatings for the titanium-molybdenum alloy provide adequate protection at temperatures up to 3,000 F for the durations of the tests in these facilities, approximately 70 seconds in the arc tunnel and approximately 10 minutes in the arc jet. Weight losses (less than one-half of 1 percent) experienced by a few of the coated specimens indicate that tests of longer duration in these environments may prove deleterious and that the stability of these coatings may be depreciated under the low-pressure environmental conditions encountered during reentry.

Peters, Roger W.↗

Electron-Beam Deposition of Superconducting Molybdenum Thin Films for the Development of Mo/Au TES X-Ray Microcalorimeter

We are exploring the properties of electron-beam evaporated molybdenum thin films on silicon nitride coated silicon wafers at substrate temperatures between room temperature and 650 C. The temperature dependence of film stress, transition temperature, and electrical properties are presented. X-ray diffraction measurements are performed to gain information on molybdenum crystallite size and growth. Results show the dominant influence of the crystallite size on the intrinsic properties of our films. Wafer-scale uniformity, wafer yield, and optimal thermal bias regime for TES fabrication are discussed.

Microcalorimeter↗